• 제목/요약/키워드: Warm Deep Drawing

검색결과 68건 처리시간 0.019초

고체 윤활제를 사용한 마그네슘 합금 AZ31 판재 온간 디프 드로잉의 성형성 평가 (Evaluation of Warm Deep Drawability of Magnesium Alloy AZ31 Sheet Using Solid-Type Lubricants)

  • 김흥규;김종덕
    • 소성∙가공
    • /
    • 제15권6호
    • /
    • pp.453-458
    • /
    • 2006
  • While the die casting has been mainly used to manufacture the magnesium alloy parts, the press forming is considered as an alternative to the die casting for saving the manufacturing cost and improving the structural strength of the magnesium alloy parts. Because the magnesium alloy has low formability at room temperature, forming at elevated temperatures is a necessary condition to obtain the required material flow for press forming. However, the elevated temperature forming does not always guarantee the sufficient formability under the dry friction condition because the surface damage such as scratch or wear may accelerate the material failure. In the present study, the solid-type lubricants such as PTFE, graphite and $MoS_2$ were tested for the square cup warm deep drawing using the magnesium alloy AZ31 sheet. The formability improvement by using the lubricant was examined by comparing the maximum deep drawing depth using the PTFE against no lubricant. The formability difference for the different lubricant was also examined based on the maximum deep drawing depth.

합금화 용융 아연 도금강판의 온간 디프드로잉 성형성에 관한 연구 (A Study on the Warm Beep Drawabilities of Galvannealed Steel Sheet)

  • 장성호;최치수;최이천;서대교
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2000년도 추계학술대회 논문집
    • /
    • pp.168-173
    • /
    • 2000
  • The limiting drawing ratio (LDR) under uniform heating of blanks was measured at the various temperature ranges between 25 and $250^{\circ}C$ by using two different blank shapes, square and circular blanks, and six different blank sizes with the drawing ratios(DR) of 2.4 to 2.9. The galvannealed steel sheet (SCP3CM 60/60) of 0.7mm thickness was used. The LDR at warm forming condition reached 1.2 times of that at room temperature, and the maximum drawing depth reached 1.9 times. The higher temperature was adopted, the more stable and uniform thickness strain distribution was observed.

  • PDF

AZ31 합금의 온간 디프 드로잉에 관한 연구 (Deep drawing of AZ31 alloy sheet in the warm forming temperature)

  • 김민철;이영선;권용남;이정환
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 추계학술대회논문집
    • /
    • pp.175-179
    • /
    • 2004
  • Since the formability of AZ31 magnesium alloy is not good in room temperature, it is known that high temperature forming is advantageous. However, many studies are necessary to find the proper forming temperature for Mg alloy. In this study, experimental and FEM analysis are performed to investigate the forming temperature for AZ31 sheet. The deep drawing process of square cup is used in forming experiment and FEA. The investigations are performed in three forming temperature, room temperature, $250^{\circ}C\;and\;400^{\circ}C$. The square cup is well formed in $250^{\circ}C$ forming temperature, on the other hand, the crack and failure is presented in corner section in room and $250^{\circ}C$ forming temperature. The main cause is investigated as the effect of hardening range by the experimental and FEM results.

  • PDF

가열냉각법에 의한 마그네슘합금의 판재성형성개선(II) (Improvement on the formability of magnesium alloy sheet by heating and cooling method(II))

  • ;강대민
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.385-388
    • /
    • 2005
  • The use of magnesium alloys meets the need of reducing weight of componests(especially in automotive and aerospace industry) keeping unmodified their mechanical properties. The adoption of magnesium alloys in sheet forming processes is still limited, due to their low formability at room temperature caused by the hexagonal crystal structure. In this study, the authors aim to understand the process condition which can lead to a successful improvement in the formability of a magnesium alloy(AZ31). Experiment and simulations of deep drawing were doned at various warm temperature for the blank and tool(holde and die)while the punch was kept at room temperature by cooling wale. in order to confirm that the deep drawing performance of magnesium alloy can be considerably enhanced with using the local heating and cooling technique.

  • PDF

온간성형법에 의한 클래드 강판재의 정사각컵 드로잉성 향상에 관한 연구 (Improvement of Square Cup Drawability of Clad Sheet Metal by Warm Forming Technique)

  • 류호연;김영은;김종호
    • 소성∙가공
    • /
    • 제10권3호
    • /
    • pp.253-260
    • /
    • 2001
  • This study was performed to investigate the optimized warm forming conditions which gave the maximum drawing depth in square cup drawing of clad sheet metals, by changing the temperatures of die and blankholder and also shapes and materials of blanks. Two kinds of clad sheet metals, STS304-A1050-STS304 and STS304-A1050-STS430 were selected for experiments. The relative drawing depth of STS304-A1050-STS304 clad sheet was increased up to 4.4 at $150^{\circ}C$ that was 29% higher than at room temperature, whereas STS304-A1050-STS430 material was improved to 3.9 at $120^{\circ}C$ which was 15% better than at room temperature. In addition, comparison of wall thickness and hardness of a warm drawn cup with those of room temperature showed more even distributions. No separation between each laminated material after drawing occurred through inspection by microscope as well as application of penetrant test and bond strength test. Therefore, warm forming technique was confirmed to give better results in deep drawing of stainless clad sheet metal.

