  • The development of dry etching process for sapphire wafer with plasma has been key issues for the opto-electric devices. The challenges are increasing control and obtaining low plasma induced-damage because an unwanted scattering of radiation is caused by the spatial disorder of pattern and variation of surface roughness. The plasma-induced damages during plasma etching process can be classified as impurity contamination of residual etch products or bonding disruption in lattice due to charged particle bombardment. Therefor, fine pattern technology with low damaged etching process and high etch rate are urgently needed. Until now, there are a lot of reports on the etching of sapphire wafer with using $Cl_2$/Ar, $BCl_3$/Ar, HBr/Ar and so on [1]. However, the etch behavior of sapphire wafer have investigated with variation of only one parameter while other parameters are fixed. In this study, we investigated the effect of pressure and other parameters on the etch rate and the selectivity. We selected $BCl_3$ as an etch ant because $BCl_3$ plasmas are widely used in etching process of oxide materials. In plasma, the $BCl_3$ molecule can be dissociated into B radical, $B^+$ ion, Cl radical and $Cl^+$ ion. However, the $BCl_3$ molecule can be dissociated into B radical or $B^+$ ion easier than Cl radical or $Cl^+$ ion. First, we evaluated the etch behaviors of sapphire wafer in $BCl_3$/additive gases (Ar, $N_2,Cl_2$) gases. The behavior of etch rate of sapphire substrate was monitored as a function of additive gas ratio to $BCl_3$ based plasma, total flow rate, r.f. power, d.c. bias under different pressures of 5 mTorr, 10 mTorr, 20 mTorr and 30 mTorr. The etch rates of sapphire wafer, $SiO_2$ and PR were measured with using alpha step surface profiler. In order to understand the changes of radicals, volume density of Cl, B radical and BCl molecule were investigated with optical emission spectroscopy (OES). The chemical states of $Al_2O_3$ thin films were studied with energy dispersive X-ray (EDX) and depth profile anlysis of auger electron spectroscopy (AES). The enhancement of sapphire substrate can be explained by the reactive ion etching mechanism with the competition of the formation of volatile $AlCl_3$, $Al_2Cl_6$ or $BOCl_3$ and the sputter effect by energetic ions.

  • PDF

CMP (Chemical Mechanical Polishing) characteristics of langasite single crystals for SAW filter applications

  • Jang, Min-Chul;An, Jin-Ho;Kim, Jong-Cheol;Auh, Keun-Ho
    • 한국결정성장학회지
    • /
    • 제10권4호
    • /
    • pp.309-317
    • /
    • 2000
  • Langasite is a promising new piezoelectric material for SAW filter application. Little was known until recently about the methods needed to mechanically polish and chemically polish/etch this material. In this experiment, polishing, slurry chemistry and chemical wet etching for langasite is described. Conventional quartz and LN ($LiNbO_3$) polishing methods did not produce satisfactory polished surfaces, and polishing with a colloidal silica slurries has shown to be most effective. The optimum condition was investigated by changing the slurry chemistry. As the planarization effect is very important in SAW filter applications, the examination of the effective particle number effect and the particle size effect was carried out. Z-cut langasite surface which had been polished with the colloidal silica slurries was etched in a variety of etchants. Conventional quartz etchants destroyed the polished surface. Other etchants formed a thin film on the surfaces. In this experiment, the reaction between langasite and a few etching solution was analysed. And an appropriate selective etchant solution for analyzing the defects was synthesized.

  • PDF

Ti-49.5Ni (at%)합금의 다공성 구조가 뼈 세포 흡착에 미치는 영향 (Effect of Pore Structures of a Ti-49.5Ni (at%) Alloy on Bone Cell Adhesion)

  • 임연민;최정일;강동우;남태현
    • 한국재료학회지
    • /
    • 제22권2호
    • /
    • pp.66-70
    • /
    • 2012
  • Ti-Ni alloys are widely used in numerous biomedical applications (e.g., orthodontics, cardiovascular science, orthopaedics) due to their distinctive thermomechanical and mechanical properties, such as the shape memory effect, superelasticity and low elastic modulus. In order to increase the biocompatibility of Ti-Ni alloys, many surface modification techniques, such as the sol-gel technique, plasma immersion ion implantation (PIII), laser surface melting, plasma spraying, and chemical vapor deposition, have been employed. In this study, a Ti-49.5Ni (at%) alloy was electrochemically etched in 1M $H_2SO_4$+ X (1.5, 2.0, 2.5) wt% HF electrolytes to modify the surface morphology. The morphology, element distribution, crystal structure, roughness and energy of the surface were investigated by scanning electron microscopy (SEM), energy-dispersive Xray spectrometry (EDS), X-ray diffractometry (XRD), atomic force microscopy (AFM) and contact angle analysis. Micro-sized pores were formed on the Ti-49.5Ni (at%) alloy surface by electrochemical etching with 1M $H_2SO_4$+ X (1.5, 2.0, 2.5) wt% HF. The volume fractions of the pores were increased by increasing the concentration of the HF electrolytes. Depending on the HF concentration, different pore sizes, heights, surface roughness levels, and surface energy levels were obtained. To investigate the osteoblast adhesion of the electrochemically etched Ti-49.5Ni (at%) alloy, a MTT test was performed. The degree of osteoblast adhesion was increased at a high concentration of HF-treated surface structures.

