  • Objectives: This study aimed to evaluate the influence of inorganic composition and filler particle morphology on the mechanical properties of different self-adhesive resin cements (SARCs). Materials and Methods: Three SARCs including RelyX Unicem-2 (RUN), Maxcem Elite (MAX), and Calibra Universal (CAL) were tested. Rectangular bar-shaped specimens were prepared for flexural strength (FS) and flexural modulus (FM) and determined by a 3-point bending test. The Knoop microhardness (KHN) and top/bottom microhardness ratio (%KHN) were conducted on the top and bottom faces of disc-shaped samples. Sorption (Wsp) and solubility (Wsl) were evaluated after 24 hours of water immersion. Filler morphology was analyzed by scanning electron microscopy and X-ray energy dispersive spectroscopy (EDS). FS, FM, %KHN, Wsp, Wsl, and EDS results were submitted to 1-way analysis of variance and Tukey's post-hoc test, and KHN also to paired t-test (α = 0.05). Results: SARC-CAL presented the highest FS value, and SARC-RUN presented the highest FM. SARC-MAX and RUN showed the lowest Wsp and Wsl values. KHN values decreased from top to bottom and the SARCs did not differ statistically. Also, all resin cements presented carbon, aluminum, and silica in their composition. SARC-MAX and RUN showed irregular and splintered particles while CAL presented small and regular size particles. Conclusions: A higher mechanical strength can be achieved by a reduced spread in grit size and the filler morphology can influence the KHN, as well as photoinitiators in the composition. Wsp and Wsl can be correlated with ions diffusion of inorganic particles.

Effect of irrigation protocols on smear layer removal, bond strength and nanoleakage of fiber posts using a self-adhesive resin cement

  • Rodrigo Stadler Alessi;Renata Terumi Jitumori ;Bruna Fortes Bittencourt;Giovana Mongruel Gomes ;Joao Carlos Gomes
    • Restorative Dentistry and Endodontics
    • /
    • 제48권3호
    • /
    • pp.28.1-28.13
    • /
    • 2023
  • Objectives: This study aimed to investigate the effect of the application method of 2% chlorhexidine (CHX) and its influence on the adhesion of fiberglass posts cemented with a self-adhesive resin cement. Materials and Methods: Sixty human mandibular premolars were endodontically treated and divided into 5 groups (n = 12), according to the canal irrigant and its application method: 2 groups with conventional syringe irrigation (CSI)-2.5% sodium hypochlorite (NaOCl) (control) and 2% CHX- and 3 groups with 2% CHX irrigation/activation-by passive ultrasonic irrigation (PUI), Easy Clean file, and XP-Endo Finisher file. Two roots per group were evaluated for smear layer (SL) removal by scanning electron microscopy. For other roots, fiber posts were luted using a self-adhesive resin cement. The roots were sectioned into 6 slices for push-out bond strength (BS) (7/group) and nanoleakage (NL) (3/group). Data from SL removal were submitted to Kruskal-Wallis and Student-Newman-Keuls tests (α = 0.05). Data from BS and NL were evaluated by 2-way analysis of variance and Tukey's test (α = 0.05). Results: For SL removal and BS, the CHX irrigation/activation promoted better values than CSI with CHX (p < 0.05), but it was not significantly different from CSI with NaOCl (p > 0.05). For NL, the lowest values were obtained by the chlorhexidine irrigation/activation groups (p < 0.05). Conclusions: Active 2% CHX irrigation can be used to improve the post space cleaning and adhesion before fiber post cementation with self-adhesive resin cements.

Shear bond strength of luting cements to fixed superstructure metal surfaces under various seating forces

  • Ozer, Fusun;Pak-Tunc, Elif;Dagli, Nesrin Esen;Ramachandran, Deepika;Sen, Deniz;Blatz, Markus Bernhard
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권5호
    • /
    • pp.340-346
    • /
    • 2018
  • PURPOSE. In this study, the shear bond strengths (SBS) of luting cements to fixed superstructure metal surfaces under various seating forces were investigated. MATERIALS AND METHODS. Seven different cements [Polycarboxylate (PCC), Glass-Ionomer (GIC), Zinc phospahate (ZPC), Self-adhesive resin (RXU), Resin (C&B), and Temporary cements ((RXT) and (TCS))] were bonded to a total number of 224 square blocks ($5{\times}5{\times}3mm$) made of one pure metal [Titanium (CP Ti) and two metal alloys [Gold-Platinum (Au-Pt) and Cobalt-Chrome (Co-Cr)] under 10 N and 50 N seating forces. SBS values were determined and data were analyzed with 3-way ANOVA. Pairwise comparisons and interactions among groups were analyzed with Tukey's simultaneous confidence intervals. RESULTS. Overall mean scores indicated that Co-Cr showed the highest SBS values ($1.96{\pm}0.4$) (P<.00), while Au-Pt showed the lowest among all metals tested ($1.57{\pm}0.4$) (P<.00). Except for PCC/CP Ti, RXU/CP Ti, and GIC/Au-Pt factor level combinations (P<.00), the cements tested under 10 N seating force showed no significantly higher SBS values when compared to the values of those tested under 50 N seating force (P>.05). The PCC cement showed the highest mean SBS score ($3.59{\pm}0.07$) among all cements tested (P<.00), while the resin-based temporary luting cement RXT showed the lowest ($0.39{\pm}0.07$) (P<.00). CONCLUSION. Polycarboxylate cement provides reliable bonding performance to metal surfaces. Resin-based temporary luting cements can be used when retrievability is needed. GIC is not suitable for permanent cementation of fixed dental prostheses consisting of CP Ti or Au-Pt substructures.

