Fabrication of Schottky Device Using Lead Sulfide Colloidal Quantum Dot

  • Kim, Jun-Kwan;Song, Jung-Hoon;An, Hye-Jin;Choi, Hye-Kyoung;Jeong, So-Hee
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.189-189
    • /
    • 2012
  • Lead sulfide (PbS) nanocrystal quantum dots (NQDs) are promising materials for various optoelectronic devices, especially solar cells, because of their tunability of the optical band-gap controlled by adjusting the diameter of NQDs. PbS is a IV-VI semiconductor enabling infrared-absorption and it can be synthesized using solution process methods. A wide choice of the diameter of PbS NQDs is also a benefit to achieve the quantum confinement regime due to its large Bohr exciton radius (20 nm). To exploit these desirable properties, many research groups have intensively studied to apply for the photovoltaic devices. There are several essential requirements to fabricate the efficient NQDs-based solar cell. First of all, highly confined PbS QDs should be synthesized resulting in a narrow peak with a small full width-half maximum value at the first exciton transition observed in UV-Vis absorbance and photoluminescence spectra. In other words, the size-uniformity of NQDs ought to secure under 5%. Second, PbS NQDs should be assembled carefully in order to enhance the electronic coupling between adjacent NQDs by controlling the inter-QDs distance. Finally, appropriate structure for the photovoltaic device is the key issue to extract the photo-generated carriers from light-absorbing layer in solar cell. In this step, workfunction and Fermi energy difference could be precisely considered for Schottky and hetero junction device, respectively. In this presentation, we introduce the strategy to obtain high performance solar cell fabricated using PbS NQDs below the size of the Bohr radius. The PbS NQDs with various diameters were synthesized using methods established by Hines with a few modifications. PbS NQDs solids were assembled using layer-by-layer spin-coating method. Subsequent ligand-exchange was carried out using 1,2-ethanedithiol (EDT) to reduce inter-NQDs distance. Finally, Schottky junction solar cells were fabricated on ITO-coated glass and 150 nm-thick Al was deposited on the top of PbS NQDs solids as a top electrode using thermal evaporation technique. To evaluate the solar cell performance, current-voltage (I-V) measurement were performed under AM 1.5G solar spectrum at 1 sun intensity. As a result, we could achieve the power conversion efficiency of 3.33% at Schottky junction solar cell. This result indicates that high performance solar cell is successfully fabricated by optimizing the all steps as mentioned above in this work.

  • PDF

$Pb(Sc_{1/2}Nb_{1/2})O_3$ 박막 형성에 미치는 공정변수의 영향 (Effect of the processing variables on the formation of $Pb(Sc_{1/2}Nb_{1/2})O_3$ thin layers)

  • 박경봉;권승협;김태희
    • 한국결정성장학회지
    • /
    • 제19권2호
    • /
    • pp.70-74
    • /
    • 2009
  • Sol-gel 법으로 제조한 $Pb(Sc_{1/2}Nb_{1/2})O_3$(이하 PSN) sol을 이용하여 스핀 코팅법으로 Pt(111)/Ti/$SiO_2$/Si 기판위에 제조한 박막의 제조 공정에 따른 영향을 연구하였다. Pt 기판위에 PSN sol을 증착, 건조한 후에 $370^{\circ}C$에서 5분간 열처리를 행한 후 $10^{\circ}C/sec$의 급속 가열로 $600{\sim}700^{\circ}C$에서 최종 열처리한 경우에 박막은 (111)면으로 우선 배향하는 것으로 나타났다. 그러나 중간 열처리를 거치지 않고, 급속가열에 의한 최종 열처리만을 행한 경우에는 (100)면으로 우선 배향하는 것으로 나타났다. 한편, 중간 열처리 후 $4^{\circ}C/min$의 승온속도로 관상로에서 최종 열처리를 행한 경우에는 (111)면과 (100)면이 동시에 나타나는 것으로 나타났다. 동일한 조건하에서 박막의 두께는 모두 300로 중간 열처리 공정이 어떠한 영향도 미치지 않는 것으로 나타났다.

