• Title/Summary/Keyword: Ti-Cr alloy

Search Result 188, Processing Time 0.036 seconds

A Study on the V22Ti16Zr16Ni39X7(X=Cr, Co, Fe, Mn, Al) Metal Hydride Electrodes (V22Ti16Zr16Ni39X7(X=Cr, Co, Fe, Mn, Al) 금속수소화물전극에 관한 연구)

  • Kim, Jeong-Seon;Cho, Won-Il;Cho, Byung-Won;Yun, Kyung-Suk;Kim, Sang-Joo
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.5 no.1
    • /
    • pp.1-8
    • /
    • 1994
  • Lattice structure, hydrogen absorption characteristics, discharge capacity and cycle life of $V_{22}Ti_{16}Zr_{16}Ni_{39}X_7$(X= Cr, Co, Fe, Mn, Al) alloys were investigated. The matrix phases of these alloys were the C14 Laves phase. Chromium-containing alloy had a vanadium-rich phase in addition to the Laves phase. The chromium, maganese, or aluminum-containing alloys had lower hydrogen equilibrium pressure and larger hydrogen absorption content than the cobalt or iron-containing alloys. The discharge capacities of these alloys were 270~330mAh/g. The discharge capacity according to the alloying element X decreased in the order of Mn>Cr>Co, Al)Fe. The charge/discharge cycle lives of the chromium, cobalt or iron-containing alloys were longer than those of maganese or aluminum-containing alloys due to the lower vanadium dissolution rate.

  • PDF

Microstructures and Mechanical Properties of Beryllium(Be)-free Ni-Cr-Mo based Alloys for Metal-Ceramic Crown (베릴륨(Be)이 미 첨가된 치과도재소부용 Ni-Cr-Mo계 합금의 미세조직 및 기계적 성질 특성)

  • Song, Kyung-Woo;Go, Eun-Kyoung;Lee, Jung-Hwan;Jung, Jong-Hyun;Noh, Hak;Han, Jae-Ick
    • Journal of Technologic Dentistry
    • /
    • v.28 no.2
    • /
    • pp.321-329
    • /
    • 2006
  • The popularity of Ni-Cr-Mo based metal alloys for metal-ceramic crown have increased recently because of low price, superior yield strength and rigidity. the use of these alloys give them the potential advantage of thinner copping with the required rigidity for long span bridges. The purpose of this study was to assess the microstructures and mechanical properties of Ni-Cr-Mo-(Si,Al,Nb,Zr,Ti.Cu,Mm) based Alloys not containing beryllium(Be) related toxic effects. The abtained results indicated that as-cast these specimen alloys showed compositional and microstructural differences, and mechanical properties values of Ni69Cr20Mo5Si2Al4 alloy among these specimen alloys was found to be superior to those of commercial Ni-Cr based alloy using in market place today.

  • PDF

A comparative study of frictional forces according to orthodontic wires and ligation method under dry and wet conditions (교정선의 종류, 결찰방법, 타액의 유무에 따른 마찰력의 비교연구)

  • Lee, Jin-Woo;Cha, Kyung-Suk;Han, Jung-Suk
    • The korean journal of orthodontics
    • /
    • v.31 no.2 s.85
    • /
    • pp.271-281
    • /
    • 2001
  • The Purpose of this study was fourfold - to evaluate the general laws of friction applied to orthodontic conditions, to compare archwire materials under these controlled conditions, to compare ligation method, and to measure the effect of the artificial saliva on friction with these materials Three wire alloys (Cobalt-chromium, Nickel-titanium, Beta-titanium) in two size wires (.016" , .016" ${\times}$.022" ) were examined respect to the bracket (.018" ${\times}$.025" standard), and two ligature material (stainless steel, elastomeric) in dry and wet conditions The results were as follows, 1. The order of frictional force against alloy materials was Co-Cr (lowest), Ni-Ti, and ${\beta}$-Ti(highest) - with the exception of elastomeric ligation under wet conditions. 2. S.S. ligation gave rise to significantly greater friction than elastomeric ligation did. 3. Testing in the presence of saliva, rather than in dry conditions, decreased the frictional force for S.S. ligation with .016" Co-Cr, Ni-Ti, ${\beta}$-Ti. but, increased the frictional force for S.S. ligation with .016" ${\times}$ .022" Co-Cr, Ni-Ti, ${\beta}$-Ti. 4. .016" ${\times}$.022 " wire generated more friction than .016" wire.