레진시멘트의 중합방법이 포스트의 결합강도와 접착계면에 미치는 영향 (EFFECT OF CURING METHODS OF RESIN CEMENTS ON BOND STRENGTH AND ADHESIVE INTERFACE OF POST)

  • 김문홍;김혜정;조영곤
    • Restorative Dentistry and Endodontics
    • /
    • 제34권2호
    • /
    • pp.103-112
    • /
    • 2009
  • 본 연구에서는 2종의 이원중합 레진시멘트 (RelyX ARC와 Variolink II)를 이용하여 접착제와 레진시멘트의 중합방법 (자가중합과 광중합)이 섬유포스트와 근관 상아질의 결합강도와 접착계면에 미치는 영향을 상호 비교하기 위하여 시행하였다. 단근관을 갖는 발거된 32개의 하악 소구치에 근관을 충전한 후, FRC Postec system의 Reamer로 9 mm 깊이의 포스트 공간을 형성하였다. 레진시멘트의 종류와 중합방법에 따라 4개의 군 (R-SC군, R-LC군, V-SC군, V-LC군)으로 분류하였다. 포스트 공간에 각 군의 접착제를 도포한 후 레진시멘트를 주입하고, No. 3 FRC Postec 포스트를 위치시켜 자가중합 또는 광중합시켰다. 각 군의 치근을 실온의 증류수에 24시간동안 보관한 다음, 저속의 diamond wheel saw를 이용하여 치관부에서 치근단부를 향해 1.5 mm두께로 연속적으로 횡절단하여 1개의 치근에서 3개의 절편을 얻었다. 각 군의 절편 (31개)은 만능시험기에서 push-out 검사를 시행하였고, 각 군의 강도 값은 반복측정 two-way ANOVA와 one-way ANOVA를 이용하여 비교 분석하였다. 각 군의 절편 (3개)은 주사전자현미경하에서 섬유포스트, 레진시멘트 및 치근 상아질 간의 계면을 관찰, 비교하였다. 본 연구의 결과 전 부식 레진시멘트를 이용하여 섬유포스트를 포스트 공간에 합착할 경우, 접착제와 레진시멘트의 중합방법은 근관 상아질의 결합강도에 영향을 주었으며, 광중합보다 자가중합 방법 이 우수한 결합강도와 계면을 나타내었다.

Influence of nano alumina coating on the flexural bond strength between zirconia and resin cement

  • Akay, Canan;Tanis, Merve Cakirbay;Mumcu, Emre;Kilicarslan, Mehmet Ali;Sen, Murat
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권1호
    • /
    • pp.43-49
    • /
    • 2018
  • PURPOSE. The purpose of this in vitro study is to examine the effects of a nano-structured alumina coating on the adhesion between resin cements and zirconia ceramics using a four-point bending test. MATERIALS AND METHODS. 100 pairs of zirconium bar specimens were prepared with dimensions of $25mm{\times}2mm{\times}5mm$ and cementation surfaces of $5mm{\times}2mm$. The samples were divided into 5 groups of 20 pairs each. The groups are as follows: Group I (C) - Control with no surface modification, Group II (APA) - airborne-particle-abrasion with $110{\mu}m$ high-purity aluminum oxide ($Al_2O_3$) particles, Group III (ROC) - airborne-particle-abrasion with $110{\mu}m$ silica modified aluminum oxide ($Al_2O_3+SiO_2$) particles, Group IV (TCS) - tribochemical silica coated with $Al_2O_3$ particles, and Group V (AlC) - nano alumina coating. The surface modifications were assessed on two samples selected from each group by atomic force microscopy and scanning electron microscopy. The samples were cemented with two different self-adhesive resin cements. The bending bond strength was evaluated by mechanical testing. RESULTS. According to the ANOVA results, surface treatments, different cement types, and their interactions were statistically significant (P<.05). The highest flexural bond strengths were obtained in nano-structured alumina coated zirconia surfaces (50.4 MPa) and the lowest values were obtained in the control group (12.00 MPa), both of which were cemented using a self-adhesive resin cement. CONCLUSION. The surface modifications tested in the current study affected the surface roughness and flexural bond strength of zirconia. The nano alumina coating method significantly increased the flexural bond strength of zirconia ceramics.

