섬유복합모르터의 뿜칠마감에 의한 고강도콘크리트 기둥부재의 폭렬방지 (Spatting Resistance of High Strength RC Column Covering Spray-on Materials of Fiber Composite Spray Mortar(FCSM))

  • 송용원;한동엽;이건철;고경택;김진수;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 춘계학술논문 발표대회 제6권1호
    • /
    • pp.5-8
    • /
    • 2006
  • High strength concrete has been increasingly used in high rue building and it is very obvious re consider fire resistance performance of that. Unlike the normal strength concrete, high strength concrete in sudden elevating temperature at fire is susceptible to spalling with severe explosion and surface split, due to high density of concrete. In order to endure the spalling, inner space temperature of concrete should be control less than certain point. Therefore this study investigated the influence of covering materials on high strength concrete finishing spray-on materials of fiber composite spray mortar(FCSM). Both polypropylene(PP) and polyvinyl alcohol(PVA) fiber were used in this test. Test showed that concrete, covering 18mm mortar containing PVA fiber and confining metal lath 2.3mm thickness, decreased 50% of main bar ambient temperature. compared with control concrete. In addition, concrete covering 18mm mortar without fiber caused falling of covering materials and then it was exposed in elevating temperature. As a result, spatting of the concrete occurred same as control concrete. However, concrete covering spray-on mortar containing PVA or PP fiber resisted spatting occurrence.

  • PDF

세피올라이트를 활용한 시멘트 경화체의 미세먼지 흡착 특성 (Fine Dust Adsorption of Cement Matrix Using Sepiolite )

  • 전은영;이상수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2023년도 가을학술발표대회논문집
    • /
    • pp.71-72
    • /
    • 2023
  • As industrialization and urbanization accelerate, environmental issues have moved from local concerns to global issues. Among them, air pollution is the most important issue. Modern people spend more than 88% of their day indoors, but the concentration of fine dust and pollutants flowing indoors is increasing. The indoor environment has its own complexity, and various substances used indoors, such as building materials, furniture, electronics, and cleaning agents, emit chemical substances and cause various diseases. Therefore, when selecting building materials and interior finishing materials, the pollutant emission and adsorption capacity must be greatly considered. These considerations will ensure the construction of a sustainable future environment and a healthy life within that environment. Therefore, in order to reduce the generation of indoor air pollutants, this study aims to examine the fine dust adsorption properties of cement hardening materials using sepiolite, which has a porous structure and high absorption power among clay minerals. As a result of the experiment, it was found that the concentration of fine dust decreased as the addition rate of sepiolite increased. It is believed that the fine dust concentration was reduced due to the high porosity due to the microfibrous structure and large specific surface area of sepiolite, which has a porous structure among clay minerals. It is believed that these experimental results can be used as basic research for future use of sepiolite as a construction material.

  • PDF

아토마이저를 이용한 PET 직물의 TiO2-Ag 나노입자 코팅 연구 (Study on the TiO2-Ag Nanoparticle Coated PET Fabric with an Atomizer)

  • 이현우;홍태민;손한글;임성찬;신원규;이승구
    • 한국염색가공학회지
    • /
    • 제26권2호
    • /
    • pp.99-105
    • /
    • 2014
  • In this study, $TiO_2$ and Ag powders were deposited on the PET fabric using an atomizer in order to study the characteristics of particle deposited fabric. To improve the particle deposition, the surface of the fabric was pre-treated with an electron beam and its effect was studied with the deposition of those elements on the fabric. The SEM was used to observe the morphology of the deposition fabric and through the EDS analysis, the deposition of $TiO_2$ and Ag was confirmed. Also, the absorbance of the particle deposited fabric was measured using the Methylene Blue to verify the photolysis nature of $TiO_2$. Moreover, the antibiotic nature of Ag on the surface of the PET fabric was identified through the antibiosis test.

고강도 Self-Leveling재의 최적 결합재비 (The Optimum Binder Ratio for High-Strength Self-Leveling Material)

  • 김진만
    • 한국건축시공학회지
    • /
    • 제2권4호
    • /
    • pp.89-98
    • /
    • 2002
  • Self-leveling material(SLM) is one of the floor finishing materials which make flat surface like as water level by itself in a short time. So it is possible to increase construction speed and enhance economical efficiency In this study, author intended to develop SLM for the industrial warehouse and factory loading heavy weight machinery and vehicles. The demanded properties for this type of SLM are above 200mm of flow value and above 300kgf/$cm^2$ of 28-days compressive strength. To possess demended strength and fluidity, SLM have to be composed of many types of binders and chemical additives. So it is difficult to decide suitable mixing proportion of composition materials. In this study, author investigated the weight percentage effect of main composition materials for high-strength self-leveling material, by experimental design such as tables of orthogonal arrays and simplex design, and by statistical analysis such as analysis of variance and analysis of response surface. Variables of experiments were ordinary Portland cement(OPC), alumina cement(AC), anhydrous gypsum(AG), lime stone(LS) and sand, and properties of tests were fluidity of fresh state and strength of hardened state. Results of this study are showed that suitable mix proportions of binders for the high strength self-leveling materials are two groups. One is 78~85.5% OPC, 7.5~9.5% AC, 9~12.5% AG and the other is 72.5~78% OPC, 9~12.5% AC, 13~15% AG.

