• Title/Summary/Keyword: Surface chloride contents

Search Result 53, Processing Time 0.03 seconds

Comparison of Acidic and Alkaline Bath in Electroless Nickel Plating on Porous Carbon Substrate (다공성 탄소전극상 무전해 니켈도금의 산성과 알칼리용액 비교 연구)

  • Chun, So-Young;Kang, In-Seok;Rhym, Young-Mok;Kim, Doo-Hyun;Lee, Jae-Ho
    • Journal of the Korean institute of surface engineering
    • /
    • v.43 no.2
    • /
    • pp.105-110
    • /
    • 2010
  • Electroless nickel plating on porous carbon substrate for the application of MCFC electrodes was investigated. Acidic and alkaline bath were used for the electroless nickel plating. The pore sizes of carbon substrates were 16-20 ${\mu}m$ and over 20 ${\mu}m$. The carbon surface was changed from hydrophobic to hydrophilic after immersing the substrate in an ammonia solution for 40 min at $60^{\circ}C$. The contact angle of water was decreased from $85^{\circ}C$ to less than $20^{\circ}$ after ammonia pretreatment. The deposition rate in the alkaline bath was higher than that in the acidic bath. The deposition rate was increased with increasing pH in both acidic and alkaline bath. The content of phosphorous in nickel deposit was decreased with increasing pH in both acidic and alkaline bath. The contents of phosphorous is low in alkaline bath. The minimum concentration of $PdCl_2$ for the electroless nickel plating was 10 ppm in alkaline bath and 5 ppm in acidic bath. The thickness of nickel was not affected by the concentration of $PdCl_2$.

Development of Strength and Durability Properties of Latex-Modified Concrete with Rapid-Setting Cement (초속경 시멘트를 사용한 라텍스 개질 콘크리트의 강도발현 및 내구특성)

  • 최성욱;홍창우;김동호;최상릉;장홍균
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.1029-1034
    • /
    • 2001
  • The purpose of this research is to develop rapid setting cement latex modified concrete (RSLMC) which will be used to overlay bridge deck for maintaining and repairing. The main experimental variables were the types of rapid setting cement and variation of latex and antifoam agent contents were selected as admixture factor, then the properties of workability and strength development and durability properties were investigated. The results of this study show that latex content give increment of a slump due to surface tension in polymer particles and reduce unit weight of water for preservation of workability. In addition, When no and 1.6~3.2% antifoam agent were mixed, 8%, 2.0~3.8% were respectively obtained. An increasing the amount of latex produced concrete with increased flexural strength, but with slightly lower compressive strength. Rapid chloride permeability and freezing-thawing test carried out. As a results, according to increment of containing ratio antifoamer, strength of RSLMC increase, permeability showed lower value than ignorable 100 coulombs. Also, in the case of more than antifoamer 1.6%, the relativity dynamic modulus is mantained more than 90%, but in case of 0, 5%, it decrease. In consequence, with the view of strength and workability of RSLMC, it is considered that appropriate content ratio of antifoam agent and latex solid are respectively 1.6% by latex weight, 15% by cement weight.

  • PDF

Durability assessments of limestone mortars containing polypropylene fibres waste

  • Bendjillali, Khadra;Boulekbache, Bensaid;Chemrouk, Mohamed
    • Advances in concrete construction
    • /
    • v.10 no.2
    • /
    • pp.171-183
    • /
    • 2020
  • The main objective of this study is the assessment of the ability of limestone mortars to resist to different chemical attacks. The ability of polypropylene (PP) fibres waste used as reinforcement of these concrete materials to enhance their durability is also studied. Crushed sand 0/2 mm which is a fine limestone residue obtained by the crushing of natural rocks in aggregates industry is used for the fabrication of the mortar. The fibres used, which are obtained from the waste of domestic plastic sweeps' fabrication, have a length of 20 mm and a diameter ranging between 0.38 and 0.51 mm. Two weight fibres contents are used, 0.5 and 1%. The durability tests carried out in this investigation included the water absorption by capillarity, the mass variation, the flexural and the compressive strengths of the mortar specimens immersed for 366 days in 5% sodium chloride, 5% magnesium sulphate and 5% sulphuric acid solutions. A mineralogical analysis by X-ray diffraction (XRD) and a visual inspection are used for a better examination of the quality of tested mortars and for better interpretation of their behaviour in different solutions. The results indicate that the reinforcement of limestone mortar by PP fibres waste is an excellent solution to improve its chemical resistance and durability. Moreover, the presence of PP fibres waste does not affect significantly the water absorption by capillarity of mortar nether its mass variation, when exposed to chloride and sulphate solutions. While in sulphuric acid, the mass loss is higher with the presence of PP fibres waste, especially after an exposure of 180 days. The results reveal that these fibres have a considerable effect of the flexural and the compressive behaviour of mortar especially in acid solution, where a reduction of strength loss is observed. The mineralogical analysis confirms the good behaviour of mortar immersed in sulphate and chloride solutions; and shows that more gypsum is formed in mortar exposed to acid environment causing its rapid degradation. The visual observation reveals that only samples exposed to acid attack during 366 days have showed a surface damage extending over a depth of approximately 300 ㎛.

