OLED의 Barrier와 Encapsulation을 위한 원자층 증착 기술로 공정된 Al2O3/TiO2/Al2O3 다층 필름 (Characterization of ALD Processed Al2O3/TiO2/Al2O3 Multilayer Films for Encapsulation and Barrier of OLEDs)

  • 이사야;송윤석;김현;류상욱
    • 반도체디스플레이기술학회지
    • /
    • 제16권1호
    • /
    • pp.1-5
    • /
    • 2017
  • Encapsulation of organic based devices is essential issue due to easy deterioration of organic material by water vapor. Thin layer of encapsulation film is required to preserve transparency yet protecting materials in it. Atomic layer deposition(ALD) is a promising solution because of its low temperature deposition and quality of the deposited film. $Al_2O_3$ or $Al_2O_3/TiO_2/Al_2O_3$ multilayer film has shown excellent environmental protection characteristics despite of thin thicknesses of the films. $Al_2O_3/TiO_2/Al_2O_3$ multilayer and 1.5 dyad layer of $Al_2O_3/polymer/Al_2O_3$ deposited by ALD was measured to have water vapor transmittance rate(WVTR) well below the detection limit($5.0{\times}10^{-5}g/m^2day$) of MOCON Aquatran 2 equipment.

  • PDF

$RuO_2$ Related Schottky contact for GaN/AlGaN device

  • Jung, Byung-Kwon;Kim, Jung-Kyu;Lee, Jung-Hee;Hahm, Sung-Ho
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2002년도 추계학술대회 발표 논문집
    • /
    • pp.85-90
    • /
    • 2002
  • $RuO_2$/GaN and related contacts were investigated for Schottky contacts in GaN-Based optical and electronic devices. We demonstrated that an $RuO_2$ film forms a stable Schottky contact on a GaN layer with a barrier height (${\Phi}_B$) of 1.46 eV and transmittance of 70% in the visible and near UV region. $RuO_2$/GaN Schottky diode showed a breakdown at over -50V and leakage current of only 0.3 nA at -5V. The $RuO_2$/GaN Schottky type photodetector had the UV/Visible rejection ratio of over $10^5$ and the responsivity of 0.23 A/W at 330 nm. The $RuO_2$ gate AlGaN/GaN EFET exhibited high drain current ($I_d$) of 689.3 mA/mm and high transconductance ($g_m$) of 197.4 mS/mm. Cut-Off frequency ($f_t$) and maximum operating frequency ($f_{max}$) were measured as 27.0 GHz and 45.5 GHz, respectively.

  • PDF

A Study on Moldability by Using Fuzzy Logic Based Neural Network(FNN)

  • Kang, Seong Nam;Huh, Yong Jeong;Choi, Man Sung
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2002년도 추계학술대회 발표 논문집
    • /
    • pp.127-129
    • /
    • 2002
  • In order to predict the moldability of an injection molded part, a simulation of filling is needed. Short shot is one of the most frequent troubles encountered during injection molding process. The adjustment of process conditions is the most economic way to troubleshoot the problematic short shot in cost and time since the mold doesn't need to be modified at all. But it is difficult to adjust the process conditions appropriately in no times since it requires an empirical knowledge of injection molding. In this paper, the intelligent CAE system synergistically combines fuzzy-neural network(FNN) for heuristic knowledge with CAE programs for analytical knowledge. To evaluate the intelligent algorithms, a cellular phone flip has been chosen as a finite element model and filling analyses have been performed with a commercial CAE software. As the results, the intelligent CAE system drastically reduces the troubleshooting time of short shot in comparison with the expert's conventional way which is similar to the golden section search algorithm.

