  • The efforts which increase the strength of the auto-body structure and decrease its weight lead to develop a new concept of part production systems, such as Post-Form Strengthening by induction heat treatment. In this study, several cold and hot-rolled sheet steels were used to find out optimum induction heat treatment conditions. After induction heat treatment, strength of heat-treated sheet steels was increased significantly compared with that of as-rolled steels. From these results, auto-body structure which has more light and safe has been made by using this induction hardening method.

바나듐 첨가에 의한 저탄소 구조용강의 강화 (Strengthening of 0.25%C Low Carbon Structural Steels by Vanadium Addition)

  • 이상옥;이현권;이상우
    • 열처리공학회지
    • /
    • 제21권2호
    • /
    • pp.79-86
    • /
    • 2008
  • As a basic research for developing 600 MPa yield strength reinforcing steel bars, the strengthening of 0.25 wt.% carbon steel by vanadium addition was studied. The changes of microstructure and mechanical properties were investigated for the specimen V0 (0.00 wt.% V), V1 (0.03 wt.% V) and V2 (0.06 wt.% V) processed by various heat treatments. To set the heat treatment conditions, the continuous cooling transformation (CCT) curves were drawn for austenitizing temperatures of $900^{\circ}C$ and $1100^{\circ}C$. For specimens tempered at $600^{\circ}C$ after quenching from $900^{\circ}C$ and $1100^{\circ}C$, yield strength was increased by 19 MPa and 21 MPa for 0.01 wt % V addition, and tensile strength was increased by 25 MPa and 28 MPa for 0.01 wt % V addition, respectively. Also, for 0.06 wt.% V added specimens tempered after quenching and normalized, tensile strength was increased by 50 MPa and 30 MPa for increasing austenitizing temperature of $100^{\circ}C$, respectively.

알루미나 세라믹(Alumina Ceramic) 코팅층의 기술적인 특성과 잔류응력의 해소에 관한 연구 (A Study on the Mechanical Properties and Residual Stresses of the Thermally Sprayed Alumina Ceramic Coating Layer)

  • 김영식
    • 한국해양공학회지
    • /
    • 제10권2호
    • /
    • pp.88-97
    • /
    • 1996
  • The pupose of this study is to improve the mechanical properies and to evaluate the residual stresses of flame-sprayed Alumina ceramic coating layer. The first work in this study is to investigate the effects of strengthening heat treatments on the mechanical properties of coating layer. Strengthening heat treatments for sprayed specimens were carried out in vaccum furnace. The mechanical properties such as microhardness, thermal shock resistance, adhesive strength and erosion resistance were tested for the sprayed specimens after strengthening heat treatments. And it was clear that the mechanical properties of coating layer were much improved by strengthening heat treatments. The second work in this study is to evalute the residual stresses in coating lsyer by numerical analysis. FDM and FEM were used to analyze temperature distribution and residul stresses in coating layer. It was proved that are tensile stresses in coating layer and that residual stresses can be controlled by the appropriate selection of the spraying parameters such as preheat temperature, coating thickness and bond coat thickness.

  • PDF

Chemical Strengthening Involving Outward Diffusion Process of Na+ Ion in Iron-containing Soda-lime Silicate Glass

  • Choi, Hyun-Bin;Kang, Eun-Tae
    • 한국세라믹학회지
    • /
    • 제52권2호
    • /
    • pp.133-136
    • /
    • 2015
  • The outward diffusion of $Na^+$ ions in iron-bearing soda lime silicate glass via oxidation heat treatment before the ion exchange process is artificially induced in order to increase the amount of ions exchanged during the ion exchange process. The effect of the addition process is analyzed through measuring the bending strength, the weight change, and the inter-diffusion coefficient after the ion exchange process. The glass strength is increased when the outward diffusion of $Na^+$ ions via oxidation heat treatment before the ion exchange process is added. For the glass subjected to the additional process, the weight change and diffusion depth increase compared with the glass not subjected to the process. The interdiffusion coefficient is also slightly increased as a result of the additional process.

