Effect of Silicon Nitride Whisker Content on the Flexural Strength of Silicon Nitride-Boron Nitride-Silicon Carbide Multi-Layer Composites

  • Park, Dong-Soo;Cho, Byung-Wook
    • 한국세라믹학회지
    • /
    • 제40권9호
    • /
    • pp.832-836
    • /
    • 2003
  • Multi-layer ceramic composites were prepared by tape casting followed by hot pressing using silicon nitride layer with silicon nitride whiskers, silicon nitride layer with silicon carbide particles and boron nitride-alumina layer. The whiskers were aligned during the casting. As the whisker content of the silicon nitride layer was increased up to 10 wt%, the flexural strength of the multi-layer composite was increased. However, further increase of the whisker content in the layer resulted in a rapid decrease of the strength of the composite. The results suggest that the strength of multi-layer ceramic composite showing non-catastrophic failure behavior can be significantly improved by incorporating the aligned whiskers in the layers.

가스압 소결조건에 따른 질화규소볼의 가공성에 대한 연구 (A Study on Machinability of Silicon Nitride Ball Sintered by Various Gas Pressure Sintering(GPS) Conditions)

  • 이수완;김성호;정용선
    • 한국세라믹학회지
    • /
    • 제35권2호
    • /
    • pp.115-122
    • /
    • 1998
  • The effect of sintering conditions on the sinterability for silicon nitride has been studied by many in-vestigators. However the effect of sintering conditions on the machinability which is the major barrier to the field applications of the ceramic components has not been fully studied. In this study the sintering con-ditions such as temperature gas pressure and time in silicon nitride were varied. The physical and mechan-ical properties of the gas pressure sintered (GPS) silicon nitride were measured. The optimum mi-crostructure of silicon nitride with the excellent machinability was investigated by MFG(magnetic-fluid grinding) technique. An attempt was made to figure out how the mechanical properties influence upon the machinability of silicon nitride ball.

  • PDF

질화규소 현탁액에서 분산제와 결합제의 상호작용연구 (Polymeric Interactions of Dispersant and Binder in Aqueous Silicon Nitride Suspensions)

  • 김봉호;김명호;이수;백운규
    • 한국세라믹학회지
    • /
    • 제32권8호
    • /
    • pp.901-908
    • /
    • 1995
  • In aqueous slurry processing of silicon nitride, the interaction of dispersant and binder used as polymeric processing additives on the silicon nitride particle surface was studied to identify the effect of these processing polymeric additives on the ceramic powder processing. The adsoprtion isotherm study of anionic organic molecule as dispersant and nonionic organic molecules as binder of silicon nitricde was studied to investigate the effect of these processing organic additives on the physicochemical properties of silicon nitride particles. As anionic molecule adsorbed onto silicon nitrice surface, the IEP of silicon nitride shifted toward acidic pH and changed the stability of silicon nitride particle. However, the adsorption of binder as nonionic organic molecule onto silicon nitride surface did not changed the IEP but caused the decrease of electrostatic potentials of silicon nitride. These distinctive adsorption behaviors of organic additives on silicon nitride particles can be closely correlated to the stability of silicon nitride particles suspended in aqueous media.

  • PDF

Fracture Behavior of Silicon Nitride-silicon Carbide-boron Nitride Multi-layer Composites with Different Layer Thickness

  • Cho, Byoung-Uk;Park, Dong-Soo;Park, Hong-Chae
    • 한국세라믹학회지
    • /
    • 제39권7호
    • /
    • pp.622-627
    • /
    • 2002
  • Multi-layer composites consisting of silicon nitride, silicon nitride-silicon carbide and boron nitride-alumina layers were prepared fly stacking the corresponding ceramic tapes. The composites demonstrated self-diagnostic capability and non-catastrophic failure behavior. The composites consisting of many thin layers exhibited high strength and stepwise increase of the electrical resistance during the flexure test. The strength of the composite with too thick silicon nitride layers was low and the electrical resistance was abruptly increased to the detection limit of the digital multi-meter during the test. An extensive crack branching was observed in the weak (BN + Al$_2$O$_3$)layer.

Effect of the Amount of the Sintering Additives on the Microstructural Development and the Mechanical Properties of Silicon Nitride with Aligned Whisker Seeds

  • Bae, Byoung-Chan;Park, Dong-Soo;Kim, Hai-Doo;Han, Byung-Dong;Park, Chan;Zou, Lin-Hua
    • 한국세라믹학회지
    • /
    • 제39권8호
    • /
    • pp.715-720
    • /
    • 2002
  • Silicon nitride samples with aligned whisker seeds were prepared with different amounts of yttria and alumina as the sintering additives. Their sintering behaviors and the microstructural developments between 2123K and 2323K were examined. The sample with larger amount of the sintering additives showed faster densification and grain growth. Even though addition of the aligned whisker seeds slightly retarded densification of silicon nitride, it improved the flexural strength and the fracture toughness. Both the flexural strength and the fracture toughness of silicon nitride with the aligned whisker seeds were increased as the amount of the sintering additives was increased.