  • PDF

PAALD 방법을 이용한 TaN 박막의 구리확산방지막 특성

  • 부성은;정우철;배남진;권용범;박세종;이정희
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2002년도 추계학술대회 발표 논문집
    • /
    • pp.14-19
    • /
    • 2002
  • In this study, as Cu diffusion barrier, tantalum nitrides were successfully deposited on Si(100) substrate and SiO2 by plasma assisted atomic layer deposition(PAALD) and thermal ALD, using pentakis (ethylmethlyamino) tantalum (PEMAT) and $NH_3$ as precursors. The TaN films were deposited on $250^{\circ}$C by both method. The growth rates of TaN films were $0.8{\AA}$/cycle for PAALD and $0.75{\AA}$/cycle for thermal ALD. TaN films by PAALD showed good surface morphology and excellent step coverage for the trench with an aspect ratio of h/w - $1.8 : 0.12 \mu\textrm{m}$ but TaN films by thermal ALD showed bad step coverage for the same trench. The density for PAALD TaN was $11g/\textrm{cm}^3$ and one for thermal ALD TaN was $8.3g/\textrm{cm}^3$. TaN films had 3 atomic % carbon impurity and 4 atomic % oxygen impurity for PAALD and 12 atomic % carbon impurity and 9 atomic % oxygen impurity for thermal ALD. The barrier failure for Cu(200nm)/TaN(l0nm)/$SiO_2(85nm)$/Si structure was shown at temperature above $700^{\circ}$C by XRD, Cu etch pit analysis.

  • PDF

Soft Magnetic Properties of CoNbZr amorphous Films with Pd addition

  • Song, J.S,;Wee, S.B,
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2002년도 추계학술대회 발표 논문집
    • /
    • pp.54-58
    • /
    • 2002
  • The present paper is to investigate the phase stability and soft magnetic properties of amorphous CoNbZr films when Pd is added as a substitution for CoNbZr alloys. The films were prepared by a RF magnetron sputtering method. The CoNbZrPd films deposited on Si wafers exhibited amorphous structures being independent upon the amount of Pd added in the films. On the addition of 4.34% Pd, the excellent soft magnetic characteristics of the films were observed with a coercive force of 0.54 Oe and an anisotropy field of 11 Oe, whereas a coercive force of 1 Oe and an anisotropy field of 3.5 Oe were shown in the film without the addition of Pd. The increased anisotropy field and low coercive force of the films may be attributed to the occupancy of Pd in the preferred sites parallel to the external magnetic field applied on the deposition process. A permeability of about 1100 was kept constant in the operation frequency ranging up to 100 MHz, which can be explained by the Landau-Lifshitz formula.

  • PDF

Preparation of $(Bi,La)Ti_{3}O_{12}$ Thin Films on $Al_{2}O_{3}/Si$ Substrates by the Sol-Gel Method

  • Chang, Ho Jung;Hwang, Sun Hwan;Chang, Ho Sung;Sawada, K.;Ishida, M.
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2002년도 추계학술대회 발표 논문집
    • /
    • pp.69-71
    • /
    • 2002
  • $(Bi, La)Ti_{3}O_{12}(BLT)$ ferroelectric thin films were prepared on $Al_{2}O_{3}/Si$ substrates by the sol-gel method. The as-coated films were post-annealed at the temperature of $650^{\circ}C$ and $700^{\circ}C$ for 30 min. The crystallinty, surface morphologies and electrical properties were affected by the annealing temperatures. The BLT films annealed at above $650^{\circ}C$ exhibited typical bismuth layered perovskite structures with (00$\ell$) preferred orientation. The granular shaped grains with a size of approximately 90nm was formed in the film sample annealed at $700^{\circ}C$. The memory window volatge of the BLT film was 2.5V. The leakage current of BLT films annealed at $650^{\circ}C$ was about $1\times10^{-7}A/\textrm{cm}^2$ at 3V.

  • PDF

Electrical and Optical Characteristics of Isoelectronic Al-doped GaN Films

  • Lee, Jae-Hoon;Ko, Hyun-Min;Park, Jae-Hee;Hahm, Sung-Ho;Lee, Jung-Hee
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2002년도 추계학술대회 발표 논문집
    • /
    • pp.81-84
    • /
    • 2002
  • The effects of the isoelectronic AI-doping of GaN grown by metal organic chemical vapor deposition were investigated for the first time using scanning electron microscopy (SEM), Hall measurements, photoluminescence (PL), and time-resolved PL. When a certain amount of Al was incorporated into the GaN films, the room temperature photoluminescence intensity of the films was approximately two orders larger than that of the undoped GaN. More importantly, the electron mobility significantly increased from 130 for the undoped sample to $500\textrm{cm}^2/Vs$ for the sample grown at a TMAl flow rate of $10{\mu}mol/min$, while the unintentional background concentration only increased slightly relative to the TMAl flow. The incorporation of Al as an isoelectronic dopant into GaN was easy during MOCVD growth and significantly improved the optical and electrical properties of the film. This was believed to result from a reduction in the dislocation-related non-radiative recombination centers or certain other defects due to the isoelectronic Al-doping.

