저항업셋 용접법을 이용한 Zr-4 End Cap용접부의 특성에 관한 연구 (A Study on the Characteristics of Zr-4 End Cap Welded Joints Using Resistance Upset Welding)

  • 박철주;김형수;이영호;강원석
    • Journal of Welding and Joining
    • /
    • 제10권4호
    • /
    • pp.240-249
    • /
    • 1992
  • The objective of this study is to investigate the characteristics of welded joints on the Zircaloy-4 resistance upset welding for HWR(Heavy Water reactor)fuel rods. To estimate the characteristics of welded joints, the various tests were performed on the test coupons systematically with a wide range of each welding parameters in terms of a tensile test, burst test, knoop hardness test and metallography. Major results obtained in this study are as follows: 1. The tube and machined with 120.deg. projection was the reliable weld joint design for the nuclear fuel rod end cap welding. 2. As the weld current and the amount of upset increased linearly with increasing welding main heat input, it could make an estimate of their variation in accordance with the phase shift control. 3. It was found that an increase in squeeze force has an effect on the upset contour of welded joint because the amount of upset were increased by the change of squeeze force.

  • PDF

대형 Tubular K-Joint의 피로수명에 관한 연구 (A Study on the Fatigue Life of Large-Scale Tubular K-joints)

  • 임성우;장인화
    • 한국해양공학회지
    • /
    • 제22권2호
    • /
    • pp.58-64
    • /
    • 2008
  • Large-scale tests of welded tubular K-joint sunder balanced in-plane bending braces were carried out to observe the fatigue behavior of the API 2W Gr.60 steel plate produced by POSCO. Toe grinding and weld profiling were used to improve the fatigue life of a tubular K-joint. The effects of the steel grade and chord wall thickness on the fatigue life were also investigated. The present results were compared with the UK DEn design curve.

차체용 1.2GPa급 초고장력 TRIP강의 Weldbond 접합부의 기계적 거동 (Mechanical Behavior of Weldbond Joint of 1.2GPa Grade Ultra High Strength TRIP Steel for Car Body Applications)

  • 이종대;이소정;방정환;김동철;강문진;김목순;김준기
    • Journal of Welding and Joining
    • /
    • 제32권5호
    • /
    • pp.44-49
    • /
    • 2014
  • The effect of weldbond hybrid joining process on the mechanical behavior of single lap and L-tensile joints was investigated for the newly developed 1.2GPa grade ultra high strength TRIP(transformation induced plasticity) steel. In the case of single lap shear behavior, the weldbond joint of 1.2GPa TRIP steel showed lower maximum tensile load and elongation than that of the adhesive bonding only. It was considered to be due to the reduction of real adhesion area, which was caused by the degradation of adhesive near the spot weld, and the brittle fracture behavior of the spot weld joint. In the case of L-tensile behavior, however, the maximum tensile load of the weldbond joint of 1.2GPa TRIP steel was dramatically increased and the fracture mode was change to the base metal fracture which is desirable for the spot weld joint. These synergic effect of the weldbond hybrid joining process in 1.2GPa TRIP steel was considered to be due to the stress dissipation around the spot weld joint by the presence of adhesive which resulted in the change of crack propagation path.

고(高) Energy밀도용접(密度熔接)에 의(依)한 용접(熔接)이음에 있어서의 잔류응력(殘留應力)과 피로특성(疲勞特性)에 관(關)한 연구(硏究) -HT80강(鋼)의 전자(電子) Beam 용접(熔接)이음 피로강도(疲勞强度)- (Study on the Residual Stress and Fatigue Strength of Welded Joint by High Energy Density Welding -Fatigue Scrength of Welded Joint of HT80 Steel by Electron Beam Welding-)

  • 박종은
    • 대한조선학회지
    • /
    • 제20권2호
    • /
    • pp.51-59
    • /
    • 1983
  • The versatile practical use of electron beam welding which is very high energy density is still in early stage, but in the special welding field, the welding process is used in manufactured goods. The investigation for electron beam welding up to the present was almost achieved not for the mechanical properties of welded joint but for the process itself. On this investigation, the fatigue strength, crack propergation phenomena and hardness of weld metal and heat affected zone of partially penetrated welded joint of HT80 steel by electron beam welding was accomplished. The tensile fatigue strength in weld line direction of the joint was about $25kg/mm^2$. There still appeared spikes on the tips of penetration, and the crack initiated at the tips of spikes not from the roots. The hardness of the weld metal was higher than it of base metal because of production of martensite by rapid cooling.

