• Title/Summary/Keyword: Red phosphor$(Y,Gd)_2O_3$

Search Result 26, Processing Time 0.026 seconds

Improved methods for the preparation of $(Y_{1-x}Eu_x)_2O_3$:MX and $(Y_{1-x-y}Gd_xEu_y)_2O_3$:MX as red phosphor materials

  • Lee, You-Hui;Han, Sang-Do;Kim, Jung-Duk;Chang, Mi-Yeon;Singh, Ishwar.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2004.08a
    • /
    • pp.715-718
    • /
    • 2004
  • Substantially improved methods for the preparation of europium-doped yttrium oxide red phosphor with the inclusion of alkali metal halides having a general formula $(Y_{1-x}Eu_x)_2O_3$:MX where 0.025${\leq}$x${\leq}$0.2 and MX is alkali halide in the mole ratio 0.025 to 0.6, more preferably between 0.05 to 0.2 mole, are reported. Another series of the red phosphor materials with general formula $(Y_{1-x-y}Gd_xEu_y)_2O_3$:MX where 0.05${\leq}$x${\leq}$0.40 and 0.025${\leq}$y${\leq}$0.20 and MX is alkali halide in the mole ratio 0.025 to 0.5, more preferably between 0.1 to 0.2 mole, has also been presented. The inclusion of alkali halide greatly increase the luminance of the materials. The materials are very soft with fine particle size less than 100nm. The phosphorescent materials have good luminance in VUV region.

  • PDF

Degradation of PDP Phosphors Under VUV Excitation (PDP 형광체의 진공 자외선 조사에 따른 열화 특성)

  • Lee, R.Y.;Lee, S.H.;KIm, Y.H.
    • Korean Journal of Materials Research
    • /
    • v.12 no.9
    • /
    • pp.735-739
    • /
    • 2002
  • $(Y,Gd)BO_3$: Eu, $Zn_2$$SiO_4$ : Mn and $BaMgAl_{10}$ $O_{17}$ : Eu phosphors used in PDP were continuously irradiated by vacuum ultra violet generated from the penning gas (96%Ar+4%Xe) discharge and then the change of emitting intensity with time was investigated. The brightness of these phosphors decreased exponentially with VUV excitation time. The experimental data showed that the degradation rate increased in the order of $Zn_2$$SiO_4$ : Mn>(Y,Gd)$BO_3$: Eu>$BaMgAl_{10}$ $O_{17}$ : Eu phosphor. This different degradation property of phosphors was interpreted in terms of brightness saturation and stability against VUV irradiation. It was found that the degradation property of $(Y,Gd)BO_3$ : Eu red phosphor synthesized by ultrasonic thermal spray was superior to commercial phosphor.

Photoluminescence Characteristic of Gallate-Based Red Emitting Phosphors with High Color Purity (색순도가 우수한 갈륨 산화물계 적색 형광체의 광발광 특성)

  • Kim, Kyoung-Un;Choi, Sung-Ho;Jung, Ha-Kyun;Nahm, Sahn
    • Korean Journal of Materials Research
    • /
    • v.18 no.3
    • /
    • pp.159-162
    • /
    • 2008
  • $Eu^{3+}$-activated $R_3GaO_6$ (R = Y, Gd) phosphors were prepared in a conventional solid-state reaction and their optical properties were investigated. These compounds exhibit strong red emission under light excitation at 254 nm. The emission spectra are dominated by peaks appearing around 610-630 nm that are induced by the electric dipole transition of $^5D_0\;{\rightarrow}\;^7F_2$ of $Eu^{3+}$. In addition, the appropriate CIE (Commission Internationale de l'clairage) chromaticity coordinates, (x = 0.656, y = 0.336) for $Y_3GaO_6$ and (x = 0.655, y = 0.334) for $Gd_3GaO_6$, become closer to the NTSC (National Television System Committee) standard values. With the optimized activator concentrations, the maximum emission brightness is approximately 80% of $Y_2O_3$:$Eu^{3+}$ typical red-emitting phosphor with improved color purity under an excitation condition of 254 nm.

Synthesis of $Eu^{3+}$ activated $LnAlO_{3}$(Ln=Y and Gd) Phosphors by combusition method (연소법에 의한 $LnAlO_{3}$(Ln=Y and Gd):$Eu^{(3+)}$ 형광체의 합성)

  • Khatkar, S.P.;Taxak, V.B.;Han, Sang-Do;Kim, Byeong-Kwon;Jung, Young-Ho;Park, Jo-Yong;Liang, Y.;Myung, Kwang-Shik
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.116-119
    • /
    • 2002
  • A different route to the synthesis of $Eu^{3+}$ - activated matrices such as $YAlO_{3}$ and $GdAlO_{3}$ and luminiscent properties of these compounds, were studied. The new route (Combustion method) consist of the redox reactions between the respective metal nitrates and urea in a preheated furnace at ${500^{\circ}C}$. The Phosphor thus obtained were then heated at ${1000^{\circ}C}$ for 2-3 hours to get better luminiscent properties. The incorporation of $Eu^{3+}$ activator in these phosphors were checked by luminiscence investigations. Scanning electron microscopy (SEM) studies were carried out to understand surface morphological features and the particle size. X-ray energy dispersive analysis (EDAX) was also performed for the qualitative analysis of the phosphors.