Cytotoxicity and biocompatibility of Zirconia (Y-TZP) posts with various dental cements

  • Shin, Hyeongsoon;Ko, Hyunjung;Kim, Miri
    • Restorative Dentistry and Endodontics
    • /
    • 제41권3호
    • /
    • pp.167-175
    • /
    • 2016
  • Objectives: Endodontically treated teeth with insufficient tooth structure are often restored with esthetic restorations. This study evaluated the cytotoxicity and biological effects of yttria partially stabilized zirconia (Y-TZP) blocks in combination with several dental cements. Materials and Methods: Pairs of zirconia cylinders with medium alone or cemented with three types of dental cement including RelyX U200 (3M ESPE), FujiCEM 2 (GC), and Panavia F 2.0 (Kuraray) were incubated in medium for 14 days. The cytotoxicity of each supernatant was determined using 3-(4,5-dimethylthiazole- 2-yl)-2,5-diphenyltetrazolium bromide (MTT) assays on L929 fibroblasts and MC3T3-E1 osteoblasts. The levels of interleukin-6 (IL-6) mRNA were evaluated by reverse transcription polymerase chain reaction (RT-PCR), and IL-6 protein was evaluated by enzyme-linked immunosorbent assays (ELISA). The data were analyzed using one-way ANOVA and Tukey post-hoc tests. A p < 0.05 was considered statistically significant. Results: The MTT assays showed that MC3T3-E1 osteoblasts were more susceptible to dental cements than L929 fibroblasts. The resin based dental cements increased IL-6 expression in L929 cells, but reduced IL-6 expression in MC3T3-E1 cells. Conclusions: Zirconia alone or blocks cemented with dental cement showed acceptable biocompatibilities. The results showed resin-modified glass-ionomer based cement less produced inflammatory cytokines than other self-adhesive resin-based cements. Furthermore, osteoblasts were more susceptible than fibroblasts to the biological effects of dental cement.

인산염계 기능성 단량체가 첨가된 수종의 자가 접착 레진시멘트와 지르코니아 세라믹 사이 열순환 전후 전단결합강도 비교 (Evaluation of shear-bond strength between different self-adhesive resin cements with phosphate monomer and zirconia ceramic before and after thermocycling)

  • 이지훈;김민경;이정진;안승근;박주미;서재민
    • 대한치과보철학회지
    • /
    • 제53권4호
    • /
    • pp.318-324
    • /
    • 2015
  • 목적: 본 연구에서는 서로 다른 인산염계 기능성 단량체가 첨가된 5종의 자가 접착 레진시멘트와 지르코니아 사이의 열순환 전후 전단결합강도를 비교 평가하고자 하였다. 재료 및 방법: Airborne particle abrasion ($50{\mu}m$ $Al_2O_3$)을 시행한 디스크 모양의 Y-TZP 지르코니아 블록을 총 100개 준비하였다. 그리고 composite resin cylinder ($Filtek^{TM}$ Z250, 3M ESPE, St. Paul, MN, USA) 100개를 준비하였다. 서로 다른 인산염계 기능성 단량체가 첨가된 5종의 이중 중합형 자가 접착 레진시멘트 즉, Permacem 2.0 (DMG, Hamburg, Germany), $Clearfil^{TM}$ SA Luting (Kuraray Medical, Tokyo, Japan), $Multilink^{(R)}$ Speed (Ivoclar Vivadent, Schaan, Liechtenstein), $RelyX^{TM}$ U200 Automix (3M ESPE, Neuss, Germany), G-Cem $LinkAce^{TM}$ (GC Corporation, Tokyo, Japan)를 이용하여 지르코니아 블록과 composite resin cylinder를 접착하고 1군당 20개의 시편을 갖는 5개의 군을 만들었다. 시편을 $37^{\circ}C$ 의 증류수에 24시간 동안 보관한 후 각 군의 시편 절반(n=10)은 곧 바로 그리고 나머지 절반(n=10)은 5000회 열순환(5 - $55^{\circ}C$) 후에 전단결합강도를 측정하였다. 파절면은 FE-SEM을 이용하여 관찰하였다. 통계분석은 레진시멘트 종류 및 열순환 유무에 따른 전단결합강도의 비교를 위해 Two/One-way ANOVA를 시행하고 Tukey HSD post-hoc test를 이용하여 사후 검정하였으며, 열순환 전후의 비교를 위해 paired t-test를 이용하였다($\alpha$=.05). 결과: 열순환 전과 후 모두 $Multilink^{(R)}$ Speed 군은 나머지 4종류의 시멘트 군 보다 큰 전단결합강도를 나타내었다. G-Cem $LinkAce^{TM}$ 군은 열순환 전과 비교하여 열순환 후에 유의하게 낮은 전단결합강도를 나타내었지만, 다른 4종류 군은 열순환 전후 유의한 차이가 없었다. 결론: 인산염계 단량체를 포함한 대부분의 이중 중합형 자가 접착 레진시멘트는 지르코니아와 높은 전단결합강도를 보이고 열순환에 의해 유의한 영향을 받지 않아 지르코니아 보철물의 접착에 유용할 것이라고 사료된다.

