A Special Pre-Service-Inspection Using Radiographic Testing(RT) for Brazing Fitting Uused in Aircraft Hydraulic System

  • Kim, Gyu-Ho
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.30 no.3
    • /
    • pp.271-281
    • /
    • 2010
  • Brazing fitting which is one of the aircraft hydraulic power system components is widely used for saving weight and achieving higher reliability. Any inherent defects or damage of fitting can cause system failure and/or physical damage of human body due to highly pressurized fluid. Radiographic testing(RT) technique and additional micro-structure investigation on cut-away surfaces have been accomplished to find out some defect-like-inhomogeneity in the fittings. The radiography results showed that some defect-like-inhomogeneity existed inside body. Additional micro-structure investigation on cut-away surface reveals that the inhomogeneity is due to internal voids. In this study, it can be is said that RT technique can be a useful tool for field acceptance test of hydraulic brazing fitting in short time.

Comparative Reliability of Nondestructive Testing for Weld: Water Wall Tube in Thermal Power Plant Boiler Case Study (용접부 비파괴 검사의 신뢰성 비교: 화력 발전소의 보일러 수냉벽 배관 사례연구)

  • Choi, Chang Deok;Lim, Ik Sung
    • Journal of Applied Reliability
    • /
    • v.18 no.3
    • /
    • pp.240-249
    • /
    • 2018
  • Purpose: The purpose of this research is to find which technique, between the PAUT (Phased array ultrasonic test) that has been used widely in practice and RT (Radiographic test) that was used widely in the past, has the higher reliability as a non-destructive testing of welding points in water wall tubes. Methods: To evaluated the reliability of non-destructive testing, eleven test pieces that were fabricated intentionally, which have the most frequently occurred defect types in water wall tubes and then both the PAUT and RT were performed on those eleven test pieces to compare their reliability. Results: The differences of type of defect, length are occurred due to the characteristics of nondestructive testing. The RT could not detect the lack of fusion defect type in specimen #4 and #8 while PAUT could not detect the lateral crack and 1 mm size small porosity in specimen #11. Conclusion: It is concluded that applying both the RT and PAUT result the best reliability rather than applying only one test method, if it is possible, in nondestructive testing of weld water wall tube in thermal power plant boiler case.

Study on the Image Quality Comparison between in Digital RT and Film RT (용접부에 대한 디지털 방사선투과영상과 필름 방사선투과영상의 상질 비교에 관한 연구)

  • Park, Sang-Ki;Ahn, Yean-Shik;Gil, Doo-Song
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.31 no.4
    • /
    • pp.391-397
    • /
    • 2011
  • Conventional film radiographic test has been generally and widely used in the inspection on the weldment for quality assurance. On the other hand, since the analog RT is well known for typical time and cost consuming method with complex process of inspection, the industry has researched various ways how to improve radiographic test technology. In this study, we verified the fact that digital RT provides a lot more benefit in effectively detecting defects, ever film details, through digital processing of image enhancement, compared to film RT. As a result, we reached conclusion that digital RT is positively able to replace the film RT in industry in part or in whole.

Development of Inspection System for Aluminum Castings with X-Ray TDI Camera (X-Ray TDI Camera를 이용한 알루미늄 주강품 검사장치 개발)

  • Nam, Mun-Ho;Park, Seong-Wook;Kim, Chang-Ho;Chung, Chan-Soo
    • Proceedings of the KIEE Conference
    • /
    • 2011.07a
    • /
    • pp.1734-1735
    • /
    • 2011
  • In case of inspection on aluminum castings, traditional RT (Radiographic Testing) method have been utilized for its advantages in interpretation, cost and perpetual storage. But it has disadvantages like time consumption in film processing, low efficiency in storage and environmental pollution. In this thesis, a DRS (Digital Radiography System) utilizing X-Ray TDI Camera (Time Delay and Integration Camera) is developed. Inspections on aluminum castings are performed using the developed Digital Radiography System, DRS and reviewed if newly developed system can substitute for the traditional method.

