SHS 화학로에 의한 (Ti.W)C 복탄화물의 합성 및 기계적 특성에 관한 연구 (A Study on Synthesis and Mechanical Properties of (Ti.W)C Complex Carbide by SHS Chemical Furnace)

  • 이형복;오유근;이풍헌;장동환
    • 한국세라믹학회지
    • /
    • 제33권4호
    • /
    • pp.418-424
    • /
    • 1996
  • (Ti.W)C complex carbide was synthesized by self-propagating high temperature synthesis (SHS) chemical furnace. Attempt to find the optimal condition for synthesis of (Ti.W)C the effects of molar ratio of Ti:W:C on the synthesized powders and mechanical properties were investigated, Optimum molar ratio of these synthe-sized powder was Ti:W:C=0.7:0.2:1.0 The bulk density M,O.R Hardness Fracture toughness of (Ti.W)C complex carbide sintered at 200$0^{\circ}C$ for 60 min by hot-pressing under the pressure of 20 MPa were 7.6g/cm3, 475 MPa, 17,.7 GPa respectively.

  • PDF

SHS 화학로에 의한 (B.Si)C 복합체의 합성 및 기계적 특성에 관한 연구 (Study on Synthesis and Mechanical Properties of (B.Si)C Composite by Self Propagating High Temperature Synthesis Chemical Furnace)

  • 이형복;조덕호;이재원
    • 한국세라믹학회지
    • /
    • 제32권4호
    • /
    • pp.413-418
    • /
    • 1995
  • The (B.Si)C composite was prepared form the mixture of metal boron, silicon, and carbon powders in Ar atmosphere by Self-propagating High-temperature Synthesis Chemical Furnace. The characterization of synthesized power and sintered body were investigated. The microstructure of sintered body suggested that SiC boundary was made between B4C grains. The most excellent mechanical properties, the relative density of 95% oftheoretical value, 3 point flexural strength of 360MPa, and fracture toughness of 3.6MN/m3/2 could be obtained in 80wt% B4C-20 wt% SiC composite were obtained.

  • PDF

SHS화학로에 의한 SiC의 합성 (Synthesis of SiC by Self-Propagating High Temperature Synthesis Chemical Furnace)

  • 김도경;박성;조건;이형복
    • 한국세라믹학회지
    • /
    • 제31권11호
    • /
    • pp.1283-1292
    • /
    • 1994
  • Ultra-fine $\beta$-SiC powders were fabricated by self-propagating high temperature synthesis process (SHS) using chemical furnace. The dependences of the C powders with different surface areas, the molar ratios of C/Si, the weight ratios of chemical fuel content, and pellet diameter-size on synthesis were investigated. Compositional and structural characterization of these powders was carried out by scanning electron micrograph and X-ray diffraction. The $\beta$-SiC powders which had C/Si mole ratio=1.05, 3 times chemical fuel contents, and pellet diameter=20 mm were optimum for synthesis efficiency. By optimizing process-variables, it is possible to fabricate $\beta$-SiC powders which have little secondary phases ($\alpha$-SiC).

  • PDF

SHS of Oxide Systems Based on MCR of Quartz Modified by Organometallic Compounds

  • Soh, Dea-Wha;Tlek, Ketegenov;Z.A., Mansurov
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.666-669
    • /
    • 2002
  • The differences of the effects of mechanical substance pre-activation in the mills with divers force effect schemes on the self-propagating high temperature synthesis (SHS) of the $SiO_2$ + 37.5% Al system were investigated. The power saturation of activated material state are estimated referring on the variations of dilatometry curve paths. The effects of activation time on the temperature of sample self-ignited in the furnace, combustion temperature and completeness of the quartz reaction with aluminium were determined. The enhancing effects of organic modifiers of quartz particle surfaces on the further SHS synthesis development were shown.

  • PDF

SHS법에 의한 탄화텅스텐 분말 합성 (Synthesis of Tungsten Carbide Powders by SHS Method)

  • 전호병;조덕호;이형복;박성
    • 한국세라믹학회지
    • /
    • 제31권10호
    • /
    • pp.1159-1168
    • /
    • 1994
  • We powders were synthesized from W powders in differnet particle sizes by Self-propagating High-temperature Synthesis process (SHS) using a chemical furnace. The effects of the mole ratio of chemical fuel content, pellet thickness and the mole ratio between carbon and tungsten (C/W Ratio) on synthesis were investigated with the tungsten powders have different particle size each other. Compositional and structural characterization of these powders was carried out by scanning electron microscope (SEM0 and x-ray diffractometer. Powder characterization was carried out by the measurement of particle size distribution with laser-particle size analyzer. The amounts of WC obtained by SHS process depend very much on the particle size of tungsten powder and heat contents given in a product, i.e. as the particle size of W powder is smaller, the amounts of WC produced increase. Also the more heat contents is given, the more amounts of WC increase. By optimizing the synthesis conditions, it is possible to fabricate WC powders which have little secondary phases (W2C, C).

