음향방출과 초음파를 이용한 TIG 용접탄소강의 미시적 손상평가 (Evaluation of Microscopic Damage to TIG Welded Carbon Steel using Acoustic Emission and Ultrasonic Test)

  • 이준현;이진경
    • 한국해양공학회지
    • /
    • 제26권5호
    • /
    • pp.5-10
    • /
    • 2012
  • In this study, carbon steel (A53) is used as the material for the pipes in a marine plant and ship industry. Welds are necessary to join the carbon steel, and the effect of this welding on the properties of the carbon steel has been studied by many researchers. In this study, the dynamic behavior of welded carbon steel was studied using an acoustic emission (AE) technique, which is a nondestructive test. There are numerous AE parameters that can be used to analyze the damage behavior of carbon steel by external loading. The AE parameters of energy, cumulative count, amplitude, and AE event were used, and each parameter was differentiated according to the degree of damage to the carbon steel. The energy showed a high level at the elastic range of the load curve, while the amplitude had the highest value at the hardening region. The cumulative count showed a growth tendency similar to the loading curve. In addition, an ultrasonic technique and hardness test were applied to evaluate the mechanical properties according to the base zone, HAZ region, and weld zone of the weld specimen. The velocity and attenuation ratio showed little change between zones, and an evaluation of the ultrasonic waves on each zone of the specimen was found to be a useful method to clarify the mechanical properties of the carbon steel.

저탄소강 SS41 연속파형 Nd:YAG 레이저 겹치기 용접의 기공제어 기술 (The Porosity Control Technology of Lap Joint Welding Using Continuous Wave Nd:YAG Laser of the Low Carbon Steel SS41)

  • 이가람;황찬연;양윤석;박은경;유영태
    • 한국생산제조학회지
    • /
    • 제22권4호
    • /
    • pp.665-672
    • /
    • 2013
  • With the development of advanced processing technology, laser processing systems, which require high-quality precision processing, have attracted considerable attention. Although laser equipment is expensive, it enables quick processing and less deformation of materials. This technology is often applied to secondary batteries, which has thus farinvolved the use of argon tungsten inert gas (TIG) welding. However, the welding characteristics of argon TIG welding are not yet good, and a laser is used for welding to address this problem. In this study, lap-joint welding was conducted, and the desired welding characteristics were obtained when the laser power was 1800W and the laser beam travel speed was 1.8 m/min. Lap-joint welding was conducted on Ni-coated SS41. Two cases were compared. No pores were observed in the Ni-coated SS41 lap-joint welding part, and cracks appeared from the lap-joints. Moreover, the pole rod and tap were welded together in a T-joint form to improve the output of the secondary battery. T-joint laser welding showed better welding characteristics than TIG welding.

LNG선용 INVAR(Fe-36%Ni)강 Lap 이음부의 피로강도와 허용응력에 관한 연구 (A Study on the Fatigue Strength and Allowable Stress of INVAR(Fe-36% Ni) Steel Lap Joint Applied to Cargo Containment of LNG Carrier)

  • 한명수;한종만;한용섭
    • Journal of Welding and Joining
    • /
    • 제12권1호
    • /
    • pp.102-115
    • /
    • 1994
  • This paper is to evaluate the fatigue strength of lap joints of materials applied to LNG carrier cargo containment of GAZ-TRANSPORT(GT) type, which was welded by manual and automatic TIG welding process. The thicknesses of lapped members were 1.5mm/1.5mm or 1.5mm/0.7mm in Invar to Invar joint, and 1.5mm/8.0mm in Invar to stainless steel joint, respectively. These lap joints were mainly applied to the membrance fabrication of GT-LNG carrier. Fatigue tests of Invar/Inar lap joints were conducted under the stress ratio R=0 at room temperature. The effect of mean stress and cumulative fatigue damage on the allowable stress of Invar lap joint was evaluated on the basis of test results. Fatigue test was also conducted on Inver/Stainless steel lap joints welded by automatic TIG process without filler metals. The fatigue test of the joint was carried out under the same conditions as those of Invar/invar lap joints. The fatigue strength of the joint welded without filler metal was comparable to those welded with filler metal quoted from reference. The fatigue strength of Invar/stainless steel lap joint was only dependent on the lap throat thickness, and not on the welding process. Based on test results, the applicability of TIG welding process without filler metal in Invar/stainless steel lap joint was reviewed by controlling welding variables to assure the valid throat thickness of lap joints.

