  • In this study we measured the changes according to time respectively on the basis of 0, 30, 60 and 90 minutes, taking into consideration the decline in fluidity of concrete according to elapsed time to analyze manufacturing capability of batcher plant according to elapsed time of ready-mixed concrete manufactured in batcher plant, and offer basic data for mixture design of ultra-high strength concrete. The proportion of water-binder was 23.55, water content was 160kg/m3, proportion of replacement of crushed sand was 0, 20 and 40% at 3 level, and we applied to the same condition of triaxial component using blast furnace slag powder and silica fume as admixture. And to meet the demand of certain fluidity, we measured respectively on property before and after hardening of ultra-high strength concrete using superplasticizer. As a result of experiment, before hardening of ultra-high strength concrete showed the best fluidity in conditions of crushed sand replacement rates of 20% and superplasticizer composition of 1.95%, but it appeared that fluidity drops as time goes by in the same composition condition. And it appeared that when it comes to hardened, the changes of compression strength according to elapsed time by crushed sand replacement rates were within 1MPa. Therefore, it turned out that the difference of strength according to elapsed time was low and compression strength of 280dys in composition mentioned above appeared highly as 88MPa.

  • PDF

Numerical study on axially loaded ultra-high strength concrete-filled dual steel columns

  • Pons, David;Espinos, Ana;Albero, Vicente;Romero, Manuel L.
    • Steel and Composite Structures
    • /
    • 제26권6호
    • /
    • pp.705-717
    • /
    • 2018
  • This paper presents a numerical investigation on the mechanical performance of concrete-filled dual steel tubular columns of circular section subjected to concentric axial load. A three-dimensional numerical model is developed and validated against a series of experimental tests. A good agreement is obtained between the experimental and numerical results, both in the peak load value and in the ascending and descending branches of the load-displacement curves. By means of the numerical model, a parametric study is carried out to investigate the influence of the main parameters that determine the axial capacity of double-tube columns, such as the member slenderness, inner and outer steel tube thicknesses and the concrete grade - of both the outer concrete ring and inner core -, including ultra-high strength concrete. A total number of 163 numerical simulations are carried out, by combining the different parameters. Specific indexes are defined (Strength Index, Concrete-Steel Contribution Ratio, Inner Concrete Contribution Ratio) to help rating the relative mechanical performance of dual steel tubular columns as compared to conventional concrete-filled steel tubular columns, and practical design recommendations are subsequently given.

Axial behavior of FRP-wrapped circular ultra-high performance concrete specimens

  • Guler, Soner
    • Structural Engineering and Mechanics
    • /
    • 제50권6호
    • /
    • pp.709-722
    • /
    • 2014
  • Ultra-High Performance Concrete (UHPC) is an innovative new material that, in comparison to conventional concretes, has high compressive strength and excellent ductility properties achieved through the addition of randomly dispersed short fibers to the concrete mix. This study presents the results of an experimental investigation on the behavior of axially loaded UHPC short circular columns wrapped with Carbon-FRP (CFRP), Glass-FRP (GFRP), and Aramid-FRP (AFRP) sheets. Six plain and 36 different types of FRP-wrapped UHPC columns with a diameter of 100 mm and a length of 200 mm were tested under monotonic axial compression. To predict the ultimate strength of the FRP-wrapped UHPC columns, a simple confinement model is presented and compared with four selected confinement models from the literature that have been developed for low and normal strength concrete columns. The results show that the FRP sheets can significantly enhance the ultimate strength and strain capacity of the UHPC columns. The average greatest increase in the ultimate strength and strain for the CFRP- and GFRP-wrapped UHPC columns was 48% and 128%, respectively, compared to that of their unconfined counterparts. All the selected confinement models overestimated the ultimate strength of the FRP-wrapped UHPC columns.

Research on eccentric compression of ultra-high performance fiber reinforced concrete columns

  • Ma, Kaize;Ma, Yudong;Liu, Boquan
    • Structural Engineering and Mechanics
    • /
    • 제71권3호
    • /
    • pp.211-221
    • /
    • 2019
  • To study the eccentric compression behavior of ultra-high performance fiber reinforced concrete (UHPFRC) columns, six UHPFRC columns and one high-strength concrete (HSC) column were tested. Variation parameters include load eccentricity, volume of steel fibers and stirrup ratio. The crack pattern, failure mode, bearing capacity, and deformation of the specimens were studied. The results showed that the UHPFRC columns had different failure modes. The large eccentric compression failure mode was the longitudinal tensile reinforcements yielded and many horizontal cracks appeared in the tension zone. The small eccentric compression failure mode was the longitudinal compressive reinforcements yielded and vertical cracks appeared in the compressive zone. Because of the bridging effect of steel fibers, the number of cracks significantly increased, and the width of cracks decreased. The load-deflection curves of the UHPFRC columns showed gradually descending without sudden dropping, indicating that the specimens had better deformation. The finite element (FE) analysis was performed to stimulate the damage process of the specimens with monotonic loading. The concrete damaged plasticity (CDP) model was adopted to characterize the behaviour of UHPFRC. The contribution of the UHPFRC tensile strength was considered in the bearing capacity, and the theoretical calculation formulas were derived. The theoretical calculation results were consistent with the test results. This research can provide the experimental and theoretical basis for UHPFRC columns in engineering applications.