다이빙용 웨트수트(wetsuit) 소재에 대한 소비자 인식조사와 물성 비교 (Consumer recognition and mechanical property comparison of wetsuit material for diving)

  • 상정선;오경화
    • 한국의상디자인학회지
    • /
    • 제20권4호
    • /
    • pp.163-174
    • /
    • 2018
  • Consumer and property evaluation of wetsuit materials were conducted to obtain useful data for developing competitive products that meet consumer expectations and improving industrial competitiveness. Data were collected through online surveys of 213 domestic consumers who have experienced wearing wetsuit among marine leisure activities. Five types of commercial wet suit materials by brand and four types of commercial wet suit materials with the same quality by thickness were collected. Then, their physical properties, salt water resistance and thermal insulation rate were evaluated and compared. As a result, the most commonly used wetsuit material is 3 to 5 mm thick, and the basic jersey material is bonded on both sides. As a processing for imparting functionality, processing for improving warmth and reducing surface resistance are most frequently used. Consumers often feel uncomfortable when wearing a wetsuit, such as wearing comfort, weight, ease of movement, stretchability, and clothing pressure, which are different from those of casual wear. Also, mechanical strength and warmth were considered to be the most important criteria for selection of wetsuit material for purchase or rental. The mechanical properties of brand A and B were better than those of brand C, D, and E. Resilience and thermal shrinkage were better in brand C, D, and E. On the other hand, there was no significant difference in the physical properties due to the difference in thickness of the material at the same quality. Also, it was found that the thicker the material, the more stable it is in the heat. Brand A and B had superior salt water resistance than brand C, D, and E. In the thermal insulation test, brand A and B showed better insulation characteristics than brand C, D, and E, but the types of bonded fabric and surface finishing of materials were thought to have affected. In comparison of the thickness, the thicker the materials, the better the salt resistance and the thermal insulation.

표면개질 스페셜티 카본블랙의 제조 및 잉크 특성 평가 (The Evaluation of the Preparation and Characterization of Inks based on Surface-modified Specialty Carbon Black(SCB))

  • 박동준;김송희;박수열
    • 한국염색가공학회지
    • /
    • 제30권3호
    • /
    • pp.168-179
    • /
    • 2018
  • The modified surface of specialty carbon black(SCB) is one of the main technical factors for producing a uniform color and stable dispersion. In this work, the carboxylation or sulfonation process of SCB was used to improve the dispersive properties of hydrophilic solvents such as 1,6-hexanediol and propylene glycol monomethyl ether acetate(PGMEA). The results showed that the color strength of SCB DC2500G changed little with a range of 0.128~0.941(${\Delta}E$) compared to other SCB DC2500G material. In contrast, in the case of SCB EG410, there was a uniform color value with a range of 0.144~0.252(${\Delta}E$). Also, in our experiments, a modified SCB was confirmed by printing ink material as a melt coating paper. It may be possible that the SCB EG410 material can be advantageous as a gravure ink product. Finally, the modified SCB obtained from this research will have a large impact on the industry as a potential material for toners, paint, rubber, fillers, and other carbon black additives.

표면마감처리에 따른 목질보드의 포름알데히드 방산특성에 관한 연구 (Study on the Characteristics of Formaldehyde Emission from Wood-Based Panels Treated with Several Surface Finishing Materials)

  • 소원택;임진아
    • Journal of the Korean Wood Science and Technology
    • /
    • 제34권3호
    • /
    • pp.30-37
    • /
    • 2006
  • 본 연구는 각종 실내디자인에 이용되는 목질보드의 포름알데히드(HCOH) 방산 특성과 몇 가지 VOC 저감 방법에 대한 포름알데히드의 방산량 변화를 측정하였다. 포름알데히드 방산량은 온도가 증가함에 따라 뚜렷이 증가하는 경향을 보였고, 측정 전 처리조건에 따라 포름알데히드 방산량의 현저한 변화가 나타났다. bake-out 처리후의 목질보드의 포름알데히드 방산량은 대조구와 비교하여 감소함을 나타냈다. 시편에 urethane, cashew, water stain, oil stain coating을 했을 때 각 마감재료에 따라 포름알데히드 방산량의 차이가 확인되었으며, edge sealing 처리 후 두드러진 감소경향이 나타났다. $TiO_2$ coating은 일반광보다는 자외선 램프의 포름알데히드 저감효율이 좋았고, 자외선 램프의 조사시간이 길어지면 포름알데히드의 감소량도 증가하였다.

