Relationship between the Applied Torque and CCT to obtain the Same Corrosion Resistance for the Plate and Cylindrical Shape Stainless Steels

  • Chang, Hyun Young;Kim, Ki Tae;Kim, Nam In;Kim, Young Sik
    • Corrosion Science and Technology
    • /
    • 제15권2호
    • /
    • pp.58-68
    • /
    • 2016
  • Many industries need the universal standard or technique to obtain the identical CCT regardless of specimen geometries. This study aimed to determine an appropriate applied torque to the cylindrical specimen defining the apparatus and the procedure to measure the temperature of initiating crevice corrosion in tubular shape products such as pipes, tubes and round rods etc; the test method also proved applicable to the plate type specimen. A series of experiments for CCT measurements with the plate type and cylindrical stainless steel specimens of various diameters with different microstructures (austenitic and duplex) and PRENs were conducted to determine the relationship among geometries on CCT. Thus, the apparatus that could measure the CCT of stainless steels with both plate and cylindrical geometries was newly designed. The use of the apparatus facilitated the same CCT value for both geometries only if the specimens were made of the same alloy. The applied torque can be calculated for various diameters of the cylindrical specimens using the following relation; Applied torque, $Nm=-0.0012D^2+0.019D+2.4463$ (D; the diameter of cylindrical specimen, mm). However, upwards of 35 mm diameter cylindrical specimens require 1.58Nm, which is the same torque for the plate type specimen; in addition, this test method cannot be used for cylindrical specimens of less than 15 mm diameter.

수종(數種) 구치부(臼齒部) 충전용(充塡用) 복합(複合)레진의 물리적(物理的) 성질(性質)에 관(關)한 실험적(實驗的) 연구(硏究) (AN EXPERIMENTAL STUDY ON PHYSICAL PROPERTIES OF VARIOUS POSTERIOR RESTORATIVE COMPOSITE RESINS)

  • 박선재;박상진;민병순;최호영
    • Restorative Dentistry and Endodontics
    • /
    • 제12권1호
    • /
    • pp.7-24
    • /
    • 1986
  • The purpose of this study was to observe the compressive strength, compressive fatigue strength, surface hardness, water sorption and solubility of eight different posterior restorative composite resins. Eight composite resins were tested for their strength of the compressive and compressive fatigue with prepared two different types of specimens (I and T-type) using a Instron universal testing machine (model No. 1332). The hardness was measured with a Knoop hardness tester (MVH-2, Tokyo) for each cylindrical specimen, 7mm in diameter and 5mm thick. The water sorption and solubility were evaluated with the prepared composite resin disks, 20mm in diameter and 1mm thick. The results were as follows: 1. The compressive strength, compressive fatigue strength and hardness were noticed to be Increased by increasing the volume content of filler. 2. The compressive strength was appeared to be independent on the type of specimen, but the compressive fatigue strength was found to be greatly influenced by the type of specimens. 3. The composite resins having higher compressive strength had also higher compressive fatigue limits. 4. The compressive fatigue limits at $10^5$ stress cycles were about 50-80% of the compressive strength and were showen to be dependent on the materials and type of specimens. 5. The larger the filler particle size was, the lower was the water sorption. And the water sorption of BIS-GMA resin was higher than that of urethane resin. 6. The visible light-cured composite resin had a higher value of solubility than the chemically- cured composite resin. And the solubility tended to decrease by increasing the volume content of filler.

  • PDF

광중합 Glass Ionomer Cement와 Amalgam의 결합강도에 관한 연구 (A STUDY ON THE BOND STRENGTHS OF LIGHT-CURING GLASS IONOMER CEMENTS TO DENTAL AMALGAM)