Preparation and Release Characterization of Sodium Alginate Bead Containing Phytoncide Oil (편백정유를 함유한 알지네이트 비드의 제조 및 방출 특성)

  • Yoon, Doo-Soo;Lee, Eung-Jae
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.4
    • /
    • pp.557-562
    • /
    • 2018
  • High molecular weight sodium alginate (HMWSA)/low molecular weight sodium alginate (LMWSA) microcapsules containing phytoncide oil were prepared with different LMWSA contents. The effects of the stirring rate and ratio of HMWSA/LMWSA on the diameter and morphology of the phytoncide/alginate beads were investigated by optical microscopy and the release behaviors of phytoncide oil from the phytoncide/alginate beads were characterized by UV/Vis. spectrophotometry. The mean particle size of the phytoncide/alginate beads decreased with increasing stirring rate and concentration of the calcium chloride solution. The surface morphology of the phytoncide/alginate beads changed from smooth surfaces to skin-like rough surfaces with increasing LMWSA content. These results were due mainly to the increased hydrophilic groups at the bead surface, resulting in an increase in the release rate of phytoncide oil in the phytoncide/alginate beads.

Effects of Chlorine Contents on Perovskite Solar Cell Structure Formed on CdS Electron Transport Layer Probed by Rutherford Backscattering

  • Sheikh, Md. Abdul Kuddus;Abdur, Rahim;Singh, Son;Kim, Jae-Hun;Min, Kyeong-Sik;Kim, Jiyoung;Lee, Jaegab
    • Electronic Materials Letters
    • /
    • v.14 no.6
    • /
    • pp.700-711
    • /
    • 2018
  • CdS synthesized by the chemical bath method at $70^{\circ}C$, has been used as an electron transport layer in the planar structure of the perovskite solar cells. A two-step spin process produced a mixed halide perovskite of $CH_3NH_3PbI_{3-x}Cl_x$ and a mixture of $PbCl_2$ and $PbI_2$ was deposited on CdS, followed by a sub-sequential reaction with MAI ($CH_3NH_3I$). The added $PbCl_2$ to $PbI_2$ in the first spin-step affected the structure, orientation, and shape of lead halides, which varied depending on the content of Cl. A small amount of Cl enhanced the surface morphology and the preferred orientation of $PbI_2$, which led to large and uniform grains of perovskite thin films. In contrast, the high content of Cl produces a new phase PbICl in addition to $PbI_2$, which leads to the small and highly uniform grains of perovskites. An improved surface coverage of perovskite films with the large and uniform grains maximized the performance of perovskite solar cells at 0.1 molar ratio of $PbCl_2$ to $PbI_2$. The depth profiling of elements in both lead halide films and mixed halide perovskite films were measured by Rutherford backscattering spectroscopy, revealing the distribution of chlorine along with the thickness, and providing the basis for the mechanism for enhanced preferred orientation of lead halide and the microstructure of perovskites.

A Study on the Durability Evaluation Criteria for the Vertical Extension Remodeling of Apartment (수직 중축형 리모델링 안전진단 내구성 평가기준 합리화에 관한 연구)

  • Yoon, Sang-Chun;Shin, Dong-Cheol
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.6
    • /
    • pp.197-205
    • /
    • 2020
  • In 2014, The Housing Act amended to allows vertical extension and increases the units of housing (or total floor area) to site. Currently, the feasibility of performing vertical extension is evaluated based on safety diagnosis provisions and manuals with 1st investigation stage on slope, uneven settlement, load-bearing capacity, and durability. However, a need for more reasonable evaluation criteria for the investigation is still required because there had not been any other case study on the diagnosis for the vertical extension, and the engineering basis on evaluation criteria were not suggested. Accordingly, this study is intended to suggest feasible evaluation criteria on the carbonation, chloride ion contents, corrosion of reinforcements, crack and surface deterioration of concrete for durability assessment by codes and standards of domestic and foreign countries. The results of this study are expected to be beneficial for establishing more reasonable durability evaluation criteria, and in turn, more reliable assessment protocol for vertical extension.

Study on the Hollow Fiber Nano-composite Membrane Preparation onto the Porous PVDF Membrane Surfaces using the Interfacial Polymerization (다공성 PVDF 막의 polyamide 계면중합법처리를 통한 나노 중공사 복합막 제조 연구)

  • Kang, Su Yeon;Cho, Eun Hye;Kim, Ihl hyung;Kim, Cheong Sik;Rhim, Ji Won
    • Membrane Journal
    • /
    • v.24 no.2
    • /
    • pp.107-112
    • /
    • 2014
  • The composite membranes were prepared on the surface of hydrophobic porous poly (vinylidene fluoride) (PVDF) hollow fiber membranes through the interfacial polymerization. The preparation variables were the concentrations of piperazine (PIP), trimesoyl chloride (TMC) and the contents of polyethylene glyco l (PEG). The separation characterization of the resulting membranes were carried out for aqueous 100 ppm solution of NaCl, $CaSO_4$, and $MgCl_2$ and also mixed 300 ppm solution of NaCl and $CaSO_4$ in terms of the flux and rejection. Both the flux and rejection were the highest when the interfacial polymerization was conducted using TMC. When TMC concentration was 0.1 wt%, the flux and rejection were shown 48.3 LMH ($L/m^2{\cdot}hr$) and 59%, respectively. To improve the flux, the annealing post-treatment and the addition of PEG into piperazine were done. As expected, the overall flux was enhanced while the rejection was reduced.