고도정수처리용 콘크리트 금속용사 피막의 내오존성 및 오존처리 후 부착강도 평가에 관한 실험적 연구 (Experimental Study on Evaluation of Bond Strength after Ozone Treatment and Ozone Resistance of Concrete Metal Spray Coating for Advanced Water Treatment)

  • 박진호;장현오;이한승
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제22권4호
    • /
    • pp.68-75
    • /
    • 2018
  • 기존의 정수처리 방법으로는 제거되지 않는 물질이 발생함에 고도정수 처리 시설의 도입이 증가하고 있다. 그러나 오존을 이용한 고도정수처리 시설의 내부 방수 방식재는 오존의 산화력에 의해 열화되며 콘크리트까지 영향을 미쳐 내구성 저하의 원인이 된다. 본 연구에서는 내오존성 및 내화학성이 뛰어난 금속 패널을 기존의 시공법 보다 손쉬운 방법으로 시공하기 위한 방법으로 금속용사 공법을 이용하여 수처리 시설 콘크리트 구조물의 열화를 원천적으로 방지하기 위한 마감공법 개발 연구의 일원으로 용사금속 종류 및 피막의 표면처리 방법에 따른 내오존성 평가를 실시하였으며, 오존처리 후의 부착강도를 평가하였다. 실험결과 용사금속 Ti이 용사 후에도 내오존성이 뛰어난 것으로 나타났으며 표면처리 방법으로는 테프론계 봉공처리제를 사용하여 마감하는 것이 내오존성 및 부착성능 확보에 가장 적합한 방법이라 판단된다.

친환경.고유동 세라믹 수지 모르타르를 이용한 주차장 바닥용 표면 마감의 재료적 특성에 관한 실험적 연구 (An Experimental Study on Material Property of Parking Zone Flooring Occupancy Surface Finishing Used to Environment-friendly.High-liquidity Ceramic Resin Mortar)

  • 이선규;문유석;이형준;이완휘;오상근
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2008년도 춘계 학술발표회 제20권1호
    • /
    • pp.829-832
    • /
    • 2008
  • 1980년대 초반부터 대량 주택 공급과 고층 건축물의 급증으로 주차공간 부족현상이 사회적 문제점으로 지적되어져 왔다. 단적인 예로 서울시의 년간 주차장 개소 통계 연보를 살펴보면 2003년에 206,281 개소인 것이 2006년 237,770 개소로 약 15%의 증가율이 나타났다. 이와같이 매년 많은 주차시설이 확충되고 있는 것에 반하여 주차장 바닥에 사용되어지는 마감 재료의 대부분이 유기계 재료가 시공되어 지고 있다. 그러나 최근 "웰빙적 문화현상"에 따라 유기계 재료의 문제점(환경호르몬 배출, 휘발성유기화합물의 화재 위험 등)이 부각되고 있는 실정이다. 이에 본 연구에서는 작업자 뿐만아니라 사용자의 안전을 고려하여 인체 무해한 친환경 고유동 세라믹 수지 모르타르를 이용한 주차장 바닥 표면 마감재의 재료적 특성 분석 및 물성평가를 통하여 기존 유기계 바닥재의 문제점을 보완하고 새로운 개념의 주차장 바닥 마감재에 대한 현장 적용성을 확인하였다.

  • PDF

자기연마를 이용한 ELID 연삭면의 나노경면연마 (Nano-level mirror finishing for ELID ground surfsce using magnetic assisted polishing)

  • 이용철;곽태수;안제 정박;대삼 정
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.629-632
    • /
    • 2005
  • ELID(ELectrolytic In-process Dressing) grinding is an excellent technique for mirror grinding of various advanced metallic or nonmetallic materials. A polishing process is also required for elimination of scratches present on ELID grinded surfaces. MAP(Magnetic Assisted Polishing) has been used as a polishing method due to its high polishing efficiency and to its resulting in a superior surface quality. This study describes an effective fabrication method combining ELID and MAP of nano-precision mirror grinding for glass-lens molding mould, such as WC-Co, which are extensively used in precision tooling material. And for the optics glass-ceramic named Zerodure, which is extensively used in precision optics components too. The experimental results show that the combined method is very effective in reducing the time required for final polishing. The best surface roughness of the polished glass-ceramic was within 1.7nm Ra in this study.

  • PDF