A Study on the Shear Behaviors of Non-Grouted and Cement Grouted Sawtoothed Artificial Joints (톱니형 인공 절리의 시멘트 그라우팅 전.후의 전단거동에 관한 연구)

  • 이영남;천병식;김대영
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2000.11a
    • /
    • pp.721-728
    • /
    • 2000
  • The shear behavior of sawtoothed artificial joints grouted with cement milk was investigated in the laboratory under constant normal stress conditions. Tests were conducted on joints with asperities having inclinations of 16.7$^{\circ}$ and 26.6$^{\circ}$, compresive strengths having 15MPa and 47MPa under a given range of normal stresses varying from 0.76 to 1.91 MPa and at a free condition of pitching, rolling and dilatancy. Results show that the effect of asperities on shear strength increase is significant up to asperity height to grout thickness (t/a) ratio of 0.3∼1.0. Increase of cohesion is the main cause of shear strength increase in cement grouted sawtoothed artificial joints.

  • PDF

Grouting Effect of Rock Joint (암반절리면에서의 그라우팅 효과)

  • 이영남;천병식;김대영
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2000.10a
    • /
    • pp.265-270
    • /
    • 2000
  • AESTRACI: The shmr behior of sawtoothed artrjicial joints grouted with cement milk rm investiguted in the lahotconstant normal stress conditions. Tests were amducted on joints with asperities h i n g inclinations cf 16.7" and 26.6" ,strengths h i n g 15MPa and 47MPa under a given nmge of n o d stresses wrying frcm 0.76 to 1.g MPa md at a freepitching, rolling and dihtmuy. Results show that the gect of asperities on shmr strength increme is signifamt up to as,to grout thidness (t/a) mtio 4 0.3-1.0. Increme of ahesim is the nmn muse cf shmr strength increme in cemmtoothed artificial iointsed artificial ioints

  • PDF