나일론과 폴리아세탈의 왕복동 마찰마멸특성에 관한 고찰 (Reciprocating Sliding Wear of Nylon and Polyacetal Against Steel)

  • 김충현;안효석;정태형
    • 대한기계학회논문집A
    • /
    • 제24권3호
    • /
    • pp.786-793
    • /
    • 2000
  • Nylon, Polyacetal and PTFE were studied to gain a better understanding of their tribological behavior. Wear tests were conducted with reciprocating motion under dry sliding conditions. Friction coefficient and specific wear rate were measured as a function of sliding distance. The worn surfaces were examined with a Scanning Electron Microscope(SEM). Polyacetal showed lowest specific wear rates and PTFE exhibited lowest friction coefficient. The dominant wear mechanism found were adhesion and abrasion.

마모를 고려한 드릴 절삭력 모델 (Drilling force model considering tool wear)

  • 최영준;주종남
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.1042-1047
    • /
    • 2001
  • A mechanistic model is developed to predict the thrust force and cutting torque of drilling process including wear. A mechanistic oblique cutting force model is used to develop the drilling force model. The cutting lips are divided into small elements and elemental forces are calculated by multiplying the specific cutting pressure with the elemental chip area. The specific cutting pressure is a function of chip thickness, cutting velocity, rake angle and wear. The total forces are then computed by summing the elemental forces. Measured cutting forces are in good agreement with the simulated cutting forces.

  • PDF

STD 61 공구강과 상대재인 핫 프레스 가공용 Al-9%Si 코팅강의 고온 미끄럼 마모 (High Temperature Wear of STD 61 Tool Steels Sliding Against Al-9%Si Coated Steels Used for Hot Press Forming)

  • 최병영;김홍기
    • 대한금속재료학회지
    • /
    • 제47권10호
    • /
    • pp.667-674
    • /
    • 2009
  • High temperature wear of STD 61 tool steels sliding against the Al-9%Si coated steels used for hot press forming has been studied in comparison with that of the tool steels sliding against the uncoated steels. Wear tests have been performed using a pin-on-disc configuration under an applied normal load of 50N for 20 min with heating the coated and uncoated steels up to 800$^{\circ}C$. It was found on the worn surface of the STD 61 tool steels sliding against the Al-9%Si coated steels that the formation of the glazed layers containing Al transferred from the coated tribopair may contribute to a reduction of the coefficient of friction, and detachment in part occur due to delamination wear, resulting in higher specific wear rate. On the other hand the Fe-oxide wear debris entrapped on the softer surface of the uncoated steels can act as a tribosurface, leading to decreased adhesive wear of the STD 61 tool steels, resulting in a lower specific wear rate.

탄소섬유강화 질화규소 세라믹스의 마찰마모 특성 (Sliding Wear Properties of Carbon Fiber Reinforced $Si_3N_4$ Ceramics)

  • 박이현;윤한기;김부안;박원조
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2004년도 학술대회지
    • /
    • pp.347-351
    • /
    • 2004
  • [ $Si_3N_4$ ] composites have been extensively studied for engineering ceramics, because it has excellent room and high temperature strength, wear resistance properties, good resistance to oxidation, and good thermal and chemical stability. In the present work, carbon short fiber reinforced $Si_3N_4$ ceramics were fabricated by hot press method in $N_2$ atmosphere at $1800^{\circ}C$ using $Al_2O_3\;and\;Y_2O_3$ as sintering additives. Content of carbon short fiber was $0\%,\;0.1\%\;and\;0.3\%$. The composites were evaluated in terms of density, flexural strength and elastic modulus through the 3-point bending test at room temperature. Also, The wear behavior was determined by the pin on disk wear tester using silicon nitride ball. Experimental density and flexural strength decreased with increasing content of carbon fiber. But specific modulus increased with increasing content of carbon fiber. In addition, friction coefficient and specific wear loss decreased with increasing content of carbon short fiber by reason of interfacial defects between matrix and fiber.

