  • This paper is an experimental study on shear capacity of the high strength lightweight reinforced concrete beams with shear-depth ratio between 1.5 and 2.5. Thirteen T & rectangular beams were tested to determine their diagonal cracking and ultimate shear capacity. The major variables are shear span-depth ratio (a/d=1.5, 2.0, 2.5), concrete compressive strength(f'c=210, 24., 270㎏/㎠) and tensile steel ratio( =0.6, 1.2%). Based on results obtained from experiment of high strength lightweight reinforced concrete Beam & normal concrete, the following conclusions were drawn. (1) The shear capacity of high-strength lightweight concrete is less 15% than that of normal concrete under same condition. (2) As the results of Comparing this experimental datas with other various formulas. It is regarded that ACI 318-89 shear strength formula related tensile strength is proper to design formula of shear strength of high-strength lightweight reinforced concrete using lightweight concrete.

  • PDF

전단 하중을 경험한 후설치 고전단 링앵커의 인장 강도 (Tensile Strength of Post-Installed High-Shear Ring Anchors (HRA) After Shear Loading)

  • 전상현;천성철;김재열
    • 한국공간구조학회논문집
    • /
    • 제18권4호
    • /
    • pp.61-68
    • /
    • 2018
  • Tensile load tests were conducted on High-Shear Ring Anchors (HRAs) after shear load had been applied to the HRAs, which had been developed to reduce the number of the anchors. Test variables include the embedment length of the rod and the width of the specimens and a total of 12 specimens were tested. Test results show that the HRAs pulled out due to bond failure or steel failure occurred in case that the HRAs were installed to the members with 300mm or greater width and the embedment length of 160mm (the actual embedment of rod is 140mm) or deeper. Except 4 HRAs showing steel failure of rod, the minimum and average of test-to-prediction by ACI 318-14 ratios are 1.18 and 1.79, respectively. The tensile strength of HRAs, after shear load was applied to the HRAs, can be safely evaluated by the minimum among the concrete breakout strength and bond strength with the actual embedment length of the rod.

An evolutionary fuzzy modelling approach and comparison of different methods for shear strength prediction of high-strength concrete beams without stirrups

  • Mohammadhassani, Mohammad;Nezamabadi-pour, Hossein;Suhatril, Meldi;shariati, Mahdi
    • Smart Structures and Systems
    • /
    • 제14권5호
    • /
    • pp.785-809
    • /
    • 2014
  • In this paper, an Adaptive nerou-based inference system (ANFIS) is being used for the prediction of shear strength of high strength concrete (HSC) beams without stirrups. The input parameters comprise of tensile reinforcement ratio, concrete compressive strength and shear span to depth ratio. Additionally, 122 experimental datasets were extracted from the literature review on the HSC beams with some comparable cross sectional dimensions and loading conditions. A comparative analysis has been carried out on the predicted shear strength of HSC beams without stirrups via the ANFIS method with those from the CEB-FIP Model Code (1990), AASHTO LRFD 1994 and CSA A23.3 - 94 codes of design. The shear strength prediction with ANFIS is discovered to be superior to CEB-FIP Model Code (1990), AASHTO LRFD 1994 and CSA A23.3 - 94. The predictions obtained from the ANFIS are harmonious with the test results not accounting for the shear span to depth ratio, tensile reinforcement ratio and concrete compressive strength; the data of the average, variance, correlation coefficient and coefficient of variation (CV) of the ratio between the shear strength predicted using the ANFIS method and the real shear strength are 0.995, 0.014, 0.969 and 11.97%, respectively. Taking a look at the CV index, the shear strength prediction shows better in nonlinear iterations such as the ANFIS for shear strength prediction of HSC beams without stirrups.

Soil-Bentonite 혼합토의 강도 특성 (Strength Characteristics of Soil-Bentonite Mixture)

  • 김광일;신동훈;임은상;김기영
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2009년도 춘계 학술발표회
    • /
    • pp.844-851
    • /
    • 2009
  • A soil mixture with low permeability and bentonite as an additive has been highly utilized as a cutoff material in landfills, banks, and dams. Even though it is anticipated that the water can seep through shear failures in the filter layer due to external loads and embankment loads during construction, usually only the coefficient of permeability of the soil mixture is considered rather than the changes of strength from the different amounts of additives. Therefore, the amount of bentonite was changed between 0%~4% in the soil mixture of the bed material to conduct a series of unconfined compressive strength, tensile strength, and shear strength tests on a specimen in order to study the characteristics of the strength. In the result, the unconfined compressive and tensile strength were increased along with the increased amount of bentonite in the low water content; however, the tensile strength in the consolidated-drained shear test generally showed similar values without significant changes.

