• Title/Summary/Keyword: TiN 코팅강

Search Result 27, Processing Time 0.025 seconds

A Study on the High Speed Characteristics of Plastic Mould Steel using Ball End Mill AlTiN Coated Layers (볼 엔드밀 AlTiN코팅 층수에 따른 플라스틱금형강의 고속가공에 관한 연구)

  • Lee, Seung-Chul;Cho, Gyu-Jin
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.9 no.1
    • /
    • pp.81-86
    • /
    • 2010
  • This paper investigated into process characteristics of AlTiN coated layers for machining to the direction of upper and lower in plastic mold material (KP-4) with the cemented carbide ball endmill with the diameter of 8mm coated AlTiN layers (1~4) step by step using machining center. The material used in experiments was KP-4 that was machined by three types of inclined angles; $15^{\circ}$, $30^{\circ}$ and $45^{\circ}$ As estimated mechanical properties of AlTiN coated layers, it was shown the most result in the condition of three layered coating that the coating that the coating depth, the hardness of the coated layer and the surface roughness of the coated layer were $13{\mu}m$, Hv 3027.3 and $0.042{\mu}m$, respectively. The cutting component was better at the condition of upper direction than that of lower direction in all experimental conditions and indicated to be less which the bigger angle of the material was increased the effective diameter of the tool.

Comparative Study on Effect of the Surface Characteristics of the SKH51 and SKD11 Steels with Deposition Times by AIP-TiN Coating (AIP-TiN 코팅에서 증착시간이 SKH51과 SKD11 강의 표면특성에 미치는 영향에 관한 비교 연구)

  • Kim, Hae-Ji;Kim, Nam-Kyung
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.7 no.1
    • /
    • pp.67-74
    • /
    • 2008
  • In this paper, the surface characteristics of the AIP-TiN coated of the SKH51 and SKD11 steels under various deposition times are presented with emphasis on the comparison of the two materials. The micro-particle, the surface roughness, the micro-hardness, the coated layer thickness, the atomic distribution of Ti, N and Fe elements and the adhesion are measured for various deposition times. It has been shown that the micro-particle, the surface roughness, the coated layer thickness and the atomic distribution of Ti, N and Fe elements are similar for the two cases regardless of the test deposition time from 10 to 180 minutes. However, it has been shown that the micro-hardness and the adhesion of the SKH51 steel are higher than the SKD11 steel, indicating that they are much affected by the hardness of the material to be coated.

  • PDF

Effect of additional gases on the Color of TixN Coated Film (TixN Coating층의 색상에 미치는 첨가원소의 영향)

  • 김학동;조성석
    • Journal of the Korean Vacuum Society
    • /
    • v.7 no.2
    • /
    • pp.127-134
    • /
    • 1998
  • Stainless steel is being used widely for various purposes due to its good corrosion resistance. There has been much research to produce a colored and corrosion-resistant stainless steel by several methods to use in decorating. In this experiment, we coated TiN(C,O,H)films on the SUS304 substrates with the DC magnetron sputtering system and then studied the texture and color of the films as a function of additional gases being inserted into the system. A (220) texture of TixN film changed to (200) by the addition of either hydrogen or the acetylene and changed further to (111) with an increase of the additional acetylene content. The addition of oxygen gas changed from the texture(220) to (111) to (200). The color of the TixN film changed from gold to gray to green with the increase of the content by the addition of oxygen gas, while it changed to pink and finally to gray with the increased of the content by the addition of acetylene gas. Reflectance increased in the region of short wavelength by the addition of hydrogen, but decreased with the increase of the oxygen and the acetylene content.

  • PDF

Heat and Surface treatments for the Longevity of Prehardened Steels (사출금형용 프리하든 강의 수명 향상 기술)

  • Kim, Sung Wan;Moon, Kyoung Il;Kim, Sang Gweon;Cho, Yong Ki
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.18 no.6
    • /
    • pp.383-393
    • /
    • 2005
  • 본 고에서는 사출금형소재로 널리 사용되는 프리하든 강의 수명을 극대화 시킬 수 있는 열 표면처리 기술에 대해 소개하였다. 이러한 열 표면처리 기술 및 기술 적용시 고려해야할 점을 다시 정리해 보면, 제조하는 대상물을 고려한 최적 금형 재료의 선택 (표 1~3) 선택된 금형의 물성을 최적으로 구현할 수 있는 열처리 선택 (표 4) 금형의 사용 환경을 고려한 최적 열 표면처리 선택 (표 5) 질화 열처리에 의한 수명 향상 피로 수명이 중요한 경우 : 질화층 $100{\mu}m$이내 열간 내마모성, 크립저항성이 요구되는 경우 : 질화층 $300{\sim}400{\mu}m$ TiN, CrN 등 세라믹 코팅에 의한 성능 향상 내식성 중요시 CrN, DLC의 적용 내마모성 및 초저마찰계수의 구현 : 방향성 코팅, 나노구조화 금형의 국제경쟁력을 향상시키기 위해서는 고품위 금형 제조 기술이 필요하고 이를 위하여, 표면개질처리가 필수불가결하다는 것이다. 또한, 열 표면처리에는 각각의 특징이 있고, 적용 상황의 미묘한 차이에 따라 특성이 바뀌기 때문에 고품위, 품질 금형을 얻고자 하면 어느 때보다 사용자, 금형기술자, 열 열 표면처리 기술자들과의 협력이 요구된다.