  • 정태성
    • 대한소아치과학회지
    • /
    • 제23권2호
    • /
    • pp.357-364
    • /
    • 1996
  • 소아치과 임상에서 자주 사용되는 3 종의 광중합형 GIC의 아말감에 대한 접착능을 평가 할 목적으로 60 개의 아말감 부착시편을 이용하여 중간결합제인 Scotchbond 의 사용여부에 따른 경화된 아말감에 대한 광중합 GIC의 전단결합강도를 측정하고 경계부의 파절양상을 관찰한 결과, 다음과 같은 결론을 얻었다. 1. 아말감에 대한 광중합형 GIC의 전단강도는 Fuji II LC, Vitremer, Vitrebond의 순으로 높게 나타났다 (p<0.05). 2. 중간결합제인 Scotchbond를 사용하지 않은 경우에서 Scotchbond 를 사용한 경우에 비해 전단결합강도가 높게 나타났다(p<0.05). 3. 결합파절면은 Scotchbond를 사용한 경우의 대부분에서 Scotchbond와 아말감의 경계부에서 시편의 탈락이 나타났다. 아말감과 광중합 GIC의 결합을 시도할 경우에는 Scotchbond는 사용하지 않는 것이 바람직할 것으로 사료되었다.

  • PDF

교정용 광중합형 및 화학중합형 레진접착제의 전단결합강도와 파절양상에 대한 연구 (A STUDY OF SHEAR BOND STRENGTH AND FAILURE PATTERNS IN LIGHT-AND SELF-CURED ORTHODONTIC RESIN)

  • 이민하;양규호;박영준
    • 대한소아치과학회지
    • /
    • 제23권2호
    • /
    • pp.549-558
    • /
    • 1996
  • Light-cured orthodontic composite resin has been widely advertised recently for use in bonding brackets. However, the curability of light-cured resin when light waves are diffused through metal brackets in questionable. The purposes of this study were to evaluate shear bond strength and failure patterns of visible light-cured resin(Lightbond) and chemically cured-resin(Mono-Lok 2), and to determine the relative value of light-cured resin as an alternative to conventional chemically cured resin. Each of the two resins was tested on twenty extracted human first premolars. Standard edgewise metal brackets were bonded to the teeth in accordance with the manufacturers' recommendation. After bonding, the teeth were stored for 24 hours at $37^{\circ}C$, 100% humidity. The shear bond strength was tested with a universal testing machine(Instron 4302), at 0.5mm/min crosshead speed. After debonding, brackets and enamel surfaces were examined with a scanning electron microscope and a stereoscopic microscope. The results were as follows : 1. Metal brackets bonded with Lightbond showed statistically higher shear bond strength than metal brackets bonded with Mono-Lok2. 2. The predominant failure site in Lightbond was the enamel-resin interface, and in Mono-Lok 2 it was the resin itself. 3. Enamel cracks were not found in any specimen. The above results suggest that direct bonding of metal brackets to enamel with light-cured resin bonding agent can be used effectively in clinics.

  • PDF

지르코니아 코어와 전장용 세라믹의 결합 강도에 대한 표면 처리 방법 평가 (Evaluation of surface treatment methods on the bond strength of veneer ceramic to the zirconia core)

  • 이광영;홍민호
    • 대한치과기공학회지
    • /
    • 제42권3호
    • /
    • pp.213-219
    • /
    • 2020
  • Purpose: This study aimed to identify the impact of physical surface roughing with a polishing tool onto the pre-sintering yttria-stabilized tetragonal zirconia polycrystals (TZP) core and liner treatment for chemical bonding on the bond strength of TZP core and veneering ceramic. Methods: Overall, 80 specimens were classified into two groups (non-liner, NL; and usingliner, UL ) depending on the use of liner, and these two groups were then subclassified into four groups depending on the polishing tool used. (1) Non-liner groups: NS, non-liner+stone point; NC, non-liner+carbide bur; NP, non-liner+paper cone point; NT, non-liner+silicon point. (2) Using-liner groups: US, using-liner+stone point; UC, using-liner+carbide bur; UP, usingliner+paper cone point; UT, using-liner+silicon point. The pre-sintering surface roughing values and shapes were observed, and after burning up the veneering ceramic, the shear bond strength was measured using a universal testing machine. For significance testing, a one-way analysis of variance and Tukey's multiple comparison test were conducted. An optical microscope was used to observe the fracture plane, and the following results were obtained. Results: Surface roughness NP (4.09±0.51 ㎛) represented a higher value than other groups (p<0.001). In shear bond strength, NS (35.21±1.44 MPa) of the NL group showed the highest bond strength (p<0.001). The UL group did not show a statistically significant difference between groups (p=0.612). Conclusion: Our study findings reveal that the bond strength of TZP core and veneering ceramic was improved by pre-sintering physical surface treatment than by chemical bonding with liner surface treatment.