  • PDF

A 5-17 GHz Wideband Reflection-Type Phase Shifter Using Digitally Operated Capacitive MEMS Switches

  • Kim, Jung-Mu;Lee, Sang-Hyo;Park, Jae-Hyoung;Baek, Chang-Wook;Kwon, Young-Woo;Kim, Yong-Kweon
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2003년도 추계학술대회 발표 논문집
    • /
    • pp.117-121
    • /
    • 2003
  • In this paper, a micromachined low-loss and ultra wide band reflection-type phase shifter (RTPS) is proposed. The phase shifter shows a constant phase shift from 5 to 17 GHz and consists of two cascaded reflection-type phase shifter. Low-loss reflection termination consists of digital capacitive switches, and air-gap overlay CPW couplers are used in order to employ the low-loss 3 dB coupling. The fabricated phase shifter showed the 5 discrete states, $0^{\circ},{\;}22.5^{\circ},{\;}45^{\circ},{\;}67.5^{\circ},{\;}90^{\circ}$ respectively, the average insertion loss of 3.48 dB, and maximum rms phase error of ${\pm}1.80^{\circ}$ for the relative phase shift from $0^{\circ}{\;}to{\;}90^{\circ}$ over 5-17 GHz.

  • PDF

SHAPE EFFECT ON PERFORMANCE OF MULTILAYER CERAMIC ACTUATOR

  • Wee, S. B.;Jeong, S. J.;Song, J. S.
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2003년도 추계학술대회 발표 논문집
    • /
    • pp.163-168
    • /
    • 2003
  • In the present study, the piezoelectricity and polarization of multilayer ceramic actuator, being designed to stack PMN-PZ-PT ceramic layers and Ag-Pd electrode layers alternatively, were investigated under a consideration of geometric factor, the volume ratio of the ceramic to the electrode layers. The actuators were fabricated by tape casting of $0.2Pb(Mg_{1/3}Nb_{2/3)O_3-0.38PbZrO_3-0,42PbTiO_3$ followed by lamination and burnout & co-firing processes. The actuators of $10\times10\times0.6~2\textrm{mm}^3$ in size were formed in a way that $60 ~ 200\mu\textrm{m}$ thick were stacked alternatively with $5\mu\textrm{m}$ thick electrode layer. Increases in polarization and electric field-induced displacement with thickness of the ceramic layer were attributed to change of $90^{\circ}$/$180^{\circ}$ domain ratio, which was affected by interlayer internal stress. The piezoelectricity and actuation behaviors were found to depend upon the volume ratio (or thickness ratio) of ceramic to electrode layers.

  • PDF

$EU^{2+}$ Activated Green Phosphor $Ba_{2}CaMgSi_{2}O_{8}:Eu^{2+}$

  • Kim, Jeong-Seog;Piao, Ji-Zhe;Choi, Jin-Ho;Cheon, Chae-Il;Park, Joo-Suk
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2004년도 춘계학술대회 발표 논문집
    • /
    • pp.97-100
    • /
    • 2004
  • We report $EU^{2+}$ activated green phosphor $Ba_{2}CaMgSi_{2}O_{8}:Eu^{2+}$. The phosphor absorbs ultroviolet radation and emits a green visible light. The phosphors were synthesized by conventional solid state reaction method. The high purity $BaCO_3$, $CaCO_3$, MgO, $SiO_2$, $Eu_{2}O_{3}$ were used as raw materials. The raw materials were mixed thoroughly with an appropriate amount of ethanol in an agate mortar and then dried at $90^{\circ}C$ for 2 hours. The mixture was sintered at $900^{\circ}C$ for 2 hours and reheated at the mild reducing atmosphere 5% $H_2$ gas mixed with 95% $N_2$ gas at about $900^{\circ}C$ to $1200^{\circ}C$ for 2 hours. The photoluminescence spectra of the phosphor powders were measured by a fluorescent spectrophotometer. The crystal structure of phosphor powders were investigated by X -ray diffractometer.

  • PDF