  • PDF

핵융합로용 저방사화 철강재료(JLF-1)의 강도와 파괴인성 (Strength and fracture toughness of reduced - activation ferritic steel (JLF-1) for fusion reactor application)

  • 윤한기;김동현;이상필;박이현;공유식
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.13-18
    • /
    • 2003
  • Reduced activation ferritic steel, JLF-1 steel (Fe-9Cr-2W-V-Ta), is one of the promising candidate materials for fusion reactor applications. Fracture toughness ($J_IC$) and tensile tests were carried out at room temperature and elevated temperature ($400^{\circ}C$). Two types of CT specimen were prepared to examine the effect of rolling direction on the fracture toughness of JLF-1 steel. Four types of tensile specimen were also prepared to investigate the property by the rolling direction and welding. The Micro Vickers hardness was measured at various distances of a cross section of the TIG joints of JLF-1 steel according to the heating history of each position. Finally, the fracture surface was observed by scanning electron microscopy (SEM).

  • PDF

열간 곡면성형된 Al5083 후판의 TIG 용접 시 루트갭 최소화를 위한 최적 블랭크 형상 결정 (Determination of Optimum Blank Shape to Minimize the Root Gap during TIG Welding in Hot Curvature Forming of Al5083 Thick Plate)

  • 이정민;고대훈;이경훈;이찬주;김병민
    • 한국정밀공학회지
    • /
    • 제30권8호
    • /
    • pp.815-823
    • /
    • 2013
  • The hot curvature forming of large aluminum plates is a process used to produce spherical liquefied natural gas (LNG) tanks. In this study, we describe a method to determine the optimum shape of blanks to minimize the root gap in the forming process. The method proposed in this study was applied to a small-scale model for thick plates with a curvature of 1500 mm and thickness of 6 mm. First, the shape of the curved shells was determined as the target shape, and then a coordinate transform was used to determine the optimum blank shape, which was then iteratively modified using the results of finite element method (FEM) simulations, including heat transfer, until the shape error was minimized. Experiments in forming using Al5083 thick plate were carried out, showing that the method can determine the optimum blank shape within an allowable root gap of 0.1 mm.

해수용 재료의 TIG용접후 열처리에 따른 특성 평가 (Evaluation of the Properties of Seawater Materials by Heat Treatment after TIG Welding)

  • 배동수;이진경
    • 한국산업융합학회 논문집
    • /
    • 제24권5호
    • /
    • pp.517-523
    • /
    • 2021
  • In this study, in the selection of materials for the elements of a small plant, those with high resistance to corrosion are selected and the material properties of coatings for corrosion prevention are evaluated. In addition, corrosion characteristics and material analysis were performed on the welded part, and the hardness characteristics of the welded part, heat-affected part, and the base metal were evaluated. In the case of the post-weld-heat-treated(PWHT) specimen, the corrosion resistance of STS 316 was lower than that of the specimen without the PWHT due to the formation of intergranular carbide. As a result of evaluating the distribution of the hardness of the weld before and after the PWHT, the hardness of the specimen after the PWHT increased by about 20 Hv. As a result of the corrosion test on the welded specimen, the weight loss tended to increase as the time increased. In the case of the PWHT specimen, the corrosion resistance tended to be significantly lower than that of the specimen without PWHT due to the formation of intergranular carbide.

