분체의 종류에 따른 고유동 콘크리트의 품질성능에 관한 연구 (A study on the quality performances of the high flowing concrete for binder types)

  • 권영호;이현호;하재담
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.567-572
    • /
    • 2002
  • This research investigates experimentally an effect on the quality performances of the high flowing concrete according to binder types. The purpose of this study is to determine the optimum mix proportion of the high flowing concrete having good flowability, viscosity and no-segregation. For this purpose, two types using belite cement+lime stone powder(LSP) and furnace slag cement+lime stone powder are selected and tested by design factors including water cement ratio, fine and coarse aggregate volume ratio. As test results of this study, the optimum mix proportion for binder types is as followings. 1) One type based belite cement ; water cement ratio $51^{\circ}C$, fine aggregate volume ratio $43^{\circ}C$ and coarse aggregate volume ratio $53^{\circ}C$, replacement ratio of LSP $42.7^{\circ}C$. 2) Another type based slag cement : water cement ratio $41^{\circ}C$, fine aggregate volume ratio $47^{\circ}C$ and coarse aggregate volume ratio $53^{\circ}C$, replacement ratio of LSP $13.5^{\circ}C$.

  • PDF

13mm이하 순환 굵은골재 치환에 따른 콘크리트의 역학적 특성 및 건조수축 (Mechanical and Drying Shrinkage of Concrete Replaced with Recycled Coarse Aggregate with Less than 13mm in Size)

  • 이순재;김상섭;박용준;한동엽;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 춘계 학술논문 발표대회
    • /
    • pp.63-64
    • /
    • 2015
  • This study has analyzed mechanical and dry shrinkage properties according to the recycled coarse aggregate by nominal strength actually being widely used at the Remicon companies for the purpose of qualitative improvement of concrete, practical use and examination at various strengths. As a result, although the modulus of elasticity showed a tendency of getting decreased as the replacement ratio of recycled coarse aggregate has increased, the difference was insignificant while the compressive strength showed a tendency of about 3MPa increase in the recycled coarse aggregate replacement ratio of 30% compared to the ratio of 0%. In case of the dry shrinkage length variation ratio, the recycled coarse aggregate replacement ratio of 30% showed a tendency of about 20% shrinkage reduction compared to the ratio of 0%.

  • PDF

순환골재를 이용한 플라이애시 콘크리트의 역학적 특성 (Mechanical Properties of Recycled Aggregate Concrete Containing Fly Ash)

  • 양인환;전병관
    • 한국건설순환자원학회논문집
    • /
    • 제5권2호
    • /
    • pp.144-151
    • /
    • 2017
  • 이 연구에서는 순환굵은골재와 플라이애시를 사용한 콘크리트의 압축강도 및 탄성계수의 역학적 특성을 연구하였다. 실험변수로써 굵은순환골재의 치환율과 플라이애시 치환율을 고려하였다. 실험에서 고려된 순환굵은골재의 치환율은 0, 30, 50 및 70%이고, 플라이애시 치환율은 0, 15 및 30%이다. 실험변수에 따른 순환골재 콘크리트의 7일, 28일 및 91일 재령의 압축강도와 탄성계수 특성을 분석하였다. 플라이애시를 혼입하지 않은 콘크리트의 압축강도와 탄성계수에 비해 플라이애시 치환율이 30%인 배합의 각 재령별 압축강도와 탄성계수 감소효과는 뚜렷하게 나타난다. 따라서 순환골재콘크리트에서 30%이하 수준의 플라이애시의 혼입이 역학적 특성 측면에서 적정하다고 판단된다.