  • PDF

Axially-loaded multiplanar tubular KTX-joints: numerical analysis

  • Zhang, Chenhui;Zou, Bo;Yang, Guotao
    • Steel and Composite Structures
    • /
    • 제42권2호
    • /
    • pp.173-190
    • /
    • 2022
  • With the development of spatial structures, the joints are becoming more and more complex to connect tubular members of spatial structures. In this study, an approach is proposed to establish high-efficiency finite element model of multiplanar KTX-joint with the weld geometries accurately simulated. Ultimate bearing capacity the KTX-joint is determined by the criterion of deformation limit and failure mechanism of chord wall buckling is studied. Size effect of fillet weld on the joint ultimate bearing capacity is preliminarily investigated. Based on the validated finite element model, a parametric study is performed to investigate the effects of geometric and loading parameters of KT-plane brace members on ultimate bearing capacity of the KTX-joint. The effect mechanism is revealed and several design suggestions are proposed. Several simple reinforcement methods are adopted to constrain the chord wall buckling. It is concluded that the finite element model established by proposed approach is capable of simulating static behaviors of multiplanar KTX-joint; chord wall buckling with large indentation is the typical failure mode of multiplanar KTX-joint, which also increases chord wall displacements in the axis directions of brace members in orthogonal plane; ultimate bearing capacity of the KTX-joint increases approximately linearly with the increase of fillet weld size within the allowed range; the effect mechanism of geometric and loading parameters are revealed by the assumption of restraint region and interaction between adjacent KT-plane brace members; relatively large diameter ratio, small overlapping ratio and small included angle are suggested for the KTX-joint to achieve larger ultimate bearing capacity; the adopted simple reinforcement methods can effectively constrain the chord wall buckling with the design of KTX-joint converted into design of uniplanar KT-joint.

용접부 피로강도에 미치는 후처리의 영향 (Effect of post treatment on the fatigue strength of welded joint)

  • 윤중근;김현수;황주환;박동환
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.240-242
    • /
    • 2004
  • Effect of post treatment on the fatigue strength of a box weldment was investigated in order to improve fatigue life of the weldment. The post treatment applied were the smooth grinding of weld bead, weld toe grinding and hammer peening at the weld toe. The fatigue strength of the weldment after post treatment clearly increased, compared with that of the weldment in as-welded condition. After smooth grinding of weld bead, fatigue crack initiated at the root of the weldment, while fatigue crack initiated at the weld toe for the other methods.

  • PDF

A Study on Real-time Control of Bead Height and Joint Tracking Using Laser Vision Sensor

  • Kim, H. K.;Park, H.
    • International Journal of Korean Welding Society
    • /
    • 제4권1호
    • /
    • pp.30-37
    • /
    • 2004
  • There have been continuous efforts on automating welding processes. This automation process could be said to fall into two categories, weld seam tracking and weld quality evaluation. Recently, the attempts to achieve these two functions simultaneously are on the increase. For the study presented in this paper, a vision sensor is made, a vision system is constructed and using this, the 3 dimensional geometry of the bead is measured on-line. For the application as in welding, which is the characteristic of nonlinear process, a fuzzy controller is designed. And with this, an adaptive control system is proposed which acquires the bead height and the coordinates of the point on the bead along the horizontal fillet joint, performs seam tracking with those data, and also at the same time, controls the bead geometry to a uniform shape. A communication system, which enables the communication with the industrial robot, is designed to control the bead geometry and to track the weld seam. Experiments are made with varied offset angles from the pre-taught weld path, and they showed the adaptive system works favorable results.

  • PDF

초내열합금 IN713LC와 SCM440의 마찰용접 및 레이저용접에 대한 특성 비교 (Comparison of the weld quality of friction welding and laser welding for IN713LC and SCM440 steel)

  • 황형철;염종택;박노광;이종욱;박진형
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 추계학술대회논문집
    • /
    • pp.207-210
    • /
    • 2003
  • The purpose of this work is to find an appropriate welding approach for rotor assembly of a marine turbocharger. The friction welding and laser welding of dissimilar materials, IN713LC and SCM440 were investigated. The quality of the welded joints obtained from two welding processes was evaluated by microstructure observation, micro-hardness and tensile tests. The friction welded joint indicated a good bonding structure in the weld interface. On the other hand, the laser welded joint showed the weld defects and non-welded area in the weld interface.

  • PDF

아연도금강판의 $CO_2$ 용접특성(1) - 용접부 결함의 종류와 특성 - ($CO_2$ Weldability of Zn Coated Steel Sheet(1) - Weld Defects and Its Characteristics in Welds -)

  • 이종봉;안영호;박화순
    • Journal of Welding and Joining
    • /
    • 제18권1호
    • /
    • pp.91-96
    • /
    • 2000
  • Characteristics of the weld defect, such as a blowhole and a pit in lap-jointed fillet Co₂ welds of Zn-coated steel sheet were studied in order to make clear the sequence of the blowhole formation during welding. Main conclusions obtained are as follows: 1) Blowhole, wormhole and pit were found in fillet welds, although the optimum welding condition of 200A-23V-100cm/min was applied. 2) Zn was only detected at the solidification boundary at the early stage of the blowhole formation. 3) Most of the blowholes was started to form at lap-joint by the Zn vapor. With increasing of the Zn vapor and its pressure, the blowhole was develope to th bed surface until the completion of weld solidification. 4) The behavior of the blowhole in growth was similar to that of the columnar dendrite during welding.

  • PDF

용접부 품질향상을 위한 지능형 용접 와이어 공급 장치 개발 (Development of Intelligent Filler Wire Feeding Device for Improvement of Weld quality)

  • 이재석;손영일;박기영;이경돈
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.950-955
    • /
    • 2005
  • This paper describes an intelligent filler wire feeding device which can control 3- dimensional seam tracking and the filler wire speed by measuring the gap position and the joint gap width in laser welding. By means of visual sensor controlled filling the missing material into the joint gap and 3 dimensional seam tracking, lineup errors from manufacturing tolerances and the repeatability of lineup jigs and weld robot can be balanced and at an even seam quality which avoids weld defects. In this paper, we assessed weld quality in 2mm sheets of A16061 which had various gap width by using the intelligent filler wire feeding device.

  • PDF