Fabrication of Hierarchical Nanostructures Using Vacuum Cluster System

  • Lee, Jun-Young;Yeo, Jong-Souk
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.389-390
    • /
    • 2012
  • In this study, we fabricate a superhydrophobic surface made of hierarchical nanostructures that combine wax crystalline structure with moth-eye structure using vacuum cluster system and measure their hydrophobicity and durability. Since the lotus effect was found, much work has been done on studying self-cleaning surface for decades. The surface of lotus leaf consists of multi-level layers of micro scale papillose epidermal cells and epicuticular wax crystalloids [1]. This hierarchical structure has superhydrophobic property because the sufficiently rough surface allows air pockets to form easily below the liquid, the so-called Cassie state, so that the relatively small area of water/solid interface makes the energetic cost associated with corresponding water/air interfaces smaller than the energy gained [2]. Various nanostructures have been reported for fabricating the self-cleaning surface but in general, they have the problem of low durability. More than two nanostructures on a surface can be integrated together to increase hydrophobicity and durability of the surface as in the lotus leaf [3,5]. As one of the bio-inspired nanostructures, we introduce a hierarchical nanostructure fabricated with a high vacuum cluster system. A hierarchical nanostructure is a combination of moth-eye structure with an average pitch of 300 nm and height of 700 nm, and the wax crystalline structure with an average width and height of 200 nm. The moth-eye structure is fabricated with deep reactive ion etching (DRIE) process. $SiO_2$ layer is initially deposited on a glass substrate using PECVD in the cluster system. Then, Au seed layer is deposited for a few second using DC sputtering process to provide stochastic mask for etching the underlying $SiO_2$ layer with ICP-RIE so that moth-eye structure can be fabricated. Additionally, n-hexatriacontane paraffin wax ($C_{36}H_{74}$) is deposited on the moth-eye structure in a thermal evaporator and self-recrystallized at $40^{\circ}C$ for 4h [4]. All of steps are conducted utilizing vacuum cluster system to minimize the contamination. The water contact angles are measured by tensiometer. The morphology of the surface is characterized using SEM and AFM and the reflectance is measured by spectrophotometer.

  • PDF

삼차원 집적화를 위한 초박막 실리콘 웨이퍼 연삭 공정이 웨이퍼 표면에 미치는 영향 (Effect of Si Wafer Ultra-thinning on the Silicon Surface for 3D Integration)

  • 최미경;김은경
    • 마이크로전자및패키징학회지
    • /
    • 제15권2호
    • /
    • pp.63-67
    • /
    • 2008
  • 전자산업의 소형화와 경량화 추세에 맞추어 최근 집적 칩(IC)이나 패키지를 적층시키는 삼차원 집적화(3D integration) 기술 개발은 차세대 핵심기술로 중요시되고 있다. 본 연구에서는 삼차원 집적화 공정 기술 중 하나인 초박막 실리콘 웨이퍼 연삭(grinding)공정이 웨이퍼 표면에 미치는 영향에 대해서 조사하였다. 실리콘 웨이퍼를 약 $30{\mu}m$$50{\mu}m$ 두께까지 연삭한 후, 미세연삭(fine grinding) 단계까지 처리된 시편을 건식 연마(dry polishing) 또는 습식 애칭(wet etching)으로 표면 처리된 시편들과 비교 분석하였다. 박막 웨이퍼 두께는 전계방시형 주사전자현미경과 적외선 분광기로 측정하였고, 표면 특성 분석을 위해선 표면주도(roughness), 표면손상(damage), 경도를 원자현미경, 투과정자현미경 그리고 나노인덴터(nano-indentor)를 이용하여 측정하였다. 표면 처리된 시편의 특성이 표면 처리되지 않은 시편보다 표면주도와 표면손상 등에서 현저히 우수함을 확인 할 수 있었으나, 경도의 경우 표면 처리의 유무에 관계없이 기존의 벌크(bulk)실리콘 웨이퍼와 오차범위 내에서 동일한 것으로 보였다.

  • PDF

태양전지용 규소의 texture etching에 미치는 초음파의 영향 (The effect of the ultrasonic wave on the texturisation of the silicon crystal-line solar cell)

  • 김정민;김영관
    • 한국결정성장학회지
    • /
    • 제13권6호
    • /
    • pp.261-266
    • /
    • 2003
  • 결정질 규소를 이용한 태양전지의 제조에 필요한 texture 식각 공정에 초음파를 적용하였다. 이 결과 $60^{\circ}C$에서 초음파를 적용하여 식각된 규소 기판으로 제조된 태양전지의 광전변환효율이 기존의 방식대로 $70^{\circ}C$에서 초음파 없이 식각된 규소 기판으로 제조된 태양전지의 광전변환효율보다 높았다. 이 결과는 규소를 이용한 태양전지의 제조에 필요한 식각공정에서 초음파를 적용하면 공정 온도를 낮출 수 있고 또한 사용되는 고가의 용액을 줄일 수 있어 전체적으로 태양전지의 제조 가격을 낮출 수 있는 가능성을 보여준다.