LASER WELDING OF SINGLE CRYSTAL NICKEL BASE SUPERALLOY CMSX-4

  • Yanagawa, Hiroto;Nakamura, Daisuke;Hirose, Akio;Kobayashi, Kojiro F.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.193-198
    • /
    • 2002
  • In 1his paper, applicability of laser welding to joining process of single crystal nickel base superalloy turbine blades was investigated. Because heat input of laser welding is more precisely controlled 1han TIG welding, it is possible to optimize solidification microstructure of the welds. Since in single crystal nickel base superalloy the crystal orientation have a significant effect on the strength, it is important to control the solidification microstructure in the fusion zone. A single crystal nickel base supera1loy, CMSX-4, plates were bead-on welded and butt welded using a $CO_2$ laser. The effects of microstructure and crystal orientation on properties of the weld joints were investigated. In bead-on weldling, welding directions were deviated from the base metal [100] direction by 0, 5, 15 and 30 degrees. The welds with deviation angles of 15 and 30 degrees showed fusion zone transverse cracks. As the deviation angles became larger, the fusion zone had more cracking. In the cross section microstructure, the fusion zone grains in 0 and 5 degrees welds grew epitaxially from the base metal spins except for the bead neck regions. The grains in the bead neck regions contained stray crystals. As deviation angles increased, number of the stray crystals increased. In butt welding, the declinations of the crystal orientation of the two base metals varied 0, 5 and 10 degrees. All beads had no cracks. In the 5 degrees bead, the cross section and surface microstructures showed that the fusion zone grains grew epitaxially from the base metal grains. However, the 10 degrees bead, the bead cross section and surface contained the stray crystals in the center of the welds. Orientations of the stray crystals accorded with the heat flow directions in the weld pool. When the welding direction was deviated from the base metal [100] direction, cracks appeared in the area including the stray crystals. The cracks developed along the grain boundaries of the stray crystals with high angles in the final solidification regions at the center of the welds. The fracture surfaces were covered with liquid film. The cracks, therefore, found to be solidification cracks due to the presence of low melting eutectic. As the results, in both bead-on welding and butt welding the deviation angles should be control within 5 degrees for preventing the fusion zone cracks. To investigate the mechanical properties of the weld joints, high temperature tensile tests for bead-on welds with deviation angles of 0 and 5 degrees and the butt welds with dec1ination angles of 0, 5 and 10 degrees were conducted at 1123K. The the tensile strength of all weld joints were more 1han 800MPa that is almost 80% of the tensile strength of the base metal. The strength of the laser weld joints were more than twice that of tue TIG weld joints with a filler metal of Inconel 625. The results reveals 1hat laser welding is more effective joining process for single crystal nickelbase superalloy turbine blades 1han TIG welding.

  • PDF

초음파 적외선 열화상을 이용한 마찰교반용접부의 결함 검출 (Using ultrasound infrared thermography to detect defects in lap joint Friction stir welding)

