Fracture Behaviour of PSZ Composite (부분 안정화 지르코니아의 파괴거동)

  • Kim, Hwan;Lim, Eung-Keuk;Koh, Jeong-Kyu;Hwang, Kyu-Hong
    • Journal of the Korean Ceramic Society
    • /
    • v.21 no.3
    • /
    • pp.239-244
    • /
    • 1984
  • The effect of tetragonal $ZrO_2$ phase on the mechanical behavior in 7 mole% calcia partially stabilized zirconia has been studied. The $ZrO_2$ powder containg 7 mole% CaO prepared by Hot Petroleum Drying Method calcined at 80$0^{\circ}C$ for 1 hour was nearly 100% tetragonal but as the calcining temperature increased certain amount of monoclinic phase appeared. The sintered specimen at 1$700^{\circ}C$ for 5 hours was aged at 130$0^{\circ}C$ for 0, 24, 48, 72 hours. X-ray diffraction data showed that in the aged specimen monoclinic tetragonal and cubic phase coexisted. The Kc value of aged specimen for 48 hr was about 4.5MN/m3/2 much greater than unaged sample. But aged for 72 hr the KiC value was decreased. The increasing of toughness in PSZ is based on the Stress-Induced Phase Transformation that is metastable tetra-gonal $ZrO_2$ changes t stable monoclinic phase within the stress field of crack and the mechanical fracture energy absorption is occured But in this case due to certain amount of tetragonal phase transformed to monoclinic phase during cooling the microcrack effect by transformation also considered. Trerefore both Stress-Induced Phase Transformation and inclusion induced microcracking effect contrbute to the increase of fracture toughness of 7 mole% CaO-$ZrO_2$ containing monoclinic and tetragnola phase simulataneously.

  • PDF

A Study on the Properties of Fe-Se-Te System (Fe-Se-Te계의 특성 연구)

  • Choe, Seung-Han
    • Korean Journal of Materials Research
    • /
    • v.9 no.8
    • /
    • pp.854-857
    • /
    • 1999
  • The properties of Fe-Se-Te system(FeSe(sub)1-xTe(sub)x, x=0.2, 0.5, 0.8) have been studied by means of the X-ray diffraction method and Mossbauer spectroscopy. The results of X-ray diffraction patterns show that three samples have the ixed structure of tetragonal PbO and a small amount of hexagonal NiAs structure respectively. For x=0.5 the lattice parameters of tetragonal PbO structure are a=3.795$\AA$, c=5.896$\AA$ and c/a=1.55. The Mossbauer spectra were obtained with the various temperature variation and than they do not exhibit magnetic hyperfine structure but show a strong doublet. The values of observed isomer shift and quadrupole splitting suggest that the irons of all samples exist in the +2 oxidation state with a major covalent contribution. The temperature dependence of isomer shift values for x=0.8 seems to be originated from the second order Doppler effect.

  • PDF

Study on Optical Properties and Phase Transition of $TlGa_xIn_{1-x}Se_2$ Solid Solutions ($TlGa_xIn_{1-x}Se_2$ Solid Solution의 광학적 특성 및 상전이에 관한 연구)

  • Yoon, Chang-Sun;Kim, Byong-Ho;Cha, Duk-Joon
    • Journal of the Korean Vacuum Society
    • /
    • v.2 no.2
    • /
    • pp.220-226
    • /
    • 1993
  • An investigation was made of the dependences of the lattice constants and the energy gap on the composition of $TlGa_xIn_{1-x}Se_2$ single cystals grown by Bridgman method. It was found that a discontinuity in $TlGa_xIn_{1-x}Se_2$ solid solutions occurred in the composition range 0.25$0.0{\leq}X{\leq}0.25$) to the monoclinic structure ($0.65{\leq}X{\leq}1.0$) was observed in this composition range. The temperature dependences of the energy gap and the dielectric constant in $TlGaSe_2$ single crystal have shown that the anomalies appeared at 107 K and 120 K corresponding to first-order and second-order phase transitions, respectively.

