APPLICATION OF TIN ION-PLATING TO THE ORTHODONTIC APPLIANCE (교정용 장치물에 대한 TiN Ion Plating의 응용)

  • Kwon, Oh-Won;Kim, Kyo-Han
    • The korean journal of orthodontics
    • /
    • v.21 no.1 s.33
    • /
    • pp.7-16
    • /
    • 1991
  • To estimate the possibility of the application of TiN ion-plating to the orthodontic appliance, colorimetric properties, and characteristics of ion-plated film as well as adhesive strength of TiN film to the substrate and mechanical properties of ion-plated orthodontic appliance were investigated. The obtained results were as follows: 1) TiN ion-plated film had the colorimetric properties which were the hue of about 2.5 Y, the brightness of about 6, and the chroma of about 4 by the standard color chip of JIS. 2) TiN ion-plated film was $2{\mu}m$ in thickness and its deposition pattern was rather irregular. 3) TiN phase was confirmed on the X-ray diffraction pattern. 4) Critical load for delamination of ion-plated film from stainless steel band was 10N. 5) Tensile and yield strength of ion-plated specimen was increased about 10Kg $f/mm^2$, while elongation was decreased $1\%$ compairing to the values of the non ion-plated specimen.

  • PDF

A study on Airborne Concentration of Welding Fumes and Metals in Confined Spaces of a Shipyard (모조선소의 밀폐된 작업장에서의 공기중 용접흄 및 중금속 농도에 관한 조사 연구)

  • Kwag, Young-Soon;Paik, Nam-Won
    • Journal of Korean Society of Occupational and Environmental Hygiene
    • /
    • v.7 no.1
    • /
    • pp.113-131
    • /
    • 1997
  • This study was performed to evaluate the exposure levels of worker exposed to welding fume and metals in confined spaces of a shipyard. The airborne concentration of welding fumes and metal elements in confined spaces were compared with those in open working areas. Results of the study were as follows. 1. The geometric mean of welding fume concentration in a confined space was $16.6mg/m^3$, which contained $3.9mg/m^3$ Fe, $1.2mg/m^3$ Mg, $0.8mg/m^3$ Zn, $0.008mg/m^3$ Cu, $0.008mg/m^3$ Pb, $0.005mg/m^3$ Ni, $0.003mg/m^3$ Cr, $0.003mg/m^3$ Cd. The geometric mean of welding fume concentration in open working areas was $5.2mg/m^3$, which contained $1.1mg/m^3$ Fe, $0.3mg/m^3$ Mg, $0.3mg/m^3$ Zn, $0.004mg/m^3$ Cu, $0.008mg/m^3$ Pb, $0.005mg/m^3$ Ni, $0.003mg/m^3$ Cr, $0.0003mg/m^3$ Cd. The geometric mean of welding fume concentration in confined spaces was 3,2 times higher than that in open working areas. The geometric mean concentrations of such metals as Fe, Mg, Zn, or Cu within fume in confined spaces were 2-4 times higher than those in open working areas, while little difference made such metals as Pb, Ni, Cr, Cd. 2. In 32 samples out of a total of 39 samples (82.1%) collected in confined spaces, the concentrations of welding fume exceeded TLV. while so did 19 samples out of 33 samples (57.6%) in open working areas. As for the concentrations of metals in welding flume from confined spaces, Fe exceeded TLV in 14 out of a total of 38 samples (36.8%), Mn exceeded TLV in 23 out of a total of 38 samples (60.5%). As for the concentration of metals in welding fume from open working areas, Fe exceeded TLV in 3 out of a total of 34 samples (8.8%), Mn exceeded TLV in 6 out of a total of 34 samples (17.6%). Considering additive effect among metals, in 31 out of a total of 39 samples (79.5%) collected in confined spaces, the concentrations of welding fume exceeded TLV, while so did 14 out of 38 samples (55.6%) in open working areas. 3. In respect of base metal and welding type the concentration of total welding fume by $CO_2$ gas W./mild steel was the highest, followed by semiauto MMA/mild steel, then followed by TIG or $CO_2$ gas W./stainless steel. ; as for concentration of metal within fume, a decreasing order was Fe, Zn, Mn, and Pb in $CO_2$ gas W./mild steel and semiauto MMA/mild steel, but Fe, Mn, Cr, and Ni in TIG or $CO_2$ gas W./stainless steel. 4. In case of welding base metal covered by paint, contents of Zn within red paint chip and within gray paint chip were 14.0% and 0.08% respectively, which showed a little difference, while the airborne concentrations of Zn within fume during welding base metal covered red paint and gray paint were $1.351mg/m^3$ and $1.018mg/m^3$ respectively, which showed little difference. As for Pb, contents of red paint chip and gray paint chip were 0.14% and 0.08% respectively, and the airborne concentrations within fume during welding base metal covered red paint and gray paint were $0.009mg/m^3$ and $0.007mg/m^3$ respectively, both of which showed little difference.