  • PDF

모터링 엔진의 시동 사이클 및 시동 정지 사이클에서 저어널베어링의 마모 연구 - II. 해석 결과 (Study on Wear of Journal Bearings during Start-up and Coast-down Cycles of a Motoring Engine - II. Analysis Results)

  • 전상명
    • Tribology and Lubricants
    • /
    • 제31권3호
    • /
    • pp.125-140
    • /
    • 2015
  • In this paper, we present the results of the wear analysis of journal bearings on a stripped-down single-cylinder engine during start-up and coast-down by motoring. We calculate journal bearing wear by using a modified specific wear rate considering the fractional film defect coefficient and load-sharing ratio for the asperity portion of a mixed elastohydrodynamic lubrication (EHL) regime coupled with previously presented graphical data of experimental lifetime linear wear in radial journal bearings. Based on the calculated wear depth, we obtain a new oil film thickness for every crank angle. By examination of the oil film thickness, we determine whether the oil film thickness at the wear scar region is in a mixed lubrication regime by comparing dimensionless oil film thickness, h/σ, to 3.0 at every crank angle. We present the lift-off speed and the crank angles involved with the wear calculation for bearings #1 and #2. The dimensionless oil film thickness, h/σ, illustrates whether the lubrication region between the two surfaces is still within the bounds of the mixed lubrication regime after scarring of the surface by wear. In addition, we present in tables the asperity contact pressure, the real minimum film thickness at the wear scar region, the modified specific wear rate, and the wear angle, α, for bearings #1 & #2. To show the real shape of the oil film at wear scar region, we depict the actual oil film thickness in graphs. We also tabulated the ranges of bearing angles related with wear scar. We present the wear volume for bearings #1 and #2 after one turn-on and turn-off of the engine ignition switch for five kinds of equivalent surface roughness. We show that the accumulated wear volume after a single turn-on and turn-off of an ignition switch normally increases with increasing surface roughness, with a few exceptions.

PTFE 복합재료의 마찰 . 마모 특성에 미치는 첨가제의 영향 (Effects of Additives on the Friction and Wear Properties of PTFE Composites)

  • 김용직;엄수현;김윤해
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 1999년도 추계학술발표대회 논문집
    • /
    • pp.88-94
    • /
    • 1999
  • Recently, PTFE-polyimide composites are being used self-lubricating parts for industrial field. Thus, this study is mainly concerned with friction and wear properties for the piston ring of non-lubricating air compressor which made of PTFE-polyimide composites. The friction and wear test was carried out for the different composition ratio under the atmosphere room temperature and constant load of 7.69N and their friction and wear properties were compared with each other at various sliding speed. Notable results are summarized as follows. PTFE 100% showed that friction coefficient was almost same values at 0.94 and 1.88m/s but the value was decreased at 2.83m/s because the friction temperature is higher than low speed. PTFE 80%-PI 20% showed the lowest mean friction coefficient at 2.83m/s. PTFE 20%-PI 80% showed the highest friction coefficient at 0.94m/s and the value was decreased at high speed but the value is higher than other materials except PTFE 100 %. PI 100% showed the highest friction coefficient at 0.94 and 1.88m/s because adhesive wear mainly occurred that speed. PTFE 100% showed highest specific wear rate on the whole. Specific wear rate of PTFE 80%-PI 20% was almost the same value with PTFE 20%-PI 80%. PI 100% showed the lowest value at high sliding speed because the friction surface was thicken and carbonated by high friction temperature.

  • PDF

에폭시 기지 나노복합재료의 마모 특성 (Wear Properties of Epoxy Matrix Nanocomposites)

  • 김재동;김형진;고성위;김영식
    • 동력기계공학회지
    • /
    • 제14권6호
    • /
    • pp.83-88
    • /
    • 2010
  • The wear behavior of epoxy matrix composites filled with nano sized silica particles is discussed in this paper. Especially, the variation of the coefficient of friction and the wear resistance according to the change of apply load and sliding velocity were investigated for these materials. Wear tests of pin-on-disc mode were carried out and the wear test results exhibited as following ; The epoxy matrix composites showed lower coefficient of friction compared to the neat epoxy through the whole sliding distance. As increasing the sliding velocity the epoxy matrix composites indicated lower coefficient of friction, whereas the neat epoxy showed higher coefficient of friction as increasing the sliding velocity. The specific friction work of both materials were increased with apply load. In case of the epoxy matrix composites, the running in periods of friction were reduced as increase in apply load. The epoxy matrix composites were improved the wear resistance by adding the nano silica particles remarkably. It is expected that the load carrying capacity of the epoxy matrix composites will be improved by increase of Pv factor.