정공 주입층 및 수송층에 따른 고분자 유기발광다이오드의 특성 연구 (The Properties of Hole Injection and Transport Layers on Polymer Light Emitting Diode)

  • 신상배;장호정
    • 마이크로전자및패키징학회지
    • /
    • 제14권4호
    • /
    • pp.37-42
    • /
    • 2007
  • 본 연구에서는 ITO/PEDOT:PSS/PFO:MEH-PPV/LiF/Al의 구조를 갖는 고분자 유기발광다이오드를 제작하여 정공 주입층으로 사용되는 PEDOT:PSS의 두께 변화와 PVK 정공 수송층을 도입하여 ITO/PEDOT:PSS/PVK/PFO:MEH-PPV/LiF/Al 구조를 갖는 고분자 유기발광 다이오드를 제작하여 정공수송층이 유기발광다이오드의 전기 광학적 특성에 미치는 영향에 대하여 조사, 비교하였다. 실험에 사용된 모든 유기물은 플라즈마 처리된 ITO/glass 기판위에 스핀 코팅법으로 도포하였다. 정공 주입층인 PEDOT:PSS 두께를 약 80 nm에서 50 nm로 감소한 경우 PLED 소자의 휘도는 약 $220cd/m^2$ 에서 $450cd/m^2$으로 크게 증가하였다. 이러한 결과는 정공 주입층의 두께가 감소할수록 ITO 전극에서 발생한 정공이 보다 쉽게 발광막으로 전달되기 때문이다. 또한 PVK 정공 수송층을 도입한 PLED소자에서 최대 전류밀도와 휘도는 $268mA/cm^2$$540cd/m^2$ (at 12V)의 값을 각각 나타내었다. PVK 정공 수송층이 도입되지 않은 소자에 비해 전류밀도는 약 14%, 휘도는 약 22%의 특성개선을 나타내었다.

  • PDF

PEDOT:PSS 정공 수송층에 금 나노입자를 첨가한 유기태양전지의 제작 및 특성 연구 (Fabrication and Characterization of Organic Solar Cells with Gold Nanoparticles in PEDOT:PSS Hole Transport Layer)

  • 김성호;최재영;장호정
    • 마이크로전자및패키징학회지
    • /
    • 제20권2호
    • /
    • pp.39-46
    • /
    • 2013
  • 본 논문은 캐리어의 이동도 및 전도도를 개선하고, 흡수된 빛의 이동 경로를 증가시켜 광흡수도를 높이기 위하여 정공 수송층 재료에 금 나노입자를 첨가하여 유기태양전지를 제작하였다. 광활성층으로는 P3HT와 PCBM의 bulk-heterojunction 구조를 사용하였다. 유기태양전지에서 금 나노입자를 첨가한 정공 수송층의 효과를 관찰하기 위하여 금 나노입자의 첨가량(0, 0.5, 1.0 wt% Au)과 열처리온도(상온, $110^{\circ}C$, $130^{\circ}C$, $150^{\circ}C$)에 따른 광학적 전기적 특성을 조사하였다. 최대전력변환효율을 갖는 유기태양전지는 0.5 wt% 금 나노입자 첨가한 소자와 $130^{\circ}C$에서 열처리한 소자에서 관찰되었다. 이때 유기태양전지의 전기적 특성은 금 나노입자를 0.5 wt% 첨가한 경우, 단락전류밀도, 곡선인자 및 전력변환효율은 각각 10.2 $mA/cm^2$, 55.8% 및 3.1%로 나타났으며, $130^{\circ}C$에서 열처리한 경우, 12.0 $mA/cm^2$의 단락전류밀도와 64.2%의 곡선인자를 가지며, 4.0%의 전력변환효율이 관찰되었다.

