금 합금 및 비 귀금속 합금에 대한 의치상 레진의 결합강도에 관한 연구 (A STUDY ON THE FLEXURAL BOND STRENGTH OF THE GOLD AND THE Co-Cr ALLOY TO THE DENTURE BASE RESINS)

  • 박현주;김창회;김영수
    • 대한치과보철학회지
    • /
    • 제38권4호
    • /
    • pp.500-509
    • /
    • 2000
  • In general, the three major oral functions of edentulous patients-mastication, phonation, esthetics-can be rehabilitated by the complete dentures, and both the resin based complete denture and the metal based complete denture are commonly used by many clinicians today. For the sake of many advantages such as the excellent thermal conductivity, low volumetric change, high strength, low risk of fracture and the better patient's adaptation, the metal based complete dentures are indicated to the several cases. But, there are common failures of these type of dentures mainly by the fracture or the debonding between the resin structures and the metal frameworks which is caused by the discrepancies of the flexural strength and the coefficient of thermal expansion. This is aggravated by the water contamination of the interface when exposed to the oral environment and results in the failure of complete denture treatment. So, the purpose of this study is to compare the bond strength and the fracture patterns of the gold alloy based and the Co-Cr alloy based complete dentures using the PMMA resins and the 4-META adhesive resins. The results of this study were as follows. 1. Both to the PMMA resin and the 4-META resin, the flexural bond strength of gold alloy is lower than that of Co-Cr alloy(P<0.05) 2. To the Co-Cr alloy, the bond strength of the 4-META resin is significantly higher than that of PMMA resin(P<0.05). 3. The flexural strength of the group with the mechanical retention form is significantly higher than that of the group without retention form(P<0.05). 4. Comparing with the other groups, the fracture patterns of the group 3 are quite different from the group 1,2,5.

  • PDF

짧은 티타늄 지대주에 합착된 CAD/CAM 금속 코핑의 시멘트 종류에 따른 유지력 비교 (Retention of CAD/CAM Metal Copings Cemented on Short Titanium Abutments with Different Cements)

  • 김효정;송은영;윤지영;이시호;이용근;오남식
    • 구강회복응용과학지
    • /
    • 제28권2호
    • /
    • pp.119-126
    • /
    • 2012
  • 시멘트 유지 임플란트 지지 수복물은 치과 치료에 일상적으로 사용된다. 임플란트와 지대주 나사연결의 안정적인 견고함과 골유합 임플란트의 높은 생존율로 인해 높은 강도를 가진 시멘트의 사용이 점차 늘어나고 있다. 그러나 CAD/CAM을 이용하여 제작한 금속 코핑의 유지력에 대해 이용할 수 있는 임상 자료가 없다. 네 종류의 시멘트를 이용하여 티타늄 지대주와 CAD/CAM을 이용하여 제작한 금속 코핑의 유지력을 평가하는 것과 시멘트 유지력에 대한 sandblasting의 효과를 알아보고자 함이다. 40개의 티타늄 지대주 블록(Innovium, 세라젬바이오시스, 대한민국)을 제작하여 네 그룹으로 나누었다. 40개의 금속 코핑을 CAD/CAM을 이용하여 제작하고 금속 코핑의 교합면 상방부에 유지력 테스트를 위해 구멍을 형성하였다. 네 종류의 시멘트는 Fujicem(Fuji, Japan), Maxcem Elite(Kerr, USA), Panavia F2.0(Kurarary, Japan), Superbond C&B(Sunmedical, Japan)이다. 금속 코핑과 티타늄 지대주를 제조사의 지시대로 시멘트 혼합하여 합착하고 100% 습도 하에 37도에서 24시간 동안 보관 후 유지력 테스트하였다. 유지 실패가 발생하는 힘을 newton으로 기록하고 실패의 양상 또한 기록하였다. 유지력의 평균과 표준 편차를 ANOVA와 Paired t-test 로 통계분석하였다. Panavia F2.0이 Fujicem과 Maxcem Elite보다 통계적으로 유의하게 높은 유지력을 보였다(p<0.05). Sandblasting이 모든 시멘트에서 유의하게 유지력을 증가시켰다(p<0.05). 유지력 실패의 양상은 대부분의 시멘트가 금속 코핑 내부에 남아있는 접착성 실패였다. 본 연구의 한계 내에서 Panavia F2.0이 Fujicem이나 Maxcem Elite보다 통계적으로 유의하게 큰 유지력을 보였고(p<0.05), Fujicem과 Maxcem Elite는 유지력의 차이를 보이지 않았다. Sandblasting처리는 모든 실험군에서 유지력의 향상을 보였다. 따라서 임플란트 지대주에 합착된 금속 코핑의 유지력은 표면 거칠기와 시멘트의 종류에 영향을 받는다.

