• 제목/요약/키워드: SI direction

검색결과 600건 처리시간 0.025초

Wear Behaviors of Unidirectionally Oriented $Si_{3}N_{4w}/Si_{3}N_{4}$ Composites

  • Liang, Ya-Nan;Lee, Soo-Wohn;Park, Dong-Soo
    • The Korean Journal of Ceramics
    • /
    • 제4권4호
    • /
    • pp.377-381
    • /
    • 1998
  • Wear behaviors of unidirectionally oriented $Si_3N_{4w)/Si_3N_4$ composites, sintered at different temperatures with different alignments of whiskers, have been studied in parallel and perpendicular sliding directions with respect to the orientation of the whiskers by using a ball-on-disk reciprocating sliding apparatus. The results show that wear rate in parallel direction is much greater than that in perpendicular direction. With decreasing alignment of the whiskers, the wear rate decreases in parallel sliding direction and increases in perpendicular direction. With increasing sintering temperature, the wear rate increases obviously in both parallel and perpendicular directions.

  • PDF

Electronic Structures and Magnetic Properties of Fe/Si/Fe Trilayer

  • Park, Jin-Ho;Youn, Suk-Ju;Min, Byung-Il;Yi, Jae-Yel
    • Journal of Magnetics
    • /
    • 제1권1호
    • /
    • pp.4-8
    • /
    • 1996
  • Employing the LMTO band method, we have studied electronic and magnetic properties of Fe/Si/Fe trilayer in which the z-direction is chosen to be (111) direction of FeSi with B2 phase, We have also determined electronic structure of bulk FeSi, as a reference material. The ground state of FeSi is paramagnetic insulator with a band gap of 0.05 eV. Band structures of Fe/Si/Fe with varying the thickness of the spacer layer reveal that the spacer layer is metallic, and the states along the growth direction do not disperse much reflecting a two-dimensional nature. Magnetic moment of Fe atom in the interfacial layer of Fe/Si/Fe is reduced a lot as compared to the bulk value, suggesting a strong hybridization between Fe and Si states. The geometry of the Fermi surface indicates that the magnetic coupling period of ~8ML (monolayers) in Fe/Si/Fe is explained with a short Fermi wave vector of bcc Si.

  • PDF

광전소자 응용을 위한 무극성 6H-SiC 기판의 특성 (Characterization of Non-polar 6H-SiC Substrates for Optoelectronic Device Applications)

  • 여임규;이태우;최정우;서정두;구갑렬;이원재;신병철;김영희
    • 한국전기전자재료학회논문지
    • /
    • 제22권5호
    • /
    • pp.390-396
    • /
    • 2009
  • The present research was focused to investigate the quality of non-polar SiC substrates grown by a conventional PVT method for optoelectronic applications. The half part of the PVT-grown 6H-SiC crystal boules was sliced along a-direction and m-direction to extensively analyze non-polar planes and then remaining part of that was sliced along the basal plane to produce wafers. The non-polar SiC m-plane and a-plane exhibited apparent peaks around 2 theta=$120^{\circ}$((3-300) plane) and 2 theta=$60^{\circ}$ ((11-20) plane), respectively. FWHM values of m-plane measured along a-direction and c-direction were 60 arc see and 57 arcsec respectively, a-plane measured along m-direction and c-direction were 41 arcsec and 51 arcsec respectively. The typical absorption spectra of SiC crystals indicated that each of SiC crystals were the 6H-SiC with fundamental absorption energy of about 3.04 eV. Non-polar planes contained no micropipe on etched surface. The carrier concentration and mobility of non-polar SiC wafers have estimated by Raman spectrum. It was observed that the carrier mobility is low in the area far from seed crystal with compared to other places.

