• 제목/요약/키워드: Sand-Binder ratio

검색결과 78건 처리시간 0.024초

Effects of Sand/Binder Ratios on the Mechanical Properties of Mortars Containing Fly ash and Silica fume

  • Park, Ki-Bong;Lee, Han-Seung
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 추계 학술발표회 제17권2호
    • /
    • pp.777-780
    • /
    • 2005
  • The paper presents details of an investigation into the effect of sand content upon the strength and shrinkage of mortar. This strategy was to produces more durable strength mortar with less cement. Cement mortars containing $20\;wt.\;\%$ Class F fly ash, and/or $6\;wt.\;\%$ silica fume were prepared at a water/binder ratio of 0.45 and sand/binder ratios of 2.0, 2.5, 2.7, and 3.0. The increase in sand/binder ratio caused a decrease in the mortar flow. However, the sand/binder ratio did not affect the strength development. Drying shrinkage decreased with increasing the sand contents.

  • PDF

폴리머 디스퍼션을 이용한 프리팩트 콘크리트용 주입 모르타르의 배합에 관한 연구 (Mix Design of Polymer Grouting Mortar for Prepacked Concrete Using Polymer Dispersions)

  • 조영국;김완기
    • 한국건축시공학회지
    • /
    • 제8권5호
    • /
    • pp.85-91
    • /
    • 2008
  • Prepacked concrete has recently been used in the special constructions fields such as underwater concrete work, heavy-weight concrete work, underground structure work, partial repair works for damaged reinforced concrete structures. and polymer-modified mortars have been employed as grouting mortars for the prepacked concrete. The purpose of this study is to recommend the optimum mix design of polymer-modified grouting mortars for prepacked concrete. Polymer-modified mortars using SBR and EVA emulsions as admixture of grouting mortars for prepacked concrete are prepared with various mix proportions such as sand-binder ratio, fly ash replacement ratio, polymer-binder ratio. and tested for flowability, viscosity of grouting mortars, bleeding ratio, expansion ratio, flexural and compressive strengths of grouting mortars and compressive and tensile strengths of prepacked concretes. From the test results, it is apparent that polymer-modified mortars can be produced as grouting mortars when proper mix design is chosen. We can design the mix proportions of high strength mortars for prepacked concrete according to the control of mix design factors such as type of polymer, polymer-binder ratio, sand-binder ratio and fly ash replacement ratio. Water-binder ratio of plain mortars for a constant flowability value are in the ranges of 43% to 50%. SBR-modified mortar has a little water-binder ratios compared to those of plain mortar, however, EVA-modified mortar needs a high water-binder ratio due to a high viscosity of polymer dispersion. The expansion and bleeding ratios of grouting mortars are also controlled in the proper value ranges. Polymer-modified grouting mortars have good flexural. compressive and tensile strengths, are not affected with various properties with increasing fly ash replacement to cement and binder-sand ratio. In this study, SBR-modified grouting mortar with a polymer-binder ratio of 10% or less, a fly ash replacement of 10% to cement and a sand-binder ratio of 1.5 is recommended as a grouting mortar for prepacked concrete.

프리팩트 폴리머 시멘트 콘크리트용 주입 폴리머 시멘트 모르터의 성질에 관한 연구 (A Study on Basic Properties of Grouting Motars for polymer-Modified preplaced Aggregate Concrete)

  • 이철웅;김완기;조영국;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표논문집(II)
    • /
    • pp.350-355
    • /
    • 1998
  • Preplaced aggregate concrete in the building fields has recently been used in the partial repair works for damaged reinforced concrete structures, and polymer-modified mortars have been employed as grouting mortars for the preplaced aggregate concrete. The objective of this study is to clear the properties of polymer-modified grouting mortars. Polymer-modified mortars using a polystyrene acrylic(St/Ac) emulsion as grouting mortars for preplaced aggregate concrete are prepared with various mix proportions, and tested for flexural and compressive strengths, adhesion in tension. The flexural strength of emulsion-modified grouting mortars does not give much variation with increasing fly ash replacement for cement and sand-binder ratio. With increasing polymer-binder ratio, the flexural strength and adhesion in tension of St/Ac emulsion-modified grouting mortars increases, become nearly constant or reaches a maximum at a polymer-binder ratio of 5%. From the test results, St/Ac emulsion-modified grouting mortar with a polymer-binder ratio of 5%, a fly ash replacement of 10% for cement and sand-binder ratio of 1.0 is recommended as a grouting mortar for preplaced aggregate concrete.

