CSG 재료의 압축강도 특성 및 동결융해 저항성 (Compressive Strength Properties and Freezing and Thawing Resistance of CSG Materials)

  • 연규석;김영익;현상훈;김용성
    • 한국농공학회논문집
    • /
    • 제52권1호
    • /
    • pp.51-59
    • /
    • 2010
  • The cemented sand and gravel (CSG) method is a construction technique that adds cement and water to rock-like materials, such as rivered gravel or excavation muck which that can be obtained easily at areas adjacent to dam sites. This study was performed to evaluate the unconfined compressive strength properties and freezing and thawing resistance of CSG materials with unit cement content. The three types of CSG-80, CSG-100 and CSG-120 with cement content were designed to evaluate the optimum water content, dry density, strength, stress-strain, micro structure and durability factor. As the results, the optimum water content ratio with cement content showed almost similar tendency, and the unconfined compressive strength and dry density increased as cement content increases. The strength ratio of 7 days for 28 days were in the range of 55~61 % and the strain ratio in stress-strain curve were in the range of 0.8~1.6 % nearby maximum strength in 28 days. It is expected that this study will contribute to increasing application of CSG method as well as to increasing the utilizing of CSG materials as a environmentally friendly CSG method.

황토와 플라이 애시를 혼입한 시멘트 모르타르 벽돌의 물리 · 역학적 특성 (Physical and Mechanical Properties of Cement Mortar Brick with Loess and Fly Ash)

  • 임성수;성찬용
    • 한국농공학회논문집
    • /
    • 제46권3호
    • /
    • pp.57-63
    • /
    • 2004
  • This study was performed to evaluate the engineering properties of cement mortar brick with loess and fly ash. The unit weight was in the range of $2,068{\sim}2,137\;kgf/m^{3}$ and $1,899{\sim}2,045\;kgf/m^{3}$ in water and dry curing, respectively It was decreased with increasing the loess content. The absorption ratio was in the range of $5.2{\sim}13.1%$ and $8.5{\sim}13.2%$ in water and dry curing, respectively. The compressive strength was decreased with increasing the loess content. The compressive strength of the 193 $kgf/m^{2}$ in water and 188 $kgf/m^{2}$ in dry curing at the curing age 28 days of the binder volume ratio 35% was exceeded in 163 $kgf/m^{2}$ of standard compressive strength about cement bricks. The carbonation depth was in the range of $0.9{\sim}1.4$ mm, $1.2{\sim}3.6$ mm, $1.4{\sim}6.7$ mm and $2.4{\sim}12.5$ mm in dry curing of curing age 14days, 28days, 90days and 360days, respectively.

풍쇄슬래그 잔골재를 사용한 콘크리트의 공학적 특성에 관한 실험적 연구 (An Experimental Study on the Engineering Properties of Concrete using Fine Aggregate of PS ball Slag)

  • 이상수;송하영;김을용
    • 한국건축시공학회지
    • /
    • 제6권3호
    • /
    • pp.107-114
    • /
    • 2006
  • In this study, the experiment was carried out to investigate and analyze the engineering properties of concrete using fine aggregate of PS bal slagl. The main experimental variables were water/cement ratio 30, 40, 50(%), water content $170kg/m^3$, replacement ratio of slag fine aggregate 0, 25, 50, 75(%) in experiment I and water/cement ratio 30, 40, 50(%), water content 165, 170, 175($kg/m^3$), replacement ratio of fine aggregate of PS ball 0, 50 in experiment II. According to the test results, the principle conclusions are summarized as follows (1) The workability of slag fine aggregate-mixed concrete tends to improve, as the replacement rate increases. (2) The air content of slag fine aggregate-mixed concrete tends to decrease, as the replacement rate increases. (3) The unit volume weight of slag fine aggregate-mixed concrete tends to significantly increase, as the replacement rate increases. (4) The compressive strength of slag fine aggregate-mixed concrete tends to show more increasing propensity, in case the curing period is relatively long, as the replacement rate increases.

충전 시스템과 SBR의 미세 구조가 SBR 복합체의 수팽윤 거동에 미치는 영향 (Influence of reinforcing systems and microstructures of SBR on water swelling behaviors of SBR composites)

  • 최성신;하성호
    • Elastomers and Composites
    • /
    • 제42권2호
    • /
    • pp.102-106
    • /
    • 2007
  • 카본블랙, 커플링제가 없는 실리카, 그리고 커플링제를 함유한 실리카 등 다른 충전 시스템을 갖는 SBR 가황물의 수팽윤 거동에 대해 연구하였다. 증류수와 3.5% NaCl 용액을 팽윤 매질로 사용하였다. 증류수에서의 수팽윤비가 소금물에서의 그것보다 높았다. 카본블랙으로 보강된 가황물의 수팽윤비가 실리카로 보강된 것보다 낮았다. 실리카로 보강된 SBR 가황물의 경우, 커플링제가 없는 것이 커플링제를 함유한 것보다 더 큰 수팽윤비를 나타내었다. 1,2-유니트 함량이 다른 SBR 가황물의 수팽윤 거동에 대해서도 비교하였다. 수팽윤비는 1,2-유니트 함량이 증가함에 따라 감소하는 경향을 보였다.

