• 제목/요약/키워드: Semi-solid forming

검색결과 89건 처리시간 0.034초

나선형 기계 교반 장치를 이용한 Al 합금 레오로지 소재의 제조 (Manufacture of Aluminum Alloy Rheology Materials Using Spiral Stirring Equipment)

  • 배정운;한수훈;강충길
    • 소성∙가공
    • /
    • 제17권1호
    • /
    • pp.9-12
    • /
    • 2008
  • Recently, industries and academic institutes have been interested in the rheology forming technology for light weight materials. However, this rheocasting process has advantages such as the high initial investment cost and the lower mechanical properties than thixocasting. In this study, the continuous fabrication of rheological material with a spiral stirring equipment(mechanical stirring system) was newly devised to overcome the disadvantages of rheocasting process. The experimental parameters were stirring time($0{\sim}1200sec$), stirring velocity ($0{\sim}100rpm$) and stirring temperature($650{\sim}680^{\circ}C$). The optimal conditions for fabricated rheological material of A6061 alloy were stirring time at 300sec, stirring velocity at 60rpm and stirring temperature at $650^{\circ}C$. At these results, the equivalent diameter was $45{\sim}65{\mu}m$, mean roundness was $1.4{\sim}1.6$ and Vickers hardness was 60Hv.

알루미늄 분말 합금의 반응고 미세조직 특성 연구 (A Study on the Characteristics of Microstructures in the Semi-solid State of Aluminum Powder Alloys)

  • 이상용
    • 열처리공학회지
    • /
    • 제21권4호
    • /
    • pp.205-212
    • /
    • 2008
  • Characteristics of microstructures, mechanical properties and formability of two Al-20Si-5Fe-2Ni alloys produced by gas atomizing (P/M) and spray forming (S/F) respectively were compared at temperatures up to $560^{\circ}C$. Room temperature hardness values and tensile strengths of both alloys were increased in accordance with temperature after heat treatment above $300^{\circ}C$. The highest values of hardness and tensile strength of both alloys were obtained at $490^{\circ}C$. It was interpreted that increase in hardness and tensile strength according to heating temperature between $300{\sim}490^{\circ}C$ was mainly related to increase in internal stress between Al matrix and reprecipitated particles. S/F alloys showed better formability and wear property than P/M alloys due to the homogenity of microstructures above $300^{\circ}C$.

전자교반을 이용한 A356 합금의 결정립제어 (The grain size control of A356 alloy by electromagnetic stirring)

  • 배정운;강충길
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.247-248
    • /
    • 2006
  • In this study, the morphology of the change of primary Al phase in A356 alloy by two kinds of electromagnetic stirrers(vertical and horizontal) were investigated to obtain the globular structure. The effects of the stirring current, the stirring time and the pouring temperature were determined. The greater stirring current and longer stirring time were to get the finer the Al phase. However, over a certain stirring current and stirring time, the primary Al was merged together and was increased. The reason is the degree of breakdown of initial dendrites has been decreased by the collision and coalescence of particles with increasing stirring current and stirring time. The optimum conditions and difference of the two kinds of electromagnetic stirrers have been investigated for rheology forming with controlled solid fraction.

  • PDF

($AlSi_7Mg$알루미늄 합금의 초정 구형화에 대한 주조조건의 영향 (Effect of the Casting Conditions on the Globulization of Primary Al of $AlSi_7Mg$ Alloy)

  • 한요섭;이호인;이재철
    • 한국주조공학회지
    • /
    • 제23권1호
    • /
    • pp.40-46
    • /
    • 2003
  • Semisolid forming requires alloys with non-dendritic microstructure of the thixotropy. Recently, low pouring temperture method without stirring, i.e. liquidus casting has been found out new fabrication method of the semisolid metals. Effects of melt superheat and mold conditions on the globulization of primary Al of $AlSi_7Mg$ alloy were investigated in gravity casting process without stirring. The microstructures of primary Al as function of melt superheat and mold temperature show globular, rosette and dendritic shapes. The conditions for globular microstructure of primary Al were low melt superheat < 35 K and low mold temperature < 500 K. The thermal conditions for globular microstructure of primary Al were undercooled melt at early solidification stages and slow cooling < 0.6 K/s. It was found that the initial microstructure was maintained throughout the solidification and the globules of primary Al can be obtained by high nucleation of fine and spherical nuclei due to enhanced undercooling of melt.

