Corrosion Resistance of SD460 Reinforcing Rod by Ceramic Coating (SD460 철근의 세라믹 코팅에 의한 내식성 향상연구)

  • Park, Ki Y.;Lee, Jong K.;Hong, Seok W.
    • Corrosion Science and Technology
    • /
    • v.8 no.4
    • /
    • pp.157-161
    • /
    • 2009
  • The corrosion resistance of reinforcing bar was studied to endure the marine environment during shipment. The red rust on the surface did not damage the adherence in the concrete structures, especially in highly alkaline environment, but made the consumer doubt of the quality. The passivation process by alkalization of the quenching water in the tempcore process failed to endure the long shipping period. The ceramic coating by sol-gel process improved the corrosion resistance without damaging the mechanical properties and adherence between concrete and reinfiorcing bar. Optimal concentration of the coating solution and coating temperature were tested. No additional energy was necessary for the coating process by spraying during cooling process, resulting simplified process and low cost. Salt spray test, cyclic corrosion test and atmospheric test were employed to confirm the resistance. The corrosion rates were presented by rating number and polarization resistance. The coating layer was examined by FIB, XRD and SEM etc.

A Study on the Effect of Corrosion Resistance According to the Composition Variety of C, Cr, N in Duplex Stainless Steel

  • Kim, Hyeong-Jin;Cho, Kye-Hyun;Jung, Jae-young
    • Corrosion Science and Technology
    • /
    • v.3 no.5
    • /
    • pp.179-186
    • /
    • 2004
  • Recently the alloy development of duplex stainless steel has been done. On this study we studied the effect of the corrosion resistance according to the composition variety of C, Cr, N in the alloy elements of duplex stainless steel. materials which have below 0.1[mm/year] corrosion rate enable to use for corrosion-resisting materials, generally. On this experiment we inspected the effect of the composition variety of C, Cr, N in duplex stainless steel and the heat treatment, which the condition was the water quenching after the heat treatment for 1hr. The experiment was done on the basis of the ASTM G48A test, Critical pitting temperature(CPT), and ASTM G-61(Electrochemical tests for cyclic polarization).

Engineering Properties of Lightweight Aggregate Concrete Using Dry Bottom Ash as Coarse Aggregate (건식 바텀애시 굵은골재를 사용한 경량골재 콘크리트의 공학적 특성)

  • Sung, JongHyun;Sun, JungSoo;Choi, SunMi;Bok, YoungJae;Kim, JinMan
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2013.11a
    • /
    • pp.166-167
    • /
    • 2013
  • Bottom ash, which is discharged through a wet process in a thermal power plant, contains much unburned coal due to quenching and much salt due to seawater. However, dry bottom ash discharged through a dry process contains low unburned coal and salt, and has light -weight due to many pores. Therefore, it is expected that it can be used as lightweight aggregate. This study deals with the basic properties of concrete used dry bottom ash as coarse aggregate. As a results, the concrete having high content of dry bottom ash aggregate showed high slump by using water reducing agent and its air content was within 5±1.5% as designed value, similarly to normal weight concrete. It also showed a lower compressive strength than 100% of crushed stone.

  • PDF

Electrochemically Fromed Nanotube Shape on Ternary Ti Alloy with Hf Content

  • Kim, Jeong-Jae;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2015.05a
    • /
    • pp.106-106
    • /
    • 2015
  • In this study, we investigated electrochemically formed nanotube shape on ternary Ti-25Ta-xHf alloys with Hf contents. Ti-25Ta-xHf (x=0~15 wt.%) alloys were manufactured by vacuum arc-melting furnace. The obtained ingots were homogenized in an argon atmosphere at $1050^{\circ}C$ for 2h and then water quenching. The specimens were cut from ingots to 4 mm thickness and first ground and polished using SiC paper (grades from #100 to #2000). The anodization treatments on Ti-25Nb-xHf alloys were carried out at room temperature for experiments. The formation of nanotubular film was conducted by electrochemical method in mixed electrolytes with 1 M $H_3PO_4$ + 0.8 wt. % NaF at 30 V for 2 h. The morphologies of nanotube depended on the Hf content in Ti-25Ta-xHf ternary system.