  • PDF

Gene Expression Analysis of Lung Injury in Rats Induced by Exposure to MMA-SS Welding Fume for 30 Days

  • Oh, Jung-Hwa;Park, Han-Jin;Heo, Sun-Hee;Yang, Mi-Jin;Yang, Young-Su;Song, Chang-Woo;Yoon, Seok-Joo
    • Molecular & Cellular Toxicology
    • /
    • v.3 no.4
    • /
    • pp.306-313
    • /
    • 2007
  • The welding fume has been implicated as a causal agent in respiratory disease such as pneumoconiosis. The molecular mechanism by which welding fume induces toxicity in the lung is still unknown, but studies have focused on histological structure and indirect approach measuring the pulmonary damage markers. In the present study, gene expression profiles were analyzed in the lung of rats exposed by manual metal-arc stainless-steel (MMA-SS) welding fume for 30 days using Affymetrix GeneChip$^{(R)}$. Totally, 379 genes were identified as being either up- or down-regulated over 2-fold changes (P<0.01) in the lung of low- or high-dose group and were analyzed by using hierarchical clustering. We focused on genes involved in immune/inflammation responses were differentially regulated during lung injury induced by welding fume exposure. The information of these deregulated genes may contribute in elucidation of the inflammation mechanism during lung injury such as lung fibrosis.

A Study on the Flank Wear of Carbide Tool in Machining SUS304 (SUS304 절삭시 Carbide 공구의 Crater 마모에 관한 연구)

  • Jeong, Jin-Yong;O, Seok-Hyeong;Kim, Jong-Taek;Seo, Nam-Seop
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.8 no.3
    • /
    • pp.44-54
    • /
    • 1991
  • A Study was made on falnk wear in carbide tools in turning SUS304 steel. When an austenitic stainless steel (SUS304 steel) is cut with the tool, saw-toothed chip are produced. It is found that machining SUS304 steel would make a tool worn fast. For increasing productivity, tool wear has to be predicted and controlled. An amended cutting geometry consisting of a negative rake angle ($-6^{\circ}$ ) and a high clearance angle ($-17^{\circ}$ ) is proposed for decreasing carbide tool wear (flank) in the machining of SUS304 steel. The amended cutting geometry is found to make the flank wear lower than a general cutting geometry (rake angle $6^{\circ}$ , clearance angle $5^{\circ}$). The effects of the three cutting variables (cutting speed, feed, tool radius) on the flank wear analyzed by fiting a simple first-order model containing interaction terms to each flank wear parameter by means of regression analysis and the predicted from first-order regression analysis model equation of flank wear.

