An Experimental Investigation on Low Cycle Fatigue Behavior of Alloy 617 Base Metal and Alloy 617/Alloy 617 Weld Joints (Alloy 617 모재와 용접부재의 저사이클피로 거동에 관한 실험적 고찰)

  • Choi, Pil-Ho;Kim, Seon-Jin;Kim, Woo-Gon;Kim, Min-Hwan
    • Journal of Power System Engineering
    • /
    • v.18 no.5
    • /
    • pp.115-121
    • /
    • 2014
  • Alloy 617 is the one of the leading candidate materials for intermediate heat exchangers(IHX) of a very high temperature reactor(VHTR) system. Some of the components are joined by many welding techniques and therefore the welded joints are inevitable in the construction of systems. In the present paper, the low cycle fatigue(LCF) behaviors of Alloy 617 base metal(BM) and the gas tungsten arc welded (GTAWed) weld joints(WJ) are investigated experimentally under strain controlled LCF tests. Fully axial total-strain controlled tests have been conducted at room temperature with total strain ranges of 0.6, 0.9, 1.2 and 1.5%. The weld joints have shown a lower fatigue lives compared with base metals at all the testing conditions. The weld joints have shown a higher cyclic stress response behavior than base metal. Both BM and WJ exhibited cyclic strain hardening behavior, depending on the total strain range. In addition, the strain-life parameters for BM and WJ were determined, based on Coffin-Manson equations.

Evaluation of Fatigue Life on Alloy 617 Base Metal and Alloy 617/Alloy 617 Weld Joints under Low Cycle Fatigue Loading (저사이클피로 하중하의 Alloy 617 모재와 용접부재에 대한 피로 수명 평가)

  • Dewa, Rando Tungga;Kim, Seon-Jin;Kim, Woo-Gon;Kim, Min-Hwan
    • Journal of Power System Engineering
    • /
    • v.18 no.5
    • /
    • pp.122-128
    • /
    • 2014
  • Generally, the mechanical components and structures are joined by many welding techniques, and therefore the welded joints are inevitable in the construction of structures. The Alloy 617 was initially developed for high temperature applications above $800^{\circ}C$. It is often considered for use in aircraft and gas turbines, chemical manufacturing components, and power generation structures. Especially, the Alloy 617 is the primary candidate for construction of intermediate heat exchanger (IHX) on a very high temperature reactor (VHTR) system. In the present paper, the low cycle fatigue (LCF) life of Alloy 617 base metal (BM) and the gas tungsten arc welded (GTAWed) weld joints (WJ) are evaluated by using the previous experimental results under strain controlled LCF tests. The LCF tests have been performed at room temperature with total strain ranges of 0.6, 0.9, 1.2 and 1.5%. The LCF lives for the BM and WJ have been evaluated from the Coffin-Manson and strain energy based life methods. For both the BM and WJ, the LCF lives predicted by both Coffin-Manson and strain energy based life methods was found to well coincide with the experimental data.