  • PDF

SHS 화학로에 의한 $B_4C$ 합성 및 기계적 특성에 관한 연구 (Study on Synthesis and Mechanical Properties of $B_4C$ by Self Propagating High Temperature Synthesis Chemical Furnace)

  • 이형복;조덕호;박성;이재원
    • 한국세라믹학회지
    • /
    • 제30권8호
    • /
    • pp.685-693
    • /
    • 1993
  • Boron cabride was prepared from the mixture of metal boron and graphite powders in Argon atmosphere by Self-propagating High-temperature Synthesis Chemical furnace. The most excellent mechanical properties were in the case that Fe was added as a sintering agent before the synthesis of the B4C in the Chemical furnace. Sintered B4C-5wt% Fe specimen showed the relative density of 95%, of theoretical value, and 3-point-flexural strength of 380MPa.

  • PDF

고압 자전 고온반응 합성법에 의한 B4C-Al2O3복합분말 제조 (Preparation of B4C-Al2O3 Composite Powder by Self-propagation High-temperature Synthesis(SHS) Process under High Pressure)

  • 임경란;강덕일;김창삼
    • 한국세라믹학회지
    • /
    • 제40권1호
    • /
    • pp.18-23
    • /
    • 2003
  • 정량의 B$_2$O$_3$/A1/C의 혼합분말을 화학노 대신 고압의 알곤 분위기를 사용하여 SHS 공정으로 B$_4$C-A1$_2$O$_3$ 복합분말을 제조하였다. 2B$_2$O$_3$+4A1+C=B$_4$C-2A1$_2$O$_3$의 반응식에 해당하는 B$_2$O$_3$(-100 메쉬), Al(-200 메쉬), C(-200 메쉬)의 분말을 2시간 건식 볼밀로 혼합한 후, 고온 고압의 SHS 반응기에 넣고 약 10기압의 알곤 분위기에서 점화하여 SHS을 일으켰다. 반응 생성물은 XRD 분석으로 안과 겉이 균일하게 반응이 일어났으며 반응 생성물로 화학노 사용시 동반되는 부산물 AlB$_{12}$C$_2$가 없는 B$_4$C-A1$_2$O$_3$ 복합 분말을 얻었다. 이 복합 분말은 SEM으로 보면 약 0.3~l $mu extrm{m}$ 크기의 결정이 모인 약 60~100$\mu\textrm{m}$ 크기이었다. 그러나 약 15기압을 사용하였을 때는 부분 소결이 일어나 15~25$\mu\textrm{m}$ B$_4$C 분말에 0.1~0.2$\mu\textrm{m}$의 알루미나가 분산되어 있는 고강도의 복합 분말이 생성되었다.

콘덴서용 다공성 Ta 분말의 제조 및 특성 (The Properties and Manufacture of Porous Tantalum Powder for Capacitor)

  • 이상일;이승영;원창환
    • 대한금속재료학회지
    • /
    • 제48권4호
    • /
    • pp.326-334
    • /
    • 2010
  • Porous and net-shaped tantalum powder for a capacitor was formulated in a SHS (self-propagating high-temperature synthesis) process. However, this powder, which has weak strength among its particles and low flow ability, cannot be used for a capacitor. Therefore, this powder was sintered in a high-vacuum furnace to increase agglomeration to improve the flow ability, bonding strength among the particles, and shrinkage during pellet sintering. Finally, it was deoxidated with 2 wt% Mg powder to remove the increased surface oxygen that arose during the sintering process. The final product was analyzed in terms of its chemical and physical properties and was compared with a commercial powder used by a capacitor manufacturer.

SHS법에 의한 Ti-Si계 세라믹스의 합성 및 소결체의 특성에 관한 연구 (Study on Synthesis and Sintering Characterization of Ti-Si System Ceramics by Self-Propagating High Temperature Synthesis)

  • 김도경;박성;조덕호;조건;이형복
    • 한국세라믹학회지
    • /
    • 제31권3호
    • /
    • pp.265-274
    • /
    • 1994
  • Intermetallic Ti-Si system ceramics were synthesized from stochiometric mixtures of titanium and silicone powders in vacuum by Self-propagating High-temperature Synthesis(SHS). In each cases of Ti5Si3, Ti5Si4 and TiSi, and TiSi2 synthesis, 20wt% product dilution, direct ignition and SHS chemical furnace method were employed. The combustion modes, which were observed during the synthesis process by using the high speed camera, of Ti5Si3, Ti5Si4, TiSi, and TiSi2 exhibit spin, osciallatory, steady-state, and spin combustion, respectively. With increasing Ti/Si molar ratio an decrease of combustion velocities was found. From the results on the measurement of the flexural strength, the specimen hot pressed at 135$0^{\circ}C$ for 30 min using synthesized Ti5Si4 powders showed the highest flexural strength at 215 MPa.