SENB 시험편의 측면함몰과 소성영역관계 (Relationship between Side-Necked Volume in a SENB specimen and Plastic Deformation Volume)

  • 이정현;김도형;김동학;강기주
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.420-425
    • /
    • 2004
  • Lee and Kang measured side-necking deformation near a crack-tip for CT specimen using Stereoscopic Digital Speckle Photography and Digital Image Correlation. In this work the same technique was applied to SENB specimen. We happened to find that the deformation shape of the side-necking is similar to the one of plastic region estimated by McClictock using slip line theory. Based on volume constancy of plastic deformation as well as this finding, it is expected that a linear relationship holds between the volume of plastic deformation region and the one of side-necking upon the lateral surface of a specimen. To prove the idea, a preliminary study has been performed using 3-D finite element method on a model with modified boundary layer formulation. As the result, it is shown that the idea works well with acceptable error.

  • PDF

Stereo Vision과 디지털 화상상관법을 이용한 파괴시험편의 측면 함몰의 현장 측정 (In situ Measurement of Lateral Side-Necking of a Fracture Specimen Using a Stereo Vision and Digital Image Correlation)

  • 이정현;강기주
    • 한국정밀공학회지
    • /
    • 제21권10호
    • /
    • pp.154-161
    • /
    • 2004
  • An experimental method for measuring side-necking deformation near a crack-tip is described. It is based on Stereoscopic Digital Speckle Photography and Digital Image Correlation, and it is simple and robust to mechanical vibration inherent to a hydraulic material test system. The validity and accuracy are evaluated through a calibration fur rigid body translation. A case study has been performed for a CT specimen made of a ductile steel and the three dimensional profiles of the side-necked region are presented as the load increases. Also, the details of the procedure and the surface treatment are discussed.

균열선단 부근의 측면함몰로부터 응력삼축성의 결정 방법 (Methods to Evaluate Stress Triaxiality from the Side Necking Near the Crack Tip)

  • 김동학;강기주
    • 대한기계학회논문집A
    • /
    • 제28권7호
    • /
    • pp.1021-1028
    • /
    • 2004
  • Kim et al. suggested an experimental method to determine the Q parameter in situ from the out-of-plane displacement and the in-plane strains on the surface of side necking near the crack tip. In this paper, the procedure to evaluate the stress triaxiality near a crack tip such as the Q parameter is to be polished in the details for simplicity and accuracy. That is, Q and hydrostatic stress are determined only from the out-of-plane displacement, but not using in-plane strain, which is hard to measure. And also, the plastic modulus is determined by an alternative way. Through three-dimensional finite element analyses for a standard CT specimen with 20% side-grooves, the validities of the new procedures are examined in comparison to the old ones. The effect of location where the displacements are measured to determine the stress triaxiality is explored.

Q의 실험적 측정법 (The Experimental Method of Measuring Q)

  • 김동학;이정현;강기주
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.285-291
    • /
    • 2003
  • An experimental method to measure Q-parameter in-situ is described. The basic idea comes from the fact that the side necking near a crack tip indicates the loss of stress triaxiality, which can be scaled by Q. From the out-of-plane displacement and the in-plane strain near the surface of side necking, stress field averaged through the thickness is calculated and then Q is determined from the difference between the stress field and the HRR field corresponding to the identical J-integral. To prove the validity, three-dimensional finite element analysis has been performed for a CT configuration with side-groove. Q-value which was calculated directly from the near-tip stress field is compared with that determined by simulating the experimental procedure according to the proposed method, that is, the Q-value determined from the lateral displacement and the inplane strain. Also, the effect of location where the displacement and strain are measured is explored.

  • PDF

파괴 시 발생하는 측면함몰과 소성영역크기와의 관계 (Relationship between Side-Necking and Plastic Zone Size at Fracture)

  • 김도형;김동학;강기주
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 추계학술대회
    • /
    • pp.365-371
    • /
    • 2004
  • Generally, fracture of a material is influenced by plastic zone size developed near the crack tip. Hence, according to the relative size of plastic zone in the material, the mechanics as a tool for analyzing the fracture process are classified into three kinds, that is, Linear Elastic Fracture Mechanics, Elastic Plastic Fracture Mechanics, Large Deformation Fracture Mechanics. Even though the plastic zone size is such an important parameter, the practical measurement techniques are very limited and the one for in-situ measurement is not virtually available. Therefore, elastic-plastic FEA has been performed to estimate the plastic zone size. In this study, it is noticed that side necking at the surface is a consequence of plastic deformation and lateral contraction and the relation between the plastic zone and side necking is investigated. FEA for modified boundary layer models with finite thickness, various mode mixities $0^{\circ}$, $30^{\circ}$, $60^{\circ}$, $90^{\circ}$ and strain hardening exponent n=3, 10 are performed. The results are presented and the implication regarding to application to experiment is discussed.