  • PDF

고로슬래그 미분말을 함유한 고유동 모르터의 유동성상에 미치는 영향 요인에 관한 연구 (A Study on the Factors Affecting the High Fluid Mortar Containing Ground Granulated Blast-furnace Slag)

  • 김재훈;윤상천;지남용
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2002년도 학술.기술논문발표회
    • /
    • pp.29-36
    • /
    • 2002
  • High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of molar and fineness modulus of ,and on the properties of fresh mortar. The effect of water-binder ratio, sand-binder ration, content; of ggbs (by mass of total cementitious materials), and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the following conclusion; can be drawn: (1) The mixing time needed (or high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

  • PDF

수중에 노출된 농업용 콘크리트 구조물 보수용 라텍스개질 모르타르의 적정 배합비 도출 (Optimum Mix Proportions of Latex Modified Repair Mortar for Agricultural Underwater Concrete Structure)

  • 원종필;이재영;박찬기;이상우;김완영
    • 한국농공학회논문집
    • /
    • 제49권3호
    • /
    • pp.43-50
    • /
    • 2007
  • The purpose of this study was to determine the optimum mix proportion of latex modified mortar for agricultural underwater concrete structures repair. The experimental variables included a latex and antiwashout admixture amount, binder-sand ratio, water-binder ratio. This study were evaluated a repair performance and environment effect of latex modified repair mortar for agricultural underwater concrete structures. The pH test was conducted to evaluated the environmental effect and the flow test was peformed to evaluated the workability. Also, compressive, flexural and bond tests were conducted. Test results show that the optimum mix proportion of latex modified repair mortar for agricultural underwater concrete structures, was achieved by 1:1.5 binder-sand ratio, 5% latex ratio (weight of binder), 1.3% antiwashout admixture ratio (weight of binder), 0.33 water-binder ratio and 10% silica lune replacement ratio (weight of cement). The environmental effect and repair performance of optimum mix proportion satisfied all target performance.

고로슬래그 미분말을 함유한 고유동 모르터의 유동성상에 미치는 영향 요인에 관한 연구 (A Study on the Factors Affecting the High Fluid Mortar Containing Ground Granulated Blast-furnace Slag)

  • 김재훈;윤상천;지남용
    • 한국건축시공학회지
    • /
    • 제2권4호
    • /
    • pp.145-152
    • /
    • 2002
  • High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of mortar and fineness modulus of sand on the properties of fresh mortar. The effect of water-binder ratio. sand-binder ration. contents of ggbs (by mass of total cementitious materials). and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the fellowing conclusions can be drawn: (1) The mixing time needed for high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

기상재해 대응 긴급보수용 패브릭 콘크리트 혼합물의 역학적 특성 및 내구성능 평가 (Evaluation of Mechanical Properties and Durability of Fabric Concrete Binder for Emergency Repair)

  • 전상민;조성문;오리온;김황희;차상선;박찬기
    • 한국농공학회논문집
    • /
    • 제62권4호
    • /
    • pp.23-31
    • /
    • 2020
  • Recently, meteorological disasters have been increasing by climate change, excessive rainfall, and landslide. The purpose is to develop new fabric concrete that can prevent and recover from damages because some of areas are vulnerable to meteorological disaster. Specifically, this technology can minimize time and space constraint when repairing the concrete structure and installing a formwork. The structure of fabric concrete is a mixture of fabric concrete and a high-speed hardened cement, Silica sand, wollastonite mineral fiber, fabric material and waterproof PVC fabric. In this study, the ratio of mechanical properties and durability of the fabric concrete mixture was evaluated by deriving the binder: silica sand mix ratio of the fabric concrete mixture and substituting part of the cement amount with wollastonite mineral fiber. Best binder in performance evaluation: Silica sand mix ratio is 6: 4 and the target mechanical performance and durability are the best when over 15% wollastonite binder is replaced by silicate mineral fiber.