구상흑연주철의 강인화에 미치는 특수열처리와 합금원소의 영향 (Effect of Special Heat Treatments and Alloying Element(Ni) on Strengthening and Toughening of Ductile Cast Iron)

  • 김석원;최용선
    • 한국주조공학회지
    • /
    • 제10권4호
    • /
    • pp.299-308
    • /
    • 1990
  • Ductile cast iron has a good ductility and ductility and toughness than those of gray cast iron, because the shape of graphite is spheroidal. It has been reported that the strengthening and toughening of the ductile cast iron was resulted from the good modification of various matrix structures obtained by the heat treatment or addition of alloying elements. This study aims to investigate the effect of various special heat treatment(Cyclic Heat Treatment, Intermediate Heat Treatment, Step Quenching), austempering and alloying element(Ni) on the strength and toughness of ductile cast iron. The results obtained from this study are summarized as follows. 1) With addition of Ni, the amount of pearlite or bainite were increased and the morphologies of pearlite or bainite became finer by special heat treatments. 2) As the Ni added and not added ductile cast iron were treated by austenitizing at $900^{\circ}C$ and $840^{\circ}C$, in the latter the austenite was mostly formed in the vicinity of eutectic cell boundary, but in the former on the whole matrix. 3) In cyclic heat treatment, the volume fraction of pearlite was increased and the shape of pearlite was fined with increase of the number of cycle. 4) The shape of pearlite was mostly bar type in the intermediate heat treatment, but spheroidal type in step quenching. 5) The mechanical properties of ductile cast iron containing 1.5%Ni austempered at $400^{\circ}C$ for 25min. after austenitizing at $900^{\circ}C$ for 15min. were a good value of hardness 105(HRB), impact energy 12.5(kg.m), tensile strength 112($kg/mm^2$) and elongation 6.8(%).

  • PDF

나노압입시험법을 이용한 열처리 소재의 미소 변형 거동 평가 (Characterizing Small-scale Mechanical Behaviors of Heat-treated Materials with Nanoindentation Technique)

  • 최인철
    • 열처리공학회지
    • /
    • 제33권2호
    • /
    • pp.72-79
    • /
    • 2020
  • To improve the mechanical properties of most structural materials for industrial applications, the control of microstructure is essential by heat treatment process or plastic deformation process. Since the mechanical behavior of structural materials is significantly influenced by their microstructure, it is inevitably preceded to understand the relationship between microstructure and strengthening mechanisms of materials which can be easily changed by heat treatment. In this regard, the nanoindentation test is useful technique for analyzing the influence of the localized microstructural change on small-scale mechanical behavior of various structural materials. Here, the interesting studies performed on various heat-treated materials are reviewed with focus on micromechanical properties obtained by nanoindentation, which are reported in the available literature.

오스템퍼 처리(處理)한 구상흑연주철(球狀黑鉛鑄鐵)의 강인화(强靭化)에 관(關)한 연구(硏究)(1) (The Study on the Strength and Toughness of Austempered Ductile Cast Iron)

  • 이영기;김석원;김동건;이방식
    • 한국주조공학회지
    • /
    • 제10권2호
    • /
    • pp.144-153
    • /
    • 1990
  • Ductile cast iron has good ductility and toughness, for the graphite morphology is spheroidal. It has been reported that the strengthening and toughening of the ductile cast iron was resulted from the modification of matrix structure by the heat treatment or the addition of alloying elements. In this study, effects of various special heat treatments (cyclic heat treatment and intermediate heat treatment) and Ni addition on the toughness and strength of the austempered ductile cast iron were studied. The results obtained from this study were as follows : 1. The amount of fine pearlite was increased with the Ni content and the number of cycle in cyclic heat treatment. 2. When the specimens treated and not by special heat treatment at 820 was austempered, in the former the austenite was formed on grain boundary entirely, but in the latter on grain boundary partially. 3. The impact energy was decreased with the Ni content, because the coarisen austenite pools formed with the Ni content was transformed into martensite during quenching. 4. The mechanical properties of austempered ductile cast iron containing 2%Ni treated cyclic heat treatment(5 cycles)was very excellent in handness 99(HRB), impact energy 12(kg-m) maximum fracture load 1500(kg-f).