• Title/Summary/Keyword: Ti-15-3

Search Result 911, Processing Time 0.029 seconds

Characteristics of a CW Ti:sapphire Laser in a Folded Geometry (접힌 공진기 형태의 연속 발진 티타늄 사파이어 레이저의 발진 특성)

  • 강영일;차용호;남창희
    • Korean Journal of Optics and Photonics
    • /
    • v.6 no.4
    • /
    • pp.282-287
    • /
    • 1995
  • We have studied the characteristics of a cw Ti:sapphire laser pumped by an Ar-ion laser. Ti:sapphire is one of the most attractive materials for the generation of ultra-short pulses because of its very broad gain bandwidth. We used a 4.1 mm thick, 0.15 wt. % $Ti^{3+}$ -doped, Brewster-angled Ti:sapphire crystal and made a folded cavity to create a strong focusing mode. The folding angle of the cavity was adjusted to $15.4^{\circ}$ to compensate for the astigmatism from the Brewster-angled Ti:sapphire crystal. 5 WAr-ion laser was used as a pumping source. We observed that the Ti:sapphire cw output power was sensitively changed with respect to the condition of the folded cavity. The threshold pumping power was 2 Wand the slope efficiency was 16% when an output coupler of 10% transmission was used. The maximum output power was more than 450 mW at 5 W pumping. mping.

  • PDF

Effect of Ti, B, Zr Elements on Grain Refinement and Castability of Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe Casting Alloy (주조용 Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe 합금의 결정립 미세화와 주조특성에 미치는 Ti, B, Zr 첨가원소의 영향)

  • Kim, Heon-Joo;Park, Su-Min
    • Journal of Korea Foundry Society
    • /
    • v.35 no.5
    • /
    • pp.120-127
    • /
    • 2015
  • The effects of Ti, B and Zr on grain refinement and castability were investigated in Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe alloy. Measurement of cooling curve and micro-structure observation were performed to analyze the effects of the addition of minor elements Ti, B and Zr during solidification. The prominence of effect on grain refinement was in increasing order for Ti, Zr and B element. Fine grain size and an increase of the crystallization temperature for ${\alpha}$-Al solution were evident as the amount of addition elements increased in this study. Addition of 0.15wt% Ti was most effective for grain refinement, and the resulting grain size of ${\alpha}$-Al solution for shell mold and steel mold were $72.3{\mu}m$ and $23.5{\mu}m$, respectively. Fluidity and shrinkage tests were perform to evaluate the castability of the alloy. Maximum fluidity length and minimum ratio of micro shrinkage were recorded for 0.15wt% Ti addition due to the effect of the finest grain size.

Laser brazing molybdenum using two titanium base fillers

  • Lin, Chia-Chen;Lee, Cheng-Han;Shiue, Ren-Kae;Shy, Hsiou-Jeng
    • Advances in materials Research
    • /
    • v.1 no.3
    • /
    • pp.183-190
    • /
    • 2012
  • Brazing Mo using Ti and Ti-15-3 foils has been investigated in the experiment. For traditional furnace brazing, solidification shrinkage voids cannot be completely removed from the joint even the brazing temperature increased to 2013 K and 160 ${\mu}m$ thick Ti foil applied in brazing. Similar results are observed from the joint using Ti-15-3 filler. In contrast, the quality of laser brazed joint is much better than that of furnace brazed joint. A sound joint is achieved after laser brazing. Tensile strengths of 418 and 373 MPa are obtained from laser brazed joints at the power of 800W and travel speed of 5 mm/s using Ti and Ti-15-3 fillers, respectively. All laser brazed joints are fractured at the brazed zone and cleavage dominated fractures are widely observed from their fractographs. The Ti base fillers show potential in laser brazing Mo substrate.

