• Title/Summary/Keyword: Waste silk

Search Result 21, Processing Time 0.017 seconds

Properties of the Handsheet Paper made from Silk Fibers and Paper Mulberry (楮皮를 포함하는 絹紙의 特性)

  • 강경돈;이기훈;정병희;류운영;남중희
    • Journal of Sericultural and Entomological Science
    • /
    • v.41 no.3
    • /
    • pp.201-204
    • /
    • 1999
  • The silk/paper mulberry paper was prepared by recycling of the hard twisted silk waste and its mechanical properties was investigated. The silk waste was pretreated with sodium hydroxide(0.5%) and sodium carbonate(4%) to make it easy for beating and fibrillation. The silk/paper mulberry hand sheet paper has better mechanical properties of tearing strength and air permeability compared with the traditional and modified traditional paper. Treating with alkaline solution, the hard twisted silk waste could be used for an novel composite material.

  • PDF

Optimization of Decolorizing and Carding Condition for Recycle Materials of Colored Waste Silk Fabrics (폐견직물의 재활용을 위한 탈색과 개섬조건의 최적화)

  • Lee, Youn-Eung;Lee, Sun-Kun;Joo, Chsang-Whan
    • Textile Coloration and Finishing
    • /
    • v.17 no.6 s.85
    • /
    • pp.42-50
    • /
    • 2005
  • Silk fabrics are widely used as high quality cloth, interior, quilting and bedding materials because of having excellent touch, drape, resilience and low specific gravity characteristics. But, many waste silk materials are produced during the reeling, spinning, weaving, dyeing and finishing processes. From this fact, the recycle of waste silks is interested in studying for the application of industrial textile materials such as filter, oil absorbent and wound protector. Thus, this research has surveyed the decolorizing and carding characteristics in order to recycle the colored waste silk materials. As the results, the carding condition of waste silk fabrics was optimized with different fiber lengths and curding passage. In addition, the fiber failure mechanism from the wasted silk microdamage caused by carding process was investigated. Also it was found that longitudinal and transverse cracks, abrasion and pilling were formed on the surface of wasted silk fibers.

Features of Waste Water form By-Product Silk Treatment and Composition of Extracted Lipid (부잠폐수의 성상과 유출 유지의 성분)

  • 남영락;설대석
    • Journal of Sericultural and Entomological Science
    • /
    • v.33 no.2
    • /
    • pp.100-102
    • /
    • 1991
  • The features of waste water from by-product silk treatment of silk reeling process were investigated and the lipid extracted from waste water was analysed. The COD of waste water from by-product silk treatment was at the level of 605 mgO/$\ell$ Total Dissolved Solid Particles 2,335mg/$\ell$and Total Suspended Solid Particles 2,123mg/$\ell$. The lipid extracted from the waste water from by-product silk treatment was composed of triglyceride 76.8%, free fatty acids 12.5%, diglyceride 5.7% and free sterol 5.0%. In fatty acid composition of lipid, the content of loeic acid, linoleic and linolenic acid was 64.93%, whereas that of palmitic acid was 29.39% and stearic acid 4.93%.

  • PDF

Preparation of Fine Silk Powder and It′s Application for Surface Modification (폐견사류의 미세분말화 및 표면 가공제 적용)

  • 이용우;이광길;여주홍;김종호
    • Journal of Sericultural and Entomological Science
    • /
    • v.43 no.1
    • /
    • pp.41-48
    • /
    • 2001
  • The purification, dissolution and powdering of stained waste silk obtained from weaving and dyeing process were studied for the surface modification of textile fabric and plastic materials. The whiteness of stained waste silk could be improved through degumming and bleaching with sodium hydrosulfite. The water-soluble fibroin solution can be obtained by dissoving the degummed waste silk in a boiling solution of 50% calcium chloride for 60 minutes. The salts and heavy metals contained in fibroin solution were removed by electric dialysis, wool fiber filtration and gel filtration chromatography. The fibroin powder was prepared by using a fine grinder after the alkali treatment for weakening the silk fiber. The fine fibroin powder of particle size around 30 ㎛ was obtained with a ultra fine-mill, while it was finer below 10 ㎛ with a ball-mill. The dissolved or powdered silk was applied to the surface of fabric with addition of the binder (a urethane resin). The moisture content of polyester and nylon fabrics treated with the silk solution was improved due to hygroscopic property of silk. The fine fibroin powder mixed with the binder ws coated on the surface of synthetic film by use of the air pressed sprayer. It was revealed that the hygroscopicity as well as the softness of fibroin powder coated film was much improved. Therefore, it is thought that the fine silk fibroin powder is applicable as an coating agent for the surface modification of plastic and synthetic leather.

