Kim, Kyung-Su;Kim, Sung-Chan;Shim, Chun-Sik;Park, Jin-Young;Cho, Hyung-Min
Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
/
2003.05a
/
pp.306-311
/
2003
A growing fatigue crack is known to be retarded on application of an overload cycle. The retardation may be characterized by the total number of cycles involved during retardation and the retarded crack length. The overload ratio plays an important role to influence the retardation behavior. The objective of the present investigation is to study the effect of different overload ratio on the retardation behavior. For DENT(double edge notched tension) specimens and ESET(eccentrically-loaded single edge crack tension) specimens, fatigue crack growth tests are conducted under cyclic constant-amplitude loading including a single tensile overloading with different overload ratios. The proposed crack retardation model predicts crack growth retardation due to a single tensile overloading. The predictions are put into comparison with the experimental results to confirm the reliability of this model.
Constant .DELTA.K fatigue crack growth rate experiments were performed by applying an intermediate single and multiple overload for structural steel, SM45C. The purpose of the present study is to investigate the influence of multiple overloads at various stress intensity factor ranges and the effect of statistical variability of crack retardation behavior. The normalized delayed load cycle, delayed crack length and the minimum crack growth rate are increased with increasing baseline stress intensity factor range when the overload ratio and the number of overload application were constant. The crack retardation under low baseline stress intensity factor range increases by increasing the number of overload application, but the minimum crack growth rate decreases by increasing the number of overload application. A strong linear correlation exists between the minimum crack growth rate and the number of overload applications. And, it was observed that the variability in the crack growth retardation behavior are presented, the probability distribution functions of delayed load cycle, delayed crack length and crack growth life are 2-parameter Weibull. The coefficient of variation of delayed load cycle and delayed crack length for the number of 10 overload applications data are 14.8 and 9.2%, respectively.
Transactions of the Korean Society of Mechanical Engineers
/
v.19
no.2
/
pp.451-462
/
1995
Single overload tests performed to examine the crack retardation behavior for the specimen thickness and overload ratios. Delayed crack length was tend to increase in small thickness and big overload ratio but was difference between delayed crack length and plastic zone size that expected in specimen thickness. So retardation behavior that estimated in plastic zone size, was not sufficient. Crack tip branching and striation distribution, secondary mechanisms that effected in retardation behavior, was examined by experiment and finite element analysis. Crack tip branching was affected by micro structure, and appeared the more complicatedly according to increasing damage by overload and decreasing crack driving force in base line stress level. And crack tip branching the branching angle decreased crack driving force in the crack tip. And a characteristic of the fractography on retardation zone was that striation distribution did not appear due to decreased crack driving force.
In this study, retardation behavior of fatigue crack under single overloading of the mixed mode I+II state was experimentally investigated. To produce single overload in the mixed mode I+II state, the compact tension shear (CTS) specimen and loading device were used. The propagation tests for fatigue crack were performed under mode I loading overloading afterwards. We examined the observed deformation aspects, variation of fatigue life and crack propagation rate, and the aspects of retardation behavior from tests. The retardation effect of mixed-mode single overload on fatigue crack propagation behavior was smaller than that of mode I single overload. It has been confirmed that the retardation behavior did not immediately appear and the retardation length was short when the component of mixed-mode overload was changed.
Aircraft structures and engineering structures are always subject to variable amplitude loads. Variable amplitude loads include some kind of loading history; for example, constant amplitude load, single peak overload and block overload etc. Crack growth under variable amplitude loading exhibits retardation effect. In this study, the 4 point bending fatigue test was performed by hydrolic servo fatigue testing machine on 7075-T6 Al-alloy. The retardation effect of overload ratio and numbers of overload cycle was quantitatively studied. 1) Change of retardation effect against increment of overload ratio is more evident when the multiple overload is applied than single overload is done. 2) The number of overload cycle is very important factor about the crack growth retardation effect when the overload ratio is more than 1.75; that is not when the overload ratio is less than 1.75. 3) Overload affected zone size increased gradually by increment of crack growth retardation effect. 4) Crack driving force is more greatly reduced when the crack tip branched off two direction than it sloped to one direction.