NITE-SiC 복합재료의 미세구조 특성에 미치는 섬유배열방향 영향 (Effects of Fiber Arrangement Direction on Microstructure Characteristics of NITE-SiC Composites)

  • 이영주;윤한기;박준수
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2006년 창립20주년기념 정기학술대회 및 국제워크샵
    • /
    • pp.158-161
    • /
    • 2006
  • SiC materials have been extensively studied for high temperature components in advanced energy conversion system and advanced gas turbine. However, the brittle characteristics of SiC such as law fracture toughness and law strain-to fracture impose a severe limitation on the practical applications of SiC materials. SiC/SiC composites can be considered as a promising candidate in various structural materials, because of their good fracture toughness. In this composite system, the direction of SiC fiber will give an effect to the mechanical properties. It is therefore important to control a properdirection of SiC fiber for the fabrication of high performance SiC/SiC composites. In this study, unidirection and two dimension woven structures of SiC/SiC composites were prepared starting from Tyranno SA fiber. SiC matrix was obtained by nano-powder infiltration and transient eutectoid (NITE) process. Effect of microstructure and density on the sintering temperature in NITE-SiC/SiC composites are described and discussed with the fiber direction of unidirection and two dimension woven structures.

  • PDF

$Si_{1-y}Ge_y$ 위에 성장시킨 $Si_{1-x}Ge_x$ 에서 성장방향과 응력변형 조건에 따른 정공의 이동도 연구 (Dependence of Hole Mobilities on the Growth Direction and Strain Condition in $Si_{1-x}Ge_x$ Layers Grown on $Si_{1-y}Ge_y$ Substrate)

  • 전상국
    • 한국전기전자재료학회논문지
    • /
    • 제11권4호
    • /
    • pp.267-273
    • /
    • 1998
  • The band structures of $Si_{1-x}Ge_x$ layers grown on $Si_{1-y}Ge_y$ substrate are calculated using k$\cdot$p and strain Hamiltonians. The hole drift mobilities in the plane direction are then calculated by taking into account the screening effect and the density-of-states of the impurity band. When $Si_{1-x}Ge_x$ is grown on Si substrate, the mobilities of (110) and (111) $Si_{1-x}Ge_x$ layers are larger than that of (001) $Si_{1-x}Ge_x$. However, due to the large defect and surface scattering, (110) and (111) $Si_{1-x}Ge_x$ layers may not be useful for the development of the fast device. Meanwhile, when Si is grown on $Si_{1-y}Ge_y$ substrate, the mobilities of (001) and (110) Si layers are greatly enhanced. Based on the amount of defect and the surface scattering, it is expected that Si grown on (001) $Si_{1-y}Ge_y$ substrate, where the Ge contents is larger than 10%(y>0.1), has the highest mobility.

  • PDF

SiC 휘스커 보강 Al 6061 복합재료의 피로균열진전 특성에 관한 기초 연구 (The Basic Study on Fatigue Crack Growth Behavior of SiC Whisker Reinforced Aluminium 6061 Composite Material)

  • 권재도;안정주;김상태
    • 대한기계학회논문집
    • /
    • 제18권9호
    • /
    • pp.2374-2385
    • /
    • 1994
  • SiCw/Al composite material is especially attractive because of their superior specific strength, specific stiffness, corrosion fatigue resistance, creep resistance, and wear resistance compared with the corresponding wrought Al alloy. In this study, Fatigue crack growth behavior and fatigue crack path morphology(FCPM) of SiC whisker reinforced Al 6061 alloy with 25% SiC volume fraction and Al 6061 allay were performed. Result of the fatigue crack growth test sgiwed that fatigue crack growth rate of SiCw/Al 6061 composite was slower than that of Al 6061 matrix therefore it was confirmed that Sic whisker have a excellent fatigue resistance. And Al 6061 matrix had only FCPM perpendicular to loading direction. On the other hand SiCw/Al 6061 composite had three types in fatigue crack path morphology. First type is that both sides FCPM of artificial notch are perpendicular to loading direction. Second type is that a FCPM in artifical notch has slant angle to loading direction and the other side FCPM is perpendicular to loading direction. Third type is that both sides FCPM of notch have slant angle to loading direction. It was considered that this kinds of phenomena were due to non-uniform distribution of SiC whisker and confirmed by SEM observation for fracture mechanism study.