Constitutive property behavior of an ultra-high-performance concrete with and without steel fibers

  • Williams, E.M.;Graham, S.S.;Akers, S.A.;Reed, P.A.;Rushing, T.S.
    • Computers and Concrete
    • /
    • 제7권2호
    • /
    • pp.191-202
    • /
    • 2010
  • A laboratory investigation was conducted to characterize the constitutive property behavior of Cor-Tuf, an ultra-high-performance composite concrete. Mechanical property tests (hydrostatic compression, unconfined compression (UC), triaxial compression (TXC), unconfined direct pull (DP), uniaxial strain, and uniaxial-strain-load/constant-volumetric-strain tests) were performed on specimens prepared from concrete mixtures with and without steel fibers. From the UC and TXC test results, compression failure surfaces were developed for both sets of specimens. Both failure surfaces exhibited a continuous increase in maximum principal stress difference with increasing confining stress. The DP tests results determined the unconfined tensile strengths of the two mixtures. The tensile strength of each mixture was less than the generally assumed tensile strength for conventional strength concrete, which is 10 percent of the unconfined compressive strength. Both concretes behaved similarly, but Cor-Tuf with steel fibers exhibited slightly greater strength with increased confining pressure, and Cor-Tuf without steel fibers displayed slightly greater compressibility.

강섬유 혼입율 및 형상비가 초고강도 콘크리트의 역학적 성질에 미치는 영향 (The Effects of Mixture Rate and Aspect Ratio of Steel Fiber on Mechanical Properties of Ultra High Performance Concrete)

  • 최중구;이건철;고경택
    • 한국건설순환자원학회논문집
    • /
    • 제5권1호
    • /
    • pp.14-20
    • /
    • 2017
  • UHPC는 초고층 건물 및 초장대교의 경우 필연적으로 사용되어진다. 일반적으로 콘크리트는 압축강도보다 낮은 휨강도 및 인장강도를 가지므로 취성균열이 발생하여 에너지 흡수능력이 저하된다. 이러한 문제를 해결하기 위해 본 연구에서는 강섬유의 혼입율과 형상비가 UHPC의 기계적 물성에 미치는 영향을 조사하고자한다. 시리즈 I에서, 20mm 직선형 강섬유가 0, 1.0, 1.3, 1.5 및 2.0%의 혼입율로 첨가되었다. 시리즈 II에서는 16mm 강섬유를 0, 1, 1.5%로 혼입한 후 형상비에 따라 역학적 성질을 조사하였다. 실험결과, 압축강도의 차이는 미비했다. 하지만 휨강도 및 인장강도와 관련하여 혼입율 및 형상비가 증가함에 따라 휨성능 및 인장성능이 개선되었다.

패턴 디자인이 적용된 LEFC 시제품 제작 및 현장적용 (Prototyping and Field Application of Light Emotion Friendly Concrete with Pattern Design)

  • 서승훈;김수연;김병일
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2019년도 춘계 학술논문 발표대회
    • /
    • pp.203-204
    • /
    • 2019
  • Recently, exposed concrete designs have been placed everywhere due to increased interest in indoor residential environments. In addition, in order to overcome the disadvantages of litracon, which was developed by mixing optical fiber, LEFC(Light Emotion Friendly Concrete) was developed in Korea, which improved unit price and constructivity by inserting hard acrylic rods. LEFC, using foaming agent and lightweight aggregate for light weighting, has disadvantages that decrease mechanical properties, and thus improved mechanical properties by using ultra-high performance concrete. Also, due to the characteristics of UHPC materials, it showed excellent self-consolidating performance. Considering these characteristics, a LEFC mold with pattern design was developed. The LEFC blocks were built so that pattern shapes could be seen and these were applied on-site to Sewoon plaza, located in Seoul.

  • PDF

Strength Characteristics of Ultra High Performance Concrete at early age

  • Kim, Sung-Wook;Park, Jung-Jun;Ryu, Guem-Sung;Koh, Kyoung-Taek;Hong, Ki-Nam
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2009년도 춘계 학술대회 제21권1호
    • /
    • pp.563-564
    • /
    • 2009
  • Ultra-High Performance Concrete (UHPC) compared to normal concrete is exhibiting extremely high strength characteristics with compressive strength and tensile strength reaching 200MPa and 15MPa, respectively. The mechanical characteristics of UHPC can be thus exploited advantageously in the construction of structure through the reduction of the cross-sectional area and fabrication of slim and light-weight of the structural members. In the case where the structural member is made of UHPC, the occurrence of crack can be prevented by releasing the restraint provided by the form in due time. This research performs parametric study of the failure characteristics of concrete such as failure energy and softening curve suggested by the viscous crack model approximating the failure of concrete. The scope of this research contains the results of tests performed to investigate the strength of UHPC during early elapsed time.

  • PDF