Transactions of the Korean Society of Mechanical Engineers A
/
v.29
no.6
s.237
/
pp.828-834
/
2005
Recently, injection molded plastic optical products are widely used in many fields, because injection molding process has advantages of low cost and high productivity. However, there remains residual birefringence and residual stresses originated from flow history and differential cooling. The present study focused on developing a technique to measure the birefringence in optical plastic parts using R-G-B separation of white light. The main idea of an analysis comes from the fact that more information can be obtained from the distribution of retardation caused by different wavelengths. A complete system to give the quantitative values of retardation covering high order 2-D birefringence will be demonstrated. Further investigation is under way to improve the accuracy of the system using diodes as light sources.
Proceedings of the Korean Society for Technology of Plasticity Conference
/
2004.10a
/
pp.290-293
/
2004
Recently, injection molded plastic optical products are widely used, because injection molding process has advantages of low cost and high productivity. However, there remains residual birefringence and residual stresses originated from flow history and differential cooling. The present study focused on developing a technique measuring birefringence in optical plastic parts using R-G-B separation of white light. The main idea of an analysis comes from the fact that more information can be obtained from the distribution of retardation caused by different wavelengths. A complete system to give the quantitative values of retardation covering high order 2-D birefringence will be demonstrated. Further investigation is under way to improve the accuracy of the system using diodes as light sources.
Journal of the Society of Naval Architects of Korea
/
v.40
no.3
/
pp.45-53
/
2003
Ships and ocean structures are subjected to random loads caused by irregular waves. The irregularity of amplitude from random loading affects on fatigue crack growth and fatigue life. However the effects of irregularity of loading on fatigue including random loading have not been explained exactly. Therefore in this paper crack growth tests on DENT specimens under constant-amplitude loading including a single tensile overload are conducted to investigate the effect of overload on crack growth rate. The size of plastic zone and crack growth rate before and after a single tensile overloading are measured using ESPI system. Crack growth retardation model that is characterized by crack growth length and the size of plastic zone was proposed and compared with test result. From the research, the validity of proposed model is examined on crack growth retardation, and consequently fatigue life.
Purpose : Nowadays, there are many studies of growth retardation treatment by oriental medical therapy. This study was performed to evaluate the effect of Hwalhyulsungjang-san (Huoxuechengzhang-san) and KC101 on physical development in growth, Methods : 60 young (3 weeks old) male rats, whose mean weight was $46.8{\pm}0,7g$, were divided into 5 groups : groups A, B, C, and D were fed an experimental diet containing respectively Hwalhyulsungjang-san 2.5%, Hwalhyulsungjang-san 7.5%, KC101 5.0%, and KC101 10.0%, and the other group were fed an AIN-diet containing neither Hwalhyulsungjang-san nor KC101 as a control. Study of each group used 2 rats and was repeated in 6 times. Body weight, daily weight gain, dietary intake, body length, femur length, backbone length and serum concentration of IGF-I and hemoglobin were measured. Result : 1. Body weight and daily weight gain of group D (KC101 10%) were highest; dietary intake of group D was also increased by 13% over the control group. 2. Average body length of group D was increased to 1.69cm, which was 3.2% over the control group. Backbone length of group D was also increased 4% compared to control group. 3. Serum concentration of IGF-I of group D increased 17% compared to control group. 4. Serum concentration of hemoglobin of group B (Hwalhyulsungjang-san 7.5%) increased 8% compared to control group. Conclusion : This study showed that Hwalhyulsungjang-san and KC101 composed of oriental medicinal stuffs have effect on physical development in growing rats. There were not any statistical meaning compared to control group, but this study suggests that intake of these compounds from a young age may lead to increase physical development in growth.
Journal of Advanced Marine Engineering and Technology
/
v.8
no.1
/
pp.49-63
/
1984
The 5086-H116 Al-Alloy plate specimens having an edge through-thickness notch were investigated to find out the characteristics of the corner crack propagation by the plane bending fatigue. The experiments were also carried out in order to clarify the change of the corner crack propagation behaviour due to the various materials and their thicknesses. In addition, the retardation effect of overload on the corner crack propagation was quantatively studied. Main results obtained are as follows; 1. In the case of estimating the crack propagation rate of the corner crack, it is more reasonable to consider the growth rate of fracture surface area than that of crack length. 2. The shape of the corner crack growing in the plane plate under the bending fatigue can be estimated. 3. The crack propagation rate increases with the increasing of the thickness and the decreasing of the Young's modulus of materials. 4. Regardless of a thickness and kind of materials of specimen, the characteristics of the corner crack propagation can be concluded. 5. The retardation effect of overload is distinct in the corner crack propagation.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.