Microwave Dielectric Properties of the $BaO-(Nd,Bi)_2 O_3-TiO_2$$_2$ Ceramic for Mobile Communication Component (이동 통신 부품에 이용되는 $BaO-(Nd,Bi)_2 O_3-TiO_2$계 마이크로파 유전체의 유전 특성)

  • 윤중락;이헌용;김경용;이석원
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.11
    • /
    • pp.947-953
    • /
    • 1998
  • The microwave dielectric properties of X BaO-0.15($Nd_{0.87}Bi_{0.13})_2O_3-(0.85-X)TiO_2 (X=0.14~0.17) and 0.16BaO-0.15(Bi_xNd_{1-x})_2O_3-0.69TiO_2$ (X=0.12~0.15) ceramics sintered at 1320~$1380^{\circ}C$ were investigated. The microwave dielectric properties of X BaO-0.15(Nd_{0.87}Bi_{0.13})_2O_3-(0.85-X)TiO_2$ (X=0.14~0.17) can be controlled effectively by adjusting X content : with increasing X from 0.14 to 0.17 both dielectric constant and temperature coefficient of resonant frequency decreased from 94.6 to 86 and from 22 ppm/^${\circ}C to -7 ppm/^{\circ}C$, respectively, while quality factor increased from 1300 to 1920 (at 4GHz). The microwave dielectric properties of 0.16BaO-0.15(Bi_x/Nd_{1-x2}O_3 -0.69TiO_2$ (X=0.12~0.15) can be controlled effectively by adjusting X content : with increasing X from 0.12 to 0.15 both quality factor and temperature coefficient of resonant frequency decreased from 1920 to 1430 and from 9 ppm/^${\circ}C to -10 ppm/^{\circ}C$, respectively, while dielectric constant increased from 87.5 to 92.6.

  • PDF

The Dielectrical Properties of $(1-x)(Sr_a.Pb_b.Ca_c)TiO_3-xB_i2O_3.TiO_2$ system affected by $Bi_2O_3.3TiO_2$ amounts and $MnO_2$ ($(1-x)(Sr_a.Pb_b.Ca_c)TiO_3-xB_i2O_3.TiO_2$계에서의 $Bi_2O_3.3TiO_2$$MnO_2$첨가에 따른 유전특성에 관한 연구)

  • 박상도;이응상
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.2
    • /
    • pp.123-130
    • /
    • 1997
  • In this study, (Sr.Pb.Ca)TiO3-Bi2O3.3TiO2(SPCT) systems were investigated to develop a new material which has a high dielectric constant, a low dielectric loss and a small TCC(Temperature Coefficient of Capa-citance), and are suitable for high voltage applications as a function of the additions of Bi2O3.3TiO2 from 5 mol.% to 9 mol.%. The result obtained from our investigation showed that up to 6 mol.% Bi2O3.3TiO ad-dition the dielectric constant increased and it deteriorated at higher concentrations with increasing amount of the acicular grains. As a result of some dopants (SiO2, Nb2O3, MnO2) addition to SPCT, the specimens with MnO2 showed good dielectric properties. The dielectric constant decreased, but the TCC was improved with the addition of MnO2 from 0.15 wt.% to 0.45 wt. %.

  • PDF

Dielectric Properties of Barium Titanate with $Sb_2O_3$ and ZnO ($Sb_2O_3$와 ZnO를 첨가한 Barium Titanate의 유전성)

  • 윤기현;김종우;송효일
    • Journal of the Korean Ceramic Society
    • /
    • v.21 no.2
    • /
    • pp.121-126
    • /
    • 1984
  • The dielectric properties of $BaTiO_3$ containing 0~0.3mol% and ZnO respectively as additives were investigated as a function of temperature from $25^{\circ}C$ to 14$0^{\circ}C$ and frequency from 24 KHz to 15MHz. The density of sintered $BaTiO_3$ was increased with addition of increasing to 0.15mol% amounts of $Sb_2O_3$ and the dielectric constant was also increased. This is due to space charge polarization with Ba vacancies. Above 0.15mol% $Sb_2O_3$ the density was decreased and the dielectric constant was also decreased due to occuring the discharge through voids. The density of sintered $BaTiO_3$ was decreased with addition of increasing to 0.15mol% amounts of ZnO and the dielectric constant was decreased due to occuring the discharge through voids. Above 0.15mol% ZnO the density was increased and the dielectric constant was also increased.