  • PDF

Processing, structure, and properties of lead-free piezoelectric NBT-BT

  • Mhin, Sungwook;Lee, Jung-Il;Ryu, Jeong Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.25 no.4
    • /
    • pp.160-165
    • /
    • 2015
  • Lead-free piezoelectric materials have been actively studied to substitute for conventional PZT based solid solution, $Pb(Zr_xTi_{1-x}O_3)$, which occurs unavoidable PbO during the sintering process. Among them, Bismuth Sodium Titanate, $Na_{0.5}Bi_{0.5}TiO_3$ (abbreviated as NBT) based solid solution is attracted for the one of excellent candidates which shows the strong ferroelectricity, Curie temperature (Tc), remnant polarization (Pr) and coercive field (Ec). Especially, the solid solution of rhombohedral phase NBT with tetragonal perovskite phase has a rhombohedral - tetragonal morphotropic phase boundary. Modified NBT with tetragonal perovskite at the region of MPB can be applied for high frequency ultrasonic application because of not only its low permittivity, high electrocoupling factor and high mechanical strength, but also effective piezoelectric activity by poling. In this study, solid state ceramic processing of NBT and modified NBT, $(Na_{0.5}Bi_{0.5})_{0.93}Ba_{0.7}TiO_3$ (abbreviated as NBT-7BT), at the region of MPB using 7 % $BaTiO_3$ as a tetragonal perovskite was introduced and the structure between NBT and NBT-7BT were analyzed using rietveld refinement. Also, the ferroelectric and piezoelectric properties of NBT-7BT such as permittivity, piezoelectric constant, polarization hysteresis and strain hysteresis loop were compared with those of pure NBT.

Effect of Metastable Tetragonal $ZrO_2$ Phase on the Mechanicmal Properties in $Al_2O_3-ZrO_2$ System ($Al_2O_3-ZrO_2$계에서 기계적 성질에 미치는 준안정 저앙 $ZrO_2$상의 효과)

  • Kim, Jin-Young;Hwang, Kyu-Hong;Kim, Hwan
    • Journal of the Korean Ceramic Society
    • /
    • v.21 no.2
    • /
    • pp.149-155
    • /
    • 1984
  • The effect of $ZrO_2$ dispersed phase on the mechanical properties in $Al_2O_3$-$ZrO_2$system has been studied. There are both metastable tetragonal phase and stable monoclinic phase of $ZrO_2$particles diespersed in Al2O3 matrix at room temperature. Metastable tetragonal $ZrO_2$ changes to the stable monoclinic structure within the stress field of the crack. And microcracks are formed by the expansion of $ZrO_2$during the tetragonal-monoclinic transformation on cooling. Therefore stress-induced phase transformation and inclusion-induced microcracking contribute to the mec-hanical properties of $Al_2O_3$-$ZrO_2$system. Sintered composites containing 10m/o $ZrO_2$ yield KiC values of 6.5MN/$m^{3/2}$ much greater than that of pure $Al_2O_3$ This increase results from microcrack extension and stress-induced phase transformation absor-bing energy by crack propagation. Flexural strength of composites is decreased considerably in comparison with pure $Al_2O_3$ This decrease results from microcrack as a crack former and higher porosity than pure $Al_2O_3$.

  • PDF

Studies on the Pathogenicity of Cytoplasmic Polyhedrosis Virus and the Phenomena of Induction and Interference by Oral Inoculation of Foreign Virus to the Silkworm, Bombyx mori L. (가잠에 있어서 세포질다각체 바이러스의 병원성 및 이형 바이러스 접종에 의한 유발 간섭현상에 관한 연구)