Al 합금 컨트롤 암의 제조 공정 비교 연구 (Processing Comparison for Fabrication of Al Control Arm)

  • 권용남;이영선;이정환
    • 소성∙가공
    • /
    • 제15권7호
    • /
    • pp.490-495
    • /
    • 2006
  • The application of Al parts in passenger car has been increasing for the last decade, which gives many advantages such as better fuel efficiency, driving performance and safety. Control arm is one of the most preferably substituted parts from steel into Al alloys among numerous automotive parts. Currently, both wrought and cast Al alloys can find the application for control arm in passenger car. The balance between performance and cost determines a material as well as a fabrication process for a particular part model. In the present study, comparison among various processing techniques has been carried out to build up a data base for Al control arm fabrication.

반용융 단조를 위한 복합재료의 수직형 고주파 유도가열 (Induction Heating of Vertical Type for Semi-Solid Forging with Metal Matrix Composites)

  • 이동건;허재찬;강충길
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.385-388
    • /
    • 2001
  • In part forming process of metal matrix composites, the die casting and squeeze casting process are limited the size and dimension in term of final parts without machining. The thixoforming process for metal matrix composites has numerous advantages compared to die casting squeeze casting and compocasting. However, for the thixoforming process, the billet with the desired volume fraction must be heated to obtain a uniform temperature distribution over the entire cross-sectional areas. To obtain the reheating conditions of composites, the particulate reinforced metal matrix composites for thixoforming were fabricated by combined stirring process which is simultaneously performed with electro-magnetic stirring and mechanical stirring process.

  • PDF

저속 전기자동차용 알루미늄 차체 조인트 노드의 반응고 성형 (Fabrication of a Joint Node for an Aluminum Frame for a Low Speed Electric Vehicle using Thixoforming Technology)

  • 이상용
    • 소성∙가공
    • /
    • 제23권4호
    • /
    • pp.244-249
    • /
    • 2014
  • The thixoforming process has been applied to forming of a joint node for the aluminum frame of a low speed electric vehicle. A joint node should connect three aluminum extruded chassis showing different profiles. The MHS(magnetohydrodynamic stirring) A357 billet was selected because homogeneous globular grains are necessary as the billet materials for thixoforming. A careful design of joint node has been performed by the considerations of structural demands and the simulation results for the thixoforming process using the MAGMAsoft. Optimum heating temperature for the A357 billet was between 580 and $585^{\circ}C$ corresponding to the semi-solid temperatures showing 20-30% of liquid fraction. An injection speed of around 100mm/s and preheating of die at temperatures of $200^{\circ}C$ were also necessary conditions to obtain reasonable thixoformed parts.

Thixoforming 공정에서 Si의 크기가 대형 suspension 부품의 기계적 성질에 미치는 영향 (The effect of the size of the Si on mechanical properties of large suspension part in thixoforming process)

  • 신현기;서판기;박계주;강충길
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.808-811
    • /
    • 2002
  • In thixoforming process, the size of Si particles is changed by many parameters of forming. Especially, reheating and heat treatment are very important parameters. It was found that the mechanical properties was significantly improved by the thixoforming process. In this study, to investigate the relation between the mechanical properties and Si particles, the experiment of semi-solid die casting has been performed. Large suspension part with A356 alloy was fabricated with controlled ram speed. The effect of the size and shape of silicon particles on microstructure of tensile test has been investigated.

  • PDF

중공형 금속복합재료의 Thixoforging 금형설계 및 공정해석 (Thixoforging Die Design and Process Analysis of Hollow Shape Part with Metal Matrix Composites)

  • 허재찬;이승후;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 추계학술대회 논문집
    • /
    • pp.268-271
    • /
    • 2001
  • The die design of the liquid and semi-solid forming process is performed by CAE technology, The die design by the computer simulation has some advantages compared with the conventional method which has been performed by the designer's experiences in trials and emu. The defect zones such as porosity and shrinkage has been predicted by simulation results. The result of the numerical analysis for the proposed casting condition shows the characteristics of thixotropic flow, and was used to determine the geometry of the gating system and die cavity. The optimized production conditions were also proposed by result of computer aided engineering.

  • PDF