  • PDF

Ingot Casting with Ferro-Titanium Pretreatment Process using Ti Scrap (타이타늄 스크랩을 활용한 페로 -타이타늄 전처리 공정 적용 모합금 주조)

  • Lee, Cho-Long;Park, Jong-Bum;Kang, Tae-Woong;Min, Tae-Sik;Jeon, Soo-Hyeok;Ro, Yoon-Gyeong
    • Journal of Korea Foundry Society
    • /
    • v.41 no.2
    • /
    • pp.139-143
    • /
    • 2021
  • A type of titanium alloy, ferro-titanium, is the main material used to manufacture steel and stainless steel. Considering economic aspects, ferro-titanium ingots are intended to be manufactured using low-cost titanium scrap, and the best pretreatment process for removing impurities from recycled titanium scrap surfaces was studied here. Instead of ordinary acid or organic solvents, ecofriendly methods were researched and applied, and chip scrap materials were used. A high-quality ferro-titanium ingot was manufactured from titanium scrap after a pretreatment process was applied, and the impurities and properties were analyzed and compared with commercial material standards through a component analysis.

The Study of Fast X-ray Fluorescence Analysis Using a SSQ Program (SSQ 프로그램을 이용한 빠른 X-선형광분석법 고찰)

  • Park, Yong Joon
    • Analytical Science and Technology
    • /
    • v.11 no.2
    • /
    • pp.112-119
    • /
    • 1998
  • A Siemens SemiQuant (SSQ) 3000 program, a precalibrated 'standardless' analytical program handling up to 90 elements, was evaluated for the fast analysis of various types of reference materials using a wavelength dispersive X-ray spectrometer. Various types of standard reference materials such as metal discs, metal chips, and geological materials in powder form were analysed and it took 23 minutes of measuring time for 75 elements. Measurements of geological reference materials using different sampling methods were carried out and their data were interactively evaluated. The analysis of materials of a known matrix concentration such as stainless steels provided higher precision value compared to totally unknown samples. The analyses of materials prepared as pressed pellets or fused glass beads provided higher precision values compared to the measurement of loose powders with a foil on the sample surface and helium operation, though their sampling procedures were more complicate and took more time. Since very light elements such as boron, carbon, and oxygen have a strong influence on the matrix effects and also on the calculation of effective matrix corrections, the rhodium Compton check was applied to verify the reliability of the defined light element concentrations of light matrix materials and the defined major sample compounds. Failure of defining correct matrix resulted in an unoptimized matrix correction and therefore in the wrong calculation of the element concentration.

  • PDF

Effect of Physical Control Technology on Aspergillus ochraceus Reduction (물리적 제어기술이 Aspergillus ochraceus 저감화에 미치는 영향)

  • Lee, Eun-Seon;Kim, Jong-Hui;Kim, Bu-Min;Oh, Mi-Hwa
    • Journal of Food Hygiene and Safety
    • /
    • v.36 no.5
    • /
    • pp.447-453
    • /
    • 2021
  • In this study, the effectiveness of physical control technology, a combined light sterilization (LED, UV) and hot water treatment in reducing Aspergillus ochraceus for food production environment was investigated. In brief, 1 mL aliquot of A. ochraceus spore suspension (107-8 spore/mL) was inoculated onto stainless steel chips, which was then dried at 37℃, and each was subjected to different physical treatment. Treatments were performed for 0.5, 1, 2, 5, 8, and 11 hours to reduce the strains using a light-emitting diode, but no significant difference was confirmed among the treatments. However, a significant reduction was observed on the chips treated with UV-C exposure and hot water immersion. After being treated solely with 360 kJ/m2 of UV-C on stainless steel chip, the fungi were significantly reduced to 1.27 log CFU/cm2. Concerning the hot water treatment, the initial inoculum amount of 6.49 log CFU/cm2 was entirely killed by immersion in 83℃ water for 5 minutes. Maintaining a high temperature for 5 minutes at the site is difficult. Thus, considering economic feasibility and usability, we attempted to confirm the appropriate A. ochraceus reduction conditions by combining a relatively low temperature of 60℃ and UV rays. With the combined treatments, even in lukewarm water, A. ochraceus decreased significantly through the increases in the immersion time and the amount of UV-C irradiation, and the yield was below the detection limit. Based on these results, if work tools are immersed in 60℃ lukewarm water for 3 minutes and then placed in a UV sterilization device for more than 10 minutes, the possibility of A. ochraceus cross-contamination during work is expected to be reduced.