심미보철 치료의 경향과 이해 : part 1. IPS e.max (Understanding and trends of esthetic treatment in prosthodontics : IPS e.max)

  • 강정인;허유리;이명선;손미경
    • 한국치위생학회지
    • /
    • 제14권4호
    • /
    • pp.447-452
    • /
    • 2014
  • With the increase of esthetic demands, most patients want to have restorations which are not only functional but also esthetic. For the esthetic restoration, many ceramic systems have been introduced and applied in dentistry. Among those ceramic restorations, IPS e.max system composed of lithium disilicate glass ceramic is one of the most commonly used systems because it has strength and esthetic characteristics. IPS e.max system is divided into IPS e.max Press and IPS e.max CAD according to the manufacturing methods. IPS e.max Press is fabricated through heat-pressed technique with ceramic ingot, which is very simple. The restorations which are made using IPS e.max system can apply to 3 units restoration for the anterior teeth and premolar, and single posterior tooth restoration. Cementation is one of the most important clinic procedure for the longevity of the restorations. All ceramics are bonded by resin cements, it is classified into three groups including adhesive, self-adhesive, and conventional. Variolink N, which is an adhesive resin cement and manufactured by same company with IPS e.max, is recommended for the bonding of IPS e.max restoration. Conventional and self-adhesive resin cement is also available. The aim of this review article is to provide the understanding of material properties, production procedure and clinical application of IPS e.max system.

Effect of Timing of Light Curing on the Shear Bond Strength of Three Self-adhesive Resin Cements

  • Yoo, Yeon-Kwon;Kim, Sung-Hun;Ryu, Jae-Jun;Ryu, Jae-Jun
    • Journal of Korean Dental Science
    • /
    • 제1권1호
    • /
    • pp.28-34
    • /
    • 2008
  • Objectives. The objectives of this study were: 1) to compare the effect of varying timing of light curing on shear bond strength, and; 2) to compare the shear bond strength of three self-adhesive cements. Materials and methods. A total of 72 extracted non-carious teeth were divided into 24 for Unicem tests, 24 for Maxcem tests, and 24 for Biscem tests; they were assigned 3 * 2 subgroups of 12 teeth each. The specimens were prepared as follows: 1) The calculus and periodontal ligament were removed from the teeth; 2) The teeth were stored in normal saline; 3) The occlusal enamel of each tooth was removed using high-speed coarse diamond burs under water cooling, and; 4) Finally, the teeth were flattened by 600-grit silicone carbide paper disks. Resin blocks were adhered using either Unicem, Maxcem, or Biscem. Light curing timing was divided into two groups: U10, M10, and B10 were exposed to light after 10 seconds, and; U150, M150, and B150 on the other side were exposed to light after 150 seconds. Shear bond strength was measured by a Universal testing machine with cross head speed of 1mm/min. T-test and One way ANOVA were used for the statistical analysis of data. Results. The shear bond strength of U150 was not significantly higher than that of U10 (U150: 20.55.7Mpa, U10: 18.73.80Mpa). On the other hand, the shear bond strength of M150 was significantly higher than that of M10. The shear bond strength of B150 was also significantly higher than that of B10 (M150:14.45.7Mpa, M10: 9.94.2Mpa, B150: 24.38.3Mpa, B10: 17.27.3Mpa). When the light curing timing was 10sec after bonding, the shear bond strength of Unicem was highest; the shear bond strength of Biscem was highest when the light curing timing was 150sec after bonding (U10: 18.73.80Mpa, B150: 24.38.3Mpa). Significance. Since Unicem is less sensitive based on light curing timing, dentists seem to use it without considering the light curing timing. Maxcem showed the lowest bonding strength (especially M10). Thus, when using Maxcem, dentists need to delay the light curing after adhesion.