화학혼화제의 성분함유율 변화에 따른 콘크리트의 특성분석 (Analysis of concrete characteristic depending on chemical admixtures changing component content ratio)

  • 류현기
    • 한국건축시공학회지
    • /
    • 제9권2호
    • /
    • pp.85-91
    • /
    • 2009
  • W/C and unit volume, which significantly affect quality of concrete related to strength and durability, are regulated at below $185kg/m^3$ for regular concrete generally used in standard specification for constructions. The aim of this research is to develop chemical admixture and find out its potential use by identifying characteristics of admixtures added to soft concrete and hardening concrete, of which content ratio of component for each type of admixtures is subject to change in accordance with unit volume within KS' allowable range. Sodium gluconate, polyoxyethylene nonylphenyl ether, poly carboxylic copolymer in slump, which is characteristic of soft concrete, are deemed highly sensitive while there is no air entrainment except for $10\sim70%$ in WE, WR component content ratio and NP. In hardening concrete, strength in general showed higher action in compressive strength and tensile strength than in plain strength. Use of proper AE agent and AE water reducing agent at the same time is deemed to be used as chemical admixtures capable of manufacturing high-quality, high-quantity concrete.

Paclobutrazol 처리가 Perennial Ryegrass의 생육 및 고온과 건조 Stress에 미치는 영향 (Effect of Paclobutrazol on Growth, and High Temperature and Drought Stress in Perennial Ryegrass)

  • 김태일;구자형;원동찬
    • 아시안잔디학회지
    • /
    • 제3권1호
    • /
    • pp.24-33
    • /
    • 1989
  • This study was conducted to investigate the effect of paclobutrazol [(2 RS , 3 RS )1-(4- chlor-ophenyl )-4, 4- dimethyl -2- (1, 2, 4- triazol -1- yl )- pentan -3-01] on the tolerance of hi-gh temperature and drought stress as related to growth retardation , iranspiration rate , soil water content , nitrogen level and photosynthetic rate in perennial ryegrass ( Loliurn perenne L . ' Omega H , ). Plants were given a 30 ml soil drench of paclohutrazol at the concentrations of 0, 0.01, 0.1, 1.0, 10.. 0, mg / 6 .5cm- diameter pot . The rcsults were as follows : 1. Increasing concentrations of paclohutrazul reduced plant height , leaf area , fresh weight and dry weight , hut increased chlorophyll content per unit area . The number of tillers and leaf width were not affected hy the paclobutrazol concentrations . 2. The proper concentration of paclohatrazol on growth retardation in perennial ryegrass was about I mq /pot , hut leaf deformity and severe growth retardation were shown at high concentration of 10 mq / pot . 3. Perennial ryegrasses grown at 30˚C were shown significantly short plant height and low leaf nitrogen level compared with those grown at 20˚C. Increasing concentrations of paclohutrazol at 20˚C increased nitrogen level hut it could not increase nitrogen level at 30˚C . 4. During the drought stress , increasing temperatures significantly promoted transpiration rate and wilting time . It took about 5 days at 20˚C and 3 days at 30˚C to reach wilting time of leaves from water stress treatment . Soil water contents at wilting time of non-treated controls were averaged 6. 871% at 20˚C and 6. 17% at 30˚C 5. Paclohutrazol reduced transpiration rate at high temperature and drought stress . Wilting appeared at the lower water content of soil according to increasing concentrations of paclobutrazol at 30˚C hut there were no differences among concentrations of at 20˚C. 6.Paclohutrazol treatment at 1 rag /pot reduced injury rate of leaves from 67.1 % and 100 % in control plants to 15.7% and 80% at 20˚C and 3010, respectively. 7. Photosynthetic rate per unit area was significantly reduced at high temperature . Paclohutrazol stimulated photosynthetic rate with increase of concentrations at 20˚C but there was no increasing effect at 30˚C.