  • PDF

Preparation of Multi Skin Care Gauze by Blending of Silk Fiber and Separated Cellulose from Waste Milk Pack (견사와 폐 우유팩으로부터 분리한 셀룰로오스가 함유된 복합 위생포 제작)

  • 여주홍;이광길;이용우;김종호
    • Journal of Sericultural and Entomological Science
    • /
    • v.42 no.2
    • /
    • pp.109-113
    • /
    • 2000
  • The preparation of skin care gauze could be make to mixing separated cellulose from waste milk pack and degummed silk fibroin fiber. Also, its wound covering and anti-bacterial activity were investigated in order to find out the enhancement of their functionality. By the 30% silk fibroin fiber including skin care gauze, the anti-bacterial activity values of Staphylococcus strain are much 4 times higher than of 0∼10% silk fibroin fiber including skin care gauze. The average yield of cellulose from waste milk pack was obtained 50-60%, and their morphologies, physical properties, modulus and biodegradation ratios are studies, respectively.

  • PDF

Natural Dyeing Using Tea Extract II - The Effect of Dyeing Condition on Dyeing Characteristics of Coffee Extract Dyed Silk Farbic-

  • Yoo, Hyun-Geun;Kim, Sin-Hee
    • Journal of Fashion Business
    • /
    • v.10 no.3
    • /
    • pp.78-86
    • /
    • 2006
  • Coffee extract dyeing on silk fabric using various mordanting agents at different mordanting condition was studied in our previous research. Coffee extract dyeing can exert beautiful colors and have several advantages over the conventional natural dyeing. Since most of natural dyes are expensive for mass production, strongly season and source dependent, and hard to store, and therefore, coffee waste was used as natural dye to create beautiful colors in this study. Coffee waste is inexpensive and easy to store, and provide a comparatively regular quality regardless of season and source. The effects of dyeing condition such as dyeing temperature, dyeing time, and liquor ratio on dyeing characteristics of silk fabrics were investigated. Coffee extract dyed silk showed brilliant colors, and the colors were different with the kind of mordant. Cu, Sn, and Al mordanted silks showed golden yellow with subtle change of hue and value, while Fe mordanted silk showed a brownish green color upon coffee extract dyeing. As the dyeing temperature increased, the dyeability generally increased in all mordanted silk fabrics except Fe mordanted silk until $45^{\circ}C$. The dyeing temperature did not affect the dyeability of Fe mordanted silk fabric. As the liquor ratio increased, the dyeability showed a gradual increase in all mordanted silk except Cu mordanted silk. Cu mordanted silk fabric showed an abrupt increase in dyeability at liquor ratio1:150. The dyeing time effect can be separated into 2 stages. During the initial half an hour, the dyeability did not change significantly, and then, increased after 45 min. dyeing time duration. A further increase in dyeing time after 45 min. did not affect the dyeing efficiency in all mordanted silk fabrics except the Cu mordanted.

Silk Filament Progression with Backcross Breeding Generations in Tropical Tasar Silkworm, Antheraea mylitta D

  • Reddy, Rangareddygari Manohar;Suryanarayana, Nagabathula;Sinha, Manoj Kumar;Gahlot, Nand Singh;Hansda, Ganga;Ojha, Nand Gopal;Prakash, Nanjappa Basappa Vijaya
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.19 no.1
    • /
    • pp.187-192
    • /
    • 2009
  • Silk filament progression study applying backcross breeding with recipient parent Jata and donor parent Daba ecoraces of tropical tasar silkworm, Antheraea mylitta Drury conducted during 2006 to 2008, revealed introgression of filament denier (10.2 d) superior to both parents at BC4 level. Also, the silk waste (0.35%) and filament breaks (2.6 nos) were reduced compared to both parents, while the filament length (973 m) and non break filament (296 m) improved over donor and could attain closer to recipient parent. The best performance of Jata $\times$ Daba at F1 level, with highest silk filament length (1646 m) of 12.5 d denier, denotes heterosis impact on silk trait with parental heterogenousity, an advantage to exploit silk filament yield. The progression of quality in terms of finer filament denier, less silk waste and least number of filament breaks over both parents and improvement in filament length and non break filament over donor parent except for a marginal shortage against recipient at BC4 level indicates the prospects of Jata and Daba ecoraces as source of breeding material for qualitative improvement of tasar silk filament. The study suggests that the commercially important finer denier of tasar silk filament can be attained with minor reduction in silk yield of wild Jata ecorace by adopting repeated backcrossing for four generations with semi domesticated Daba ecorace.