A Study on the friction and Wear Characteristics of C-N Coated SCM415 Steel (C-N코팅 SCM415강의 마찰$\cdot$마모 특성에 관한 연구)

  • Lyu Sung-ki;Lu Long;Jin Tai-yu;Lian Zhe-Man;Cao Xing-Jin;Cho Sung-Min
    • Journal of the Korean Society of Safety
    • /
    • v.20 no.1 s.69
    • /
    • pp.18-23
    • /
    • 2005
  • This study deals with the friction and wear characteristics of C-N coated SCM415 steel. The PSII(plasma source ion implantation) apparatus was built and a SCM415 test piece with steel substrate was treated with carbon nitrogen by this apparatus. The composition and structure of the surface layer were analyzed and compared with that of PVD(physical vapor decomposition) coated TiN layer. It was found that both of friction coefficient of C-N coating and TiN coating decreased with increasing load, however, C-N coating showed relatively lower faction coefficient than that of TiN coating. The micro-vickers hardness of C-N film is 3200 Hv, which is $32\~43\%$ higher than that of TiN film. The critical load of C-N film is 52N, which is $25\%$ higher than that of TiN film. The hardness of C-N film fabricated by Plasma ion implantation is $61\~70\%$ higher than that of base material, and faction coefficient is $14\~50\%$ lower than that of base material. It is also interesting to note that the friction was changed from adhesive wear mode to light oxidizing wear mode.

Joining properties and thermal cycling reliability of the Si die-attached joint with Zn-Sn-based high-temperature lead-free solders (Zn-Sn계 고온용 무연솔더를 이용한 Si다이접합부의 접합특성 및 열피로특성)

  • Kim, Seong-Jun;Kim, Keun-Soo;Suganuma, Katsuaki
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.72-72
    • /
    • 2009
  • 전자부품의 내부접속 및 파워반도체의 다이본딩과 같은 1차실장에는 고온환경에서의 사용과 2차실장에서의 재용융방지를 위해 높은 액상선온도 및 고상선온도를 필요로 하여, Pb-5wt%Sn, Pb-2.5wt%Ag로 대표되는 납성분 85%이상의 고온솔더가 널리 사용되고 있다. 생태계와 인체에 대한 납의 유해성이 보고된 이래, 무연솔더에 대한 연구가 활발히 진행되어 왔으나, Sn-Ag-Cu계로 대표되는 Sn계 합금으로 대체 중인 중온용 솔더와는 달리, 고온용 솔더에 대해서는 대체합금에 대한 연구가 미흡한 실정이다. 대체재의 부재로 인해 기존의 납을 다량함유한 솔더로 1차실장이 지속됨으로서, 2차실장의 무연화에도 불구하고 전자부품 및 기기의 재활용에 큰 어려움을 겪고 있다. 지금까지 고온용 무연솔더로서는 융점에 근거해 Au-(Sn, Ge, Si)계, Bi-Ag계, Zn-(Al, Sn)계의 극히 제한된 합금계만이 보고되어 왔다. Au계 솔더는 현재 플럭스를 사용하지 않는 광학, 디스플레이 분야 등 고부가가치 공정에 사용되고 있으나, 합금가격이 매우 비싸며 가공성이 나빠 대체재료로서는 적합하지 않다. Bi-Ag계 솔더 또한 취성합금으로 와이어 및 박판으로 가공하는데 어려움이 크며, 솔더로서 중요한 특성중 하나인 전기전도도 및 열전도도가 나쁜 편이다. 이에 비해, Zn계 합금은 비교적 낮은 합금가격, 적절한 가공성과 뛰어난 인장강도, 우수한 전기전도도 및 열전도도를 지녀, 고온용솔더 대체재료의 유력한 후보로 생각된다.이전 연구에서, 필자의 연구그룹은 Zn-Sn계 합금을 고온용 무연솔더로서 제안한 바 있다. Zn-Sn계 합금은 충분히 높은 융점과 함께, 금속간화합물이 없는 미세조직, 우수한 기계적 특성, 높은 전기전도도 및 열전도도 등의 장점을 나타내었다. 본 연구에서는 기초합금특성상 고온솔더로서 다양한 장점을 지닌 Zn-30wt%Sn합금을 고온용 솔더의 대표적인 적용의 하나인 다이본딩에 적용하여, 접합부의 강도 및 미세조직, 열피로 신뢰성에 대해 분석을 함으로서 실제 공정에의 적용가능성에 대해 검토하였다. Zn-30wt%Sn을 이용해 Au/TiN(Titanium nitride) 코팅한 Si다이를 AlN-DBC(aluminum nitride-direct bonded copper)기판에 접합한 결과, 양측에 완전히 젖은 기공이 없는 양호한 다이접합부를 얻었으며, 솔더내부에는 금속간화합물을 형성하지 않았다. Si다이와의 계면에는 TiN만이 존재하였으며, Cu와의 계면에는 Cu로부터 $Cu_5Zn_8,\;CuZn_5$의 반응층을 형성하였다. 온도사이클시험을 통한 열피로특성평가에서, Zn-30wt%Sn를 이용한 다이접합부는 1500사이클 지점에서 Cu와 Cu-Zn금속간화합물의 사이에서 피로균열이 형성되며, 접합강도가 크게 감소하였다. 열피로특성 향상을 위해 Cu표면에 TiN코팅을 하여 Zn-30wt%Sn 솔더로 다이접합한 결과, Si다이와 기판 양측에 TiN만으로 구성된 계면을 형성하였으며, TEM관찰을 통해 Zn-30wt%Sn과 극히 미세한 접합계면이 형성하고 있음을 확인하였다. Zn-wt%30Sn솔더와 TiN층의 병용으로 2000사이클까지 미세조직의 변화 및 강도저하가 없는 극히 안정된 고신뢰성의 다이접합부를 얻을 수가 있었다.