Examination of an Algerian Clay in the Retention of Zinc Ions Charged in Brackish Water

  • Fadel, Ammar;Nacef, Saci
    • Korean Chemical Engineering Research
    • /
    • 제55권5호
    • /
    • pp.685-689
    • /
    • 2017
  • We studied the removal of zinc ions from synthetic brackish water by an adsorption method using natural Algerian Bentonite (NAB). The effect of the main physico chemical parameters-contact time, pH, temperature, ionic strength, clay weight and initial metal ion concentrations on the removal of $Zn^{+2}$-were investigated. The results showed that equilibrium was attained within 10 min of stirring time. The retention capacity of $Zn^{+2}$ increased with the increase of pH, the adsorbent dose and ionic strength. A modelization study showed that the adsorption follows Langmuir isotherm, while its kinetics was pseudo-second-order. Based on the results, it was concluded that NAB, which is natural and available, could be used as an alternative for the removal of zinc from saline aqueous solutions.

지오튜브공법의 실용화방안에 관한 연구 (Development of Geotube for Practical Use)

  • 신은철;오영인;이희재
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2000년도 봄 학술발표회 논문집
    • /
    • pp.504-511
    • /
    • 2000
  • Geotube is a tube made of permeable but soil-tight geotextile, hydraulically filled with soil include dredged sand and mud, which has been successfully applied in hydraulic and coastal engineering projects. This method is getting popular and used a lot in the advanced countries of the world because of economical, useful, and enable to store and isolate contaminated materials as obtained by harbor dredging. Laboratory and pilot scale in-situ tests were performed to determine the design methodology and construction procedures. From the results of laboratory and in-situ model tests, the retention ratio of solid particle is minimum 86% and minimum permeability and tensile strength of geotextile is ${\alpha}$${\times}$10$\^$-2/ and 20 t/m, respectively. Also, based on the environmental model test results, it can be concluded that this method does meet the Korean EPA standards.

  • PDF

비스코스 레이온 직물의 방축가공 (Shrinkproof Finish of Viscose Rayon Fabric)

  • 김성동;이인열;이종렬;김민정
    • 한국염색가공학회지
    • /
    • 제10권6호
    • /
    • pp.20-26
    • /
    • 1998
  • 100% viscose rayon fabric was treated with 1,2,3,4-butanetetracarboxylic acid (BTCA) by pad-dry-cure process in the presence of various catalysts. The dimensional stability, mechanical properties and hand values of fabric treated with BTCA were investigated. The ester-crosslinking reaction was influenced by the concentration of BTCA and type of catalyst. The fabric treated with BTCA was comparable or superior to that treated with conventional crosslinking agents such as dimethyloldihydroxyethyleneurea and 4,5-dihydroxy-1,3-dimethyl-2-imidazolidinone in respect of wrinkle recovery, shrinkproof property, retention of strength, and hand values. But in yellowing of fabric, the fabric treated with BTCA was inferior to that treated with conventional crosslinking agents. The fabric treated with BTCA/sodium formate was inferior to that treated with BTCA/sodium hypophosphite in respect of WRA, but had better strength retention and whiteness.

  • PDF

신서란 섬유를 이용한 종이 제조와 그 특성 (Manufacture and Characterization of Papers Made from New-Zealand Hemp Fibers)

  • 이현철;김봉용
    • 펄프종이기술
    • /
    • 제36권1호
    • /
    • pp.67-74
    • /
    • 2004
  • This study was carried out to investigate the characteristics of handsheets made from nonwoody New-Zealand hemp (Phormium tenax) fibers that was not used before in Korea. The results were as follows : 1. Physical properties of bleached phormium fiber were satisfactory for handsheet forming. Specially, tensile strength was improved by adding bleached phormium fiber. 2. Opacity of handsheet with phormium pulp was fine, therefore it can be useful fiber to improve opacity of light-weight printing paper. 3. Filler retention rate was improved when phormium pulp was added, while drainage time was increased. 4. Phormium fiber has good characteristics as pulp for paper manufacture. So it can be valuable non-wood fiber resource if drainage problem is solved.

마직물의 셀룰라이제 효소처리에 의한 유연가공효과에 관한 연구 (The Effect of Biopolishing with Cellulase Enzyme on Ramie and Hemp Fabrics)

  • 김정희;유혜자
    • 한국의류산업학회지
    • /
    • 제3권4호
    • /
    • pp.367-372
    • /
    • 2001
  • Five kinds of commercial ramie and hemp fabrics were treated with cellulase under different concentrations. Samples were mercerized before enzyme treatment to investigate the effect of mercerization on cellulase enzyme treatment. Physical characteristics(weight loss, tear strength retention, wrinkle recovery, drape stiffness, dyeability) of cellulase enzyme treated and untreated samples were measured and compared. X-ray diffractions were examined to verify if there were any changes in their crystallinity of enzyme treated fabrics. Weight loss, wrinkle recovery and degree of crystallinity increased as the concentration of cellulase enzyme increased. In the meanwhile, tear strength retention and drape stiffness and dyeability decreased. Enzyme activity was more effective on mercerized samples. Particularly, there was distinct tendency to increase weight loss and flexibility.

