Magnetic Properties of Monolayer-thiciness InP(001)(2×4) Reconstruction Surface (InP(001)(2×4)재구성된 표면 위에 원자층 단위로 증착된 Co 박막의 자성 특성)

  • Park, Yong-Sung;Jeong, Jong-Ryul;Lee, Jeong-Won;Shin, Sung-Chul
    • Journal of the Korean Magnetics Society
    • /
    • v.14 no.3
    • /
    • pp.89-94
    • /
    • 2004
  • We have investigated magnetic properties of monolayer (ML)-thickness Co film deposited on InP(2${\times}$4) reconstruction surface using in situ Surface Magneto-Optical Kerr Effects (SMOKE) measurement system. InP(2${\times}$4) reconstruction surface, obtained by repeated sputtering and annealing, was confirmed by reflection hish energy electron diffraction (RHEED) and scanning tunneling microscope (STM) measurements. From both longitudinal and polar SMOKE measurements, we have observed three distinguishable regions showing different magnetic properties depending on the Co thickness. In the Co film thickness smaller than 7 $m\ell$, no SMOKE signal was detected. In the following thickness between 8 $m\ell$ and 15 $m\ell$, both longitudinal and polar Kerr hysteresis loops were observed, which implies a metastable phase coexisted of in-plane and perpendicular anisotropies. In the film thickness larger than 16 $m\ell$, only longitudinal MOKE signal without polar signal was detected, which implies existence of in-plane anisotropy in this thickness region.

Improvement the Flame Retardancy of Epoxy Resin by the Addition of Montmorillonite (Montmorillonite 첨가에 의한 Epoxy Resin의 난연성 개선)

  • Song, Young-Ho;Chung, Kook-Sam
    • Fire Science and Engineering
    • /
    • v.22 no.3
    • /
    • pp.300-304
    • /
    • 2008
  • The flame retardancy was evaluated to present as the fundamental data to decrease the fire hazard of polymers and life losses according to the addition of clay. The combustion characteristics were examined to increase flame retardancy and to decrease smoke yield of epoxy by the addition of clay such as montmorillonite in this study. For this study, the experiments of flame retardancy were conducted the measurement of the limiting oxygen index (LOI), char yield, and smoke density. As MMT concentration increased, LOI and char yield increased. This result showed that the flame retardancy of epoxy/MMT composite was improved. On the contrary, smoke density increased.

Development of Packed Bed Lung Model for the Deposition Studies of Fire Smoke (흡입연기의 침착 실험을 위한 충전층 폐모델 개발에 관한 연구)

  • Goo, Jae-Hark
    • Fire Science and Engineering
    • /
    • v.22 no.2
    • /
    • pp.121-128
    • /
    • 2008
  • Adverse health effects of inhaled smokes are associated with the amount of the particles deposited in human lung. Lung model is needed to simulate smoke deposition because of the hardness of the in vivo deposition experiment. However, it is hard to realize the successively decreasing bifurcations in the model. In this work, an experimental lung model was developed to simulate the smoke deposition in the lung. Instead of bifurcating airways, the lung model was made of packed beds of which size decreased downwards. The experimental results using this model showed good agreements with existing results for real lung in the deposition characteristics. The model could be applied to the studies of health risk assessment of the inhaled smoke particles generated by fire.

Determination of Free Radicals in Mainstream Cigarette Smoke by Electron Spin Resonance (전자스핀공명에 의한 담배연기 중 자유라디칼 측정)

  • Lee, Jeong-Min;Lee, John-Tae;Park, Jin-Won;Hwang, Keun-Joong
    • Journal of the Korean Society of Tobacco Science
    • /
    • v.29 no.2
    • /
    • pp.146-151
    • /
    • 2007
  • Gas phase and particulate phase radicals in mainstream cigarette smoke were determined Electron Spin Resonance(ESR) spectroscopy. The free radicals in particulate phase have been investigated by benzene extract of Cambridge Filter Pad containing the smoke condensate. Spin trapping method in conjunction with ESR was used to investigate free radicals in the gas phase of cigarette smoke. Several analytical experiments were conducted in order to determine the optimal conditions for maximum signal intensities and reproducibility of results. All the tests were optimized and normalized using the University of Kentucky 2R4F reference cigarette. The optimal conditions were 0.6 mL for analysis volume of ESR, $4{\sim}5\;mL$ for collection volume of spin-adducts, and PBN for quantification of free radicals in gas phase. The radical levels of Kentucky 2R4F cigarettes were found $2.18{\times}10^{14}\;spins/cig.$ and $2.10{\times}10^{15}\;spins/cig.$ in gas phase.

New Smoke Risk Assessment on Wood Treated with Silicone Compound (실리콘 화합물로 처리된 목재의 새로운 연기위험성 평가)

  • Chung, Yeong-Jin;Jin, Eui
    • Fire Science and Engineering
    • /
    • v.33 no.4
    • /
    • pp.16-27
    • /
    • 2019
  • A burning test was conducted on the smoke and combustion gases generated from cypress wood treated with sodium silicate, 3-aminopropyltrimethoxysilane sol, 3-(2-aminoethylamino)propylmethyldimethoxysilane sol, and 3-(2-aminoethylamino) propyltrimethoxysilane sol. The silicone compound sol was applied to each of the cypress wood specimens three times with a brush. The smoke and combustion generation gas were analyzed using a cone calorimeter (ISO 5660-1) and the smoke was also evaluated by applying new smoke risk assessment method. The smoke performance index (SPI) of the cypress treated with silicone compound increased 1.66 to 8.42 times and the smoke growth index (SGI) was 11.8 to 88.2%, respectively. The smoke intensity (SI) is expected to be 1.0~50.5% lower than that of the base specimens, resulting in lower smoke and fire hazards. The third maximum carbon monoxide (COpeak) concentration of the specimens treated with silicone compounds was 22.5~33.3% lower than that of the base specimens. On the other hand, it produced potentially fatal toxicity that was 1.48~1.72 times higher than the US Occupational Safety and Health Administration (OSHA) acceptance standard (PEL). Cypress wood itself produced a high carbon monoxide concentration, but the silicon compound played a role in reducing this level.

