Elastic Modulus Prediction for Design of Sintered Aluminum by Ultrasonic (초음파에 의한 알루미늄 소결체 설계를 위한 탄성계수 예측)

  • Nam, Young-Hyun
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.32 no.7
    • /
    • pp.590-596
    • /
    • 2008
  • The ultrasonic velocities of sintered aluminum with varying density were measured in order to deduce the mechanical properties for optimum design of the sintered aluminum. Specimens with different densities were prepared by the plasma activated sintering machine. The density distribution of sintered aluminum becomes partially inhomogeneous because of the friction between the powder and the die during compaction. The elastic moduli are increased as the ultrasonic velocity is increased. Furthermore, Poisoon's ratio is depending on not only the density but also the size and distribution of voids. As the specimen's thickness increases, the center frequency in the frequency spectrum of the reflection wave is shifted to the low frequency. The attenuation coefficient of ultrasonic wave is decreased inversely as the density increased.

Photovoltaic Properties of Sintered CdS/CdTe Solar Cell (소결체 ITO/CdS/CdTe 태양전지의 광전압특성)

  • 김동섭;조은철;안병태;임호빈
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1994.11a
    • /
    • pp.216-220
    • /
    • 1994
  • Polycrystalline CdS films have been prepared by coating a slurry, which consisted of CdS, 11w% CdCl$_2$ and appropriate amount of propylene glycol, on glass substrate and glass substrate coated with indium tin oxide(ITO) followed by sintering in a nitrogen atmosphere. CdTe slurries consisting of Te powder and Cd powder were coated on the sintered CdS films and ITO/CdS films and were sintered in nitrogen to prepare sintered CdS/CdTe and ITO/CdS/CdTe solar cells. The value of fill factor increased due to low series resistance and open circuit voltage decreased due to low shunt resistance in the ITO/CdS/CdTe solar cells.

The Microstructure and Mechanical Properties of Y2O3-Dispersed Fe-C and Fe-CNT Sintered Steels (Y2O3가 분산된 Fe-C 및 Fe-CNT 소결체의 미세구조 및 기계적 특성)

  • Lim, Jin Young;Ahn, Jung-Ho
    • Journal of Powder Materials
    • /
    • v.24 no.4
    • /
    • pp.298-301
    • /
    • 2017
  • In the present work, we use multiwall carbon nanotubes (MWCNT) as the starting material for the fabrication of sintered carbon steel. A comparison is made with conventionally sintered carbon steel, where graphite is used as the starting material. Milling is performed using a horizontal mill sintered in a vacuum furnace. We analyze the grain size, number of pores, X-ray diffraction patterns, and microstructure. Changes in the physical properties are determined by using the Archimedes method and Vickers hardness measurements. The result shows that the use of MWCNTs instead of graphite significantly reduces the size and volume of the pores as well as the grain size after sintering. The addition of $Y_2O_3$.to the Fe-MWCNT samples further inhibits the growth of grains.

Circulating Mechanism of the Oil in Brief Operating for the Oil-impregnated Sintered Bearing

  • Harakawa, Toshiro;Maruyama, Tsuneo;Shimizu, Teruo
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1006-1007
    • /
    • 2006
  • The oil-impregnated sintered bearings are used for various aplecations and, wide usages without refueling. The oil circulating mechanism operates smoothly the behavior of oil If doing at the time of passing and becoming a stationary state, and there is little thing where trouble is caused. On the other hand, the trouble of such as starting noise might be caused in the unstationary state that repeats operation for a short time. To study the behavior of oil of each parameter, we execute the numerical simulation and various verification experiments. As a result, we developed that the bearings were able to be used enough for various brief operating time in the unstationary state. Finally we have expanded the usage of the oil-impregnated sintered bearings by adding the consideration of the behavior of oil.

  • PDF

Gigacycle Fatigue Crack Initiation in Cr-Mo Prealloy Sintered Steel

  • Xu, Chen;Danninger, Herbert;Khatibi, Golta;Weiss, Brigitte
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.136-137
    • /
    • 2006
  • Crack initiation and short crack propagation was studied on the polished notched surfaces of Cr-Mo prealloy sintered steels with 7.35 $g.cm^{-3}$ sintered density. An ultrasonic resonance test system operating in push-pull mode at 20 kHz and R=-1 was used. It showed that crack initiation took place in several places, small cracks growing oriented to the local pore structure rather than to stress orientation. Their growth rate is markedly higher than the corresponding one of long cracks. Finally, several microcracks join to form a dominant crack.

  • PDF

Effect of Sintering Temperature, Heat Treatment and Tempering on Hardness of SH737-2Cu-0.9C Sintered Samples

  • Anand, S.;Verma, N.;Upadhyaya, A.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.555-556
    • /
    • 2006
  • The study examines hardness pattern of SH737-2Cu-.9C samples transient liquid phase sintered at different temperatures viz. $1120^{\circ}C$, $1180^{\circ}C$ and $1250^{\circ}C$, heat treated by various methods and then tempered at different temperatures. Sintered samples were characterized for density and densification parameter, and austenitized at $900^{\circ}C$, subsequently cooled by four different methods viz. annealing, normalizing, oil and brine quenching. Hardness pattern was found minimum for air cooled and maximum for brine quenched, and samples sintered at $1250^{\circ}C$ had relatively higher hardness. The O.Q and B.Q samples were then tempered at $200^{\circ}C$, $400^{\circ}C$, $600^{\circ}C$ and $700^{\circ}C$. Hardness pattern typically showed secondary hardness taking place, with maximum around $600^{\circ}C$.

  • PDF

Gigacycle Fatigue Endurance Strength of High Density Mo and Cr-Mo Prealloyed Sintered Steel

  • Xu, Chen;Danninger, Herbert;Khatibi, Golta;Weiss, Brigitte
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.385-386
    • /
    • 2006
  • For attaining optimum fatigue resistance of PM steels, high density levels are necessary. In this work, sintered steels Fe-1.5%Mo-0.6%C and Fe-1.5%Cr-0.2%Mo-0.6%C were produced with density levels of 7.1 to $7.6\;g.cm^{-3}$. Ultrasonic fatigue testing with 20 kHz was performed in push-pull mode up to 10E9 cycles. It was shown that the fatigue endurance strength is strongly improved by higher density levels, but also higher sintering temperatures are beneficial. The Cr-Mo steels proved to be superior to the plain Mo alloyed, due to a more favourable as-sintered matrix microstructure.

  • PDF

Electroless Copper Plating on 304L Stainless Steel Powders and Corrosion Resistance of the Sintered Compacts of Composite Powders (304L 스테인리스강 분말의 내식성 개선을 위한 무전해 구리 도금과 분말 소결체의 내식성 조사 연구)

  • Ahn, Jae-Woo;Lee, Jae-Hoon
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.2
    • /
    • pp.79-90
    • /
    • 2009
  • A study has been made about the effects of powder content, reaction temperature, reaction time, and stirring speed on the preparation of the stainless steel(STS) 304L powders plating with copper by an electroless plating method. The behavior of corrosion resistance of the sintered STS-Cu composite powders was also investigated by the salt spraying test The electroless plating technique was an effective method to manufactur the copper-uniform plating composite powders, the corrosion resistance of this sintered specimen was improved bysuppressing Cr precipitates on grain boundaries in the sintered compacts of composite powders.