  • PDF

섬유강화 복합재료에서 섬유열화에 따른 계면특성의 변화 (Change of Interfacial properties by the Fiber Degradation in the Fiber Reinforced Composites)

  • 문창권;김영대;노태영
    • 한국해양공학회지
    • /
    • 제12권3호통권29호
    • /
    • pp.31-41
    • /
    • 1998
  • Single fiber fragmentation technique was used to evaluate the change of interfacial properties by degradation of fiber tensile strength in the fiber reinforced composites. The influences of fiber tensile strength on the interfacial properties have been evaluated by the fragmentation specimens(weak fiber samples) of glass fiber/epoxy resin that was made using the pre-degraded glass fiber in distilled water at $80^{circ}C$ for specified periods. The effects of the immersion time on the interfacial properties in the distilled water at $80^{circ}C$ also have been evaluated by the fragmentation specimens(original fiber samples) of glass fiber/epoxy resin that was made using the received glass fiber. As the result, the tensile strength of glass fiber was decreased with the increasing of the treatment time in the distilled water at $80^{circ}C$ and the interfacial shear strength was independent of the change of the glass fiber strength in the single fiber fragmentation test. But in the durability test using the single fiber fragmentation specimen, interfacial shear strength decreased with the increasing of the immersion time in distilled water ar $80^{circ}C$. And it turned out that the evaluating of interfacial shear strength using original fiber tensile strength was valuable in the durability test for the water environment by the single fiber fragmentation technique.

  • PDF

점용접 아연도금판의 강도특성에 대한 온도 및 침수의 영향 (Effect of Temperature and Water Assumtion on Strength of Spot Welded Zine Steel Plates)

  • 서도원;윤호철;최준용;임재규
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.358-363
    • /
    • 2003
  • Spot welded structure is operated in diverse situation because of temperature, humidity and precipitation. In addition factors of environmental pollution such as acid rain, that courses corrosion, have the tendency to increase, But spot welded structure strength is affected by dampness and environment temperatures. Therefore, it is important to evaluate effect of temperature of spot welded part, In this study, the strength distribution of spot welded plates is evaluated about the environmental temperature of zine coated steel plates and test is conducted with welded part immersed in distilled and synthetic sea water. Specimens are immersed into water for 10, 100, 500 and 1000hours to evaluate the effects of water immersion time on tensile-shear strength under the conditions of -40, 0, 20 and $50^{\circ}C$. Strength is evaluated by tensile-shear test. The conditions of spot welding are 240kgf electrode force, 10KA welding current with 0 and 5mm clearance. From this study, spot welded specimens with clearance have lower tensile-shear strength in the distilled water or synthetic sea water comparing with spot welded specimens without clearance. And they have lower tensile-shear strength under $-40^{\circ}C$ and over $50^{\circ}C$.

  • PDF

전단경간비와 주인장철근비가 철근콘크리트 보의 최소전단철근비에 미치는 영향 (Effects of Shear Span-to-depth Ratio and Tensile Longitudinal Reinforcement Ratio on Minimum Shear Reinforcement Ratio of RC Beams)

  • 이정윤;김욱연;김상우;이범식
    • 콘크리트학회논문집
    • /
    • 제16권6호
    • /
    • pp.795-803
    • /
    • 2004
  • 현행 구조설계기준식에서는 취성적으로 파괴하는 최소전단보강철근 파괴를 방지하기 위하여 철근콘크리트 보에 최소전단보강철근을 배근하도록 규정하고 있다. 최소전단철근비는 콘크리트의 압축강도와 함께 주인장철근비와 전단경간비에 영향을 받는다. 이 연구에서는 주인장철근비와 전단경간비가 철근콘크리트 보의 최소전단철근비에 미치는 영향을 파악하기 위하여 14개의 철근콘크리트 보를 실험하였다. 실험에 의하면 전단 여유율은 주인장철근비가 증가할수록 증가하였고, 전단경간비가 증가할수록 감소하였다. 실험 결과는 ACI 318-02 기준식과 선행 연구의 제안식과 비교되었다.

