• 제목/요약/키워드: Spray Dry

검색결과 184건 처리시간 0.046초

분산계 특성이 질화규소 미분의 과립특성 및 충진거동에 미치는 영향 (Effect of Suspension Property on Granule Characteristics and Compaction Behavior of Fine Si3Na4 Powder)

  • 이해원;오성록
    • 한국세라믹학회지
    • /
    • 제32권4호
    • /
    • pp.462-470
    • /
    • 1995
  • The characteristics of spray-dried granules are important for dry pressing operation since they have great influences on die-filling, compaction ratio, and resulting green microstructure. An attempt was made to control granule morphology and the packing structure of fine Si3N4 particles in granules by adjusting suspension property. Mercury porosimetry was used to characterize the pore structures of both granules and green compacts. Finally, the effects of particle packing structure in granules and green microstructure on sintering behavior were investigated.

  • PDF

괴화추출물에 의한 견섬유의 염색성 (Dyeing of Silk with Chinese Scholar Tree Extract)

  • 배정숙;김성숙
    • 한국염색가공학회지
    • /
    • 제12권3호
    • /
    • pp.183-191
    • /
    • 2000
  • The dyeing of silk fabric with chinese scholar tree extract was investigated. The colorant was extracted with distilled water, and concentrated under reduced pressure, and, finally spray-dried. The optimum temperature and dyeing time for the dyeing of silk with the scholar tree extract was $60^\circ{C}$ and 60 minutes respectively. In mordant dyeing, pre-mordanting method was most effective for color yield, and 1~2 % of mordant concentration was acceptable. Fastness of the dyed silk fabric to laundering and rubbing was shown to be good, but fastness to light, dry cleaning, and perspiration were varied with used mordants.

  • PDF

Spray Dryer Absorber 배연탈황공정의 모델 개발 (Model Development of Spray Dryer Absorber FGD Process)

  • 장순희;오의경;이형근;김선근
    • 청정기술
    • /
    • 제2권1호
    • /
    • pp.80-95
    • /
    • 1996
  • 반건식 배연탈황공정에서 사용되는 spray dryer absorber(SDA)에 대한 수치모사를 행하였다. 기본 방정식으로는 기체와 액적의 각 성분들의 물질수지식, 에너지수지식과 액적의 운동 방정식등이 포함되었다. 만들어진 모델은 대부분이 기존의 SPRAYMOD-M보다 실제의 pilot plant data를 더 잘 모사하였다. 실제 pilot plant에서 사용되는 값의 범위 내에서 선정된 공정변수가 SDA의 성능에 미치는 효과를 계산하고, 이를 $SO_2$의 흡수속도, 배연기체의 체류시간, 그리고 액적의 건조시간 및 속도 등에 의해 검토하였다. 또 $SO_2$ 제거율을 두 개의 독립된 공정 변수의 함수로 구하였으며, 그 결과를 3차원 또는 2차원의 등가선으로 표시하여 SDA의 설계에 쉽게 적용될 수 있도록 하였다.

  • PDF

레이저충격파를 이용한 웨이퍼 세정 (Wafer cleaning efficiency by Laser Shock Wave)

  • 강영재;이상호;박진구;이종명;김태훈
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2003년도 기술심포지움 논문집
    • /
    • pp.256-259
    • /
    • 2003
  • To develop cleaning process various particles should be deposited on wafer surfaces to measure particle removal efficiencies. The purpose of the article in to evaluate, removal efficient)r of silica and alumina particles from wafer surfaces when they are deposited by dry and wet method. Dry deposition in air and wet spray deposition using solutions are used. van der Waals are considered to calculate the adhesion force of particles on surfaces. Higher adhesion force is measured on alumina particles on silicon when particles are deposited in air.

  • PDF

Cut Edge Corrosion of Painted Zn and 55%Al-Zn Coated Steels under Alternate Wetting and Drying

  • Nishikata, A.;Tsuda, T.;Tsuru, T.
    • Corrosion Science and Technology
    • /
    • 제9권1호
    • /
    • pp.34-38
    • /
    • 2010
  • Electrochemical study on cut edge corrosion of prepainted Zn coated (GI) and 55%Al-Zn coated (GL) steels has been performed in wet-dry cyclic conditions. Maximum width of delaminated polymer coating from the cut edge for GI and GL specimens was evaluated under wet-dry cyclic conditions. The cyclic tests were carried out for 1000 h by changing of relative humidity, where the salt of NaCl was deposited on the specimen every 48 h. The cut edge corrosion test under NaCl deposit indicated that the delamination of the GL specimen progresses at a higher rate than the GI. The electrochemical corrosion monitoring was also performed under condition of alternate exposure to immersion in NaCl solution and drying at 60%RH and $25^{\circ}C$. On the basis of the results of the delamination tests and electrochemical measurements, the mechanism of cut edge corrosion for GI and GL were discussed.

