• Title/Summary/Keyword: Tribology test

Search Result 676, Processing Time 0.028 seconds

The Change of Sliding wear properties of Carbon Steel against several hardened steels (미끄럼 접촉을 하는 탄소강의 경도차 조합에 따른 마모특성변화 연구)

  • Lee Han Yeong;Kim Geun Yeong
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.85-90
    • /
    • 2003
  • Although wear resistance of material improves with increasing its hardness, it is known that the wear resistance of steel is varied with hardness of counter material. In this context, wear properties of steel must be depended on the difference of hardness between the testpiece and the counter material. In this study, using the pin-on-disc type wear machine, annealed carbon steels were tested against ahoy tool steels with various levels of hardness. Then the changes of wear properties of carbon steel according to the hardness of counter material were investigated and the morphology of worn surface after test were evaluated. The results indicate that if there are no remarkable difference of hardness between them, wear resistance of carbon steel in running-in wear decreases with increasing the hardness of counter material. However, its wear properties at the range of high sliding speed have no relation with hardness of counter material. It is clear that wear properties is influenced by the formation of oxide of steel on their worn surface during wear.

  • PDF

내저온열화 특성을 갖는 지르코니아/알루미나 복합세라믹의 마멸평가

  • Kim H.;Lee KY;Kim DJ;Lee MH;Seo WS
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.91-94
    • /
    • 2003
  • Ceramic femoral heads in the total hip replacement have been developed to reduce the polyethylene liner wear. Alumina and zirconia (3Y-TZP) are using in clinical application worldwide and there are many good test reports. However, alumina has a risk of catastrophic failure, and zirconia has the low temperature degradation in spite of enhanced fracture toughness. Recently, novel zirconia/alumina composite having low temperature degradation-free character and high fracture tough . was developed and it leads the lower wear 3f polyethylene than alumina and zirconia. In the present study, in order to optimise the microstructure of low temperature degradation (LTD)-free zirconia/alumina composite for the best wear resistance of polyethylene, various compositions of (LTD)-free zirconia/alumina composites were fabricated, and the sliding wear of UHMWPE against these novel composites were examined and compared with that against alumina and zirconia ceramics used for total hip joint heads.

  • PDF

A Study On the Application of VHVI Base Oil - Hydraulic Fluid for Construction Equipments (VHVI 기유의 제품 적용 기술에 관한 연구 - 건설 중장비용 유압유)

  • Kwon W.S.;MOON W.S.;Yoon H.H.;Kim K.W.
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.152-157
    • /
    • 2003
  • This study represents the newly advanced formulation of hydraulic fluids for extended drain interval and introduces the performance results of used oil samples from various excavators. The used oil samples, in this paper show that there is a sharp change in viscosity drop and moderate additive depletion when viscosity index of hydraulic oil is very high. For the extension of hydraulic fluid life, it is necessary to improve the stability of viscosity and oxidation. New target properties from the used oil analysis were proposed for extended life. Performance of newly developed hydraulic oil based on used oil analysis is compared with previously used one. The properties of new formulation are the viscosity index of 140 and improved thermal stability consists of VHVI base oil. Field test results showed the possibility of extension of fluid life. Additionally, for development of high performance product, new required properties and performances were discussed.

  • PDF

A Study on the Wear Characteristics of Bearing According to its Material in Scroll Compressor (스크롤 압축기의 크랭크 샤프트의 베어링 재질에 따른 마모특성에 관한 실험적 연구)

  • Sung, Chi-Un;Park, Young-Do;Hwang, Yu-Jin;Back, Gee-Dae;An, Sung-Young;Lee, Jae-Keun
    • Proceedings of the SAREK Conference
    • /
    • 2008.06a
    • /
    • pp.194-202
    • /
    • 2008
  • In this study, we investigated the tribology behaviour of two different bearing materials. One of these alloys content is Cu(90)-Sn(10) alloy and is widely used in the automotive industry.The other is Al alloy. This bearing content is Al-Sn-Si-Cu. Therefore, it is required to study on the lublicating characteristics of bearing according to different materials. In this study, compressor bearings made by respectively "PTFE solid lubricant" and "AI alloy with superior load carrying capacity, rubbing and impact endurance", have gone through journal bearing test. Lubrication and abrasion characteristics are evaluated by analyzing the material characteristics of a scroll compressor bearing bush. The AI alloy bearing showed the most excellent lubrication and abrasion characteristics than Cu-Sn alloy under high load condition.