  • PDF

Diamond 박막의 밀찰력 향상에 대한 연구

  • 이건환;이철룡;권식철
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 1999.07a
    • /
    • pp.139-139
    • /
    • 1999
  • 다이아몬드는 지구상에서 가장 단단한 물질로 잘 알려져 있을 뿐만 아니라 공업적 측면에서 볼 때, 여러 가지 특출한 성질들을 동시에 지니고 있다. 인장강도, 압축강도, 탄성계수 등 기계적 특성이 우수하고 넓은 광투과성과 내열, 내화학, 내방사성을 지니고 있으며, 열전도율이 높고 전기적으로 절연체이다. 또한 hole이동도가 높고 도핑에 의해서 반도체적 특성을 나타낸다. 이와 같이 매우 뛰어난 성질을 공업적으로 응용하기 위하여 이전부터 많은 연구가 행해져 왔으며, 1980년대에 들어와 박막이나 코팅 형태로의 합성이 가능한 기상합성법이 큰 발전을 보임으로써 다이아몬드의 우수한 특성을 여러 분야에서 폭넓게 응용할 수 있게 되었다. 특히 마찰 응용분야에 최적의 재료로 추천되고 있다. 지금도 Epitaxial 다이이몬드를 기지 위에 성장시키고 다결정질박막을 여러 가지 비다이아몬드(Si, W, Mo 등) 기지 위에 성장시키는 연구가 계속되고 있으며 공구강 위엥 경질코팅으로써 한층 개선된 다이아몬드박막 제조를 위한 수많은 연구노력들이 집중되고 있다. 그러나 일반탄소강에 다이아몬드박막을 성장시키기 위한 많은 노력들은 크게 바람직하지 않은 non-diamond carbon(black carbon or graphitic soot)의 형성 때문에 방해를 받고 있다. 계면에서 이들의 형성은 증착된 다이아몬드박막과 금속기지의 저조한 밀착력을 나타내게 된다. 이외 같이 다이아몬드박막의 응용을 위하여 다이아몬드피막에 요구되는 중요한 조건은 기지에 대해서 강한 밀착력을 나타내는 것이며, 동시에 상대물에 대하여 낮은 마찰계수를 가져야 한다. 그러나 다이아몬드와 금속기지는 서로 다른 열챙창계수(각각 0.87$\times$10-6K-1, 12$\times$10-6K-1)의 차이로 인하여 밀착력이 현저히 떨어진다는 단점으로 인해 산업화에 많은 제약을 받아왔다. 이러한 문제점을 해결하기 위하여 본 연구에서는 다이아몬드박막과 금속기지 사이에 중간층을 이용하는 방법을 제안하였다. 이러한 시도는 일반적으로 중간층 형성 금속인 Ti 또는 TiN 등이 적용되었으나 원하는 결과를 얻지 못하였다. 즉 carbon과 Fe의 상호확산, non-diamond carbon상의 형성 그리고 열잔류응력을 완화시키고 일반탄소강 위에 다이아몬드박막을 형성시켜 우수한 밀착력을 얻기 위한 목적에 미흡하였던 것이다. 이에 중간층으로 Cr 또는 Cr계 화합물 박막을 이용하였는 바, 이 중간층을 이용한 결과 우수한 밀착력을 나타내는 다이아몬드박막을 얻었으며 열적, 구조저으로 모재와 다이아몬드에 적합한 결과를 얻을 수 있었다. 본 연구에 의해 얻어진 결과들은 재료 가공을 위하여 높은 경도와 내마모성등이 요구되는 절삭공구나 금형의 수명 향항에 크게 기여할 것이며 산업적으로 큰 응용이 기대된다.

  • PDF