  • 김근영;문재유;임종성;정태암
    • Journal of Sericultural and Entomological Science
    • /
    • v.17 no.2
    • /
    • pp.101-118
    • /
    • 1975
  • The pathogenicity of hexagonal and tetragonal cytoplasmic polyhedron virus to one of present leading silkworm varieties, Jam 103${\times}$Jam 104, and its parents, Jam 103 and Jam 104, was investigated. The activation of occult virus by oral inoculation of foreign virus as well as the interference phenomena between the activated and inoculated cytoplasmic polyhedron viruses was observed and the results obtained are as follows. 1. The pathogenicity of cytoplasmic polyhedrosis viruses. 1) There was a high significant difference in the pathogenicity of hexagonal polyhedron virus between the hybrid and its parents showing the lowest infection rate in the hybrid (Jam 103${\times}$Jam 104), medium infection rate in the Japanese line (Jam 103) and the highest infection rate in the Chinese line (Jam 104). In the pathogenicityof tetragonal polyhedron virus, a significant difference was observed only between the hybrid (Jam 103${\times}$Jam 104) and the Chinese line (Jam 104) by showing a higher infection rate in the Chinese line than in the hybrid. 2) The pathogenicity of both hexagonal and tetragonal polyhedron viruses showed a high significant difference in different silkworm instars inoculated by showing a higher infection rate at the second instar than at the fourth instar. 3) The pathogenicity of both hexagonal and tetragonal polyhedron viruses was increased as the concentration of viruses inoculated increased. 2. The phenomena of induction and interference by oral inoculation of foreign virus. 1) The induction rate of cytoplasmic polyhedrosis virus was higher in the parents than in the hybrid. In the parents. a higher rate in the Chinese line than in the Japanese line was observed. 2) The effect of inoculation at different instars on the induction was studied and the induction rate was higher at the second instar inoculated than at the fourth instar inoculated. 3) The degree of activation of hexagonal polyhedron virus with inoculation of tetragonal polyhedron virus was very high when a lower concentration of virus was inoculated and it was very low when a higher concentration of virus was inoculated 4) The degree of activation of tetragonal polyhedron virus with inoculation of hexagonal polyhedron virus was very low when a lower concentration of virus was inoculated and it was not observed when a higher concentration of virus was inoculated. 5) The mixed infection rate with hexagonal and tetragonal polyhedron viruses was higher at the second instar inoculated than at the fourth instar inoculated. 6) It was observed that the secondary hexagonal pc]yhedron virus activated interfered with the primary tetragonal polyhedron virus inoculated when the inoculated concentration of the primary virus is low and the primary virus inoculated interfered with the secondary virus activated when the inoculated concentration of the primary virus is high.

  • PDF

Effect of Transition Metal Oxides Addition on Yttria - stabilized Zirconia for improving Physical and Mechanical Properties

  • Park, Jaesung;Lee, Yeongshin
    • Journal of Korea Society of Digital Industry and Information Management
    • /
    • v.12 no.3
    • /
    • pp.25-31
    • /
    • 2016
  • Mechanical properties of Y2O3-containing tetragonal ZrO2 polycrystals(Y-TZP) were investigated. Several additives were used to modify the hardness and fracture toughness of Y-TZP. The effects of these individual additives were discussed and their interactions were also analysed. Each additive, such as CoO, Fe2O3, MnO2 was found to deteriorate the mechanical properties of Y-TZP when it was used singly. But the fracture toughness of Y-TZP was significantly improved when these additives and Al2O3 were added in combination at a certain ratio. The addition of CoO, Fe2O3 and MnO2 into Y-TZP resulted in the more complex behavior of fracture toughness and hardness. The specimen with 1.5 wt%-Fe2O3, 3.0 wt% -Al2O3 and 1.5 wt%-CoO showed the monoclinic to tetragonal phase ratio of 18% and the highest toughness of $10.8MPa{\cdot}m1/2$ with Vickers hardness of 1201 kgf/mm2. However, the toughness decreased as the ratio increased and macrocracks developed beyond the ratio of 25%. Sample No. 16 is improved high Physical and Mechanical Properties.