Sol-Gel 법으로 제작한 Zn1-xCoxO 박박의 미세조직 및 자기적 특성 (Microstructure and Magnetic Properties of Zn1-xCoxO Thin Films Grown by Sol-Gel Process)

  • 고윤덕;태원필;김응권;김기출;최춘기;김종민;송준태;박태석;서수정;김용성
    • 한국세라믹학회지
    • /
    • 제42권7호
    • /
    • pp.475-482
    • /
    • 2005
  • Zn$_{l-x}$Co$_{x}$O (x = 0.05 - 0.20) films were grown on Coming 7059 glass by sol-gel process. A homogeneous and stable Zn$_{l-x}$Co$_{x}$O sol was prepared by dissolving zinc acetate dihydrate (Zn(CH$_{3}$COO)$_{2}$$\cdot$2H$_{2}$O), cobalt acetate tetrahydrate ((CH$_{3}$)$_{2}$$\cdot$CHOH) and aluminium chloride hexahydrate (AlCl$_{3}$ $\cdot$ 6H$_{2}$O) as solute in solution of isopropanol ((CH$_{3}$)$_{2}$$\cdot$CHOH) and monoethanolamine (MEA:H$_{2}$NCH$_{2}$CH$_{2}$OH). The films grown by spin coating method were postheated in air at 650°C for 1 h and annealed in the condition of vacuum (5 $\times$ 10$^{-6}$ Torr) at 300$^{\circ}C$ for 30 min and investigated the nature of c-axis preferred orientation and physical properties with different Co concentrations. Znl_xCOxO thin films with different Co concentrations were well oriented along the c-axis, but especially a highly c-axis oriented Zn$_{l-x}$Co$_{x}$O thin film was grown at 10 at$\%$ Co concentration. The transmittance spectra showed that Zn$_{l-x}$Co$_{x}$O thin films occur typical d-d transitions and sp-d exchange interaction became activated with increasing Co concentration. The electrical resistivity of the films at 10 at$\%$ Co had the lowest value due to the highest c-axis orientation. X-ray photoelectron spectroscopy and alternating gradient magnetometer analyses indicated that no Co metal cluster was formed, and the ferromagnetic properties appeared, respectively. The characteristics of the electrical resistivity and room temperature ferromagnetism of Zn$_{l-x}$Co$_{x}$O thin films suggested the possibility for the application to dilute magnetic semiconductors.

적층된 산화그래핀 분리막의 기체 투과 거동 평가 (Gas Transport Behaviors through Multi-stacked Graphene Oxide Nanosheets)

  • 이민용;박호범
    • 멤브레인
    • /
    • 제27권2호
    • /
    • pp.167-181
    • /
    • 2017
  • 그래핀 기반 소재는 높은 가공성과 초박성으로 인하여 분리막 소재로서 각광받고 있다. 본 연구에서는, 스핀 코팅법을 이용하여 제조된 산화그래핀 분리막의 기체 투과 거동을 평가하였다. 산화그래핀 분리막의 구조는 산화그래핀의 크기와 산화그래핀 용액의 pH 조절을 통하여 조절될 수 있다. 산화그래핀의 크기가 작을수록 굴곡률이 작아짐에 따라 분리막의 기체 투과도 및 선택도가 증가하는 경향을 보인다. 또한 산화그래핀에서의 기체 투과 거동은 적층된 산화그래핀 사이의 채널크기에 따라 영향을 받는다. 특히 산화그래핀 분리막의 좁은 기공과 이산화탄소 선택적인 산화그래핀 자체의 특성으로 인하여 산화그래핀 분리막은 이산화탄소에 대한 높은 투과도 및 선택성을 가지며, 이는 이산화탄소 포집에 적합한 특성을 가진다. 이러한 산화그래핀 분리막의 특이한 기체 투과 거동은 흡착-촉진 확산 거동(표면 확산 기작)으로 설명될 수 있다. 본 연구를 통하여 이산화탄소 선택성 분리막 소재 설계와 슬릿 형태의 기공과 적층 구조를 가진 분리막을 통한 기체 투과 거동 연구가 활발히 이루어질 것으로 기대한다.