질화규소의 입계상에 존재하는 불순물이 마모에 미치는 영향 (Effect of Impurities in Grain Boundary Phases on Wear Behavior of $Si_3N_4$)

  • 오윤석;임대순;이경호
    • 한국세라믹학회지
    • /
    • 제33권3호
    • /
    • pp.277-284
    • /
    • 1996
  • The water test results indicated that the impurities had detrimetal effect on the wear resistance of silicon nitride and the effects were getting severe as the temperature increased. Especially when Ca existed as an impurity the detrimental effects was the most severe. These results were resulted from the fact that impurities lowered the mechanical properties of the grain boundary phase of silicon nitride. The wear test results of glass/glass-ceramic specimens having a similar composition to the grain boundary phase of silicon nitride revea-led that the specimen containing CaO showed the lowest wear resistance. The existence of Fe and Ca at the grain boundary phase assisted forming a grain boundary phase with relatively low refractoriness. Therefore at a given wear condition the removal of deformed layer would be easier. The results showed that the glass phases could be modified by heat-treatment and this modification improved tribological characteristics of the silicon nitride.

  • PDF

A Study on Silicon Nitride Based Ceramic Cutting Tool Materials

  • Park, Dong-Soo
    • Tribology and Lubricants
    • /
    • 제11권5호
    • /
    • pp.78-86
    • /
    • 1995
  • The silicon nitride based ceramic cutting tool materials have been fabricated by gas pressure sintering (GPS) or hot pressing (HP). Their mechanical properties were measured and the effect of the fabrication variables on the properties were examined. Also, effect of adding TiN or TiC particulates on the mechanical properties of the silicon nitride ceramics were investigated. Ceramic cutting tools (ISO 120408) were made of the sintered bodies. Cutting performance test were performed on either conventional or NC lathe. The workpieces were grey cast iron, hardened alloy steel (AISI 4140, HRc>60) and Ni-based superalloy (Inconel 718). The results showed that fabrication variables, namely, sintering temperature and time, exerted a strong influence on the microstincture and mechanical properties of the sintered body, which, however, did not make much difference in wear resistance of the tools. High hardness of the tool containing TiC particulates exhibited good cutting performance. Extensive crater wear was observed on both monolithic and TiN-containing silicon nitride tools after cutting the hardened alloy steel. Inconel 718 was extremely difficult to cut by the current cutting tools.

알루미나와 이트리아가 질화규소의 가공성에 미치는 영향 (Effect of $Al_2O_3$ and $Y_2O_3$ on Machining of Silicon itride)

  • 이수완;장태석;엄호성
    • 한국세라믹학회지
    • /
    • 제33권3호
    • /
    • pp.269-276
    • /
    • 1996
  • The effect of sintering aids on the sinterability for silcion nitride has been studied by hundreds workers. However the effect of sintering aids on the machinability as the own trobles which is the major barrier for the field applications of the ceramic components has not been fully studied. in this study the contents of Al2O3 and Y2O3 in silicon nitride were varied from 0 to 8 wt% respectively. The physical and mechanical properties of the silcion nitride were measured. The optimal microstructure of silicon nitride balls with the excellent machinability by adding with various contents of sintering aids was studied by MGF(magnetic-fluid grinding)technique. An attempt to figure out how the mechanical properties influence the machinability of silicon-nitride ball was made.

  • PDF

상압소결과 열간정수압소결 질화규소의 기계적 성질 (Mechanical Properties of Sintered and HIPed Silicon Nitride)

  • 김창삼;하정수;이준근
    • 한국세라믹학회지
    • /
    • 제24권3호
    • /
    • pp.223-226
    • /
    • 1987
  • Among many densification routes for silicon nitride, HIP(hot isostatic pressing) is becomming more popular these days, mainly due to the fact that it can produce highly reliable products with superior mechanical properties. This study involves in sintering of silicon nitride followed by HIP which requires no canning. Various property changes curing sintering and HIP are observed and analyzed in terms of microstructural changes. Porosity decrease and enhanced interlocking of grains by HIP are considered to be the major causes for improved mechanical properties of silicon nitride.

  • PDF

Friction and Wear of Pressureless Sintered Ti(C,N)-WC Ceramics

  • Park, Dong-Soo;Yun, Shin-Sang;Han, Byoung-Dong;Kim, Hai-Doo
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.211-212
    • /
    • 2002
  • Friction and wear of pressureless sintered Ti(C,N)-WC ceramics were studied using a ball-on-reciprocating flat apparatus in open air. The silicon nitride ball and the cemented carbide (WC-Co) ball were used against the Ti(C,N)-WC plate samples. The friction coefficients of the Ti(C,N)-WC samples against the silicon nitride ball and the cemented carbide ball were about 0.57 and 0.3, respectively. The wear coefficient of the sample without WC addition was 5 times as large as that of the sample with 10 mole % WC addition when tested against the silicon nitride ball under 98 N. The higher wear coefficient of Ti(C,N)-0WC was explained in part by larger grain size. Wear occurred mainly by grain dislodgment after intergranular cracking mainly caused by the accumulated stress within the grains.

  • PDF