• 제목/요약/키워드: Solid state welding

검색결과 78건 처리시간 0.026초

No Root Cap Horizontal Butt-welding with MAG Process

  • Jang, T.W.;Cho, S.H.;Park, C.G.;Lee, J.W.;Woo, W.C.
    • International Journal of Korean Welding Society
    • /
    • 제3권1호
    • /
    • pp.34-38
    • /
    • 2003
  • It has been used many kinds of horizontal butt-welding methods at block-to-block erection stage in shipbuilding companies. For examples, some companies use conventional FCAW process with one side or both sides groove joint welding, others use carriage with torch holder type mechanized welding method. Although lots of efforts were done until now, some problems in quality and productivity still remain in ship's hull welding. In this study, we have attempted to raise productivity and quality on horizontal position of welding with following 3 items. 1) Prepare groove condition with no root gap for making easy fit-up work. 2) Develop improved MAG (100% $CO_2$ gas shielding) welding process with solid wire for making sound root bead from one side. 3) Develop and apply quite new automatic welding carriage. The stability of new welding process was confirmed by conducting mechanical tests of weldments to verify the soundness of weldments.

  • PDF

고상접합을 이용한 Al/Mg 합금의 이종 용접 (Solid State Joining Processes for Dissimilar Joints of Mg/Al Alloys)

  • 김흥주;김성욱;천창근;장웅성
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.41-41
    • /
    • 2009
  • To evaluate the applicability of dissimilar joining between Mg and Al alloys in automobile manufacturing process, solid state joining processes such as magnetic pulse welding(MPW), friction stir welding(FSW) and friction spot joining(FSJ) were attempted successfully. MPW process has been concentrated mainly on round section tube to tube and tube to bar welds. AZ31 Mg alloy has been successfully welded to pure Al A1070 as well as to Al alloy A3003. While, for friction stir welding of dissimilar sheet joints, AZ31B/A6061 with the thickness of 2mm were used and a square butt joint with a good quality was obtained at the conditions of 0.8mm/sec of travel speed and tool rotation speed of 850rpm. The maximum tensile strength of 179 MPa, which was about 80 % of the Mg base metal tensile strength, has been obtained. Finally, friction spot joining was attempted to make a dissimilar lap joint between AZ31(0.8mm) and A6061(1mm), while the joint exhibited the same level of tensile shear strength as that of similar Mg joint.

  • PDF

A$_2$O$_3$세라믹과 Ni-Cr-Mo鋼과의 인서트 合金을 이용한 擴散接合에 關한 硏究 (A study on the diffusion bonding of the $Al_2$O$_3$ ceramics to metal)

  • 김영식;박훈종;김정일
    • Journal of Welding and Joining
    • /
    • 제10권3호
    • /
    • pp.63-72
    • /
    • 1992
  • The joining methods of ceramics to metals which can be expected to obtain high temperature strength are mainly classified into the solid-state diffusion bonding method and the active brazing method. Between these two, the solid-state diffusion bonding method is given attentions as substituting method for active brazing method due to being capable of obtaining higher bonding strength at high temperature and accurate bonding. In this paper, the solid-state diffusion bonding of $Al_{2}$O$_{3}$ ceramics to Ni-Cr-Mo alloy steel (SNCM21) using insert metal was carried out. The insert metal employed in this study was experimentally home-made, Ag-Cu-Ti alloy. Influence of several bonding parameters of $Al_{2}$O$_{3}$SNCM21 joint was quantitatively evaluated by bonding strength test, and microstructural analyses at the interlayer were performed by SEM/EDX. From above experiments, the optimum bonding condition of the solid-state diffusion bonding of $Al_{2}$O$_{3}$/SNCM21 using Ag-Cu-Ti insert metal was determined. Futhermore, high temperature strength and thermal-shock properties of $Al_{2}$O$_{3}$/SNCM21 joint were also examined. The results obtained are as follows. 1. The maximum bonding strength was obtained at the temperature of 95% melting point of insert metal. 2. The high temperature strength of $Al_{2}$O$_{3}$/SNCM21 joint appeared to bemaximum value at test temperature 500.deg.C and the bonding strength with increasingtemperature showed parabolic curve. 3. The strength of thermal-shocked specimens was far deteriorated than those of as-bonded specimens. Especially, water-quenched specimen after heated up to 600.deg. C was directly fractured in quenching.