플라스마 디스플레이 패널의 격벽 형성의 에칭 메커니즘

  • 정유진;전재삼;성우경;김형순
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2006년도 춘계학술대회
    • /
    • pp.198-201
    • /
    • 2006
  • To produce fine structure with uniform surface of barrier ribs in PDP, acid etching process has been used in manufacture process. It is necessary to understand the mechanism of etching, particularly on the interface of ceramic fillers and matrix glass. We investigated the effect of ceramic fillers (ZnO, $Al_{2}O_3$) on the microstructure of borate glass system to find an etching mechanism of barrier ribs. The harrier ribs was etched with a several steps, dissolving a small amount of residual glass, taking out alumina fillers, and removing a cluster type of ZnO fillers and glass matrix.

  • PDF

트렌치 표면에서의 RIE 식각 손상 회복 (RIE induced damage recovery on trench surface)

  • 이주욱;김상기;배윤규;구진근
    • 한국진공학회지
    • /
    • 제13권3호
    • /
    • pp.120-126
    • /
    • 2004
  • 트렌치 소자 제조시 게이트 산화막 성장과 내압 강하의 원인이 되는 식각손상 회복과 코너 영역의 구조를 개선하기 위해 수소 분위기 열처리를 하였다. 열처리시 수소 원자에 의한 환원 반응을 이용하여 표면 에너지가 높은 코너 영역에서는 원자들의 이동에 의한 결정면 재배열, 산화막 측벽에서의 실리콘 원자 적층, 표면 거칠기의 개선 효과 등을 전자현미경 관찰을 통해 확인하였다. 실리콘 원자의 이동을 방해하는 식각 후 잔류 산화막을 수소 가스의 환원성 분위기에서 열처리함으로써 표면 에너지를 낮추는 방향으로 원자의 이동이 일어나 concave 영역, 즉 트렌치 bottom corner에서는 (111), (311) 결정면 재분포 현상이 일어남을 확인할 수 있었다. 또한 convex comer에서의 원자 이동으로 인해 corner 영역에서는 (1111) 면의 step 들이 존재하게 되고 원자 이동에 의해 산화막 측벽에 이르러 이동된 원자의 적층이 일어나며, 이는 열처리시 표면 손상 회복이 원자이동에 의함을 나타낸다. 이러한 적층은 표면 상태가 깨끗할수록 정합성을 띄어 기판과 일치하는 에피 특성을 나타내고 열처리 온도가 높을수록 표면 세정 효과가 커져 식각손상 회복효과가 커지며, 이를 이용하여 이후의 산화막 성장시 균일한 두께를 코너영역에서 얻을 수 있었다

Pore Distribution of Porous Silicon layer by Anodization Process

  • Lee, Ki-Yong;Chung, Won-Yong;Kim, Do-Hyun
    • 한국결정성장학회:학술대회논문집
    • /
    • 한국결정성장학회 1996년도 The 9th KACG Technical Annual Meeting and the 3rd Korea-Japan EMGS (Electronic Materials Growth Symposium)
    • /
    • pp.494-496
    • /
    • 1996
  • The purpose of this study is to investigate the effect of process conditions on pore distribution in porous silicon layer prepared by electrochemical reaction. Porous silicon layers formed on p-type silicon wafer show the network structure of fine porse whose diameters are less than 100${\AA}$. In n-type porous silicon, selective growth was found on the pore surface by wet etching process after PR patterning. And numerical method showed high current density on the pore tip. With this result we confirmed that pore formation has two steps. First step is the initial attack on the surface and second step is the directional growth on the pore tip.

  • PDF

Double Textured AZO Film and Glass Substrate by Wet Etching Method for Solar Cell Application

  • 정원석;남상훈;부진효
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제42회 동계 정기 학술대회 초록집
    • /
    • pp.594-594
    • /
    • 2012
  • Al doped ZnO (AZO) thin films were deposited on textured glass substrate by magnetron sputtering method. Also, AZO films on textured glass were etched by hydrochloric acid (HCl). Average thickness of etched AZO films are 90 nm. We observed morphology of AZO film by AFM with various etchant concentration and etching time. Etched AZO films have low resistivity and high haze. The surface RMS roughness of AZO film was increased from 53.8 nm to 84.5 nm. The haze ratio was also enhanced in above 700 nm of wavelength due to light trapping effect was increased by rough AZO surface. The etched AZO films on textured glass are applicable to fabricate solar cell.

  • PDF