물-결합재 비와 잔골재-결합재 비에 따른 알칼리 활성화 슬래그 모르타르의 기초특성 (The Fundamental Properties of Alkali-Activated Slag Cement (AASC) Mortar with Different Water-Binder Ratios and Fine Aggregate-Binder Ratios)

  • 김태완;함형길;이성행;엄장섭
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제17권5호
    • /
    • pp.77-86
    • /
    • 2013
  • 본 연구는 물-결합재 비 (W/B)와 잔골재-결합재 비 (F/B)에 따른 알칼리 활성화 슬래그 시멘트 (AASC)의 기초 특성에 관한 연구이다. W/B 비는 0.35, 0.40, 0.45, 그리고 0.50를 선정하였다. 그리고 F/B 비는 1.00에서 3.00까지 0.25 크기로 고려하였다. 알칼리 활성화제는 2M과 4M의 NaOH를 사용하였다. 실험은 플로우, 흡수율, 압축강도, 초음파 속도 그리고 건조수축을 측정하여 비교하였다. 플로우, 압축강도, 흡수율, 초음파 속도 그리고 건조수축 모두 W/B 비가 증가하면 감소하였다. 압축강도는 동일 W/B 비에서 F/B 비가 증가할수록 감소하였다. 또한 특정 F/B 비에서 강도가 증가하는 것을 볼 수 있었다. 그리고 S2 (river sand 2)는 S1 (river sand 1)보다 낮은 물리적 특성을 나타냈는데, 이는 조립률 때문으로 판단된다. 본 실험의 결과 AASC의 공학적 특성은 W/B 비와 F/B 비가 영향을 주는 것으로 판단된다. 최적의 F/B 비는 각 W/B 비에 대해 1.75~2.50 인 것으로 생각된다. 또한 W/(B+F) 비가 0.13과 0.14 사이일 때 AASC 모르타르의 배합설계가 효과적일 것으로 판단된다.

고로슬래그미분말을 혼입한 고유동콘크리트에서 골재조합이 콘크리트 유동성상에 미치는 영향에 관한 실험 연구 (The Effect of Combined Aggregates on Fluidity of the High Fluid Concrete Containing GGBFS)

  • 김재훈;윤상천;지남용
    • 한국건축시공학회지
    • /
    • 제3권4호
    • /
    • pp.79-86
    • /
    • 2003
  • The purpose of study is to offer base data for high fluid concrete mix property, as grasp effect of aggregate to reach much more effect for producing high fluid concrete. For this study, there are three types of combined aggregates, river sand + river aggregate(type A), river sand + crusted aggregate(type B), washed sea sand + crushed aggregate(type C) and take a factor, water-contents, water-binder ratio and S/a. And so, we had following conclusion, resulting application-ability of high fluid mortar by K-slump tester to use a handy consistency measuring instrument. And so, we had following conclusion, resulting application-ability of high fluid concrete by K-slump tester to use a handy consistency measuring instrument. 1) In cafe of regular water binder ratio, high fluid concrete suffered much effect of combined aggregates and water binder ratio. Range of water binder ratio by combined aggregates is w/b 0.4 downward(type A and B), w/b 0.35 downward(type C). 2) Water contents to need for producing high fluid concrete is minimum 170kg/$\textrm{m}^3$ without regard to combined aggregates. 3) The effect of S/a on high fluid concrete by combined aggregates is approximately S/a 50% (type A and B), s/a 50-55% (type C). 4) Consistency measuring of high fluid concrete by K-slump tester is possible and first indication value, high fluid concrete can be produced, is 6~10.5cm.

부순모래를 사용한 초고강도 콘크리트의 공학적 특성에 관한 연구 (A Study on the Engineering Properties of Ultra High-Strength Concrete Utilizing Crushed Sand)

  • 이상수;노형남;송하영
    • 한국건축시공학회지
    • /
    • 제8권4호
    • /
    • pp.45-51
    • /
    • 2008
  • Recently, the demand of ultra high-rise building is on the increase in korea due to the rapidly changing movement in economic growth and the expansion of national infrastructure. At the same time, the tendency toward the amount used of concrete has greatly increased every year. In addition, as the seriousness of quantity demanded of aggregate is gathering strength, the active areas of research proceeds to do actively in every place in order to review the usability of crushed sand as a part of the countermeasures. And, it needs to establish the quality standard and service guide, etc. for the practical use. Accordingly, this study was to establish the ratio of water-binder materials as three levels like 23.5, 27.5, and 31.5%, and the replacement ratio as three levels like 0, 50, and 100% in order to define the engineering properties of ultra high-strength concrete using the crushed sand. This study was to examine it after establishing the combined condition by the substitute of the fine aggregate percentage and admixture. From the result of this research above, it may be summed up as follows. 1) The more the replacement ratio of crushed sand and the ratio of water-binder materials increased, the mon the fluidity decreased due to the decrease of irregular grain shape of sand and unit combined discretion. 2) This study found out that 100% of replacement ratio of crushed sand was almost similar level to the compressive strength of concrete using the natural sand.