An Experimental Study of Smoke Movement in a Kindergarten Fire (어린이집 화재 시 연기 거동에 관한 실험적 연구)

  • Lee, Sung-Ryong;Han, Dong-Hun
    • Fire Science and Engineering
    • /
    • v.27 no.2
    • /
    • pp.62-69
    • /
    • 2013
  • In this study, a full scale experiment was carried out to analyze the heat and smoke movement. The experiment was conducted a kindergarten that is scheduled to reconstruction. The kindergarten is a two-story building and the area of each floor is 252 $m^2$. 36 l heptane was used as a fuel and heptane was burned in a 0.8 m square steel pool. Maximum heat release rate was 1.7 MW at natural condition. Smoke movement and temperature variation were measured during the experiment. In the first floor corridor, smoke was moved downward about 1.4 m at 1 minute after a fire. Corridor was filled with smoke at 4 minutes after a fire. In the second floor, temperature was maintained at $70^{\circ}C$ or less. But, second floor rooms were filled with smoke.

The Exhaust Gas Reduction of Diesel Engine by MDO (Marine Diesel Oil) Emulsion Fuel (MDO (Marine Diesel Oil) 에멀젼 연료에 의한 디젤엔진의 배출가스 저감)

  • Kim, Moon-Chan
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.36 no.7
    • /
    • pp.476-482
    • /
    • 2014
  • In this study, the characteristics of emulsified fuel and engine emissions were studied with engine dynamometer. Microexplosion took place in the combustion chamber. While combustion, emulsion fuel scattered to micro particles and it caused to smoke reduction. The heat produced from water vapour reduce the temperature of internal combustion chamber and it caused to inhibition of NOx production. It can be verified by the lower exhaust temperature of each ND-13 mode using emulsion fuel than that of MDO fuel. The NOx and smoke concentration were reduced by increasing water content in emulsion fuel. The power also decreased according to the increment of water content of emulsion fuel because emulsion fuel has low calorific value due to high water content than MDO. As a result of ND-13 mode test with 17% moisture content, it was achieved 24% reduction in NOx production, 76% reduction in smoke density, 11% reduction of $SO_2$ and 13% reduction in power loss.

Experimental and Numerical Studies on Heat/Smoke Behavior due to a Fire on Underground Subway Platform (I) - Experimental Approach - (지하철 역사 승강장 화재발생시 열/연기 거동 분석을 위한 실험 및 수치 연구(I) - 실험적 접근 -)

  • Park, Won-Hee;Kim, Dong-Hyeon;Chang, Hee-Chul;Kim, Tae-Kuk
    • Fire Science and Engineering
    • /
    • v.20 no.3 s.63
    • /
    • pp.9-14
    • /
    • 2006
  • In this study boundary velocity which is one of the important boundary conditions for numerical simulation for subway station on fire are experimentally obtained. The tests were conducted according to its operating mode of the ventilation systems in the platform: smoke extraction ventilation mode in occurrence of fire and normal ventilation mode for air conditioning. Velocities are measured at various points on the platform. To examine smoke extraction and air supply capacity in the platform level, air velocities were checked on opening vents. Numerical analysis under normal ventilation mode without fire is conducted by using measured boundary conditions, and the numerical results are compared with the measured velocities on the platform.

A Study on the Model Experiment for Smoke Flow in Road Tunnel Fire (도로터널 화재발생시 연기유동에 관한 축소모형실험 연구)

  • Kim, Jung-Yup;Shin, Hyun-Joon;Kang, Se-Gu;Ahn, Kyung-Chul
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.6 no.2
    • /
    • pp.141-149
    • /
    • 2004
  • In this study, smoke movement in tunnel fire with natural and longitudinal ventilation systems has been investigated. Reduced-scale experiments were carried out under the Froude scaling using 14.55kW fire source with a wick and experimental data is obtained with 1/18 model tunnel test. Temperature profiles were measured under the ceiling and vertical direction along the center of the tunnel and poisonous gas was measured at emergency exit point. The results show that refuge time for 225m intervals of emergency exit in case of natural ventilation systems is 256 seconds and critical velocity for sufficient back-layer prevention is 2.8m/s for fire strength of 20MW.

  • PDF

Assessment of Flame Retardancy for Acrylonitrile Butadiene Styrene Containing Metal Powder and Flame Retardant (금속분말-난연제 함유 ABS의 난연 특성 평가)

  • Song, Young-Ho;Chung, Kook-Sam
    • Fire Science and Engineering
    • /
    • v.21 no.2 s.66
    • /
    • pp.30-35
    • /
    • 2007
  • The flame retardancies by the addition of metal powder and flame retardant were evaluated to present as the fundamental data to decrease the fire hazard of polymers and life losses by suffocation and poisoning. For this study, the experiments of flame retardancy were conducted as follows : weight loss rate using thermogravimetric analysis, the measurement of the limiting oxygen index(LOI) and char yield. And smoke mass concentration and CO yield were measured. Acrylonitrile butadiene styrene containing metal powder and flame retardant reduced weight loss rate and increased LOI and char yield with the decreased smoke mass concentration and CO yield. It was found that the most effective complex was tricresyl phosphate-Mo complex.