• Title/Summary/Keyword: Ti-Nb

Search Result 1,190, Processing Time 0.021 seconds

Microstructure and Mechanical Properties of $Ti_3Al-Nb$ Alloys and TiB(Ti-25Al-11Nb) Metal Matrix Composite Fabricated by Spark Plasma Sintering Process (방전플라즈마 소결법으로 제작된 $Ti_3Al-Nb$ 합금 및 TiB/(Ti-25Al-11Nb) 금속기 복합재료의 미세조직과 기계적 성질)

  • 이성열
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.27 no.1
    • /
    • pp.124-133
    • /
    • 2003
  • Ti-25Al-xNb (x=0, 3, 7, 11, 13 at. %) alloys and 18 vol. % TiB/(Ti-25Al-11Nb) metal matrix composite were fabricated by spark plasma sintering process at 900-120$0^{\circ}C$. Microstructural characteristics of the sintered bodies were identified by SEM, EDX analysis, X-ray diffraction, and differential scanning calorimeterric method. $Ti_3Al$ alloy was consisted of equiaxed $\alpha_2$ phase. $Ti_3Al-Nb$ alloys and the matix of TiB/(Ti-25Al-11Nb) metal matrix composite had the morphology that O phase was precipitated at the grain boundary of $\alpha_2$phase. Volume fraction of O phase and hardness were depended on the concentration of Nb in $Ti_3Al-Nb$ alloy, Rule of mixing could be applied to hardness and Young's modulus of 18 vol. % TiB/(Ti-25Al-11Nb) metal matrix composite.

A study on corrosion resistance of Ti-Nb alloys by Nb contents (Nb 함량에 따른 Ti-Nb계 합금의 내식성에 대한 연구)

  • Park, Geun-Hyeung
    • Journal of Technologic Dentistry
    • /
    • v.28 no.1
    • /
    • pp.61-66
    • /
    • 2006
  • Titanium alloys have been used for dental materials due to it's very good biocompatibility. Ti-6Al-4V alloy instead of pure titanium is being widely used as biomaterials has some characteristics such as high fatigue strength, tensile strength and corrosion resistance. But it has been reported recently that the vanadium element expresses cytotoxicity and carcinogenicity and the aluminium element is related with dementia of Alzheimer type and neurotoxicity. The Ti-Nb alloys has designed and examined corrosion resistance. Ti-3wt.%Nb($\alpha$type), Ti-20wt.%Nb(${\alpha}+{\beta}$type) and Ti-40wt.%Nb($\beta$type) alloys were melted by vacuum arc furnace. The corrosion resistance of Ti alloys was evaluated by potentiodynamic polarization test in the solution of 0.9% NaCl and 5% HCl. The results can be summarized as follows: 1) For the corrosion test in the solution of 0.9% NaCl and 5% HCl, the corrosion behaviour of Ti-Nb alloys was similar to ASTM grade 2 CP Ti. 2) The corrosion resistance of Ti-20Nb alloy was better than that of CP-Ti, Ti-3Nb, Ti-40Nb alloy in 0.9% NaCl and 5% HCl, solutions.

  • PDF

Precipitation and Precipitate Coarsening Behavior According to Nb Addition in the Weld HAZ of a Ti-containing Steel (Nb의 첨가에 따른 Ti 첨가 저합금강 용접열영향부에서의 석출물 거동 변화)

  • Moon, Joon-Oh;Lee, Chang-Hee
    • Journal of Welding and Joining
    • /
    • v.26 no.1
    • /
    • pp.76-82
    • /
    • 2008
  • The effect of Nb addition on the precipitation and precipitate coarsening behavior was investigated in Ti and Ti + Nb steel weld HAZ. A dilatometer equipped with a He-quenching system was used to simulate the weld thermal cycle. Compared to $TiC_yN_{1-y}$ precipitate in a Ti containing steel, $Ti_xNb_{1-x}C_yN_{1-y}$ complex particle with addition of Nb is precipitated in a Ti + Nb containing steel. Meanwhile, precipitate coarsening occurred more easily in Ti + Nb steel, which may be because the high temperature stability of $Ti_xNb_{1-x}C_yN_{1-y}$ complex particle is deteriorated by the Nb addition.