순환잔골재를 활용한 콘크리트의 물리·역학적 특성에 관한 실험적 연구 (An Experimental Study on the Physical and Mechanical Properties of Concrete Using Recycled Sand)

  • 김정호;성종현;이승엽;권구혁;이세현
    • 한국건설순환자원학회논문집
    • /
    • 제5권4호
    • /
    • pp.359-365
    • /
    • 2017
  • 본 연구에서는 KS F 2573 콘크리트용 순환골재 기준에 적합한 순환잔골재의 치환율에 따른 콘크리트 특성을 검토하였다. 물리적 특성으로 슬럼프, 공기량, 경시변화, 압축강도에 대한 연구를 수행하였으며, 순환잔골재 재활용 활성화를 위한 기초자료를 제공하고자 한다. 슬럼프 경시변화 실험 결과 순환잔골재의 치환율 증가에 따라 슬럼프 경시변화 감소율은 커지는 것으로 나타났다. 공기량 측정 결과 순환잔골재의 치환율 증가에 따라 공기량 또한 증가하는 것으로 나타났으며, 경시변화의 경우 공기량 감소율은 낮아지는 것을 확인하였다. 반면 100% 치환 시 천연골재콘크리트보다 높은 공기량을 나타내 강도저하가 발생할 것으로 사료된다. 압축강도의 실험 결과 순환잔골재 치환율 증가에 따라 강도저감이 발생했으며, 24MPa 배합 결과 30% 치환 시 천연골재콘크리트와 동등한 강도발현을 나타냈다. 위의 결과를 토대로 순환잔골재 30%치환 시 천연골재콘크리트와 동등한 물리적 특성을 나타내 KS F 2573 콘크리트용 순환골재 기준에 적합한 순환잔골재 치환 시 목표강도 24MPa의 30%가 적합한 것으로 판단된다. 추후 순환골재의 사용 활성화를 위해 순환잔골재 개질을 통한 품질개선이 필요하며, 후속연구로서 개질된 순환잔골재를 이용한 순환잔골재콘크리트의 물리적 특성 평가가 수행되어야 할 것으로 판단된다.

폐내화물 골재 치환율이 고로슬래그 미분말과 순환골재 사용 모르타르의 품질에 미치는 영향 (Influence of Replacement Ratio of Wasted Refractory Aggregate on the Properties of Mortar using Blast Furnace Slag and Recycled Aggregate)

  • 송원루;문병룡;김민상;이제현;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 춘계 학술논문 발표대회
    • /
    • pp.139-140
    • /
    • 2016
  • In this research, the possibility of wasted refractory aggregate pulverized from refractory block as an expansive admixture and additional alkaline stimulant for class two and three blast furnace slag cements (BSC) was assessed with its high content of free CaO or free MgO. As the replacement ratios of wasted refractory powder and blast furnace slag were increased, flow and air content were decreased, while unit volume weight was increased under same conditions. Compressive strength of mortar was increased with increased replacement ratio of wasted refractory powder, especially, in the case of class three BSC, the highest compressive strength was obtained when wasted refractory aggregate was replaced 2%.

  • PDF

잔골재 종류 및 치환율에 따른 저탄소 무기결합재의 유동 및 강도특성 (Flowing and Strength Properties of Low Carbon Inorganic Composite Depending to Fine Aggregate Types and Replacement Ratio)

  • 박종필;배상우;이윤성;이강필;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 추계 학술논문 발표대회
    • /
    • pp.235-236
    • /
    • 2011
  • This study analyzed flowing and strength properties of mortar depending to fine aggregate types and replacement ratio by using blast furnace slag, red mud, and silica fume that are industrial by products. The findings showed that higher replacement level of fine aggregate increased air content while decreased table flow. In addition, compressive strength showed that the higher replacement level was regardless of fine aggregate types, the lower strength became. Mortar substituted by the dredged sand showed high strength.

  • PDF

프리팩트 폴리머 시멘트 콘크리트용 주입 폴리머 시멘트 모르터의 성질에 관한 연구 (A Study on Basic Properties of Grouting Motars for polymer-Modified preplaced Aggregate Concrete)

  • 이철웅;김완기;조영국;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표논문집(II)
    • /
    • pp.350-355
    • /
    • 1998
  • Preplaced aggregate concrete in the building fields has recently been used in the partial repair works for damaged reinforced concrete structures, and polymer-modified mortars have been employed as grouting mortars for the preplaced aggregate concrete. The objective of this study is to clear the properties of polymer-modified grouting mortars. Polymer-modified mortars using a polystyrene acrylic(St/Ac) emulsion as grouting mortars for preplaced aggregate concrete are prepared with various mix proportions, and tested for flexural and compressive strengths, adhesion in tension. The flexural strength of emulsion-modified grouting mortars does not give much variation with increasing fly ash replacement for cement and sand-binder ratio. With increasing polymer-binder ratio, the flexural strength and adhesion in tension of St/Ac emulsion-modified grouting mortars increases, become nearly constant or reaches a maximum at a polymer-binder ratio of 5%. From the test results, St/Ac emulsion-modified grouting mortar with a polymer-binder ratio of 5%, a fly ash replacement of 10% for cement and sand-binder ratio of 1.0 is recommended as a grouting mortar for preplaced aggregate concrete.