Thermal Environments of Children's Parks during Heat Wave Period (폭염 시 어린이공원의 온열환경)

  • Ryu, Nam-Hyong;Lee, Chun-Seok
    • Journal of the Korean Institute of Landscape Architecture
    • /
    • v.44 no.6
    • /
    • pp.84-97
    • /
    • 2016
  • This study was to investigate the user's thermal environments of the children's parks according to pavements and sunscreen types during periods of heat waves. The measurements were conducted at the sand pits, rubber chip pavement, shelters, and green shade ground of the two children's parks located in Jinju, Korea(Chilam: $N\;35^{\circ}11^{\prime}1.4{^{\prime}^{\prim}}$, $E\;128^{\circ}5^{\prime}31.7{^{\prime}^{\prime}}$, elevation 38m, Gaho: $N\;35^{\circ}09^{\prime}56.8{^{\prime}^{\prime}}$, $E\;128^{\circ}6^{\prime}41.1{^{\prime}^{\prime}}$, elevation 24m) over three days during 11-13, August, 2016. The highest ambient air temperatures at the Jinju Meteorological Office during the three measurement days were $35.9{\sim}36.8^{\circ}C$, which corresponded with the extremely hot weather. A series of experiments measured air temperature, relative humidity, wind velocity, black globe temperature, and long-wave and short-wave radiation of the six directions 0.6 m above ground level. The wet bulb globe temperature(WBGT) and the universal thermal climatic index(UTCI) were used to evaluate thermal stress. Surface temperature images of the play equipment were also taken using infrared thermography. Surface temperatures of the play equipment and grounds were used to evaluate burn risk through contact with playground materials. The results showed the following. The maximum air temperatures averaged over 1-hour period for three days were $36.6{\sim}39.4^{\circ}C$. The sun shades reduced those temperatures by up to $2.8^{\circ}C$(green shade) and $1.0^{\circ}C/2.3^{\circ}C$(shelters). The minimum relative humidity values averaged over 1-hour period for three days were 44~50%. The sun shades increased those humidity values by up to 6%(green shade) and 4%/6%(shelters). The risk of heat related illness at the measurement sites of the children's parks were extreme and high in the daytime hours. The maximum WBGT values averaged over a 30-minute period for three days were $31.2{\sim}33.6^{\circ}C$. The sun shades reduced those WBGT values by up to $2.4^{\circ}C$(green shade) and $0.5^{\circ}C/2.1^{\circ}C$(shelters) compared to sandpits, but would not block the risk of heat related illness in the daytime hours. The category of heat stress at the measurement sites of the children's parks were extreme and very strong in the daytime hours. The maximum UTCI values averaged over a 30-minute period for three days were $39.9{\sim}48.1^{\circ}C$. The sun shades reduced those UTCI values by up to $7.8^{\circ}C$(green shade) and $4.1^{\circ}C/8.2^{\circ}C$(shelters) compared to sandpits, but could not lower heat stress category from extreme and very strong to strong and moderate in the daytime hours. According to the burn threshold criteria when skin was in contact with playground materials, the maximum surface temperature of the stainless steels($70.8^{\circ}C$) surpassed three seconds $60^{\circ}C$ threshold for uncoated steel, that of the rubber chip($76.5^{\circ}C$) surpassed five seconds $74^{\circ}C$ threshold for the plastic, that of the plastic slide($68.5^{\circ}C$) and seats($71.0^{\circ}C$) surpassed the one min $60^{\circ}C$ threshold for plastic, respectively. The surface temperatures of shaded play equipment were lower approximately $20^{\circ}C$ than those of play equipment exposed to the sun. Therefore, sun shades can block the risk of burns in daytime hours. Because of the extreme and high risk of heat related illness and extreme and high heat stress at the children's parks during periods of heat waves, parents and administrators must protect children from the use of playgrounds. The risk of burn when contact with play equipments and grounds at the children's parks during periods of heat waves, was very high. The sun shades are essential to block the risk of burn from play equipments and grounds at the children's parks during heat waves.