  • PDF

저온플라즈마 및 효소처리한 면의 물성 및 염색성 (Physical Properties and Dyeing Behaviors of Cotton Fabric Treated with Low Temperature Plasma and/or Cellulase)

  • Yoon, Nam Sik;Lim, Yong Jin
    • 한국염색가공학회지
    • /
    • 제8권3호
    • /
    • pp.59-65
    • /
    • 1996
  • Cotton fabrics were treated by low temperature plasma and/or cellulase, and its physical and dyeing properties were investigated. All the pretreatments of the cotton with low temperature plasma of oxygen, nitrogen and argon slowed down the rate of weight loss of cotton in cellulase solution. Plasma pretreatment did not show any strength retention effect on cotton fiber in the subsequent cellulase treatment. Pretreatment of cotton with low temperature oxygen plasma decreased the rate of dyeing in direct dye bath, while cellulase or plasma/cellulase pretreatment increased the rate. Equilibrium dye uptake of cotton was not changed greatly by the pretreatments except the normal untreated cotton showed more or less high uptake. The pretreatment of cellulase with a water-soluble carbodiimide reduced the enzymatic activity, and did not show any strength retention of cotton in enzymatic weight loss.

  • PDF

Glass Fiber Post와 Composite Resin Core의 전단결합강도 (A STUDY FOR THE BONDING STRENGTH OF COMPOSITE RESIN CORE TO GLASS FIBER POST)

  • 김태형;심준성;이근우
    • 대한치과보철학회지
    • /
    • 제43권4호
    • /
    • pp.415-425
    • /
    • 2005
  • Statement of problem : Fracture of composite resin core will be occulted by progress of crack. Bonding interface of different materials has large possibility of starting point of crack line. Therefore, the bond strength of glass fiber post to composite resin core is important for prevention of fracture. Purpose: This in vitro study tried to find out how to get the higher strength of glass fiber post to composite resin core through surveying the maximum load that fractures the post and cote complex. Materials and methods: 40 specimens made with glass fiber Posts(Style $post^{(R)}$, Metalor, Swiss) and composite resin core ($Z-100^{(R)}$, 3M, USA) were prepared and loaded to failure with push-out type shear-bond strength test in a universal test machine. The maximum fracture load and fracture mode were investigated in the specimens that were restored with four different surface treatments. With the data. ANOVA test was used to validate the significance between the test groups, and Bonferroni method was used to check if there is any significant statistical difference between each test group. Evely analysis was approved with 95% reliance. Results: On measuring the maximum fracture load of specimens, both the treatments of sandblasted and acid-etched one statistically showed the strength increase rather than the control group (p<0.005). The scanning electric microscope revealed that sand blasting made more micro-retention form not only on the resin matrix but on the glass fiber, and acid-etching contributed to increase in surface retention form, eliminated the inorganic particles in resin matrix. Specimen fracture modes investigation represented that sand blasted groups showed lower bonding failure than no-sand blasted groups. Conclusion: Referring to the values of maximum fracture load of specimens, the bonding strength was increased by sand blasting and acid-etching.

Effects of Dietary Non-phytate Phosphorus Levels on Egg Production, Shell Quality and Nutrient Retention in White Leghorn Layers

  • Panda, A.K.;Rao, S.V.Rama;Raju, M.V.L.N.;Bhanja, S.K.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • 제18권8호
    • /
    • pp.1171-1175
    • /
    • 2005
  • An experiment was conducted (28 to 44 weeks) to study the laying performance, shell quality, and nutrient retention of White Leghorn layers fed different levels of non-phytate phosphorus (NPP). Six levels of NPP (0.15, 0.18, 0.21, 0.24, 0.27 and 0.30%) at a constant calcium (Ca) level (3.5%) in maize-soya-deoiled rice bran based diets were formulated, and each experimental diet was offered ad libitum for 16 weeks to five replicates with five birds in each replicate. The body weight of WL layers fed diet containing 0.15% NPP was significantly (p<0.05) lower than those fed diet with 0.30% NPP, at 44 weeks of age. However, the hen day egg production, egg weight, daily feed intake and feed consumed per dozen eggs were not influenced by the variation in the NPP levels in the diet. The bone ash content was significantly (p<0.05) higher in the birds fed 0.30% NPP as compared with those fed diets up to 0.24% NPP. Bone ash content was intermediate in the birds fed diet containing 0.27% NPP. The tibia strength followed the same trend as that of bone ash. Dietary NPP content had no influence on serum Ca and protein concentration and activity of alkaline phosphatase. However, serum inorganic P concentration increased linearly with NPP content in the diet. The concentration of P was significantly (p<0.05) higher in the birds fed 0.27% NPP or higher as compared with those fed 0.15% NPP. Levels of dietary NPP had no influence on egg quality parameters like shell wt, shell thickness, shell strength and specific gravity. The retention of nutrients such as DM, N and Ca were comparable among the WL layers fed different levels of NPP. However, the retention of P decreased linearly with increase in the level of NPP in the diet. The retention of P in the birds fed diets up to 0.24% NPP in the diet was comparable, however further increasing the content of NPP (either 0.27% or 0.30%) reduced the retention of P. Based on the results of the present study, 0.15% NPP (180 mg/b/d) in the diets of WL layers is adequate for optimum production performance during 28 to 44 weeks of age, however, WL layers require 0.27% NPP (324 mg /b/d) in the diet for optimum production with better bone mineralization.