액상소결한 탄화규소의 집합조직 발달에 관한 연구 (A Study on Texture Development in Liquid-Phase Sintered Silicon Carbide)

  • 성한규;조경식;박노진;최헌진;이준근
    • 한국세라믹학회지
    • /
    • 제37권4호
    • /
    • pp.320-326
    • /
    • 2000
  • Development of texture in SiC materials by hot-pressing and subsequent annealing was studied. Crystallographic texture type was characterized by measuring X-ray pole figures on the perpendicular plane to the hot-pressing direction. Observed all pole figures were nearly axially symmetric (fiber texture). In case of ${\beta}$-SiC materials, the pole density of basal plane (0004) increased as annealing time increased, in contrast, other planes (hkil) of ${\beta}$-SiC materials and all planes of ${\alpha}$-SiC materials nearly remained unchanged. In the case of ${\beta}$-SiC materials, therefore, a weak texture of (0001) plane at the normal direction took place in the 8h annealed samples, resulting from grian growth. The fracture toughness values of ${\alpha}$-SiC materials measured in both planes parallel and perpendicular to the hot-pressing direction were very similar. However, the fracture toughness of ${\beta}$-SiC materials measured parallel to the hot-pressing direction were higher than that measured perpendicular to the hot-pressing derection, relatively, because of the texture and the microstructure anisotropy.

  • PDF

DFT를 이용한 Si (001) 기판의 에피택시 NiSi 구조 연구 (Structural Study of Epitaxial NiSi on Si (001) Substrate by Using Density Functional Theory (DFT))

  • 김대희;서화일;김영철
    • 반도체디스플레이기술학회지
    • /
    • 제6권4호
    • /
    • pp.65-68
    • /
    • 2007
  • An epitaxial NiSi structure on Si (001) substrate was studied by using density functional theory (DFT). Orhorhombic and B2-NiSi structures were compared first. B2 structure was further considered as it has same crystal structure as Si and the lattice mismatch between B2 and Si is small, compared to orthorhombic-NiSi. The lattice parameters of x- and y-direction in B2-NiSi structure were modified to match with those in Si (001). The size reduction of the lattice parameter of B2-NiSi to match with that of Si increased the lattice parameter of z-direction by 10.5%. Therefore, we propose that an optimum structure of NiSi for epitaxial growth on Si (001) is a tetragonal structure.

  • PDF

LSI 공법으로 제작된 C/SiC 복합재의 압축거동 평가 (Compressive Fracture Behavior of C/SiC composite fabricated by Liquid Silicon Infiltration)

  • 윤동현;김재훈
    • 한국안전학회지
    • /
    • 제33권1호
    • /
    • pp.1-6
    • /
    • 2018
  • The effects of the fiber direction, specimen size and temperature on the compressive strength of carbon fiber reinforced silicon carbide composite (C/SiC composite) manufactured by liquid silicon infiltration(LSI) is investigated. Tests were conducted in accordance with ASTM C 695 at room temperature and elevated temperatures. Experiments are conducted with two different specimens considering grain direction. With grain (W/G) specimens have a carbon fibers parallel to the load direction, but across grain (A/G) specimens have a perpendicular carbon fibers. To verify the specimen size effect of C/SiC composite, two types of specimens are manufactured. One has a one to two ratio of diameter to height and the other has a one to one ratio. The compressive strength of C/SiC composite increased as temperature rise. As specimens are larger, compressive strength of A/G specimens increased, however compressive strength of W/G decreased.

SiCf/SiC 복합재의 마모 및 마찰에 의해 발생된 탄성파 특성 (Characteristics of Elastic Wave Generated by Wear and Friction of SiCf/SiC Composites)

  • 문창권;남기우
    • 비파괴검사학회지
    • /
    • 제34권1호
    • /
    • pp.23-30
    • /
    • 2014
  • $SiC_f$/SiC 복합재를 제작하여, $SiC_f$/SiC 복합재의 섬유배향 방향에 따르는 마모 특성을 평가하고, 마모시에 발생하는 탄성파를 검출하고 분석하였다. $SiC_f$/SiC 복합재는 섬유의 종 횡방향에 의한 마찰계수와 마모손실은 비슷하였으나, 섬유의 수직방향은 가장 작은 값을 나타내었다. 이것은 섬유의 취성 특성 때문이라 판단되며, 마모손실과 마찰계수는 정비례의 관계를 나타내었다. SiC 단상재의 탁월주파수는 58.6 kHz를 나타내고, $SiC_f$/SiC 복합재의 탁월주파수는 117.2와 136.7 kHz였다.