  • PDF

Evaluation of image quality for metal artifact using protocol parameters in the MRI (자기공명영상에서 프로토콜 변화를 이용한 금속인공물의 영상평가)

  • Lee, Su-Hyun;Kim, Do-Gyoung;Kim, Yo-Han;Yeum, Hyei-Jeong;Lee, Heon-Jun;Lim, Ju-Yeon;Choi, Woo-Jeon;Kim, Dong-hyun
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2015.10a
    • /
    • pp.582-585
    • /
    • 2015
  • In the aging society, TKRA is steadily increased because of joint diseases. Artificial joint used in TKRA generates metal artifacts in the MRI. Metal artifact may affect diagnosis. In study, We are going to minimize the effect of metal artifact to improve the value of diagnosis by changing the sequence and the type of artificial joint(Co-Cr, Ni-Ti). 1.5T AVANTO, plastic containers and each of the artificial joint (Normal, Co-Cr, NiTi) were used. After the artificial joints fixed in a paper cup was inserted in a plastic container of cylindrical, Signal intensity was measured. To obtain strong and uniform signal intensity, the plastic container was filled with water. We changed Sequences(T1 TSE, T2 TSE, PD TSE) and obtained an Axial image. After excepting the maximum and minimum values, We calculated the average of SNR, CNR and PSNR. Consequently, The SNR, CNR value of PD TSE are measured higher than these of T1 TSE, T2 TSE and The PSNR of Co-Cr is higher than this of Ni-Ti. The SNR of Co-Cr is similar to the SNR of normal comparing this of Ni-Ti. As a result, Using sequence of PD Tse and Co-Cr alloy is considered to be useful.

  • PDF

MARGINAL DISCREPANCY AND RETENTION FORCE OF CONICAL TELESCOPE OUTER CROWN WITH CO-CR-TI ALLOY (Co-Cr-Ti 합금으로 제작한 conical telescope 외관의 변연적합도와 유지력에 관한 연구)

  • Jung, Hi-Chan;Jeong, Chang-Mo;Jeon, Young-Chan;Lim, Jang-Seop
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.38 no.2
    • /
    • pp.214-225
    • /
    • 2000
  • The purpose of this study was to investigate the effects of investing conditions on the marginal discrepancy of conical telescope outer crown with Co-Cr-Ti alloy(Dentitan) and to compare the marginal discrepancy and the retention force of outer crowns using different pattern materials(plastic foil, casting wax, pattern resin). To evaluate the effects of investing conditions on the marginal discrepancy, patterns with plastic foil were invested under three different liquid/powder ratio conditions using phosphate bonded investment(Univest-nonprecious): standard, 10% decreased and 10% increased. At each liquid/powder ratio condition, metal ring was lined with single or double layers of ceramic ring liner. The marginal discrepancy of outer crown at different investing conditions was measured by ${\times}100$ compact measuring microscope(STM5, Olympus, Japan). For measurement of the marginal discrepancy and the retention force of outer crown using different pattern materials, the investing condition of 10% decreased liquid/powder ratio and double layers of ring liner was selected because this investing condition resulted in the best fit of outer crown. Marginal discrepancy was measured in the same way above and retention force on universal testing machine. Under the conditions of this study, the following conclusions were drawn: 1. The thickness of ring liner had more influence on the marginal discrepancy of outer crown than the liquid/powder ratio, and the acceptable marginal fitness could not be expected at the investing condition directed by investment manufacturer 2. There were no differences in the marginal discrepancy of outer crown among three different pattern materials(P>0.05). 3. Casting wax showed the greatest retention force(1640g) of outer crown, followed by pattern resin(1110g), plastic foil(820g). However, there was no significant difference between plastic foil and pattern resin(P>0.05). 4. Plastic foil showed the least variation in marginal discrepancy and retention force.

  • PDF

Eco-friendly Fabrication Process of Al-Ti-C Grain Refiner

  • Cho, Hoon;Kim, Bong-Hwan
    • Journal of Korea Foundry Society
    • /
    • v.30 no.4
    • /
    • pp.147-150
    • /
    • 2010
  • An eco-friendly production technique of Al-8.6Ti-0.025C refiner was developed by melting a Al-Ti master alloy in a graphite crucible, in which the potential nucleation site, TiC effectively formed by the spontaneous in-situ reaction between excessive Ti and carbon from graphite crucible. The A3003 alloy refined by the Al-8.6Ti-0.025C showed effectively refined macrostructure and enhanced mechanical properties comparable to the commercial Al-Ti-B refiner. The effective refinement was achieved in a shorter compare to the melt-treating time commercial Al-Ti-B refiner.

A STUDY OF ION BEAM ASSISTED DEPOSITION(IBAD) OF TiN ON Ni-Cr Be ALLOY FOR SURFACE CHARACTERISTIC (이온빔 보조 증착법에 의한 TiN 박막도포가 니켈-크롬-베릴륨 합금의 표면 성상에 미치는 영향에 관한 연구)