  • PDF

Effect of Cold Reduction Ratio on Spheroidization Rate of High Carbon Steel Sheet (고탄소강 열연판재의 냉간압하율에 따른 구상화 속도)

  • Lee, K.D.;Ha, T.K.;Jeong, H.T.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.05a
    • /
    • pp.543-546
    • /
    • 2008
  • In the present study, the effect of cold reduction ratio on the spherodization rate of SK85 high carbon steel sheet was investigated. High carbon steel sheet fabricated by POSCO was soaked at $800^{\circ}C$ for 2 hr in a box furnace and then treated at $570^{\circ}C$ for 5 min in a salt bath furnace followed by water quenching to obtain a fine pearlite structure. Cold rolling was conducted on the sheets of fine pearlite by reduction ratios of 20, 30, and 40 % and heat treatment for spheroidization was carried out at $720^{\circ}C$ for the various time intervals from 0.1 to 32 hrs. Area fraction of spheroidized cementite was measured with an image analyzer as a function of cold reduction ratios and duration times.

  • PDF

Axial strength of Zircaloy-4 samples with reduced thickness after a simulated loss of coolant accident

  • Desquines, Jean;Taurines, Tatiana
    • Nuclear Engineering and Technology
    • /
    • v.53 no.7
    • /
    • pp.2295-2303
    • /
    • 2021
  • To investigate wall-thinning impact on axial load resistance of Zircaloy-4 cladding rods after a LOCA transient, axial tensile samples have been machined on as-received tubes with reduced thicknesses between 370 and 580 ㎛. After high temperature oxidation under steam at 1200 ℃ with measured ECR ranging from 10 to 18% and water quenching, machined samples were axially loaded until fracture. These tests were modeled using a fracture mechanics approach developed in a previous study. Fracture stresses are rather well predicted. However, the slightly lower fracture stress observed for wall-thinned samples is not anticipated by this modeling approach. The results from this study confirm that characterizing the axial load resistance using semi-integral tests including the creep and burst phases was the best option to obtain accurate axial strengths describing accurately the influence of wall-thinning at burst region.

Characterization of Hardenability and Mechanical Properties of B-Bearing Microalloyed Steels for Cold Forging (붕소함유 냉간단조용 비조질강의 경화능 및 기계적 특성평가)

  • Park H. G.;Nam N. G.;Choi H. G.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.05a
    • /
    • pp.395-399
    • /
    • 2004
  • Four microalloyed steels containing B were investigated in terms of hardenability, mechanical properties and microstructure depending upon the cooling rates in order to develop the steel grade for the cold forged fasners. The alloy with the largest DI value among 4 alloys, which contains $0.12\%\;C,\;1.54\%\;Mn,\;0.65\%\;Cr,\;0.11\%V,\;0.040\%Ti\;and\;0.0033\%B$, showed the larest shift to the right hand side in the TTT diagram, implying the wide allowable cooling rate range subsequent to hot rolling in long bar processing, Mechanical tests indicated that yield strength are dependent upon the DI value in water quenched specimens but other properties showed almost the same values. In the same grade of steel, the increase in cooling rates causes the decrease in elongation but the increase in strength, reduction of area and Charpy impact values. Microstructural examination in steel grade with the larest DI values revealed martensitic structure In the water quenched state, a mixture of martensite and bainite in the oil quenched, and ferrite + pearlite in the air cooled and the forced air cooled but the latter showed finer microstructure.

