페라이트의 연삭성에 관한 연구 (Study on grindability of ferrite)

  • 김성청;이재우
    • 대한기계학회논문집A
    • /
    • 제21권9호
    • /
    • pp.1507-1519
    • /
    • 1997
  • This paper aims to clarify the effects of grinding conditions on bending strength in surface grinding of various ferrites with the resin bond diamond wheel. The main conclusions obtained were as follows. At a constant material removal rate, the strength improves with increased wheel depth of cut and decreased workpiece speed. It is desirable to grind at higher peripheral wheel speed and under the critical workpiece speed presented in this paper. Grinding the ferrite of higher brittleness, the wheel depth of cut limited to hold 50% of their inherent strength becomes lower. The effect of various grinding conditions on bending strength becomes more larger in the order of Sr, Mn-Zn and Cu-Ni-Zn. When using the diamond grain of the lower toughness, the bending strength becomes higher, and the wheel wear occurs faster. Considering both bending strength and wheel wear rate, the best concentration of wheel is 100. The ground surfaces exhibit that the fracture process during grinding becomes more brittle in the order of Sr, Mn-Zn and Cu-Ni-Zn.

Paint형 전파 흡수체의 전파 흡수 성능 향상에 관한 연구 (A Study on the Improvement of EM Wave Absorption Characteristics in Paint-type EM Wave Absorbers)

  • 제승훈;김동일;최정현
    • 한국전자파학회논문지
    • /
    • 제17권4호
    • /
    • pp.330-334
    • /
    • 2006
  • 본 논문에서 Sendust, Mn-Zn, Ni-Zn, Ba, Sr Ferrite를 사용하여 페인트형 흡수체를 제작하였다. 지지재로서는 enamel, epoxy, urethane 페인트들을 사용하여 각각 흡수능을 측정하였다. 그리고 $Al(OH)_3$으로 코팅한 흡수체의 대역폭은 코팅을 하지 않은 것보다 더 넓어지는 것을 알 수 있다. 또 2 mm 두께의 적층형 흡수체는 X-band에서 대략 20 dB의 흡수능을 보여준다.

도전성 고무의 충전제로 이용 가능한 $Dy_{2-x}Sr_{1+x}Fe_2O_{7-y}$ 페라이트계의 전기적 특성에 대한 연구 (Studies on the Electrical Properties of $Dy_{2-x}Sr_{1+x}Fe_2O_{7-y}$ ferrite System Which Can be used as Filler for Conducting Rubbers)

  • 이은석;최세영
    • Elastomers and Composites
    • /
    • 제28권2호
    • /
    • pp.103-107
    • /
    • 1993
  • To make new filler for conducting rubber, the sample of perovskite-related ferrite system $Dy_{2-x}Sr_{1+x}Fe_2O_{7-y}$ (x=0.0, 0.5, 1.0, 1.5, and 2.0) were synthesized at 1473K in air. $M{\ddot{o}}ssbauer$ spetrum of x=0.0 sample shows typical six line pattern with $M{\ddot{o}}ssbauer$ parameters, $I.S=3.6{\times}10^{-1}mm/sec,\;E_Q=-7.0{\times}10^{-2}mm/sec,\;H_{int}=5.19{\times}10^2\;Koe$. In case of x=2.0, the spectrum is composed of single line exhibiting coexistance of $Fe^{3+}(I.S.=3.7{\times}10^{-1}mm/sec)$ ions and $Fe^{4+}(I.S.=-1.9{\times}10^{-1}mm/sec)$ ions. With increase in x value electrical conductivity at constant temperature sharply increased and the activation energies decreased from $3.8{\times}10^{-1}\;to\;1.9{\times}10^{-1}\;eV$.