ITO/Glass 기판위에 PFO-poss 유기 발광층을 가지는 고분자 발광다이오드의 제작 (Preparation of Polymer Light Emitting Diodes with PFO-poss Organic Emission Layer on ITO/Glass Substrates)

  • 유재혁;장호정
    • 마이크로전자및패키징학회지
    • /
    • 제13권4호
    • /
    • pp.51-56
    • /
    • 2006
  • ITO(Indium tin oxide)glass 기판 위에 PEDOT:PSS[poly(3,4-ethylenedioxythiophene):poly (styrene sulfonate)]와 PVX[poly(N-vinyl carbazole)] 고분자 물질을 정공 주입 및 수송층으로, 발광층으로 PFO-poss[Poly(9,9-dioctylfluorenyl-2,7-diyl) end capped with poss]를 사용하여 ITO/PEDOT:PSS/PVK/PFO-poss/LiF/Al 구조의 고분자 발광다이오드를 제작하였다. 이때 스핀코팅을 위한 발광 유기재료의 농도와 열처리 온도가 소자의 전기적, 광학적 특성에 미치는 영향을 조사하였다. 동일한 PFO-poss 농도에서 열처리 온도가 $100^{\circ}C$에서 $200^{\circ}C$로 증가할 경우 PLED 소자의 전류밀도와 휘도특성이 증가하는 경향을 나타내었다. 1.0 wt% 농도를 갖는 PFO-poss 유기물 발광충을 $200^{\circ}C$ 온도로 열처리 할 경우 $958\;cd/m^{2}$의 최대 휘도를 나타내었으며 발광파장은 523 nm 녹색계통의 파장이 크게 증가하여 청백색에 가까운 발광을 나타내었다. PFO-poss 농도증가(0.5 wt%에서 1.0 wt%)와 함께 PLED 소자의 열처리 온도를 $100^{\circ}C$에서 $200^{\circ}C$로 증가할 경우 CIE 색좌표는 청색 (x, y : 0.17, 0.14)에서 청백색 (x, y = 0.29, 0.41)발광으로 천이하는 경향을 나타내었다.

  • PDF

ITO 투명전극의 $O_2$ 플라즈마 처리가 고분자 유기발광다이오드의 전기.광학적 특성에 미치는 영향 (Dependence of $O_2$ Plasma Treatment of ITO Electrode on Electrical and Optical Properties of Polymer Light Emitting Diodes)

  • 공수철;백인재;유재혁;임현승;양신혁;신상배;신익섭;장지근;장호정
    • 한국표면공학회지
    • /
    • 제39권3호
    • /
    • pp.93-97
    • /
    • 2006
  • Polymer light emitting diodes (PLEDs) are expected to be commercialized as next generation displays by advantages of the fast response time, low driving voltage and easy manufacturing process for large sized flexible display. Generally, the electrical and optical properties of PLEDs are affected by the surface conditions of transparent electrode. The PLED devices with ITO/PEDOT:PSS/PVK/PFO-poss/LiF/Al structures were prepared by using the spin coating method. For this, PEDOT:PSS(poly(3,4-ethylenedioxythiophene):poly(styrene sulfolnate)) Al 4083 and PVK(N-vinylcabozole) were used as hole injection and transport layers. The PFO-poss(poly(9,9-dioctylfluorene)) was used as the emitting layer. The dependence of $O_2$ plasma treatment of ITO electrode on the electrical and optical properties of PLEDs were investigated. The sheet resistances increased slightly with an improved surface roughness of ITO electrode as the RF power increased during $O_2$ plasma treatment. The PLED devices prepared on the ITO/Glass substrates, which were plasma-treated at 40 watt in RF power for 30 seconds under 40 mtorr $O_2$ pressure, showed the maximum external emission efficiency of 0.86 lm/W and the maximum luminance of $250\;cd/m^2$, respectively. The CIE color coordinates are ranged $X\;=\;0.13{\sim}0.18$ and $Y\;=\;0.10{\sim}0.16$, showing blue color. emission.

