• 제목/요약/키워드: Thermal Quenching

검색결과 204건 처리시간 0.028초

STD61 공구강의 내충격 및 내열피로 특성에 미치는 가스 퀜칭 압력의 영향 (Effect on Anti-impact and Anti-thermal Fatigue Properties of STD61 Material Affected by Gas Quenching Pressure of Quenching Process)

  • 박현준;최광진;김종엽;신승용;문경일
    • 열처리공학회지
    • /
    • 제29권6호
    • /
    • pp.277-283
    • /
    • 2016
  • The influences of cooling pressure of quenching process on the mechanical properties such as hardness, impact endurance and anti-thermal fatigue behaviour of STD61 steel were investigated. The specimens were heat-treated using a vacuum furnace in which they were austenitized at $1,030^{\circ}C$ for 1hour under the pressure of $10^{-3}$ torr and cooled with quenching gas of various pressure, i.e. 1, 2 and 6 bar. According to the observation on the specimens prepared with quenching from austenizing temperature, the mechanical properties of the samples with higher quenching pressure were better than those of prepared at lower quenching pressure. The samples prepared with high quenching pressure showed the more homogeneous microstructure with finer carbides. The size of carbides such as VC and (Fe, Cr)C in quenched specimens decreased with increasing gas quenching pressure. It is considered that the rapid cooling with pressure may restrict the formation and growth of carbide.

마이크로 연소기에서 발생하는 열 소염과 화학 소염 현상 (II)- SiOx(x≤2) 플레이트의 물리, 화학적 성질이 소염에 미치는 영향 - (Thermal and Chemical Quenching Phenomena in a Microscale Combustor (II)- Effects of Physical and Chemical Properties of SiOx(x≤2) Plates on flame Quenching -)

  • 김규태;이대훈;권세진
    • 대한기계학회논문집B
    • /
    • 제30권5호
    • /
    • pp.405-412
    • /
    • 2006
  • In order to realize a stably propagating flame in a narrow channel, flame instabilities resulting from flame-wall interaction should be avoided. In particular flame quenching is a significant issue in micro combustion devices; quenching is caused either by excessive heat loss or by active radical adsorptions at the wall. In this paper, the relative significance of thermal and chemical effects on flame quenching is examined by means of quenching distance measurement. Emphasis is placed on the effects of surface defect density on flame quenching. To investigate chemical quenching phenomenon, thermally grown silicon oxide plates with well-defined defect distribution were prepared. ion implantation technique was used to control defect density, i.e. the number of oxygen vacancies. It has been found that when the surface temperature is under $300^{\circ}C$, the quenching distance is decreased on account of reduced heat loss; as the surface temperature is increased over $300^{\circ}C$, however, quenching distance is increased despite reduced heat loss effect. Such abberant behavior is caused by heterogeneous surface reactions between active radicals and surface defects. The higher defect density, the larger quenching distance. This result means that chemical quenching is governed by radical adsorption that can be parameterized by oxygen vacancy density on the surface.

화염-표면 상호작용에 의한 예혼합 화염의 열소염 및 화학소염에 관한 연구 (A Study of Thermal and Chemical Quenching of Premixed Flame by Flame-Surface Interaction)

  • 김규태;이대훈;권세진
    • 한국연소학회지
    • /
    • 제10권2호
    • /
    • pp.1-8
    • /
    • 2005
  • Incomplete combustion due to quenching in a narrow confinement has been a major problem for realization of a reliable micro combustion device. In most micro combustors, effects of flows are absent in the quenching because the flow is laminar and no severe stretch is present. In such circumstance, quenching is caused either by heat loss or by removal of active radicals to the wall surface of the confinement. An experimental investigation was carried out to investigate the relative significance of these two causes of quenching of a premixed flame. A premixed jet burner with a rectangular cross section at the exit was built. At the burner exit, the flame stands between two walls with adjustable distance. The gap between the two walls at which quenching occurs was measured at different wall surface conditions. The results were analyzed to estimate the relative significance of heat loss to the wall and the removal of radicals at the surface. The measurements indicated that the quenching distance was independent of the wall surface characteristics such as oxygen vacancy, grain boundary, or impurities at low temperature. At high temperature, however, the surface characteristics strongly affect the quenching distance, implying that radical removal at the wall plays a significant role in the quenching process.