  • PDF

마그네슘 합금 판재의 온간 딥드로잉 해석 (Analysis of warm Deep Drawing of Magnesium Alloy Sheet)

  • 이명한;김헌영;김형종;오수익
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.294-297
    • /
    • 2007
  • Due to their low densities and high specific strength and stiffness, magnesium alloy sheets are very attractive lightweight materials for automotive and electrical products. However, the magnesium alloy sheets are usually formed at elevated temperature because of their poor formability at room temperature. To use of the magnesium alloy sheets for an industrial, their mechanical properties at elevated temperature and appropriate forming process conditions have to be developed. In this study, non-isothermal simulations of a square cup drawing from magnesium alloy sheets have been conducted to evaluate a proper forming process conditions such as the tool temperature, the tool shoulder radius, friction between the blank and the tools. According to this study, appropriate forming process conditions of square cup drawing at elevated temperature from magnesium alloy sheets are suggested.

  • PDF

SUS-Al-Mg이종판재의 드로잉성형에 관한 연구 (A Study on the Clad Sheet Metal of the Warm Drawability)

  • 이영선;정택우;권용남;이정환;최상운
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 추계학술대회 논문집
    • /
    • pp.71-74
    • /
    • 2008
  • The clad sheet is the sheet metal that joined the one or more material with the different property by rolling process. In this study, it is investigated about the mechanical property or formability of SUS-Al-Mg clad sheet. The clad sheet was formed at elevated temperature because of their poor formability at room temperature. The tensile test was confirmed at various temperature and the reduction of strain rate above $250^{\circ}C$. LDR(Limited Drawing Ratio) was obtained through deep drawing test to confirm the formability of the clad sheet. The FE analysis is performed to compare prototype products.

  • PDF

마그네슘 합금 판재의 온간 딥드로잉 공정의 성형해석 (Forming Analysis for Warm Deep Drawing Process of Magnesium Alloy Sheet)

  • 이명한;김헌영;김형종;김흥규;오수익
    • 소성∙가공
    • /
    • 제16권5호통권95호
    • /
    • pp.401-405
    • /
    • 2007
  • Due to the low densities and high specific strength and stiffness, magnesium alloy sheets are very attractive lightweight materials for automotive and electrical products. However, the magnesium alloy sheets should be usually formed at elevated temperature because of their poor formability at room temperature. For the use of the magnesium alloy sheets for an industrial, their mechanical properties at elevated temperature and appropriate forming process conditions have to be developed. In this study, non-isothermal simulation of a square cup drawing of magnesium alloy sheets have been conducted to evaluate a proper forming process conditions such as the tool temperature, the tool shoulder radius, friction between the blank and the tools. According to this study, appropriate forming process conditions of square cup drawing at elevated temperature from magnesium alloy sheets are suggested.

가열냉각법에 의한 마그네슘 합금의 판재 성형성 개선 (Improvement on the Formability of Magnesium Alloy Sheet by Heating and Cooling Method)

  • 강대민
    • 동력기계공학회지
    • /
    • 제9권3호
    • /
    • pp.66-70
    • /
    • 2005
  • Structural components for aerospace, electronics and automobile industry are the main applications for magnesium alloys due to their lightweight and high specific strength. The adoption of magnesium alloys in sheet forming processes is still limited, due to their low formability at room temperature caused by the hexagonal crystal structure. In this paper, the authors aim to improve the formability of AZ31 magnesium alloy. For this, experiment and finite element analysis on used warm deep drawing process with a local heating and cooling technique were done. Both die and blank holder were heated at various warm temperature while the punch was kept at room temperature by cooling water.

  • PDF

AZ31B 마그네슘 판재의 온.열간 ?K드로잉에 관한 연구 (A Study on the Deep Drawing of AZ31B Magnesium Sheet at Warm and Hot Temperature)

  • 김한구;배정운;추동균;강충길
    • 소성∙가공
    • /
    • 제15권7호
    • /
    • pp.504-511
    • /
    • 2006
  • The drawability of AZ31B magnesium sheet is estimated at various temperatures($200,\;250,\;300,\;350\;and\;400^{\circ}C$), and forming speed(20, 50, 100mm/min), thickness(0.5, 0.8, 1.0, 1.4mm). The deep drawing process of circular cup and square cup were used in forming experiments. Experimental and FEM analysis are performed to investigate drawability and affection of controlled blank holding force. Through the controlled blank holding force, drawability was improved. Limit drawing ratio is increased from 2.1 to 3.0 in circular cup drawing and change of thickness is decreased from 16.3 to 6.9%. This result is verified by FEM analysis. Through the observation of microstructure, the main cause is investigated as a quantity of the dynamic recrystallization.