  • PDF

Search for new phosphors for flat panel displays and lightings using combinatorial chemistry and computational optimization

  • Sohn, Kee-Sun;Jung, Yu-Sun;Cho, Sang-Ho;Kulshreshtha, Chandramouli
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2006.08a
    • /
    • pp.33-38
    • /
    • 2006
  • An evolutionary optimization process involving genetic algorithm and combinatorial chemistry was employed in an attempt to develop titanate-based red phosphors suitable for tri-color white light emitting diodes We screened a eight-cation oxide system including $(K,Li,Na)_x(Y,Gd,La,Eu)_yTi_zO_{\delta}$ in terms of luminescent efficiency. The combination of genetic algorithm and combinatorial chemistry was proven to enhance the searching efficiency when applied for phosphor screening. As a result, the composition was optimized to be $(Na_{0.92}Li_{0.08})(Y_{0.8}Gd_{0.2})TiO_4:Eu^{3+}$, The luminance of this phosphor was 110 % of that of well-known scheelite variant phosphor at an excitation of 400 nm.

  • PDF

Luminescence Characteristics of Y2-xGdxO3:Eu3+ Thin film Grown by Pulsed Laser Ablation (PLD 방법으로 Si(100) 기판위에 증착한 Y2-xGdxO3:Eu3+/ 박막의 형광특성)

  • 이성수
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.1
    • /
    • pp.112-117
    • /
    • 2004
  • $Y_2$$_{-x}$G $d_{x}$ $O_3$:E $u^{3+}$(x=0.0, 0.3, 0.6, 1.0, 1.4) luminescent thin films have been grown on Si (100) substrates using pulsed laser deposition. The films grown under different deposition conditions have been characterized using microstructural and luminescent measurements. The crystallinity, the surface morphology and photoluminescence (PL) of the films are highly dependent on the amount of Gd. The photoluminescence (PL) brightness data obtained from $Y_2$$_{-x}$G $d_{x}$ $O_3$:E $u^{3+}$ films grown under optimized conditions have indicated that Si (100) is one of promised substrates for the growth of high quality $Y_2$$_{-x}$G $d_{x}$ $O_3$:E $u^{3+}$ thin film red phosphor. In particular, the incorporation of Gd into $Y_2$ $O_3$ lattice could induce a remarkable increase of PL. The highest emission intensity was observed with $Y_{1.35}$G $d_{0.60}$ $O_3$: $E^{3+}$, whose brightness was increased by a factor of 1.95 in comparison with that of $Y_2$ $O_3$:E $u^{3+}$ films.3+/ films.films.lms.

Synthesis and Luminescent Properties of $RE^3+(Eu^3+\;and\;Tb^3+$) Ions Activated CaGd4O7 Novel Phosphors

  • Pavitra, E.;Raju, G.Seeta Rama;Ko, Yeong-Hwan;Yu, Jae-Su
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.08a
    • /
    • pp.359-359
    • /
    • 2012
  • Trivalent rare-earth ($RE^{3+}=Eu^{3+}\;and\;Tb^{3+}$) ions activated $CaGd_4O_7$ phosphors were synthesized by a sol-gel process. After annealing at $1,500^{\circ}C$, the XRD patterns of the phosphor confirmed their monoclinic structure. The photoluminescence excitation spectra of $Eu^{3+}$ and $Tb^{3+}$ doped $CaGd_4O_7$ phosphor shows the broad-band excitations in the shorter wavelength region due to charge transfer band of completely filled $O^{2-}$ to the partially filled $Eu^{3+}$ ions and f-d transitions of $Tb^{3+}$ ions, respectively. The photoluminescence spectra show that the reddish-orange ions and green emission for $Eu^{3+}$ and $Tb^{3+}$ ions, respectively. Owing to the importance of thermal quenching property in the technological parameters, the temperature-dependent luminescence properties of these phosphors were measured for examing the suitability of their applications in the development of light emitting diodes (LEDs). In addition to those measurements, the cathodoluminescence properties were examined by changing the acceleration voltage and filament current. The calculated chromaticity coordinates of these phosphors were close proximity to those of commercially available phosphors for LED and field emission display devices.

  • PDF

Upconversion luminescence from poly-crystalline Yb3+, Er3+ co-doped NaGd(MoO4)2 by simple solid state method (Er3+, Yb3+ 이온이 동시 도핑된 NaGd(MoO4)2의 업컨버젼 분석)

  • Kang, Suk Hyun;Kang, Hyo Sang;Lee, Hee Ae;Shim, Kwang Bo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.26 no.4
    • /
    • pp.159-163
    • /
    • 2016
  • Up-conversion (UC) luminescence properties of polycrystalline $Er^{3+}/Yb^{3+}$ doped $NaGd(MoO_4)_2$ phosphors synthesized by a simple solid-state reaction method were investigated in detail. Used to 980 nm excitation (InfraRed area), $Er^{3+}/Yb^{3+}$ co-doped $NaGd(MoO_4)_2$ exhibited very weak red emissions near 650 and 670 nm, and very strong green UC emissions at 540 and 550 nm corresponding to the infra 4f transitions of $Er^{3+}(^4F_{9/2},\;^2H_{11/2},\;^4S_{3/2}){\rightarrow}Er^{3+}(^4I_{15/2})$. The optimum doping concentration of $Er^{3+}$, $Yb^{3+}$ for highest emission intensity was determined by XRD and PL analysis. The $Er^{3+}/Yb^{3+}$ (10.0/10.0 mol%) co-doped $NaGd(MoO_4)_2$ phosphor sample exhibited very strong shiny green emission. A possible UC mechanism for $Er^{3+}/Yb^{3+}$ co-doped $NaGd(MoO_4)_2$ depending on the pump power dependence was discussed.