  • PDF

A Study on Low-temperature Sintering of Microwave Dielectric Ceramics Based on ZnTiO3 (ZnTiO3계 마이크로파용 유전체 세라믹스의 저온소결에 관한 연구)

  • 이지형;방재철
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.1
    • /
    • pp.30-36
    • /
    • 2002
  • The effects of the sintering additives such as B $i_2$ $O_3$ and $V_2$ $O_{5}$ on the microwave dielectric and sintering properties of ZnTi $O_3$ system were investigated. Highly dense samples were obtained for ZnTi $O_3$ at the sintering temperature range of 870~90$0^{\circ}C$ with B $i_2$ $O_3$ and $V_2$ $O_{5}$ additions of <1 wt.%, respectively. The microwave dielectric properties of ZnTi $O_3$ with 0.6 wt.% B $i_2$ $O_3$ and 0.5 wt.% $V_2$ $O_{5}$ were as follows: Qx $f_{o}$ = 48,400 GHz, $\varepsilon$$_{r}$= 22, and $\tau$$_{f}$ = -43 ppm/$^{\circ}C$. In order to improve temperature coefficient of resonant frequency, Ti $O_2$ was added to the abode system. The optimum amount of Ti $O_2$was 15 mol.% when sintered at 87$0^{\circ}C$, at which Ive could obtain following results: Qx $f_{O}$ = 44,700GHz, $\varepsilon$$_{r}$ = 26, and $\tau$$_{f}$ = 0 PPm/$^{\circ}C$.>.EX>.>.>.EX>.>.>.

Effects of $Nd_2O_3$ and $TiO_2$ Addition on the Microstructures and Microwave Dielectric Properties of $BaO-Nd_2O_3-TiO_2$ System

  • Kim, Tea-Hong;Park, Jung-Rae;Lee, Suk-Jin;Sung, Hee-Kyung;Lee, Sang-Seok;Choy, Tae-Goo
    • ETRI Journal
    • /
    • v.18 no.1
    • /
    • pp.15-27
    • /
    • 1996
  • The effects of $Nd_2O_3$ and $TiO_2$ addition on the microstructures and microwave dielectic properties of $BaO-Nd_2O_3-TiO_2$ system were investigated. $BaNd_2Ti_4O_{12}$ or $BaNd_2Ti_{5}O_{14}$ phases were observed for compositions based on BaO/$Nd_2O_3$ = 1 ratio. The compositions deviated from $BaO/Nd_2O_3=1$ ratio were composed of major phases of $BaNd_2Ti_4O_{12}$ or $BaNd_2Ti_5O_{14}$, and the compound of $Nd_2O_3$ and $TiO_2(Nd_2Ti_2O_7)$ or that of BaO and $TiO_2(BaTi_4O_9)$. The microstructure of ceramic with $BaO{\cdot}Nd_2O_3{\cdot}4TiO_2$ composition varied from spherical grains to needlelike grains with increasing sintering temperature. With increasing $Nd_2O_3$, the optimum sintering temperature with maximum density increased, and the dielectric constant(${\varepsilon}_r$) and quality factor(Q) decreased due to the formation of secondary phases. With increasing $TiO_2$, the optimum sintering temperature and the dielectric constant decreased with increased Q value. And the temperature coefficient of resonant frequency, ${\tau}_f$ shifted toward positive direction. The dielectric ceramics with $BaO/Nd_2O_3=1$ showed Q values of above 2000 and dielectric constants of above 80 at 3GHz.

  • PDF

Effects of A-site Ca and B-site Zr Substitution on the Dielectric Characteristics and Microstructure of BaTiO3-CaTiO3 Composite (A-site Ca 및 B-site Zr 첨가에 의한 BaTiO3-CaTiO3복합체의 유전특성 및 미세구조에 미치는 영향)

  • 윤만순;박영민
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.1
    • /
    • pp.37-45
    • /
    • 2003
  • The dielectric and sintering characteristics of composites made by substituting Ca ion to Ba-site and Zr ion to Ti site in $(Ba{1-x}Ca_x)(Ti{0.96-yZr_ySn_{0.04})O_3$ $(0.15{\leq}x{\leq}0.20,\;0.09{\leq}y{\leq}0.14)$ were investigated. As the content of Ca was more than 15 mol%, composite was formed by precipitating the second phase whose main element was $CaTiO_3$ and the fraction of the second phase was increased. The curie temperature of composites was depended on Ca concentration, $-1.7^{\circ}C$ per mol% and the maximum dielectric constant of composite was decreased by the rate of 200/mol%. The substitution of Zr ion decreased the curie temperature by the rate of $10^{\circ}C$ per mol% and the maximum dielectric constant was decreased by 217/mol% due to the increase of diffuse phase transition. The density and insulation breakdown characteristics were improved by suppressing the abnormal grain growth due to the increase of second phase. We developed the composition of Y5U (EIA standard) condenser which had high breakdown voltage and dielectric constant by controlling diffuse phase transition by the addition of Zr ion into composite.