  • PDF

Properties of reduced and quenched converter slag

  • Ko, In-Yong;Ionescu Denisa;T. R. Meadowcroft
    • Proceedings of the IEEK Conference
    • /
    • 2001.10a
    • /
    • pp.542-546
    • /
    • 2001
  • Converter slag has some compositional similarities to portland cement. But it has no hydration properties due to it's quite high concentrations of FeO(20-35%), MnO(4-6.5%). So it is needed to reduce the concentrations of iron and manganese of converter slag to use as cement additives by enhancing it's hydration properties. In this study, converter slag was modified it's composition by mixing of silica, alumina and quenched BF slag and reduced in induction furnace and quenched in running water. The hydraulic properties and structures of modified and quenched converter slag are significantly changed depend on the amount and kinds of additives. The addition of alumina up to 10% and BFQ slag up to 20% by weight on converter slag was effective to enhance the hydraulic properties of modified and quenched slag. The addition of reduced and quenched converter slag up to 20% by weight in replacement of portland cement in mixing of concrete mortar were shown higher compressive strength than 100% cement concrete mortar.

  • PDF

A Study on the Coolingability of Sodium Aqueous Solutions by Quenching (퀜칭시 나트륨계 수용액의 냉각성능에 관한 연구)

  • Kim, Ok Sam;Choi, Eun Soon;Min, Soo Hong
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.5 no.4
    • /
    • pp.224-232
    • /
    • 1992
  • Coolingability of coolants is important factor in cooling processor heat treatment of steel. Using standard apparatus and method defined in the Korean Industrial Standard three different shapes of probe were designed, ie, cylinderical, spherical and square on shape with same volume of standard probe. Distilled water and sodium aquious solutions with different concentration of NaOH, NaCl and $Na_2CO_3$ were examined. Estimation of coolingability of each quenchants for the probes of cylinderical, spherical or square shape, the cooling rate is greater square, cylinder and sphere in order. Coolingability of sodium aquious solution of NaCl, $Na_2CO_3$ and NaOH is found generally greater then that of distilled water. Effectiveness of ingredients is in the order of $Na_2CO_3$, NaOH and NaCl. In both solutions coolingability increases in 20%, 5%, and 10%in order. Analytical results obtained from Finite Element Method were compared with experimental ones and found as practically satisfactional.

  • PDF

Development of New Reverse Micellar Microencapsulation Technique to Load Water-Soluble Drug into PLGA Microspheres

  • Kim Hyun Joo;Cho Mi Hyun;Sah Hong Kee
    • Archives of Pharmacal Research
    • /
    • v.28 no.3
    • /
    • pp.370-375
    • /
    • 2005
  • The objective of this study was to develop a new reverse micelle-based microencapsulation technique to load tetracycline hydrochloride into PLGA microspheres. To do so, a reverse micellar system was formulated to dissolve tetracycline hydrochloride and water in ethyl formate with the aid of cetyltrimethylammonium bromide. The resultant micellar solution was used to dissolve 0.3 to 0.75 g of PLGA, and microspheres were prepared following a modified solvent quenching technique. As a control experiment, the drug was encapsulated into PLGA microspheres via a conventional methylene chloride-based emulsion procedure. The micro­spheres were then characterized with regard to drug loading efficiency, their size distribution and morphology. The reverse micellar procedure led to the formation of free-flowing, spherical microspheres with the size mode of 88 ~m. When PLGA microspheres were prepared follow­ing the conventional methylene chloride-based procedure, most of tetracycline hydrochloride leached to the aqueous external phase: A maximal loading efficiency observed our experimental conditions was below $5\%$. Their surfaces had numerous pores, while their internal architecture was honey-combed. In sharp contrast, the new reverse micellar encapsulation technique permitted the attainment of a maximal loading efficiency of 63.19 $\pm$$0.64\%$. Also, the microspheres had smooth and pore-free surfaces, and hollow cavities were absent from their internal matrices. The results of this study demonstrated that PLGA microspheres could be successfully prepared following the new reverse micellar encapsulation technique.