  • PDF

킬른더스트를 사용한 콘크리트의 공학적 특성에 관한 연구 (A Study on the Engineering Properties of Concrete Using Cement Kiln Dust)

  • 김기정;황인성;차천수;김성수;한천구
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.267-270
    • /
    • 2003
  • This study is intended to investigate the engineering properties of concrete, in which cement and fine aggregate are replaced with cement kiln dust(CKD), such as the properties of fresh concrete and hardened concrete and hydration heat history, for effective using method of CKD, a by-product produced in the process of making cement. According to the results, as the replacing ratio of CKD increases, slump and air content of concrete decreases remarkably due to an increase of viscosity and filling of the pores. As the properties of setting, initial and final setting time are shortened with an increase of the replacing ratio of CKD, and as the replacement of CKD for fine aggregate increases, setting time is shortened more greatly. Compressive strength increases due to filling of the pores and reduction of air content in comparison with plain concrete. When the replacement ratio of CKD for cement is 10% and 15%, peak temperature of hydration heat lowers slightly, but it goes up in the case of replacement of CKD for fine aggregate. Also, when cement and fine aggregate is replaced with CKD by 2.5% and 7.5% respectively(1C3S) in the case of replacement of CKD for cement and fine aggregate, it is highest.

  • PDF

가네트를 활용한 고강도 콘크리트의 건조수축 특성 연구 (A Study on Drying Shrinkage of the High-Strength Concrete using the Garnet)

  • 장주영;윤요현;박정민;김화중
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 춘계 학술발표회 제16권1호
    • /
    • pp.676-679
    • /
    • 2004
  • In this study, we considered the characteristic of drying shrinkage from age of high strength concrete with garnet minute powder to be industry by-product. The factors of experiment are unit water content$(160kg/m^3)$, water-binder ratio(30, $35\%$), fine aggregate ratio(40, 42, $44\%$), admixture replacement ratio(0, 10, $20\%$), admixture type(garnet minute powder, fly ash, blast-furnace slag). We make a comparative study of shrinkage about concrete with a passage of age(1, 3, 7, 14, 28, 56, 91 days). As a result of experiment, we reach a conclusion as follow. In the same mix condition, as unit water content and fine aggregate ratio go up, the drying shrinkage ratio increase. In the drying shrinkage ratio according to admixture replacement ratio, it goes up when admixture replacement Ratio increase in case of fly ash and blast-furnace slag. But, drying shrinkage ratio decrease when admixture replacement ratio increase in case of garnet minute powder.

  • PDF

콘크리트용 굵은 골재로서 염색공단 열원 폐재의 적용성에 관한 연구 (A Study on Application of Dyeing Industrial Heat Source Waste Aggregate as Concrete Aggregate)

  • 윤장길;김효열;임남기
    • 한국건축시공학회지
    • /
    • 제5권1호
    • /
    • pp.123-129
    • /
    • 2005
  • This study is as a part of the new disposal and recycling plans of heat-resource waste of Daegu dyeing industrial center we tried to examine applicable possibility of crushed thing(waste aggregate) as aggregates for mortar and concrete. To examine applicable possibility of waste aggregate as a lightweight-aggregate for concrete and mortar, we carried this study by mainly property examination of concrete according to replacement ratio of waste aggregate. We carried slump, unit weight, compressive strength and bending strength test according to replacement ratio of waste aggregate. As the result of that, if we use waste aggregate, lightweight of concrete and mortar will be possible. Specially it shows a strength improvement effect of cement hardening according to using this so it is judged that applicable possibility as aggregate for concrete and mortar is very excellent.