  • Choi, Soo-Young;Lee, Sun-Hyung;Chang, Ik-Tae;Yang, Jae-Ho;Chung, Hun-Young
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.37 no.2
    • /
    • pp.212-234
    • /
    • 1999
  • Dental restorative materials must have the physical properties to withstand wear and corrosion. Base metal alloys possess better mechanical properties and lower price than the gold alloys. For these reasons such alloys have largely replaced the precious metal alloys. One aspect to con-sider is the release of metal substances to oral environment. The release of elements from dental alloys is a continuing concern because the elements may have the potentially harmful biological effects on local tissues. The purpose of this study was to minimize metal release on the nonprecious metal surfaces by ion beam assisted deposition(IBAD) of titanium nitride (TiN) Ni-Cr-Be alloys with and without TiN coatings were secured in an wear test machine opposing ruby ball to determine their relative resistance to wear with loom, 200m, 300m and 400m sliding distance. And the corrosion behavior of the Ni-Cr-Be alloys with and without TiN coatings and 3 dental noble alloys have been studied. Potentiodynamic curves were used to analyse the corrosion characteristics of the alloys. The measurement of the released Ni and Cr ions was conducted by analysis of the electrolyte solution with atomic absorption spectroscopy. The results were as follows : 1. The critical sliding distance that wore down TiN coatings of $2.5{\mu}m$ thickness in this study condition was 300m. 2. Ion beam assisted deposition of TiN showed a good surface modification with respect to the properties of wear and corrosion resistance. 3. X-ray diffraction showed that the strongest peak of TiN is TiN(111) in the coatings. 4. The release of Ni and Cr ions from alloys measured by means of atomic absorption spectroscopy was reduced by ion beam assisted deposition of TiN.

  • PDF

Effects of Nonprecious Metallic Oxide on the Chemical Bonding Between Dental Alloy and Porcelain (비귀금속 산화물이 치과용 합금과 도재의 화학적 결합에 미치는 영향)

  • Kim, Kwang-Nam;Cho, Sung-Am
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.25 no.1
    • /
    • pp.317-325
    • /
    • 1987
  • A study on the shear bonding strength between dental alloy and porcelain according to various kidns of sputtered metallic thin films was established by Ingtron universal testing machine, and the change of the elemental weight % at the surface of dental alloy was studied by E.D.S. The kind of metallic thin films were Al, Ni, In, Cr. Ti and Sn with $0.3{\mu}m$ thickness. The dental alloys were Verabond made by Aalba Dent. Co. and Degudent H manufactured by Degussa Co. The control groups were Verabond and Degudent H. The obtained results were as follows; 1. The shear bonding strength of Al plated sample was the strongest of all. 2. The shear bonding strength of Ni plated sample was stronger than that of Degudent H, Sn plated samples. 3. The shear bonding strength of Verabond was weaker than that of Al, Ni, In, Cr, plated samples. 4. After degassing, it is more weight % of Ni at the alloy surface of the Ni sputtered specimen than the Sn sputtered sample.

  • PDF

Electrode characteristics of $AB_2$ type hydrogen storage alloy modified by Cr, La addition and fluorination ($AB_2$계 수소저장합금의 전극특성에 미치는 Cr, La 첨가 효과 및 표면 불화처리 효과)

  • Chang I.;Lee B. H.;Cho W. I.;Jang H.;Cho B. W.;Yun K. S.
    • Journal of the Korean Electrochemical Society
    • /
    • v.1 no.1
    • /
    • pp.45-51
    • /
    • 1998
  • [ $AB_2-type$ ] alloy, one kind of hydrogen storage alloys used as an anode of Ni-MH batteries, has large discharge capacity but has remaining problems regarding initial activation, cycle life and self-discharge. This study investigates the effects of Cr-addition and fluorination after La-addition on $Zr_{0.7}Ti_{0.3}V_{0.4}Mn_{0.4}Ni_{1.2}$, composition $AB_2-type$ alloy. EPMA and SEM surface analysis techniques were used and the crystal structure was characterized by XRD analysis. In addition, electrodes were fabricated out of the alloys and characterized by constant current cycling test, electrochemical impedance spectroscopy and potentiodynamic polarization. Cr-addition was found to be effective to cycle life and self-discharge but ineffective to initial activation due to formation of stable oxide film on surface. Fluorination after La-addition to the alloys improved initial activation remarkably due to formation of highly reactive particles on surface.

Influence of Tool Coating on Frictional Behavior of AZ31B Mg Alloy at Elevated Temperature (금형 표면 처리가 AZ31B 마그네슘 합금의 온간 마찰 특성에 미치는 영향에 관한 연구)

  • Han, S.S.
    • Transactions of Materials Processing
    • /
    • v.30 no.1
    • /
    • pp.43-48
    • /
    • 2021
  • The success of warm forming of Mg alloy sheet is greatly influenced by friction at elevated temperature, depending on the surface treatment of the tool. The tool coating affected the frictional characteristics of AZ31B Mg alloy sheet at elevated and room temperatures. The frictional behavior of the Mg alloy sheet at room temperature was not significantly affected by surface treatment conditions of the tool, but was significantly affected at elevated temperature. When the contact pressure is high, a few surface-treated tools exhibit a higher coefficient of friction than those without surface treatment. It is important to select the surface treatment conditions of the tool in order to ensure appropriate friction during warm forming of Mg alloy sheet.