  • PDF

Tribological Behavior Analysis of CrMoN Coating by XPS (XPS 분석을 통한 CrMoN 코팅의 마찰마모 거동 연구)

  • Yang, Young-Hwan;Lyo, In-Woong;Park, Sang-Jin;Lim, Dea-soon;Oh, Yoon-Suk
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.8
    • /
    • pp.549-556
    • /
    • 2012
  • The tribological behavior of CrMoN films with respect to surface chemistry was investigated by using X-ray photoelectron spectroscopy (XPS). All of the films were prepared from a hybrid PVD system consisting of DC unbalanced magnetron (UBM) sputtering and arc ion plating (AIP) sources. The tribological property of the films was evaluated by a friction coefficient using a Ball-on-disk type tribometer. The chemistry of wear track was analyzed by energy dispersive spectroscopy (EDS) and XPS. The friction coefficient was measured to be 0.4 for the CrMoN film, which is lower than that of a monolithic CrN film. EDS and XPS results imply the formation of an oxide layer on the coating surface, which was identified as molybdenum oxide phases, known to be a solid lubricant during the wear test.

Tribological Characteristics of Sliding Contact between Deferent Combinations of Ceramics (미끄럼 접촉시 이종세라믹 간의 트라이볼로지적 특성)

  • Kim Bupmin;Kim Seock-sam;Shin Dongwoo;Yoon Sang-bo
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2004.11a
    • /
    • pp.296-300
    • /
    • 2004
  • Currently. the study on structural ceramic helps to suggest the precise data of friction and wear in accordance with the various conditions in operations. Also, the study helps to predict effective operating conditions by monitoring the occurrence of wear transition. The studies in the Past were mainly concentrated in using identical materials. However, it is highly likely to have unqualified data from the differences of mechanical and chemical properties between ceramic materials. Thus, in this study, through conducting the ball-on-disk type wear testing, the different ceramic materials has been used to consider tribological characteristics between different ceramic materials. We conducted the wear test by using three kinds of specimen which are zirconia, alumina and silicon carbide against zirconia. We have changed the sliding velocity and the loading conditions in this test and found out that there is row friction coefficient and wear rate in the combination of zirconia and silicon carbide.

  • PDF

A Study on Corrosive Wear Characteristics and the Mechanism of Austempered Low-Alloy Ductile Iron (오스템퍼링 한 저합금구상흑연주철의 부식마멸특성 및 그 기구에 관한 연구)

  • 박흥식;진동규
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.6
    • /
    • pp.1404-1411
    • /
    • 1993
  • This study was undertaken to investigate the corrosive wear charateristics upon various transformation condition of austempered low-alloy ductile cast iron in corrosive environments against mating specimen made of the hardened SM45C. The corrosive wear test was carried out by rubbing the annular surface of two test pieces in distilled water and aqueous solution at constant sliding speed of 0.5m/s. In severe wear region, the corrosive wear rate Wc increased hastily with NaCl concentration owing to intermetallic adhesion but Wc went down slowly in mild wear region due to lubricating effect of the corrosion product. The critical sliding distance decreased with increasing NaCl concentration due to increased generation rate of the corrosion product and the specific corrosive wear rate has maximum in 1% NaCl aqueous solution at mild wear region. With the variation of matrix, the corrosive wear resistance of the fine acicular bainite was higher than that of coarse upper bainite because of reducing the local cell reaction by carbides. A growth in volume fraction of retained austenite in matrix increased the Wc due to soften surface, but has a declining tendency of Wc in mild wear region.

금속중간층을 이용한 나노결정질 다이아몬드 박막 코팅

  • Na, Bong-Gwon;Myeong, Jae-U;Gang, Chan-Hyeong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.99-99
    • /
    • 2013
  • 나노결정질 다이아몬드(Nanocrystalline Diamond: NCD) 박막은 고경도와 낮은 마찰계수를 가지고 있어 초경합금이나 고속도강과 같은 절삭공구 위에 코팅하여 공구의 성능 향상을 도모하려는 노력이 있어 왔다. 그러나 NCD 박막의 잔류응력이 크고, 초경합금과 철계 금속에 NCD가 증착되지 않는다는 문제점이 있다. 따라서 잔류응력 완화와 다이아몬드 핵생성을 위하여 제3의 중간층 재료가 필요하다. 본 연구에서는 W과 Ti을 중간층으로 하여 초경합금(WC-Co)과 고속도강(SKH51)에 NCD 박막을 코팅하고 기계적 특성을 비교하였다. 초경합금 또는 고속도강기판 위에 W 또는 Ti 중간층을 DC magnetron sputter를 이용해 각 1 ${\mu}m$의 두께로 증착하고 그 위에 MPCVD (Microwave Plasma Chemical Vapor Deposition)를 이용해 NCD 박막을 2${\mu}m$의 두께로 코팅하였다. FESEM을 이용하여 표면과 단면의 형상을 관찰하였고, XRD와 Raman spectroscopy를 통해 NCD 박막의 결정성을 확인하였다. 그리고 tribology test를 실시하여 코팅된 박막의 내마모성을 비교하였으며, Rockwell C indentation test를 이용하여 밀착력을 비교하였다. 초경합금에 적용 시, W이 Ti보다 중간층으로서 더 우수한 것으로 나타났으며 이는 열팽창계수 차이에 의한 잔류응력의 차이에 의한 것으로 여겨진다. 중간층 두께에 따른 박막의 기계적 특성 변화를 알아보기 위해 W 중간층의 두께를 1, 2, 4 ${\mu}m$로 변화를 주었다. 중간층 두께가 2 ${\mu}m$ 이상일 때 박막의 밀착력이 증가되는 것으로 나타났다. 고속도강 위에 같은 방법으로 1 ${\mu}m$의 W 또는 Ti 중간층 위에 2 ${\mu}m$의 NCD 박막을 코팅한 시편들은 초경합금에 코팅한 것과 달리 두 시편 모두 낮은 밀착력을 나타내었다. 열팽창계수 차이에 의한 잔류응력을 완화하기 위해 고속도강에 W/Ti 복합박막을 중간층으로 Ti, W순으로 각각 1 ${\mu}m$ 두께로 증착 후 그 위에 NCD 박막을 2 ${\mu}m$ 두께로 코팅 한 후 특성을 비교하였다. Ti/W 복합 중간층 위에 코팅된 NCD 박막의 밀착력이 W 혹은 Ti 단일 중간층에 코팅된 박막에 비해 우수한 것으로 나타났다. 그러나 실제 공구에 적용하기에는 박막의 밀착력 개선이 요구되며 이를 위해서 더 연구가 필요하다.

