Influence of the Diamond Abrasive Size during Mechanical Polishing Process on the Surface Morphology of Gallium Nitride Substrate (Gallium Nitride 기판의 Mechanical Polishing시 다이아몬드 입자 크기에 따른 표면 Morphology의 변화)

  • Kim, Kyoung-Jun;Jeong, Jin-Suk;Jang, Hak-Jin;Shin, Hyun-Min;Jeong, Hae-Do
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.25 no.9
    • /
    • pp.32-37
    • /
    • 2008
  • Freestanding hydride vapor phase epitaxy grown GaN(Gallium Nitride) substrates subjected to various polishing methods were characterized for their surface and subsurface conditions, Although CMP(Chemical Mechanical Polishing) is one of the best approaches for reducing scratches and subsurface damages, the removal rate of Ga-polar surface in CMP is insignificant($0.1{\sim}0.3{\mu}m$/hr) as compared with that of N-polar surface, Therefore, conventional MP(Mechanical Polishing) is commonly used in the GaN substrate fabrication process, MP of (0001) surface of GaN has been demonstrated using diamond slurries with different abrasive sizes, Diamond abrasives of size ranging from 30nm to 100nm were dispersed in ethylene glycol solutions and mineral oil solutions, respectively. Significant change in the surface roughness ($R_a$ 0.15nm) and scratch-free surface were obtained by diamond slurry of 30nm in mean abrasive size dispersed in mineral oil solutions. However, MP process introduced subsurface damages confirmed by TEM (Transmission Electronic Microscope) and PL(Photo-Luminescence) analysis.