ITO/PEDOT:PSS/MEH-PPV/Al 구조에서 MEH-PPV 농도에 따른 유기발광다이오드의 전기$\cdot$광학적 특성 (The Electrical and Optical Properties of Polymer Light Emitting Diode with ITO/PEDOT:PSS/MEH-PPV/Al Structure at Various Concentration of MEH-PPV)

  • 공수철;백인재;유재혁;임현승;장호정;장지근
    • 마이크로전자및패키징학회지
    • /
    • 제12권2호
    • /
    • pp.155-159
    • /
    • 2005
  • 패턴화된 ITO/Glass 기판위에 정공수송층으로 PEDOT:PSS (poly(3,4-ethylenedioxythi-ophene)poly (styerne sulfolnate))를 발광층으로 MEH-PPV (poly(2-methoxy-5-(2-ethyhexoxy)-1,4-phenylenvinylene))을 사용하여 스핀코팅법으로 ITO/PEDOT:PSS/MEH-PPV/Al 구조의 고분자 유기전계 발광소자 (polymer light emitting diode, PLED)를 제작하였다. MEH-PPV 용액의 농도(0.1, 0.3, 0.5, 0.7, 0.9, 1.5 wt$\%$)변화를 변수로 하여 제작된 PLED소자의 전기$\cdot$광학적 특성 변화를 조사하였다. MEH-PPV의 농도가 $0.5{\~}0.9 wt\%$에서 가장 양호한 전기-광학 특성을 보여 주었다. 한편 $1.5 wt\%$의 고동도의 MEH-PPV를 갖는 PLED 소자에서는 전류와 휘도 값이 크게 감소하였다. 즉, MEH-PPV의 농도가 $0.5 wt\%$일 때 9V 전압 인가시 최고 발광 휘도와 효율은 $409 cd/m^2$와 4.90 lm/W를 각각 나타내었다. PLED 소자의 발광 스펙트럼은 $560{\~}585 nm$ 파장을 갖는 오렌지 계열의 발광을 나타내었다.

  • PDF

PPV 발광층 및 전자 수송층을 가진 이종 접합구조 EL 소자의 제작 및 특성 (Fabrication and Characteristics of Hetero-junction EL Devices Containing Electron Transport Layer and PPV as Emitting Layer)

  • 박이순;한윤수;김성진;신동수;신원기;김우영;이충훈
    • 공업화학
    • /
    • 제9권5호
    • /
    • pp.710-714
    • /
    • 1998
  • Poly(p-phenylene vinylene), PPV를 발광층으로 하고 전자수송층(electron transport layer, ETL)이 도입된 이중 접합구조 유기 전기발광소자(electroluminescence device, ELD)를 제작하고 전기 발광 특성을 조사하였다. 전자 수송제로는 2-(4-biphenyl)-5-(4-tert-butylphenyl)-1,3,4-oxadiazole(PBD)를 사용하고 이를 분산시킬 기재 고분자(matrix polymer)로는 stilbene계 공단량체를 포함하는 poly(styrene-co-p-vinyl-trans-stilbene (PVTS)), poly(styrene-co-MeO-PVTS) 및 poly(styrene-co-MeO-ST)를 합성하였다. 이들 재료를 이용하여 이종 접합구조 ELD를 제조하였으며 poly(styrene-co-PVTS)를 기재 고분자로 쓴 EL 소자가 최대의 휘도를 나타냄을 확인하였다. Poly(styrene-co-MeO-PVTS) 및 poly(styrene-co-MeO-ST) 등 전자 주게 성질을 가진 methoxy기를 함유하는 기재 고분자를 쓴 EL 소자는 전자 수송층이 없는 ITO/PPV/Mg 단층 소자와 휘도가 유사 혹은 낮게 나타났다. Poly(styrene-co-PVTS)를 ETL에 쓴 EL 소자에 있어서 styrene보다 긴 conjugation 길이의 증가가 EL 발광 스펙트럼에 미치는 영향은 크지 않고 실제 발광은 PPV에 의해 주로 일어남이 관찰되었다.

  • PDF