전단희석 액적의 건조 벽면 충돌 후 전개-수축 거동의 관찰 (Examination of Spread-Recoil Behavior of a Shear-thinning Liquid Drop on a Dry Wall)

  • 안상모;이상용
    • 한국분무공학회지
    • /
    • 제14권3호
    • /
    • pp.131-138
    • /
    • 2009
  • In the present study, spread-recoil behavior of a drop of shear-thinning liquid (xanthan solution) on a dry wall (polished stainless-steel plate) was examined and compared with that of Newtonian liquid (glycerin solution). Nine different kinds of xanthan and glycerin solutions were tested, including three pairs of xanthan and glycerin solutions, each having the same viscosity in low shear rate region ($10^{-2}-10^0\;l/s$). The drop behavior was visualized and recorded using a CCD camera. The maximum diameter and the spreading velocity of the xanthan drops turned out to be significantly larger and the time to reach their final shape was much shorter compared to the cases with the glycerin solutions, due to the smaller viscous dissipation resulted from lower viscosity in the higher shear rate region (>$10^0\;l/s$). As a result, the maximum diameters were measured to be larger than the predicted values based on the model proposed for Newtonian liquids, and the deviation was more pronounced with the solution with the larger viscosity variation. Consequently, viscosity variation with the shear rate was found to be a dominant factor governing the spread-recoil behavior of shear-thinning drops.

  • PDF

Screening of Spray-Dried K2CO3-Based Solid Sorbents using Various Support Materials for CO2 Capture

  • Eom, Tae Hyoung;Lee, Joong Beom;Baek, Jeom In;Ryub, Chong Kul;Rhee, Young Woo
    • KEPCO Journal on Electric Power and Energy
    • /
    • 제1권1호
    • /
    • pp.115-120
    • /
    • 2015
  • $K_2CO_3$-based dry regenerable sorbents were prepared by spray-drying techniques to improve mass produced $K_2CO_3-Al_2O_3$ sorbents (KEP-CO2P, hereafter), and then tested for their $CO_2$ sorption capacity by a $2,000Nm^3/h$ (0.5 MWe) $CO_2$ capture pilot plant built for Unit 3 of the Hadong thermal power station in 2010. Each of the sample sorbents contained 35 wt.% $K_2CO_3$ as the active materials with various support materials such as $TiO_2$, MgO, Zeolite 13X, $Al_2O_3$, $SiO_2$ and hydrotalcite (HTC). Their physical properties and reactivity were tested to evaluate their applicability to a fluidized-bed or fast transport-bed $CO_2$ capture process. The $CO_2$ sorption capacity and percentage utilization of $K_2CO_3$-MgO based sorbent, Sorb-KM2, was $8.6g-CO_2/100g$-sorbents and 90%, respectively, along with good mechanical strength for fluidized-bed application. Sorbs-KM2 and KT were almost completely regenerated at $140^{\circ}C$. No degradation of Sorb-KM by $SO_2$ added as a pollutant in flue gas was observed during a cycle test.

배가스 이산화탄소(CO2)용 Potassium계 흡수제의 성능 향상 연구 (A Study on the Improvement of Potassium Based Sorbent for Flue Gas Carbon Dioxide(CO2))

  • 위영호;류청걸;최동혁
    • 한국기후변화학회지
    • /
    • 제2권2호
    • /
    • pp.107-113
    • /
    • 2011
  • 본 연구에서는 하동화력 0.5 MW 건식 이산화탄소 포집 공정에 적용하고 있는 Potassium 계열 흡수제의 성능 개선을 위한 실험 결과를 기술하였다. 먼저, 마그네타이트와 산화구리를 additive로 적용한 흡수제 2종을 각각 분무건조기를 이용하여 제조한 흡수제의 재생성을 포함한 물성을 평가하였다. 그 결과, 마그네타이트를 적용한 흡수제의 내마모도가 상대적으로 우수한 특성을 나타내었다. 두 번째는, 마그네타이트를 적용한 개량형 Potassium계 흡수제의 연속적인 흡수/재생 특성을 파악하기 위하여 Multi cycle TGA 반응성 평가를 수행하였다. 그 결과, 2nd cycle 이후에도 5.5 wt% 이상의 $CO_2$ 흡수능을 유지하였으며, 내마모도 값도 0.5 정도로 아주 우수하였다. 마지막으로, 공정상의 재생 온도를 낮출 수 있는 조성 선정을 위하여 supporter의 특성이 다른 흡수제의 특성을 고찰하였다. 그 결과, 염기성 지지체를 적용한 KMO 흡수제의 흡수능이 7.2 wt%로 높게 나타났다.

용사법에 의해 제조된 $Al/Al_2O_3$ 복합재료의 상대재에 따른 마모특성 (Wear Properties of Thermal Sprayed Al-based Metal Matrix Composites Against Different Counterparts)

  • 김균택;김영식
    • 동력기계공학회지
    • /
    • 제12권3호
    • /
    • pp.60-65
    • /
    • 2008
  • This study aims at investigating the wear properties of thermally sprayed $Al/Al_2O_3$ metal matrix composite(MMC) coating against different counterparts. $Al/Al_2O_3$ MMC coatings were fabricated using a flame spray system on an Al 6061 substrate. Dry sliding wear tests were performed using the sliding speeds of 0.2m/s and the applied loads of 1 and 2 N. AISI 52100, $Al_2O_3$, $Si_3N_4\;and\;ZrO_2$ balls(diameter: 8mm) were used as counterpart materials. Wear properties of $Al/Al_2O_3$ MMC coatings were analyzed using a scanning electron microscope(SEM) and energy dispersive X-ray spectroscopy (EDX). It was revealed that wear properties of $Al/Al_2O_3$ composite coatings were much influenced by counterpart materials. In the case of AISI 52100 used as counterparts, the wear rate of composites coating layer increased according to the increase of the applied load. On the contrary, in the case of ceramics used as counterparts, the wear rate of composites coating layer decreased according to the increase of the applied load.

  • PDF