Effect of Chemical Forms of Nitrogen Fertilizers on Rice Growth and Soil Characteristics (시용(施用) 질소(窒素)의 화학적(化學的) 형태(形態)가 수도생육(水稻生育) 및 토양특성(土壤特性)에 미치는 영향(影響))

  • Yoo, Sun-Ho;Song, Kwan-Cheol;Kim, Kye-Hoon
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.17 no.3
    • /
    • pp.242-252
    • /
    • 1984
  • A port experiment was conducted to compare the effect of chemical forms of nitrogen fertilizers on the rice growth and soil characteristics. The nitrogen fertilizers used for this study were ammonium sulfate, ammonium nitrate, ammonium chloride and urea. The results are summarized as follows. 1. The differences in pH of the soil and surface water between treatments during the first week after fertilizer application were great and the pH values were in the order of urea > ammonium nitrate > ammonium sulfate > ammonium chloride treatment. However the differences were insignificant after the first week. 2. The differences in pH of the air-dried soil somewhat increased and pH values were in the order of urea > ammonium nitrate > ammonium chloride > ammonium sulfate treatment. 3. Sulfur contents of the soil and the rice leaf and N content of the rice leaf were highest when ammonium sulfate was applied. But there were few differences between the treatments in total N content of the soil and in P, K, Ca and Mg contents of the soil and the rice leaf. 4. Number of tillers and dry matter weight of the rice plant were highest in ammonium sulfate plot throughout all the growing stages. 5. Number of panicle per hill was highest in ammonium sulfate plot, and this brought the highest grain yield in ammonium sulfate plot. The lowest grain yield in ammonium nitrate plot resulted from the lowest number of panicle per hill and ripened grain ratio.

  • PDF

A Study on the Rainwater Quality Monitoring and the Improvement, Collection and Storage System (빗물 집수 및 저장 시스템 개선과 수질 분석 모니터링)

  • Kim, Chul-Kyung
    • Clean Technology
    • /
    • v.17 no.4
    • /
    • pp.353-362
    • /
    • 2011
  • In our nature, the utilization of rainwater is essential for healthy water recirculation. This is one of the solutions of the increment of impermeability surface according to the development of new cities; this study of the improvement of rainwater quality has been carried on through the improvement of collecting and restoring system of rainwater. The southwestern region of Daejeon City, the rainwater coefficient of run off was 0.40 and this number had computed to 0.59 after the development. After filtration of rainwater, the heavy metal (Cu, As, Cr, Fe, Mn) contents level were lower than underground water. Moreover, collected rainwater showed better quality than underground water in following criteria; hardness, permanganate consumption quality, chloride, evaporation residue, sulfates and nitrate nitrogen. This water quality met the gray water quality standards. The rainwater quality was still suitable to use as bathroom flushing and gardening after 100 days of storage. This study proved that modification (installation of cover with gutter to existing rainwater collection system, proper filtering, and installation of underground storage tank) of collection system could improve quality of water and maintain this approximately 100 days.

Elution Patterns of Anions in Multi-layered Soils amended with Cow Manure Compost (우분퇴비 처리에 따른 다층구조 토양내 음이온의 용출특성 변화)

  • 김필주;정덕영;이병열
    • Journal of Korea Soil Environment Society
    • /
    • v.2 no.2
    • /
    • pp.25-33
    • /
    • 1997
  • To investigate the effects of cow manure compost(CMC) on soil and water environment as non-point source, the elution patterns of anions were determined in muti-layered soil columns which were consisted of one top and one bottom in combination. The top soil columns were uniformly packed with Ap horizon soils amended with air-dried CMC at different ratios(0, 2, 4, 6%, wt/wt), the bottom ones were packed with of B horizon soils of 15, 30, and 45cm in length. After saturating the each soil column, the leachate were collected from the bottom of the column while the double-ionized water was applied from the surface of the column by constant head method. From the hydraulic conductivity and anion eluted were measured in the leachate. Each saturated hydraulic conductivities for top and the bottom soils were 3$\times$$10^{-4}$sec and 1.6$\times$$10^{-3}$cm/sec. Most of water soluble chloride and sulfate, having non-specific adsorption characteristics onto the soil particles, were eluted within 1 PV, showing that there was no apparent retardation of anion movement with increasing CMC contents in the top soils. The effect of soil depths on anion movement were similar to the results of CMC contents. Sulfate of having both of non-specific and specific adsorption characteristics was also recovered in the effluent within 1 PV, while the elution curves were slightly skewed to the right showing that the CMC affected the movement of sulfate. Phosphate of specific adsorption characteristics was hardly eluted within 5 PV.

  • PDF