탄소 섬유 강화 고분자 복합재의 연삭마모 특성에 관한 연구 (Study on Abrasive Wear Behaviour of a Carbon Fiber Composites)

  • 고성위;양병춘;김형진;김재동
    • 동력기계공학회지
    • /
    • 제10권1호
    • /
    • pp.46-51
    • /
    • 2006
  • Present study was investigated the effect of the particle of the counterface of unidirectional carbon fiber reinforced composite. The friction coefficient of composite and the specific wear rate different sliding velocity were measured for this materials. The friction track of counterface was observed by an optical microscope and scanning electron microscope. There were insignificant effects of the specific wear rate under lower Sic abrasive particle, however it showed high effect on $30{\mu}m$ abrasive particle size. There were significant effects of friction and wear behavior of the fiber direction under 0.3m/s sliding speed. Major failure mechanisms can be classified such as microfracture, plowing, microcutting, cutting and cracking.

  • PDF

디젤엔진용 실린더 라이너 소재의 고온 마모특성 (Wear Characteristics of Cylinder-Liner Materials for Diesel Engine at Elevated Temperature)

  • 김진열;김재훈;오광근;이승학;장준용
    • 대한기계학회논문집A
    • /
    • 제39권11호
    • /
    • pp.1131-1136
    • /
    • 2015
  • 선박 디젤엔진용 실린더 라이너는 피스톤 링과 지속적인 왕복운동을 통해 마모가 발생한다. 마모는 디젤엔진의 성능을 저하시키고, 사용 수명을 단축시킨다. 본 논문은 선박 디젤엔진용 실린더 라이너의 GT 금속 및 기존 금속에 대하여 마모특성을 평가하였다. 마모시험은 상온, $175^{\circ}C$, $325^{\circ}C$의 온도조건과 10 N, 30 N, 50 N 의 하중조건에서 수행되었으며, 마모량, 비마마율 및 마찰계수를 평가하였다. 또한 각 조건에 대한 마모메커니즘을 분석하기 위해서 SEM 분석을 수행하였다. 두 금속 공히, 상온에서 연삭 및 응착마모가 진행되었고, 고온에서 부식마모가 발견되었다. GT 금속은 기존 금속 대비 모든 온도 범위에서 마모량 및 비마모율이 작고 마모특성이 더 우수하다.

고온하에서 질화규소의 트라이볼로지적 특성 (Tribological Characteristics of Silicon Nitride on Elevated Temperature)

  • 김대중;채영훈;김석삼
    • Tribology and Lubricants
    • /
    • 제16권4호
    • /
    • pp.282-288
    • /
    • 2000
  • A sliding friction and wear test for silicon nitride (Si,N4) was conducted using a ball-on-disk specimen configuration. The material used in this study was HIPed silicon nitride. The tests were carried out from room temperature to 1000$^{\circ}C$ using self-mated silicon nitride couples in laboratory air. The worn surfaces were observed by SEM and the debris particles from the worn surfaces were analyzed for oxidation by XPS. The normal load was found to have a more significant influence on the friction coefficient of the silicon nitride than an elevated temperature. The specific wear rate was found to decrease along with the sliding distance. The specific wear rate at 29.4 N and 1000$^{\circ}C$ was 292 times larger than that at room temperature. The main wear mechanism from room temperature to 750$^{\circ}C$ was caused by brittle fracture whereas from 750$^{\circ}C$ to 1000$^{\circ}C$ the wear mechanism was mainly influenced by the oxidation of silicon nitride due to the increased temperature. The oxidation of silicon nitride at a high temperature was a significant factor in the wear increase.