  • PDF

$80Al_2O_3-20Al$ 복합재료의 내열충격성: 실험과 유한요소 해석 (Thermal Shock Resistance of $80Al_2O_3-20Al$ Composites: Experiments and Finite Element Analysis)

  • 김일수;신병철
    • 한국세라믹학회지
    • /
    • 제37권3호
    • /
    • pp.201-204
    • /
    • 2000
  • Thermal shock resistance of 80Al2O3-20Al composite and monolithic alumina ceramics was compared. Fracture strength was measured by using a 4-pont bending test after quenching. Thermal stresses of the ceramics and ceramic-metal composites were calculated using a finite element analysis. The bending strength of the Al2O3 ceramics decreased catastropically after quenching from 20$0^{\circ}C$ to $0^{\circ}C$. The bending strength of the composite also decreased after quenching from 200~2$25^{\circ}C$, but the strength reduction was much smaller than for Al2O3. The maximum thermal stress occured in the monolithic alumina ceramics when exposed to a temperature difference of 20$0^{\circ}C$ was 0.758 GPa. The same amount of stress occured in the Al2O3-Al composite when the temperature difference of 205$^{\circ}C$ used.

  • PDF

프레스 퀜칭 공정에 의한 자동차 Flexible Plate의 형상 제어 연구 (Shape Control of Automotive Flexible Plate in Press Quenching)

  • 박인회;정우창
    • 열처리공학회지
    • /
    • 제21권4호
    • /
    • pp.189-198
    • /
    • 2008
  • The production of automotive chassis parts requiring both high hardness and good shape-holdability is better realized by using press quenching technology, comprising the austenitizaton and the subsequent press quenching in a specially designed stamping tool. The effect of press quenching mold shape on the hardness distribution, bending height, and degree of planeness of automotive flexible plate during press quenching and tempering has been investigated. The preferable shape of the projections of punch and die in contact with the flexible plate was close to oval to improve the flow of cooling oil, leading to the higher hardness. The press quenching mold with three separate parts was more effective to control the dimensional change due to thermal deformation during press quenching. Some decrease in the bending height during tempering may be related to some recovery of the residual stress at $400^{\circ}C$.

Compositional Quenching으로 제조한 PP/PU 블렌드의 모폴로지 및 물성 (Morphology and Properties of PP/PU Blends Prepared by Compositional Quenching)

  • 임경택;주민혁;김도형;송기찬;김수경
    • Elastomers and Composites
    • /
    • 제36권3호
    • /
    • pp.177-187
    • /
    • 2001
  • 폴리프로필렌(PP)/폴리우레탄(PU) 블렌드를 compositional quenching으로 제조하여 모폴로지, 인장물성, 표면에너지 그리고 열안정성 등을 조사하였다. 블렌드 제조시, 말레인산 무수물이 그라프트된 PP(MPP)와 히드록시에틸 말레이미드가 그라프트된 PP(HPP)를 반응성 상용화제로 도입하였으며, 이들의 생성 및 PU 조성과의 반응을 FT-IR로 확인하였다. Compositional quenching으로 제조한 블렌드는 용융블렌드에 비해 높은 혼화성을 보였으며, 블렌드내의 상용화제의 함량이 증가함에 따라 모폴로지, 인장물성. 표면특성, 그리고 열안정성 등의 물성이 현저하게 향상되었다. 상용화제로 MPP를 도입한 블렌드는 HPP를 도입한 블렌드에 비해, 높은 표면 에너지를 가졌다.