  • PDF

자화된 SrO 6$Fe_{2}O_{3}$ 세라믹스와 전해질 계면의 전기물리적 현상에 미치는 Curie점 열처리 효과 (The Effect of Curie Point Annealing on Electrophysical Phenomena at the Magnetized SrO 6$Fe_{2}O_{3}$ Ceramics/Electrolyte Interface)

  • 천장호;손광철;라극환
    • 전자공학회논문지A
    • /
    • 제31A권7호
    • /
    • pp.63-68
    • /
    • 1994
  • The Curie point annealing effects on electrophysical phenomena at the magnetized strontium ferrite(SrO$\cdot$ 6$Fe_{2}O_{3}$) ceramics electrode/10$^{-3}$M KC1 aqueous electrolyte interfaces have been studied using cyclic voltammetric, normal pulse voltammetric, chronocoulometric, and electrochemical impedance techiques. After the Curie point annealing the magnetic flux densities of the speciment was decreased from 900-1100 gauss to 1-2 gauss, i.e. demagnetized. The real component of interfacial impedance was decreased from 7280-7320 ohm to 790-830 ohm. The adsorption and the charge on the electrical double layer was increased from 0 $\mu$C to -58 $\mu$C. The Curie point annealing and the related electrical double layer effect can influence not only the electrophysical properties of the strontium ferrite ceramics electrode itself but also the electrochemical phenomena at the electrode interface. This experimental results suggest that the Curie point annealing and the related electrical double layer effect can be applied to electrochemical magnetic sensors.

  • PDF

페라이트의 연삭저항 및 연삭면 특성 (Study on Grinding Force and Ground Surface of Ferrite)

  • 김성청
    • 한국생산제조학회지
    • /
    • 제6권3호
    • /
    • pp.17-25
    • /
    • 1997
  • This paper aims to clarify the effects of grinding conditions on the grinding force, ground surface and chipping size of workpiece in surface grinding of various ferrites with the resin bond diamond wheel. The main conclusions obtained were as follows: In a constant peripheral wheel speed, the specific grinding energy is fitted by straight lines with grinding depth coefficient($\delta$) in a logarithmic graph. The effect of both depth of cut and workpiece speed on grinding energy becomes larger in the order of Mn-Zn, Cu-Ni-Zn and Sr. When using the diamond grain of the lower toughness, the roughness of the ground surface becomes lower. The ground surfaces show that the fracture process during grinding becomes more brittle in the order of Sr, Mn-Zn and Cu-Ni-Zn. The chipping size at the corner of workpiece in grinding increases with the the increases of the depth of cut and workpiece speed, and the decrease of peripheral wheel speed. The effect of both depth of cut and workpiece speed on chipping size becomes more larger in the order of Sr, Mn-Zn and Cu-Ni-Zn.

  • PDF

커플링제가 플라스틱 페라이트 자석의 레올로지와 자기특성에 미치는 영향 (Effects of Coupling Agents on the Rheological and Magnetic Properties of Plastic Ferrite Magnets)

  • 이석희;최준환;문탁진;정원용
    • 한국자기학회지
    • /
    • 제8권5호
    • /
    • pp.275-281
    • /
    • 1998
  • 커플링제 종류에 따른 플라스틱 페라이트 이방성 자석의 레올러지와 자기특성에 미치는 영향을 조사하여 비교하였다. 커플링제는 silane A174와 titanete TTS를 사용하였으며, 고분자 결합제는 polypropylene(PP), 자성분말은 Sr-페라이트를 사용하였다. TTS의 첨가가 A174의 첨가보다 혼합물의 점도 감소와 자기특성 증가에 더 효과적이었다. 커플링제가 첨가되지 않은 혼합물과 비교하여, A174는 23%, TTS는 50%의 점도 감소 효과를 나타내었다. (전단율 1280 sec-1에서). 4 kOe의 자장하에서 사출성현한 플라스틱 이방성 자석은 커플링제로 처리되지 않은 자석 (잔류자속밀도 : 1.89 kG, 최대자기에너지적 : 0.84 MGOe)에 비해 A174 처리에 의해 잔류자속밀도는 2.25 kG, 최대자기에너지적은 1.23 MGOe로 향상되었으며, TTS의 처리에 의해 잔류자속밀도는 2.35 kG, 최대자기 에너지적은 1.33 MGOe로 각각 향상되었다.