  • PDF

Q의 실험적 측정법 (An Experimental Method for Measuring Q)

  • 김동학;이정현;강기주
    • 대한기계학회논문집A
    • /
    • 제27권9호
    • /
    • pp.1607-1613
    • /
    • 2003
  • An experimental method to measure Q-parameter in-situ is described. The basic idea comes from the fact that the side necking near a crack tip indicates the loss of stress triaxiality, which can be scaled by Q. From the out-of-plane displacement and the in-plane strain near the surface of side necking, stress field averaged through the thickness is calculated and then Q is determined from the difference between the stress field and the HRR field corresponding to the identical J-integral. To prove the validity, three-dimensional finite element analysis has been performed for a CT configuration with side-groove. Q-value which was calculated directly from the near-tip stress field is compared with that determined by simulating the experimental procedure according to the proposed method, that is, the Q-value determined from the lateral displacement and the in-plane strain. In addition, the effect of location where the displacement and strain are measured is explored.

균열선단 응력삼축성의 측정방법;여러 형상 시험편에의 적용성 검토 (Experimental Method to Evaluate Stress Triaxiality near the Crack Tip;Applicability to Various Specimen Configurations)

  • 김동학;김도형;강기주
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.60-65
    • /
    • 2004
  • Kim et al. described and compared other methods of measuring stress triaxiality using the displacements near the side necking, proved the validities of these models and explored the effect of location where the displacements are measured using three-dimensional finite element analysis for a standard CT specimen with 20% side-grooves. In this paper, the applicability of these models to various specimen and materials are examined in detail. To consider the effects of side groove, thickness of specimen, crack length, specimen geometry and strain hardening exponents, three-dimensional finite element simulation has been performed for various specimen geometries. For a case without a side groove, in the whole the difference between the stress triaxilaity analytically evaluated and directly determined is similar. For a case with a 20% side groove the stress triaxiality is measured at the area where ${\theta}$ is smaller than $60^{\circ}$, which excludes a side grooved area.

  • PDF

현장타설말뚝의 네킹 결함 평가를 위한 전자기파의 적용성 연구 (Application of Electromagnetic Wave for Evaluating Necking Defects in Bored Piles)

  • 이종섭;송정욱;유정동
    • 한국지반공학회논문집
    • /
    • 제34권4호
    • /
    • pp.27-35
    • /
    • 2018
  • 본 연구의 목적은 현장타설말뚝에 발생한 네킹 결함을 평가하기 위해 전자기파의 적용성을 검증하는데 있다. 본 연구에서는 네킹 결함이 있는 직경 150mm, 길이 270mm의 소형 모형 말뚝에 대해 실험을 수행하였다. 말뚝에 모사된 결함은 총 4개이며, 이 중 두 개의 결함은 모형 말뚝의 서로 다른 면의 상부와 하부에 각각 모사되었으며, 나머지 두 개의 결함은 같은 면의 상부와 하부에 모사되었다. 전선을 철망을 이루고 있는 스테인리스 재질의 철사를 따라 설치하여 두개의 도체로 구성된 전송선로를 구성하였으며, time-domain reflectometer를 이용하여 전자기파를 송 수신하였다. 실험 결과, 모형 말뚝의 결함부와 선단부에서 전자기파의 반사 신호가 나타났다. 측정된 반사 신호로부터 결함의 위치를 산정한 결과, 실제의 결함 위치와 거의 같게 산정되었다. 본 연구의 결과는 전자기파가 현장타설말뚝의 네킹 결함을 평가하는데 있어 유용한 기법이 될 수 있음을 보여준다.

자동차용 타원형 디프 드로잉 제품의 다이 반경에 관한 연구 (Study on the Influence of Die Corner Radius for Deep Drawing of Elliptical Product of Automobile)

  • 허영민;박동환;강성수
    • 소성∙가공
    • /
    • 제11권8호
    • /
    • pp.668-675
    • /
    • 2002
  • The circles deform into various shape during deformation, the major and minor axes of which indicate the direction of the major and minor principal strains. Likewise, the measured dimensions are used to determine the major and minor principal strain magnitudes. This circular grid technique of measuring strains can be used to diagnose the causes of necking and fracture in industrial practice and to investigate whether these defects were caused by material property variation, changes in lubrication, of incorrect press settings. In non-axisymmetric deep drawing, three modes of forming regimes are found: draw, stretch, plane strain. The stretch mode for non-axisymmetric deep drawing could be defined when the major and minor strains are positive. The draw mode could be defined when the major strain is positive and minor strain is negative, and plane strain mode could be defined when the major strain is positive and minor strain is zero. Through experiments the draw mode was shown on the wall and flange are one of a drawn cup, while the plane strain and the stretch mode were on the punch head and the punch corner area respectively, We observed that the punch load of elliptical deep drawing was decreased according to increase of die corner radius and the thickness deformation of minor side was more large than major side.

연성 금속의 파괴과정에서 발생하는 소성영역의 현장 측정 (In-situ Measurement of Plastic Zone Developed During Ductile Fracture Process)

  • 백정현;김도형;강기주
    • 대한기계학회논문집A
    • /
    • 제30권6호
    • /
    • pp.637-642
    • /
    • 2006
  • A plastic zone size is regarded as a measure of material resistance, and also it determines the fracture behavior. The importance of estimating or measuring the plastic zone size cannot be too emphasized. In this article, SDSP(Stereo Digital Speckle Photography) is examined as a new techniques to measure the plastic zone developed in a ductile metal. This technique is simple, vibration free and non-contact, and measures simultaneously in-plane displacements as well as out-of plane displacements like the side necking. Experimental results for a CT specimen are presented to demonstrate the accuracy in comparison with those obtained by recrystallization technique and finite element analysis.