COMPARATIVE STUDY ON THE FRACTURE STRENGTH OF METAL-CERAMIC VERSUS COMPOSITE RESIN-VENEERED METAL CROWNS IN CEMENT-RETAINED IMPLANT-SUPPORTED CROWNS UNDER VERTICAL COMPRESSIVE LOAD

  • Pae, Ahran;Jeon, Kyung-A;Kim, Myung-Rae;Kim, Sung-Hun
    • 대한치과보철학회지
    • /
    • 제45권3호
    • /
    • pp.295-302
    • /
    • 2007
  • Statement of problem. Fracture of the tooth-colored superstructure material is one of the main prosthetic complications in implant-supported prostheses. Purpose. The purpose of this in vitro study was to compare the fracture strength between the cement-retained implant-supported metal-ceramic crowns and the indirect composite resinveneered metal crowns under the vertical compressive load. Material and methods. Standard implants of external type (AVANA IFR 415 Pre-mount; Osstem Co., Busan, Korea) were embedded in stainless steel blocks perpendicular to their long axis. Customized abutments were fabricated using plastic UCLA abutments (Esthetic plastic cylinder; Osstem Co., Busan, Korea). Thirty standardized copings were cast with non-precious metal (Rexillium III, Pentron, Walling ford, Conn., USA). Copings were divided into two groups of 15 specimens each (n = 15). For Group I specimens, metal-ceramic crowns were fabricated. For Group II specimens, composite resin-veneered (Sinfony, 3M-ESPE, St. Paul, MN, USA) metal crowns (Sinfony-veneered crowns) were fabricated according to manufacturer's instructions. All crowns were temporary cemented and vertically loaded with an Instron universal testing machine (Instron 3366, Instron Corp., Norwood, MA, USA). The maximum load value (N) at the moment of complete failure was recorded and all data were statistically analyzed by independent sample t-test at the significance level of 0.05. The modes of failure were also investigated with visual analysis. Results. The fracture strength of Sinfony-veneered crowns ($2292.7{\pm}576.0N$) was significantly greater than that of metal-ceramic crowns ($1150.6{\pm}268.2N$) (P < 0.05). With regard to the failure mode, Sinfony-veneered crowns exhibited adhesive failure, while metal-ceramic crowns tended to fracture in a manner that resulted in combined failure. Conclusion. Sinfony-veneered crowns demonstrated a significantly higher fracture strength than that of metal-ceramic crowns in cement-retained implant-supported prostheses.

무선통신 자료를 활용한 통행발생량 분석 (Trip Generation Analysis Using Mobile Phone Data)

  • 김경태;이인묵;민재홍;곽호찬
    • 한국철도학회논문집
    • /
    • 제18권5호
    • /
    • pp.481-488
    • /
    • 2015
  • 현재 통행발생량 산정 등 교통계획 정보의 생성 체계가 기존 조사 중심 체계에서 외부 데이터를 접목하여 조사 비용을 저감시키고 정확성을 높이는 방향으로 전환되고 있다. 우리나라는 인구보다 많은 휴대전화가 보급되어 있기 때문에 이로부터 구축된 무선통신 자료는 교통계획에 매우 유용한 정보를 줄 수 있을 것이다. 본 연구에서는 이동통신사에서 제공하는 수도권 지역 성 연령별 유동인구 자료로부터 교통계획의 중요한 자료인 통행발생량을 산정하기 위한 방안을 제시하고 이를 KTDB의 통행발생량과 상관성 분석을 통하여 자료의 활용 가능성을 확인하였다. 그 결과 무선통신 자료를 이용한 통행발생량 추정은 기존의 KTDB에서 구축한 직접 조사 방식 기반에 의한 결과와 매우 높은 상관관계를 가지는 것으로 분석되었다.