Cell response to a newly developed Ti-10Ta-10Nb alloy and its sputtered nanoscale coating

  • Kim, Young-Min;Vang, Mong-Sook;Yang, Hong-So;Park, Sang-Won;Lim, Hyun-Pil
    • The Journal of Advanced Prosthodontics
    • /
    • v.1 no.1
    • /
    • pp.56-61
    • /
    • 2009
  • STATEMENT OF PROBLEM. The success of titanium implants is due to osseointegration or the direct contact of the implant surface and bone without a fibrous connective tissue interface. PURPOSE. The purpose of this study was to evaluate the osteoblast precursor response to titanium-10 tantalum-10 niobium(Ti-Ta-Nb) alloy and its sputtered coating. MATERIAL AND METHODS. Ti-Ta-Nb coatings were sputtered onto the Ti-Ta-Nb disks. Ti6-Al-4V alloy disks were used as controls. An osteoblast precursor cell line, were used to evaluate the cell responses to the 3 groups. Cell attachment was measured using coulter counter and the cell morphology during attachment period was observed using fluorescent microscopy. Cell culture was performed at 4, 8, 12 and 16 days. RESULTS. The sputtered Ti-Ta-Nb coatings consisted of dense nanoscale grains in the range of 30 to 100 nm with alpha-Ti crystal structure. The Ti-Ta-Nb disks and its sputtered nanoscale coatings exhibited greater hydrophilicity and rougher surfaces compared to the Ti-6Al-4V disks. The sputtered nanoscale Ti-Ta-Nb coatings exhibited significantly greater cell attachment compared to Ti-6Al-4V and Ti-Ta-Nb disks. Nanoscale Ti-Ta-Nb coatings exhibited significantly greater ALP specific activity and total protein production compared to the other 2 groups CONCLUSIONS. It was concluded that nanoscale Ti-Ta-Nb coatings enhance cell adhesion. In addition, Ti-Ta-Nb alloy and its nanoscale coatings enhanced osteoblast differentiation, but did not support osteoblast precursor proliferation compared to Ti-6Al-4V. These results indicate that the new developed Ti-Ta-Nb alloy and its nanoscale Ti-Ta-Nb coatings may be useful as an implant material.

A study on microstruture and corrosion resistance of Ti-Nb alloys by hot rolling (열간압연에 의한 Ti-Nb계 합금의 미세조직 및 내식성에 대한 연구)

  • Park, Hyo-Byung
    • Journal of Technologic Dentistry
    • /
    • v.23 no.2
    • /
    • pp.223-230
    • /
    • 2002
  • Pure titanium and Ti6Al4V alloy have been mainly used as implant materials but the cytotoxicity of V, neurotoxicity of Al resulting in Alzheimer disease had been reported. This paper was described the influence of composition of Ti-Nb alloys with 3 wt%Nb, 20 wt%Nb on the microstructure and corrosion resistance. Specimens of Ti alloys were melted in vacuum arc furnace and homogenized at $1000^{\circ}C$ for 24hr. The alloys were rolled in $\beta$ and ${\alpha}+{\beta}$ regions. The corrosion resistance of Ti alloys were evaluated by potentiodymic polarization test in 0.9% NaCl and 5% HCl solutions. The results can be summarized as follows: 1. The microstructure was transformed from $\alpha$ phase to ${\alpha}+{\beta}$ phase by adding Nb 2. The hardness of Ti-20Nb alloy was greater than Cp- Ti, Ti-3Nb alloy. 3. The corrosion resistance of Ti-20Nb alloy was better than that of Cp-Ti, Ti-3Nb alloy in 0.9%NaCl and 5%HCl solutions.

  • PDF

Effects of V on the Formation of Ti-Nb-V Cabonitrides and Mechanical Properties in Low Carbon HSLA Steels (저탄소.저합금강의 Ti-Nb-V 복합 탄질화물 형성 및 기계적 특성에 미치는 V 첨가의 효과)

  • Kang, J.S.;Kim, D.J.;Park, C.G.
    • Transactions of Materials Processing
    • /
    • v.15 no.8 s.89
    • /
    • pp.581-585
    • /
    • 2006
  • Effects of V on both the formation of Ti-Nb-V carbonitrides and mechanical properties of Ti-Nb bearing low carbon HSLA steels were investigated. Hot rolling process was simulated by using Gleeble 3500 system with the steels containing three different levels of V ($0{\sim}0.1wt.%$). Vanadium precipitated as Ti-Nb-V carbonitrides at austenite region but it did not precipitate as VC during austenite to acicular ferrite or bainitic ferrite phase transformation. As V content increased, the amount of Nb precipitates was decreased but the average size of Ti-Nb-V carbonitrides was increased due to larger diffusivity of V than that of Nb. Coarsened Ti-Nb-V carbonitrides could act as heterogeneous nucleation site during ${\gamma}{\rightarrow}{\alpha}$ phase transformation, thus, acicular ferrite transformation was promoted as V content increased, resulting in increase of upper shelf energy.

