• Title/Summary/Keyword: Sn-5%Pb-1.5%Ag-x%Bi

Search Result 5, Processing Time 0.02 seconds

A study on the characteristics of low Pb Sn-5%Pb-1.5%Ag-x%Bi solder alloys (저Pb Sn-5%Pb-1.5%Ag-x%Bi계 솔더 합금의 특성에 관한 연구)

  • 홍순국;주철홍;강정윤;김인배
    • Journal of Welding and Joining
    • /
    • v.16 no.3
    • /
    • pp.157-166
    • /
    • 1998
  • Recently as environmental pollution caused by Pb has posed a serious threat to the global environment, the trend to regulate the usage of Pb in electronic industry is one the rise. Currently, the solder alloy with high Pb content, Sn-37%Pb, is utilized in the electronic assembly therefore, the objective of this study is to develop an alternative solder alloy for the existing Sn-37%Pb solder alloy. First thing, this work choosed Sn-5%Pb-1.5%Ag, Sn-5%Pb-1.5%Ag-x%Bi(x=1~5%) for candidate solder alloys, and examined their properties such as melting range, wettability, microhardness, tensile property, oxidation behavior and microstructure. Wettability was on the same level of Sn-37%Pb. Dissolution of Pb ion in Sn-5%Pb solder was 0.46ppm. This solder alloy revealed cellular dendrite microstructure $\beta$-Sn matrix, Pb-rich phase, Ag/Sn, and Cu/Sn Intermetallic compounds. The range of solidification temperature was within 3$0^{\circ}C$. Also these alloy displayed higher tensile strength and lower elongation than Sn-37%Pb. The resistance of oxidation in Sn-5%Pb-1.5%Ag solder alloy was superior to that of Sn-37%Pb solder alloy. But that of Sn-5%Pb-1.5%Ag-5%Bi solder alloy was equal to that of Sn-37%Pb solder alloy.

  • PDF

A Study on the Characteristics of Sn-Ag-X Solder Joint -The Wettability of Sn-Ag-Bi-In Solder to Plated Substrates- (Sn-Ag-X계 무연솔더부의 특성 연구 -기판 도금층에 따른 Sn-Ag-Bi-In 솔더의 젖음특성-)

  • 김문일;문준권;정재필
    • Journal of the Korean institute of surface engineering
    • /
    • v.35 no.1
    • /
    • pp.11-16
    • /
    • 2002
  • As environmental concerns increasing, the electronics industry is focusing more attention on lead free solder alternatives. In this research, we have researched wettability of intermediate solder of Sn3Ag9Bi5In, which include In and Bi and has similar melting temperature to Sn37Pb eutectic solder. We investigated the wetting property of Sn3Ag9Bi5In. To estimate wettability of Sn3Ag9Bi5In solder on various substrates, the wettability of Sn3Ag9Bi5In solder on high-pure Cu-coupon was measured. Cu-coupon that plated Sn, Ni and Au/Ni and Si-wafer adsorbed Ni/Cu under bump metallurgy on one side. As a result, the wetting property of Sn3Ag9Bi5In solder is a little better than that of Sn37Pb and Sn3.5Ag.

Optimization of Soldering Process of Sn-3.0Ag-0.5Cu and Sn-1.0Ag-0.7Cu-1.6Bi-0.2In Alloys for Solar Combiner Junction Box Module (태양광 접속함 정션박스 모듈 적용을 위한 Sn-3.0Ag-0.5Cu 및 Sn-1.0Ag-0.7Cu-1.6Bi-0.2In 솔더링의 공정최적화)

  • Lee, Byung-Suk;Oh, Chul-Min;Kwak, Hyun;Kim, Tae-Woo;Yun, Heui-Bog;Yoon, Jeong-Won
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.25 no.3
    • /
    • pp.13-19
    • /
    • 2018
  • The soldering property of Pb-containing solder(Sn-Pb) and Pb-free solders(Sn-3.0Ag-0.5Cu and Sn-1.0Ag-0.7Cu-1.6Bi-0.2In) for solar combiner box module was compared. The solar combiner box module was composed of voltage and current detecting modules, diode modules, and other modules. In this study, solder paste printability, printing shape inspection, solder joint property, X-ray inspection, and shear force measurements were conducted. For optimization of Pb-free soldering process, step 1 and 2 were divided. In the step 1 process, the printability of Pb-containing and Pb-free solder alloys were estimated by using printing inspector. Then, the relationship between void percentages and shear force has been estimated. Overall, the property of Pb-containing solder was better than two Pb-free solders. In the step 2 process, the property of reflow soldering for the Pb-free solders was evaluated with different reflow peak temperatures. As the peak temperature of the reflow process gradually increased, the void percentage decreased by 2 to 4%, but the shear force did not significantly depend on the reflow peak temperature by a deviation of about 0.5 kgf. Among different surface finishes on PCB, ENIG surface finish was better than OSP and Pb-free solder surface finishes in terms of shear force. In the thermal shock reliability test of the solar combiner box module with a Pb-free solder and OSP surface finish, the change rate of electrical property of the module was almost unchanged within a 0.3% range and the module had a relatively good electrical property after 500 thermal shock cycles.

Effects of Surface Finishes on the Low Cycle Fatigue Characteristics of Sn-based Pb-free Solder Joints (금속패드가 Sn계 무연솔더의 저주기 피로저항성에 미치는 영향)

  • Lee, Kyu-O;Yoo, Jin
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.10 no.3
    • /
    • pp.19-27
    • /
    • 2003
  • Surface finishes of PCB laminates are important in the solder joint reliability of flip chip package because the types and thicknesses of intermetallic compound(IMC), and compositions and hardness of solders are affected by them. In this study, effects of surface finishes of PCB on the low cycle fatigue resistance of Sn-based lead-free solders; Sn-3.5Ag, Sn-3.5Ag-XCu(X=0.75, 1.5), Sn-3.5Ag-XBi(X=2.5, 7.5) and Sn-0.7Cu were investigated for the Cu and Au/Ni surface finish treatments. Displacement controlled room temperature lap shear fatigue tests showed that fatigue resistance of Sn-3.5Ag-XCu(X=0.75, 1.5), Sn-3.5Ag and Sn-0.7Cu alloys were more or less the same each other but much better than that of Bi containing alloys regardless of the surface finish layer used. In general, solder joints on the Au/Ni finish showed better fatigue resistance than those on the Cu finish. Cross-sectional fractography revealed microcracks nucleation inside of the interfacial IMC near the solder mask edge, more frequently on the Cu than the Au/Ni surface finish. Macro cracks followed the solder/IMC interface in the Bi containing alloys, while they propagated in the solder matrix in other alloys. It was ascribed to the Bi segregation at the solder/IMC interface and the solid solution hardening effect of Bi in the $\beta-Sn$ matrix.

  • PDF