  • PDF

Effects of Oil Inlet Pressure and Temperature on the Dynamic Behaviors of a Full-Floating Ring Bearing Supported Turbocharger Rotor (터보차저 공급 오일 압력과 온도가 풀-플로팅 베어링의 동적 거동에 미치는 영향)

  • Lee, In-Beom;Hong, Seong-Ki
    • The KSFM Journal of Fluid Machinery
    • /
    • v.20 no.2
    • /
    • pp.53-62
    • /
    • 2017
  • In this paper, the effect of oil conditions in rotor dynamic behaviors of a FFRB (Fully-Floating Ring Bearing) is investigated. Through the characteristic of a FFRB has two films, it has several advantages such as less friction loss and better stability over a wide speed range. However, it is difficult to supply a oil to the inner film. Thus, turbocharger makers have been paid significant attention to the lubrication of a FFRB because of its importance. This work focuses on the influence of oil inlet pressure and temperature. The methodologies of computational simulation and experimental test were used to estimate the rotor dynamic behaviors. In experimental test, the single-scroll turbocharger for the 1.4L diesel engine was used. The results show that the oil inlet pressure and temperature will place considerable influence on the rotor response. Oil conditions affect RSR (Ring Speed Ratio) which is cause of sub-synchronous vibrations, which also cause of oil whirling and whip even a critical speed. At higher speed range, the phenomenon of self-excited vibrations which is cause of instability of fluid whirl is investigated through the orbit shapes that consist of small orbit and large amplitude orbit. It is shown that some performance of a FFRB can be controlled by the conditions of oil supply. Finally, it was revealed that the oil induced operating conditions will strongly affect the turbocharger rotor dynamics behaviors.

Effects of Multi-walled Carbon Nanotubes on Electrical and Wear Characteristics of High Impact Polystyrene Composites (HIPS 복합재의 전기적 및 마모 특성에 미치는 다중벽 탄소나노튜브의 영향)

  • Jeong, Yeon-Woo;Kim, Kyung-Shik;Lee, Hyun-Woo;Jeong, Man-Woo;Lee, Jae-Hyeok;Kim, Jae-Hyun;Lee, Hak-Joo;Kim, Kwang-Seop
    • Tribology and Lubricants
    • /
    • v.31 no.3
    • /
    • pp.95-101
    • /
    • 2015
  • Carbon nanotubes (CNTs) are widely used in polymer composites as filler materials to enhance various characteristics of the composites because of their remarkable mechanical, electrical, and thermal properties. In this study, we investigate the effects of MWCNTs on the electrical and wear characteristics of high-impact polystyrene (HIPS) composites, and compare the results with the effects of carbon black (CB). The HIPS composites are classified as Bare-HIPS, MWCNT-HIPS composites containing 2, 3, 4, and 5 wt% MWCNTs, and CB-HIPS containing 17 wt% CB. Electrical characteristics are evaluated by measuring the surface resistance using a 4-point probe. Wear characteristics are evaluated using the reciprocating wear test, and a chrome steel ball with a curvature of 6.3 mm is used as the counterpart. The results show that the addition of MWCNTs or CB can improve the electrical and wear characteristics of HIPS composites. In the case of MWCNT-HIPS composites, surface resistance, friction coefficient, and specific wear rate decrease as the concentrations of MWCNTs increase. Moreover, the addition of MWCNTs is more effective in improving the electrical and wear characteristics of HIPS composites compared to the addition of CB. To fabricate the HIPS composite with appropriate electrical and wear characteristics, more than 4 wt% MWCNTs is added to HIPS.