분쇄된 초경합금 분말의 산화에 미치는 진공열처리 효과 (EffEct of vacuum annealing on an oxidation of milled WC-Co powder)

  • 김소나
    • 한국분말재료학회지
    • /
    • 제3권2호
    • /
    • pp.91-96
    • /
    • 1996
  • The effect of vacuum annealing on the oxidation behavior of milled WC-15%Co powder mixture has been studied. A cobalt component in the milled powder mixture was oxidized preferentially above 175$^{\circ}C$ in air. The specimens showed a steady increase in weight at 175$^{\circ}C$ but did constant weight followed by rapid increase in specimen weight at the beginning above 20$0^{\circ}C$. Oxidation of the milled powder mixture was significantly suppressed by vacuum annealing at 30$0^{\circ}C$ for 10 h. Suppression of oxidation by vacuum annealing and different oxidation behaviors of the milled powder mixture between 175$^{\circ}C$ and 20$0^{\circ}C$, were attributed to removal of strain energy stored in the cobalt powder during vacuum annealing or oxidation treatment above 20$0^{\circ}C$. The role of stored strain energy on oxidation of milled WC-15%Co powder mixture was proved by X-ray diffraction method and differential thermal analysis.

  • PDF

On the Solubility of Chromium in Cubic Carbides in WC-Co

  • Norgren, Susanne;Kusoffsky, Alexandra;Elfwing, Mattias;Eriksson, Anders
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.338-339
    • /
    • 2006
  • The solubility of Cr in cubic carbides in the systems WC-Co-TaC and WC-Co-ZrC has been determined using equilibrium samples. Thermodynamic calculations were used to design the alloys through extrapolations of Gibbs energy expressions. The alloys were designed to have a microstructure containing the following phases: WC, liquid, $M_7C_3$, graphite and cubic carbide. The alloys were investigated using scanning electron microscopy and analyzed using energy-dispersive X-ray spectrometry. The present work shows how the Cr solubility depends on which cubic carbide former that is present. The WC-Co-Cr-Zr alloy has no detectable amount of Cr whereas the WC-Co-Cr-Ta alloy has 12% Cr in the cubic carbide.

  • PDF

기계화학적방법에 의한 나노구조 WC/Co 복합 분말의 제조에 관한 연구 (A Study On Synthesis of Nanostructured WC/Co composite Powders by Mechanochemical process)

  • 권대환;안인섭;하국현;김병기;김유영
    • 한국분말재료학회지
    • /
    • 제9권3호
    • /
    • pp.167-173
    • /
    • 2002
  • A new approach to produce nanostructured WC/Co composite powders by a mechanochemical process was made to improve the mechanical properties of advanced hardmetals. Homogeneous spherical W-Co salt powders were made by spray drying of aqueous solution from ammonium metatungstate($(NH_4)_6(H_2W_{12}O_{40})\cdo4H_2O$,AMT) and cobalt nitrate hexahydrate (Co(NO$_3$)$_2$.6$H_2O$). spray dried W-Co salt powders were calcined for 1 hr at $700^{\circ}C$ in atmosphere of air. The oxide powder was mixed with carbon black by ball milling and this mixture was heated with various temperatures and times in $H_2$. The $WO_3/CoWO_4$ composite oxide powders were obtained by calcinations at $700^{\circ}C$. The primary particle size of W/Co composite oxide powders by SEM was 100 nm. The reduction/carburization time decreased with increasing temperatures and carbon additions. The average size of WC particle carburized at $800^{\circ}C$ by TEM was smaller than 50 nm.

Co 액상 내에 공존하는 (Ti,W)(C,N)과 WC입자의 성장 거동 (Growth Behavior of (Ti,W)(C,N) and WC grains in a Co Matrix)

  • 이보아;윤병권;강석중
    • 한국분말재료학회지
    • /
    • 제11권2호
    • /
    • pp.165-170
    • /
    • 2004
  • Growth behavior of two different types of grains, faceted and rounded, in a liquid matrix has been studied in the (75WC-25TiCN)-30Co system. Powder samples were sintered above the eutectic temperature for various times under a carbon saturated condition. (Ti,W)(C,N) grains with a rounded shape and WC grains with a faceted shape coexisted in the same Co based liquid. With increasing sintering time, the average size of (Ti.W)(C,N) grains increased continuously and very large WC grains appeared. The growth of rounded (Ti,W)(C,N) grains followed a cubic law, r^3-r^3_0$=kt, where r is the average size of the grains, $r_0$ the initial average size, k the proportionality constant and t the sintering time. indicating a diffusion-controlled growth. On the other hand, the growth of the faceted WC grains resulted in a bimodal grain size distribution, showing an abnormal grain growth. These observations show that the growth behavior of different types of grains is governed by their shape, faceted or rounded, even in the same liquid matrix.

Unified Molding and Simulation for Nano-structured Tungsten Carbide

  • Park, Seong-Jin;Johnson, John L.;German, Randall M.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.362-363
    • /
    • 2006
  • Nano-structured tungsten carbide compacts with cobalt matrices (WC-Co) offer new opportunities for achieving superior hardness and toughness combinations. A unified modeling and simulation tool has been developed to produce maps of sintering pathways from nanocrystalline WC powder to sintered nano-structured WC-Co compacts. This tool includes (1) die compaction, (2) grain growth, (3) densification, (4) sensitivity analysis, and (5) optimization. All material parameters were obtained by curve fitting based on results with two WC-Co powders. Critical processing parameters are determined based on sensitivity analysis and are optimized to minimize grain size with high density.

  • PDF

A Study of Reduced and Carburized Reactions in Dry-milled $WO_3+Co_3O_4+C$ Mixed Powders with Different Carbon Content

  • Im, Hoo-Soon;Lee, Wan-Jae
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.648-649
    • /
    • 2006
  • The dry-milling technique was used for mixing and crushing oxides and graphite powders. The ratio of ball-to-powder was 30:1 and argon gas was filled in jar. The excess carbon was $10{\sim}20wt%$ of the stoichiometric amount. The dry-milling was carried for 20 hours. The mixed powders were reduced and carburized at $900{\sim}980^{\circ}C$ for 3 hours flowing Ar gas in tube furnace. The dry-milled powders showed the wide diffraction patterns of X-ray. The reactions of reduction and carburization were completed in 3 hours at $980^{\circ}C$. After the reactions, the mean size of WC particles was about 200 nm. The content of free carbon in WC/Co mixed powders was less as the reaction temperature increased.