The Structural properties of $BaTiO_3+Nb_2O_5$ ceramics with sintering temperature (소결온도에 따른 $BaTiO_3+Nb_2O_5$ 세라믹스 구조적 특성)

  • Lee, Sang-Chul;Kim, Ji-Heon;Kim, Kang;Ryu, Ki-Won;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05c
    • /
    • pp.127-130
    • /
    • 2001
  • The $BaTiO_3+xNb_2O_5$(x=6, 8, 10wt%) ceramics were prepared by conventional mixed oxide method. The structural properties of the $BaTiO_3+Nb_2O_5$ ceramics with the sintering temperature and addition of $Nb_2O_5$ were investigated by XRD and SEM. Increasing the sintering temperature, the $2{\theta}$ value of BT(110) peak was shifted to the lower degree and intensity of the $Ba_6Ti_2Nb_8O_{30}$ (133) peak was increased. Increasing the addition of $Nb_2O_5$, the intensity of $BaTiNb_4O_{13}$ (201) peak was decreased and $Ba_6Ti_2Nb_8O_{30}$ (133) peak was increased. The grain size of the $BaTiO_3+Nb_2O_5$ ceramics sintered at $1500^{\circ}C$ were almost uniform.

  • PDF

A study on cytotoxicity of Ti-Nb alloys (Ti-Nb계 합금의 세포독성에 관한 연구)

  • Park, Hyo-Byeong
    • Journal of Technologic Dentistry
    • /
    • v.25 no.1
    • /
    • pp.89-94
    • /
    • 2003
  • The use of titanium alloys as biomaterials is increasing due to their superior biocompatibility and enhanced corrosion resistance compared to conventional stainless steels and cobalt-based alloys. Ti-6Al-4V ($\alpha+\beta$type) alloy instead of pure titanium ($\alpha$type) is being widely used as biomaterials has some characteristics such as high fatigue strength, tensile strength and corrosion resistance. It also has similar characteristics to Ti in inducing bony ingrowth. But it has been reported recently that the vanadium element expresses cytotoxicity and carcinogenicity and the aluminium element is related with dementia of Alzheimer type and neurotoxicity. In order to overcome their detrimental effects, $\beta$-phase stabilizer Nb was chosen in the present study. CP-Ti(ASTM grade 2), Ti-3wt.%Nb($\alpha$type), Ti-20wt.%Nb ($\alpha+\beta$type) and Ti-40 wt.%Nb($\beta$type) alloys were melted by vacuum arc furnace. Biocompatibility of Ti-Nb alloys was evaluated by cytotoxicity test. The results can be summarized as follows: 1. For the cytotoxicity test, Ti-Nb alloys showed excellent biocompatibility compared to CP-Ti(ASTM grade 2), 316L STS and Co-Cr alloys.

  • PDF

Chemical Design of Highly Water-Soluble Ti, Nb and Ta Precursors for Multi-Component Oxides

  • Masato Kakihana;Judith Szanics;Masaru Tada
    • Bulletin of the Korean Chemical Society
    • /
    • v.20 no.8
    • /
    • pp.893-896
    • /
    • 1999
  • Novel citric acid based Ti, Nb and Ta precursors that are highly stable in the presence of water were developed. No alkoxides of Ti, Nb and Ta were utilized in the preparation, instead much less moisture-sensitive metallic Ti, NbCl5 and TaCl5 were chosen as starting chemicals for Ti, Nb and Ta, respectively. The feasibility of these chemicals as precursors is demonstrated in the powder synthesis of BaTi4O9, Y3NbO7 and LiTaO3. The water-resistant Ti precursor was employed as a new source of water-soluble Ti in the amorphous citrate method, and phase pure BaTi4O9 in powdered form was successfully synthesized at 800 ?. The Pechini-type polymerizable complex method using the water-resistant Nb and Ta precursors was applied to the synthesis of Y3NbO7 and LiTaO3, and both the powder materials in their pure form were successfully synthesized at reduced tempera-tures, viz. 500-700 ?. The remarkable retardation of hydrolysis of these water-resistant precursors is explained in terms of the partial charge model theory.

A Study on Microstructure and Mechanical Properties of Hf, Ta Added Ti-l5Sn-4Nb system Alloys for Biomaterial (Hf, Ta가 첨가된 Ti-l5Sn-4Nb계 생체용 합금의 미세조직 및 기계적 성질에 관한 연구)

  • 김대환;이경구;박효병;이도재
    • Journal of the Korean institute of surface engineering
    • /
    • v.33 no.4
    • /
    • pp.251-260
    • /
    • 2000
  • Ta and Hf added Ti-l5Sn-4Nb alloys without V and Al elements for biomaterial were melted by arc furnace in response to recent concerns about the long term safety of Ti-6Al-4V alloy. All specimens were homogenized at $1000^{\circ}C$ and solution treatment was performed at $812^{\circ}C$ and aging treatment at $500^{\circ}C$. The microstructure and mechanical properties were analysed by optical micrograph, hardness tester and instron. Ti-l5Sn-4Nb system alloys showed widmanstatten microstructure which is typical microstructure in $\alpha$$\beta$ type Ti alloys. The Ti-l5Sn-4Nb-2Hf and Ti-l5Sn-4Nb-2Ta alloys showed better hardness and tensile strength compared with Ti-6Al-4V. The result of XPS analysis, Ti-l5Sn-4Nb alloy in air atmosphere consisted of $TiO_2$, SnO and NbO.

  • PDF