Implementation and Performance Analysis of Multi-GNSS Signal Collection System using Single USRP

  • Park, Kwi Woo;Choi, Yun Sub;Lee, Min Joon;Lee, Sang Jeong;Park, Chansik
    • Journal of Positioning, Navigation, and Timing
    • /
    • 제5권1호
    • /
    • pp.11-20
    • /
    • 2016
  • In this paper, a system that can collect GPS L1 C/A, GLONASS G1, and BDS B1I signals with single front-end receiver was implemented using a universal software radio peripheral (USRP) and its performance was verified. To acquire the global navigation satellite system signals, hardware was configured using USRP, antenna, external low-noise amplifier, and external oscillator. In addition, a value of optimum local oscillator frequency was selected to sample signals from three systems with L1-band with a low sampling rate as much as possible. The comparison result of C/N0 between the signal collection system using the proposed method and commercial receiver using double front-end showed that the proposed system had 0.7 ~ 0.8dB higher than that of commercial receiver for GPS L1 C/A signals and 1 ~ 2 dB lower than that of commercial receiver for GLONASS G1 and BDS B1I. Through the above results, it was verified that signals collected using the three systems with a single USRP had no significant error with that of commercial receiver. In the future, it is expected that the proposed system will be combined with software-defined radio (SDR) and advanced to a receiver that has a re-configuration channel.

전자무역의 SaaS모형 UPnP 네트워크 활용방안에 관한 연구 (A Study on the Utilization of the SaaS Model UPnP Network in e-Trade)

  • 정분도;윤봉주
    • 통상정보연구
    • /
    • 제14권4호
    • /
    • pp.563-582
    • /
    • 2012
  • SaaS모형은 정보화 H/W 투자여력이 없는 중소기업이 인터넷 기반의 모듈별 솔루션을 임대방식으로 서비스 받는 시스템이다. 많이 활용되고 있는 UPnP(Universal Plug and Play)는 정보가전이나, 무선기기, PC 등 모든 종류의 기기들을 연결하는 네트워크 구조이다. 이것은 홈이나 작은 사무실과 같이 관리자가 없는 네트워크에서 사용자의 작업 없이 쉽게 표준화된 방법으로 기기간의 연결이나 인터넷으로의 연결을 제공한다. 따라서 이러한 연결문제는 업무의 설계나 데이터베이스의 설계가 단위 네트워크별로 설계되었기 때문으로, 어떠한 업무 네트워크시스템들도 UPnP 설계시 업무를 서로 연결 할 수 있는 복합 네트워크 환경을 고려하여야 한다. UPnP 연결구조의 SaaS모형은 네트워크 기반 접속 및 실시간 관리가 가능한 상업용 소프트웨어이어야 한다. 항상 접속이 가능하고 중앙에서 관리활동이 이루어져야 한다.

  • PDF

Comparison of polymer-based temporary crown and fixed partial denture materials by diametral tensile strength

  • Ha, Seung-Ryong;Yang, Jae-Ho;Lee, Jai-Bong;Han, Jung-Suk;Kim, Sung-Hun
    • The Journal of Advanced Prosthodontics
    • /
    • 제2권1호
    • /
    • pp.14-17
    • /
    • 2010
  • PURPOSE. The purpose of this study was to investigate the diametral tensile strength of polymer-based temporary crown and fixed partial denture (FPD) materials, and the change of the diametral tensile strength with time. MATERIAL AND METHODS. One monomethacrylate-based temporary crown and FPD material (Trim) and three dimethacrylate-based ones (Protemp 3 Garant, Temphase, Luxtemp) were investigated. 20 specimens (${\phi}\;4\;mm\;{\times}\;6\;mm$) were fabricated and randomly divided into two groups (Group I: Immediately, Group II: 1 hour) according to the measurement time after completion of mixing. Universal Testing Machine was used to load the specimens at a cross-head speed of 0.5 mm/min. The data were analyzed using one-way ANOVA, the multiple comparison Scheff$\acute{e}$ test and independent sample t test ($\alpha\;=\;0.05$). RESULTS. Trim showed severe permanent deformation without an obvious fracture during loading at both times. There were statistically significant differences among the dimethacrylate-based materials. The dimethacrylate-based materials presented an increase in strength from 5 minutes to 1 hour and were as follows: Protemp 3 Garant (23.16 - 37.6 MPa), Temphase (22.27 - 28.08 MPa), Luxatemp (14.46 - 20.59 MPa). Protemp 3 Garant showed the highest value. CONCLUSION. The dimethacrylate-based temporary materials tested were stronger in diametral tensile strength than the monomethacrylate-based one. The diametral tensile strength of the materials investigated increased with time.