An Analysis of Genetic Variation and Divergence on Silk Fibre Characteristics of Multivoltine Silkworm (Bombyx mori L.) Genotypes

  • Kumaresan P.;Koundinya P. R.;Hiremath S. A.;Sinha R. K.
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.14 no.1
    • /
    • pp.23-32
    • /
    • 2007
  • The nature of genetic variation and diversity among the 65 multivoltine silkworm genotypes was evaluated for 16 post cocoon characters. The components of genetic variation revealed higher PCV (60.487%) and GCV (44.56%) for evenness (variation 1) followed by cohesion (PCV=55.38%, GCV=40.36%) and non-broken filament length (PCV=32.05%, GCV=31.28%). The higher heritability ($h^2$ in broad sense) was observed for boil-off loss (95.6%) followed by non-broken filament length (95.22%). The both genotypic and phenotypic correlation indicated significant positive correlation of filament length with non-broken filament length, silk recovery, raw silk, neatness, and low neatness; and negative correlation with denier, renditta and silk waste. The principal component analysis (PCA) revealed 75.381 % of total variance from the five principal components extracted. On the basis of Mahalonobis' $D^2$ values (Ward's minimum variance), the sixty-five multivoltine silkworm genotypes were classified in to 9 clusters with substantial inter and intra cluster distances. Number of genotypes included in different clusters varied from 3 to 17. The results indicated that the optimum distance obtained in cluster VII (15.059) along with higher cluster mean values especially for filament length, non broken filament length, renditta, silk recovery, silk waste, and raw silk emphasized the utilization of these genotypes in the conventional silkworm breeding programme for improvement of multivoltine silk fibre quality. The possibility of exploiting genetic variation in post cocoon traits for efficient breeding programme is discussed.

Natural Dyeing Using Tea Extract I - The Effect Of Mordants On Dyeing Characteristics Of Coffee Extract Dyed Silk Fabric -

  • Yoo, Hyun-Geun;Kim, Sin-Hee
    • Journal of Fashion Business
    • /
    • v.9 no.6
    • /
    • pp.29-38
    • /
    • 2005
  • Natural dyes have attracted the worldwide attention because of its environmental advantage over synthetic dyes. However, most of natural dyes are expensive for mass production, strongly season and source dependent, and hard to store. In this study, coffee waste were used as natural dye to create beautiful colors. Coffee waste is inexpensive and easy to store, and provides a comparatively regular quality regardless of seasonand source. The effects of mordant agent concentration and mordanting temperature on dyeing efficiency of silk fabrics were investigated. Coffee extract dyed silk showed brilliant colors, and the colors were different with the kind of mordants. Cu, Sn, and Al mordanted silks showed golden yellow with subtle change of hue and value, while Fe mordanted silk showed a brownish green color. The increase in mordant concentration did not always increase the dyeability, and 0.5% o.w.f. mordant concentration was enough to get a satifactory result. Mordanting temperature also had little effect on the dyeability in case of Al, Cu, and Sn mordanted fabrics. Only Fe mordanted fabrics showed a better dyeability in the increase in mordating temperature. Coffee extract dyeing is an effective way using waste as resource and can create brilliant colors with minimal amount of mordant and under mild mordanting condition.

Preparation of Silk Nonwoven Fabrics by Needle Punching, Thermal Bonding and its properties. (니들펀칭법, 열융착법에 의한 실크 부직포의 제조 및 특성)

  • 이기훈;강경돈;정병희;주창환;남중희
    • Journal of Sericultural and Entomological Science
    • /
    • v.41 no.3
    • /
    • pp.205-210
    • /
    • 1999
  • Silk nonwoven fabrics are prepared by needle punching and thermal bonding with silk waste. To enhance the carding efficiency, the degumming rate was controlled with sodium hydrogen sulfite solution. The amount of the remained sericin was 3%(S-3), and 6%(S-6). Mixing wool and LMP(Low melting polyester) with the silk, to improve carding efficiency, was also effective. Following items were tested with prepared silk nonwovon fabrics : weight, thickness, compression, tensile strength, heat insulation, water absorption, and deodorization. The results show that the silk nonwoven fabrics could be used for apparels and new biomaterials.

  • PDF