Influence of Applied Electric Field on Low Temperature Degradation of Y-TZP (인가 전압이 Y-TZP의 저온열화에 미치는 영향)

  • 장주웅;이홍림;김대준;오남식;이득용
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.12
    • /
    • pp.1254-1260
    • /
    • 1997
  • Influence of applied electric field on the low temperature degradation of 3 mol% YaO3 stabilized tetragonal zirconia polycrystals(3Y-TZP) was investigated using X-ray diffractometry of specimens aged under the dc field of 1.1 kV/mm in silicone oil both of 12$0^{\circ}C$-21$0^{\circ}C$. After the aging, the tetragonal to monoclinic phase transformation was observed only on the specimen surface of 3Y-TZP faced to the anode. This indicated that the surface was overcrowded with oxygen ions as a result of diffusion of oxygen vacancies toward the cathode-sided surface. To elucidate an influence of the applying time of the electric field on the extent of the degradation of 3Y-TZP in air, specimens were aged fore 0-2 hours under the electric field in the oil bath of 12$0^{\circ}C$ and then subsequently aged for 3h at 22$0^{\circ}C$ in air. The longer the specimens were aged under the field, the more extensive the transformation to the monoclinic phase was on the specimen surface faced to the cathode, probably originated from a high diffusion rate of oxygen ions due to a steep oxygen vacancy concentration gradient.

  • PDF

A Study on the Ceria Stabilized Tetragonal Zirconia Polycrystals(Ce-TZP)(I) : Effect of CeO2 Content on the Mechanical Properties and Fracture Behavior of Ce-TZP (CeO2 안정화 정방정 Zirconia 다결정체(Ce-TZP)에 관한 연구(I) : CeO2 함량에 따른 Ce-TZP의 기계적 성질과 파괴거동의 변화)

  • 김문일;박정현;강대석;문성환
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.5
    • /
    • pp.719-727
    • /
    • 1989
  • By using commercial zirconia powder CeO2-ZrO2 ceramics containing 8~16mol% CeO2 was made by heat treatment at 1350~155$0^{\circ}C$ for 1~10hr. The minimum amount of CeO2 for obtaining complete tetragonal phase was 12mol%, and in the tetragonal phase region fracture toughness of Ce-TZP was decreased with increasing CeO2 content and the maximum value was obtained when 12mol% CeO2 was added. The bending strength goes through maximum at 14mol% CeO2. Fracture mode of Ce-TZP transformed from intergranular to transgranular fracture with increasing CeO2 content, so the morphology of fracture surface of 16mol% Ce-TZP was wholly transgranular and this tendency was independent on grain size. The crystal structure of the 12mol% Ce-TZP was monoclinic with fringes along the grain boundaries which are lying in the particular plane from the TEM observation. The chemical composition of the sintered body was homogeneous as a whole and some amorphism or air pocket was observed at the triple junction.

  • PDF

Structure and Electric Properties of PZT Ceramics Substituted by La and Nd (La와 Nd가 치환된 PZT 세라믹의 구조 및 전기적 성질)

  • Jung, Soo-Cheol;Park, Hyu-Bum;Kim, Jeong;Kim, Keon;Kim, Si-Joong
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.2
    • /
    • pp.155-160
    • /
    • 1994
  • PZT ceramics substituted by La3+ and Nd3+ were fabricated according to the formula: [Pb1-x(La or Nd)x][Zr0.58Ti0.42]1-x/4$\square$x/4O3(x=0.00, 0.02, 0.05, 0.08, 0.15, 0.20). The crystal structure and microstructure were investigated by XRD and SEM. It was observed that the phase transitions among rhombohedral, tetragonal, and cubic symmetry occured as the substitutional quantity increased. Dielectric constant, dissipation factor and piezoelectric coefficient (d33), of each sample were measured. The dielectric properties were changed as the substitutional quanity of rare earth ion increased. These changes could be explained by crystal structure and compositional fluctuaction. Its d33 was higher at tetragonal region near to phase boundry between rhombohedral and tetragonal, which was explained by reorientation of domain wall.

  • PDF