  • PDF

알루미늄 5456-H116 합금에 대하여 최적 마찰교반 프로세싱 조건 규명 및 기계적 특성 평가 (Evaluation of Mechanical Characteristic and Investigation on Optimum Condition in Friction Stir Processing for 5456-H116 Al Alloy)

  • 박재철;김성종
    • 한국표면공학회지
    • /
    • 제42권1호
    • /
    • pp.13-20
    • /
    • 2009
  • Friction stir welding(FSW) was developed as a new solid state welding technique by The Welding Institute (TWI). On the basis of FSW, a new processing technique, friction stir processing (FSP), has recently been developed. FSP has been applied to cast aluminum alloy to modify the microstructure to enhance mechanical characteristic. FSP is a new solid state processing technique for microstructural modification in metallic materials. FSP has been applied to aluminum alloy to modify the microstructure to enhance mechanical characteristic. In this study, we investigated optimum condition friction stir processing with the evaluation of mechanical characteristic for 5456-H116 Al alloy. The mechanical characteristics of base metal similar with in 15 mm/min, 250 RPM with full screw probe. This condition is concluded that optimum friction stir processing condition. The result of this investigation will be able to application for repair of welding part for aluminum ship.

금속 박판 Al/Al 및 Al/Cu의 초음파 용착 접합성 평가 (Ultrasonic Deposit Junction Characteristic Evaluation of Metal Sheets Al/Al and Al/Cu)

  • 서정석;백시영
    • 대한금속재료학회지
    • /
    • 제49권8호
    • /
    • pp.642-648
    • /
    • 2011
  • This paper describes an experimental study on ultrasonic welding of similar and dissimilar metals. There are optimum welding conditions which are found for welding of Al/Al and Al/Cu. It evaluated weldability using tensile test, SEM observation and EDX-ray analysis. Both ultrasonic welding of Al/Al and Al/Cu have amplitude as the variable factor. Al/Cu welding was examined again with welding time as variable factor to find the best conditions. The more welding time or amplitude increase, the better weldability. The optimum conditions for ultrasonic welding of Al/Al were formed at pressure 0.25 MPa, welding time 0.25 sec, amplitude 90%. Pressure 0.25 MPa, welding time 0.4 sec, amplitude 80% are optimized for Al/Cu ultrasonic metal welding and solid-state diffusion generated by ultrasonic vibration and frictional heat is confirmed at the welded interface.

순수 타이타늄의 기계적 특성에 미치는 마찰 교반 용접 공정 조건의 영향 (Microstructure and Mechanical Properties of Pure Titanium Processed using Friction Stir Welding)

  • 이용재;최안드레;이승준;;신세은;이동근
    • 열처리공학회지
    • /
    • 제32권3호
    • /
    • pp.124-130
    • /
    • 2019
  • Friction stir welding is one of the interesting welding methods for titanium and its alloy which proceeds with plastic flow due to thermo-mechanical stirring and friction heat. Solid-state welding can solve severe problems such as high-temperature oxidation, interstitial oxygen diffusion and grain coarsening by liquid-state welding. Dynamic recrystallization and grain refinement can vary significantly with the plunging load and rotational speed of tool during friction stir welding, and suitable process conditions must be optimized to obtain microstructure and better mechanical characteristics. Suitable FSW conditions were 1000 kg of plunging load and 200 rpm of rotational speed and it showed YS 270 MPa, UTS 332.1 MPa, and El 17.3%, which were very similar to those of wrought titanium sheet.

저잔사 플럭스를 사용한 플로우 솔더링부의 젖음성 및 결함거동에 관한 연구 (A Study on Wettability and Defects Behavior of Flow-soldered Joint using Low Residue Flux)

  • 최명기;이창열;정재필;서창제;신영의
    • Journal of Welding and Joining
    • /
    • 제16권6호
    • /
    • pp.77-85
    • /
    • 1998
  • Effects of non-cleaning and cleaning fluxes on the wetting properties and defects at flow soldered joints were investigated. Non-cleaning flux (R-type of 3.3% solid content) and cleaning flux (RMA-type of 15% solid content) were used. Wetting test was accomplished by wetting balance method with changing surface state of wetting specimen, CU. Sn-37%Pb solder was used for wetting test and flow soldering. As experimental results, the wetting time for vertical force from the surface tension being zero was mainly affected by surface state of the wetting specimen. Non-cleaning flux had a good wettability compared with cleaning flux. In case of non-cleaning flux, conveyor speed had a great affection to defects of bridge, icicle, and poor solder.

  • PDF

용접조건이 AI-7075-T651의 마찰교반용접부의 경도와 미세조직에 미치는 영향 (Effects of Welding Condition on Hardness and Microstructure of Friction Stir Welded Joints of AI-7075-T651 Plate)

  • 김치옥;손혜정;김선진
    • 동력기계공학회지
    • /
    • 제15권3호
    • /
    • pp.58-64
    • /
    • 2011
  • As well known, the friction stir welding is a novel welding process which is a solid state welding process for sheet or plate using the friction stir phenomenon. This paper describes the effect of welding condition such as the rotation speed and the travelling speed during the friction stir welding process on the micro Virkers hardness and the microstructure of friction stir welded joints in AI-7075-T651 plate. From those investigations, the highest hardness of stir zone was observed at the welding condition of SO-3. The microstructures of the friction stir welded joints was not dependent on the welding conditions, but in the SO-4 specimen, the friction stir welding defect like tunnel shape was found in stir zone.