  • PDF

순환골재의 부착 모르타르량이 콘크리트의 특성에 미치는 영향 (Effect of the Amount of Attached Mortar of Recycled Aggregates on the Properties of Concrete)

  • 이원기;최종오;정용욱
    • 한국건설순환자원학회논문집
    • /
    • 제3권2호
    • /
    • pp.132-139
    • /
    • 2015
  • 본 연구는 파쇄처리 순환골재를 사용한 콘크리트의 특성을 검토하기 위하여 순환골재의 흡수율별 단위시멘트량 및 물시멘트비를 변화시켜 콘크리트의 특성에 미치는 영향을 검토하였다. 실험결과 물시멘트비가 높은 저강도 배합에서는 파쇄처리 순환골재를 사용한 콘크리트와 쇄석 콘크리트의 압축강도가 동등한 수준으로 나타나 순환골재의 부착모르타르 영향이 작은 것으로 나타났다. 그러나, 물시멘트비가 낮은 고강도 배합에서는 파쇄처리 순환골재를 사용한 콘크리트가 부착모르타르의 영향으로 쇄석을 사용한 콘크리트보다 약 40%의 압축강도저하를 나타내었다. 한편, 흡수율 7%인 순환골재의 건조수축량은 재령 10주에서 흡수율 1%인 쇄석의 $-310{\times}10^{-6}$보다 2배 증가된 $-700{\times}10^{-6}$을 나타내어 콘크리트용 골재로의 재활용시 건조수축에 대한 검토가 선행되어야 할 것으로 사료된다. 또한 단위시멘트량 $450kg/m^3$인 부배합 콘크리트의 압축강도는 흡수율 3%인 순환골재 사용시 쇄석 사용 콘크리트와 동등하게 나타난 반면, 흡수율 7%인 순환골재를 사용한 경우에는 쇄석 사용 콘크리트에 비해 약 7%정도 낮게 나타났다. 그러나, 단위시멘트량 $350kg/m^3$인 일반배합 콘크리트의 압축강도는 쇄석 사용 콘크리트에 비해 압축강도 저하가 현저하게 나타났다.

온도에 따른 사질토의 다짐 특성 (Temperature Effect on the Compaction Characteristic of Cohesionless Soil)

  • 이기철;지수빈;김호비;김동욱
    • 한국지반공학회논문집
    • /
    • 제32권2호
    • /
    • pp.53-62
    • /
    • 2016
  • 흙의 다짐 특성에 영향을 주는 주요인자 중 하나인 온도는 지역과 계절에 따라 다양하게 변화하는 특성을 가진다. 최근 동토지방에서 많은 토목공사가 시행되고 있지만, 온도와 관련된 흙의 다짐기준 및 지침을 정량화할 수 있는 문헌은 미비한 실정이다. 따라서 본 연구는 온도에 따른 흙의 다짐특성을 시험을 통해 평가하고자 하였다. 시험을 위해 러시아 시베리아, 캐나다 앨버타 주 오일 샌드 지역 등에서 자주 쓰이는 성토재료인 모래의 온도별 다짐특성을 나타낼 수 있는 주문진 모래를 사용하였으며, 표준다짐시험을 흙의 다양한 온도조건($-10^{\circ}C$에서 $17^{\circ}C$)에서 수행하였다. 시험 결과 영상 온도에서는 다짐 시 벌킹 효과로 인해 흙 공시체의 부피 팽창이 발생하였으며, 그 범위는 0%~6%이였다. $0^{\circ}C$에서 $17^{\circ}C$까지 온도가 증가하면서 최대 부피(최소 건조단위중량)에 해당하는 함수비는 감소하였고, 최소 부피(최대 건조단위중량)에 해당하는 함수비는 온도가 증가함에 따라 약간 증가하였다. 영하 온도의 경우 함수비가 추가됨에 따라 건조단위중량은 지속적으로 감소하였다. 영하 온도에서는 벌킹이 발생하지 않았으며 물의 단위부피보다 얼음의 단위부피가 더 크기 때문에 흙 공시체의 부피가 증가하였다.

Fire resistance and residual strength of reactive powder concrete Using metakaolin

  • Jang, Hongseok;Yi, Jebang;So, Seungyoung
    • Steel and Composite Structures
    • /
    • 재36권6호
    • /
    • pp.657-669
    • /
    • 2020
  • This study investigates the fire resistance characteristics of reactive powder concrete according to changes in the cement content per unit area, mixing ratio of metakaolin (MK), and content of polypropylene fiber. A fire test was conducted, and the resulting residual strength characteristics were investigated through flexural and compressive strength measurements, as well as condition rating classification based on visual evaluation. MK effectively reduced the initial high content of calcium hydroxide, thereby reducing the water vapor pressure generated during pyrolysis and slowing spalling. Furthermore, the pore structure and loose tissue were effective for relieving the water vapor pressure in the event of a fire.