  • 박희상;최만용;박정학;이영호;최원용;고준빈;최원두
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.67-67
    • /
    • 2009
  • 알루미늄 합금 재질은 무게의 경량화와 기계적강도가 우수하며 다른 비철금속에 비하여 값이 저렴한 장점이 있다. 현재 산업현장에서 활용하는 가장 흔한 접합법으로 TIG, RSW 등과 같은 용융 용접법을 현재는 많이 사용 하고 있지만 열전도도가 높아 열 확산이 빠르고, 이에 따라 모재의 팽창이 일어나 열변형을 유발하며, 산화피막은 그 내부에 함유된 결정수가 아크용접 중 분해되어 수소를 방출함으로 기공이 발생하여 부도체로 저항용접시 전도성을 방해하는 등의 문제를 발생시킨다. 또한 철에 비해 4배정도 큰 전기전도율에 따라 저항용접시 대전류를 사용해야 하는 등의 문제점이 발생하고 있다. 이와 같은 알루미늄 합금의 용융용접 과정에서 발생하는 단점을 극복하는 기술로 고상접합 방법인 마찰교반용접법(Friction Stir Welding)이 활용되고 있다. FSW는 1991년 영국의 TWI에서 개발된 최신 용접법으로 모재를 용융점 아래에서 고상용접시키는 방법으로 용융에 따른 열변형과 흄가스(hume gas)와 스패터(spatter)를 억제시켜 주는 친환경적인 용접법이다. 이러한 마찰교반용접의 기술은 그동안 특허에 따른 로열티가 산업현장에서 사용하는데 문제가 되었으나 특허보호 기간인 20년이 1년정도의 기간밖에 남지 않은 상황에서 그 사용은 날로 증가하리라 본다. 이러한 마찰교반용접부의 결함을 평가하는 방법에는 UT, RT 등이 활용되고 있으나 얇은 박판에서의 결함검출은 용이하지 않다. 이리한 문제점을 해결하기위하여 초음파 가진을 이용한 적외선 열화상 검출 기법을 이용하여 마찰교반용접부의 결함 검출 가능성을 연구하였다. 20kHz의 주파수를 400Watt로 가진시켜 겹치기(lap joint) 마찰교반용접이된 A6061-T6의 용접부에 초음파를 입사하였을 때 발생하는 열을 적외선 열화상 카메라를 이용하여 측정함으로써 마찰교반겹치기 용접부의 결함 검출에 활용하였다. 용접부에 초음파를 입사하였을 때 부분적으로 온도차이가 발생하였고, 그에 따른 열화상을 검출 할 수 있었다. 이러한 열화상과 실제 시험편의 용접부의 강도를 평가하기 위하여 인장시험을 하였다. 그 결과 초음파 적외선 열화상 검출에서 발열부위가 나타난 부분이 인장시험에서 낮은 인장강도를 보였다.

  • PDF

NCS기반 국가기술자격 용접기능장 실기평가 방법 개선에 관한 연구 (A study on Improvement in evaluation method of practical skill test of national technique qualification of Master Craftsman Welding based on NCS)

  • 정상철;최성우
    • 한국산학기술학회논문지
    • /
    • 제17권2호
    • /
    • pp.596-600
    • /
    • 2016
  • 본 논문은 국가직무능력표준(NCS)기반 국가기술자격검정의 용접분야 실기시험 평가방법 개선을 목적으로 수행된 연구에 대한 내용을 기술한 것이다. 현행 용접기능장의 실기시험 내용을 체계적으로 분석한 후 최신 용접기술 동향을 반영하고 국가직무능력표준의 능력단위, 수행준거 등을 적용하여 용접기능장 실기시험의 새로운 평가방법을 제시하였고, 자문회의 및 시범평가를 통해 그 효과를 검증하였다. 향후 한국산업인력공단 기술자격출제실에서는 본 연구를 기초로 세부직무분야 전문가를 통한 출제 기준 개정을 완료 한 후 용접기능장 국가기술자격검정에 실제 적용할 예정이다.

용접 재료 별 해수 배관 용접부위의 부식 특성에 관한 전기화학적 평가 (An Electrochemical Evaluation of the Corrosion Property on the Welded Zone of Sea Water Pipe according to Welding Materials)

  • 김진경;원창욱;조황래;이명훈;김윤해;문경만
    • 한국해양공학회지
    • /
    • 제21권5호
    • /
    • pp.39-46
    • /
    • 2007
  • The sea water pipe of a ship's engine room is a severely corrosive environment caused by fast flawing sea water containing chloride ions and high conductivity. Therefore, leaking of sea water may occur as a result of local corrosion of the welded zone. Leaking is usually controlled by various welding methods. In this study, when the sea water pipe is welded with certain welding methods and welding electrodes, the corrosion resistance of WM (Welding metal) and HAZ (Heat affected zone) was investigated using electrochemical methods. Although the corrosion potential of the HAZ is higher than that of WM, the corrosion resistance of WM is superior to HAZ. However, when WM and HAZ are both opened to the sea water, the WM part with the anode was more seriously corroded than was the HAZ of the cathode by performance of a galvanic cell due to difference of the corrosion potential between HAZ and WM. In particular TIG welding showed relatively good results in corrosion resistance of both HAZ and WM compared to other welding methods.