Static behavior of high strength friction-grip bolt shear connectors in composite beams

  • Xing, Ying;Liu, Yanbin;Shi, Caijun;Wang, Zhipeng;Guo, Qi;Jiao, Jinfeng
    • Steel and Composite Structures
    • /
    • 제42권3호
    • /
    • pp.407-426
    • /
    • 2022
  • Superior to traditional welded studs, high strength friction-grip bolted shear connectors facilitate the assembling and demounting of the composite members, which maximizes the potential for efficiency in the construction and retrofitting of new and old structures respectively. Hence, it is necessary to investigate the structural properties of high strength friction-grip bolts used in steel concrete composite beams. By means of push-out tests, an experimental study was conducted on post-installed high strength friction-grip bolts, considering the effects of different bolt size, concrete strength, bolt tensile strength and bolt pretension. The test results showed that bolt shear fracture was the dominant failure mode of all specimens. Based on the load-slip curves, uplifting curves and bolt tensile force curves between the precast concrete slab and steel beam obtained by push-out tests, the anti-slip performance of steel-concrete interface and shear behavior of bolt shank were studied, including the quantitative analysis of anti-slip load, and anti-slip stiffness, frictional coefficient, shear stiffness of bolt shank and ultimate shear capacity. Meanwhile, the interfacial anti-slip stiffness and shear stiffness of bolt shank were defined reasonably. In addition, a total of 56 push-out finite element models verified by the experimental results were also developed, and used to conduct parametric analyses for investigating the shear behavior of high-strength bolted shear connectors in steel-concrete composite beams. Finally, on ground of the test results and finite element simulation analysis, a new design formula for predicting shear capacity was proposed by nonlinear fitting, considering the bolt diameter, concrete strength and bolt tensile strength. Comparison of the calculated value from proposed formula and test results given in the relevant references indicated that the proposed formulas can give a reasonable prediction.

기계적 프레스 접합법을 이용한 A1-5052 인장-전단 시험편의 강도 평가에 관한 실험적 연구 (An Experimental Study on the Strength Evaluation of A1-5052 Tensile-Shear Specimens Using a Mechanical Press Joining Method)

  • 임두환;이병우;류현호;김호경
    • 한국공작기계학회논문집
    • /
    • 제12권1호
    • /
    • pp.58-64
    • /
    • 2003
  • A mechanical press joining was investigated in ender for joining A1-5052 sheets for automobile body weight reduction. Static tensile and fatigue tests were conducted using tensile-shear specimens for evaluation of fatigue strength of the joint. During Tox joining process for A1-5052 plates, using the current sheet thickness and punch diameter, the optimal applied punching force was found to be 32 kN under the current joining condition. For the static tensile-shear experiment results, the fracture mode is classified into interface fracture mode, in which the neck area fractured due to influence of neck thickness, and pull-out fracture mode due to influence of plastic deformation of the joining area. And, during fatigue tests for the A1-5052 tensile shear specimens, interface failure mode occurred in the region of low cycle. The fatigue endurance limit approached to 6 percents of the maximum applied load, considering fatigue lifetime of $2.5\times10^6$ cycles.

강섬유 보강 초고성능 콘크리트(UHPFRC) I형 보의 전단 강도 (Shear Strength of Ultra-High Performance Fiber-Reinforced Concrete(UHPFRC) I-shaped Beams without Stirrup)

  • 이지형;홍성걸
    • 콘크리트학회논문집
    • /
    • 제29권1호
    • /
    • pp.53-64
    • /
    • 2017
  • 강섬유 보강 초고성능 콘크리트(UHPFRC)는 높은 압축강도 뿐 아니라 강섬유 보강에 의한 뛰어난 응력분산효과로 인해 높은 인장강도를 가지며, 미세균열의 확장을 통해 균열 후에도 경화거동을 하여 구조부재가 안정적으로 외력에 저항하도록 한다. 본 연구에서는 UHPFRC 재료 인장강도를 정의함에 있어 노치가 있는 휨실험과 직접인장실험을 비교하여 실험법 및 결과 분석의 장단점을 알아보았다. I-형 보의 전단부재실험은 복부의 면내전단거동을 알아보기 위하여 전단 경간비, 유효높이, 재료인장강도를 변수로 계획하였다. 실험결과를 통해 전단보강근이 없는 UHPFRC I형 보의 균열발생 이후 전단거동의 응력 재분배효과를 정량적으로 판단하고, 균열 후 거동을 기존 전단 강도식이 잘 반영하고 있는지 검토하였다. 전단철근 보강이 없는 UHPFRC 전단부재의 경우 파괴모드는 사인장 파괴로 동일하였고, 이러한 파괴모드를 가지는 부재는 전단 경간비와 유효높이에 크게 영향을 받게 되어 부재 설계 시 이러한 변수에 대한 고려가 필요한 것으로 나타났다.