  • PDF

Characteristic of Quenching Refrigerant for Heat Treatment Deformation Control of SM45C Steel

  • Lyu, Sung-Ki
    • Journal of Mechanical Science and Technology
    • /
    • 제16권5호
    • /
    • pp.647-654
    • /
    • 2002
  • This study deals with the characteristic of quenching refrigerant for heat treatment deformation control of SM45C steel. Heat-treatment deformation must be controlled for the progress of production parts for landing gear. Most of deformation is occurred on inconsistent cooling. The inconsistent cooling is caused by a property of quenching refrigerant. When a heated metal is deposited in the quenching refrigerant, the cooling speed is so slow in early period of cooling because of a steam-curtain. After additional cooling, the steam-curtain is destroyed. In this progress, the cooling speed is very fast. The object of this study is to control the deformation of heat-treatment for landing gear by improving the conditions of quenching. The cooling curves and cooling rates of water, oil and polymer solution are obtained and illustrated. From the characteristics of the quenching refrigerant, the effects of heat-treatments on thermal deformation and fatigue strength are also investigated.

차량용 헬리컬기어의 침탄 열처리 변형해석 (Analysis of Deformation of Automotive Helical Gear in Heat Treatment of Carburized Quenching)

  • 배강열;양영수;박병옥
    • 한국정밀공학회지
    • /
    • 제27권11호
    • /
    • pp.84-91
    • /
    • 2010
  • Heat treatment with carburized quenching process is widely used for automotive helical gear to improve its surface properties of hardness and strength. However, the gear can be deformed with the process over the allowable tolerance, which possibly makes noise, vibration and heat problems in operation. In this study, deformation of helical gear during heat treatment of carburized quenching was analyzed with a numerical method, incorporating coupled calculations of thermal conduction, carbon diffusion, phase transformation and thermal stresses. With the analysis, the effect of coolant temperature in quenching on the deformation was investigated. The result of the analysis revealed that the higher the coolant temperature became, the more change of helix angle and the more compressive stresses in the surface generated, because of delayed generation of martensite in the part.

보론강 카메라 케이스 고온성형 공정 비교 (Comparison of the Quenching Method in Hot Press Forming of Boron Steel)

  • 서오석;김헌영;홍석무;유수열;윤석진
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.185-189
    • /
    • 2009
  • Recently, ultra high strength products can be manufactured by the hot press forming process of Boron steel in automotive and electronics industries. In order to get high strength, the hot press forming should be accompanied by quenching process inducing phase transformation. There are several types of the hot press forming processes according to the quenching method, water quenching and die quenching, etc. In the study, the process was numerically and physically simulated to compare the two types of quenching processes, and then the strength, hardness and dimensions of the products were compared with try-outs.

탄소강의 퀜칭처리 과정에서 변형율이력을 고려한 탄소성열응력의 유한요소 해석(II) - 탄점소성 열응력 해석 - (An Finite Element Analysis for Elasto-Plastic Thermal Stresses Considerating Strain Hysteresis at Quenching Process of Carbon Steel(II) - Analysis of elasto-viscoplastic thermal stress -)

  • 김옥삼;구본권
    • 열처리공학회지
    • /
    • 제9권2호
    • /
    • pp.147-158
    • /
    • 1996
  • Generally, analytical consideration on the behaviour of metallic structures during quenching process, and analysis on the thermal stress and deformation after heat treatment are very important in presumption of crack and distorsion of quenched material. In this study a set of constitute equations relevant to the analysis of thermo elasto-viscoplastic materials with strain hysteresis during quenching process way presented on the basis of contimuum thermo-dynamics mechanics. The thermal stresses were numerically calculated by finite element technique of weighted residual method and the principle of virtual work. In the calculation process, the temperature depandency of physical and mechaniclal properties of the material in consideration. On the distribution of elasto-viscoplastic thermal stresses according to radial direction, axial and tangential stress are tensile stress(50MPa, 1.5GPa and 300MPa) in surface and compressive stress(-1.2GPa, -1.14GPa and -750MPa) in the inner part on the other hand, radial stress is tensile stress(900MPa) in area of analysis. According to axial direction, tangential stress gradients are average 60MPa/mm on the whole. The reversion of stress takes place at 11.5 to 16.8mm from the center in area of analysing.

  • PDF