  • PDF

Method of Radiographic Testing and Industrial Application (방사선 투과검사의 방법과 산업적용)

  • Lee, Yong
    • Journal of Welding and Joining
    • /
    • v.12 no.4
    • /
    • pp.35-40
    • /
    • 1994
  • 비파괴검사(NDT)란 시험품에 손상을 주지 않고 내.외부에 존재하는 불연속부(결함)을 찾아내는 방법으로 다음과 같이 그 종류를 분류할 수 있다. (1) 표면결함 검출을 위한 비파괴검사 - 육안검사(VT) : 확대경 등에 의한 치수, 형상확인 - 자분탐상검사(MT) : 강자성체에 적용, 표면(하) 결함검출 - 침투탐상검사(PT) : 금속, 비철금속에 적용, 표면개구 결함검출 - 와류탐상검사(ET) : 도체 표층부(봉, 관 등) (2) 내부결함 검출을 위한 비파괴검사 - 방사선 투과검사(RT) : 결함의 종류, 형상의 판별 우수 - 초음파 탐상검사(UT) : 균열 등 면상 결함검출 등 우수 (3) 기타 비파괴검사 - Strain 측정 : 안전성 평가 - 음향방출시험(AET) - 누설시험(LT) - 중성자 방사선시험(NRT) 이상에서 보는 바와 같이 여러 종류의 비파괴검사가 있으나, 그 중에서 용접부에 적용되는 가장 일반적인 검사방법인 방사선 투과검사에 대해 기술하고자 한다.

  • PDF

Evaluation of the Integrity of TIG Welding Using Non-Contact SH-EMAT (비접촉 SH-EMAT을 이용한 TIG용접부 건전성 평가)

  • Park, Tae Sung;Park, Yeong Hwan;Park, Ik Keun
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.25 no.1
    • /
    • pp.48-53
    • /
    • 2016
  • An EMAT can be used to reliably detect defects as it serves as a non-contact transducer with the ability to transmit ultrasonic waves into specimens without couplant. Moreover, an EMAT can easily generate desired waves by altering the design of the coil and magnet. This study proposes an SH-EMAT to evaluate the integrity of the TIG welding part. A stainless steel was welded using the TIG welding method. The welding current was varied to create artificial defects. Both the PA-UT and the RT were applied to verify the defect size. The experimental results generated by using the EMAT were compared with those methods. The amplitude was observed to decrease with an increase in the defect size. These results confirmed that the presence of defects can be reliably detected by attenuation of signal amplitude. The results demonstrated that the proposed method is suitable for evaluating the integrity of TIG welding.

Derivation of External Exposure Characteristics of Industrial Radiography Based on Empirical Evidence

  • Cho, Junik;Kim, Euidam;Kwon, Tae-Eun;Chung, Yoonsun
    • Journal of Radiation Protection and Research
    • /
    • v.47 no.2
    • /
    • pp.93-98
    • /
    • 2022
  • Background: This study aims to derive the characteristics of each work type for industrial radiography based on empirical evidence through expert advice and a survey of radiation workers of various types of industrial radiography. Materials and Methods: According to a Korean report, work types of industrial radiography are classified into indoor tests, underground pipe tests, tests in a shielded room (radiographic testing [RT] room test), outdoor field tests, and outdoor large structure tests. For each work type, exposure geometry and radiation sources were mainly identified through the expert advice and workers' survey as reliable empirical evidence. Results and Discussion: The expert advice and survey results were consistent as the proportion of the work types were high in the order of RT room test, outdoor large structure test, underground pipe test, outdoor field test, and indoor test. The outdoor large structure test is the highest exposure risk work type in the industrial radiography. In most types of industrial radiography, radiation workers generally used 192Ir as the main source. In the results of the survey, the portion of sources was high in the order of 192Ir, X-ray generator, 60Co, and 75Se. As the exposure geometry, the antero-posterior geometry is dominant, and the rotational and isotropic geometry should be also considered with the work type. Conclusion: In this study, through expert advice and a survey, the external exposure characteristics for each work type of industrial radiography workers were derived. This information will be used in the reconstruction of organ dose for health effects assessment of Korean radiation workers.

A Study on the Feasibility of Lead(II) Iodide and Gd2O2S:Tb Overlapping Sensors in Gamma Source Conditions using FLUKA Simulation (FLUKA 전산 모사를 통한 감마선원 조건에서의 요오드화납(II)과 Gd2O2S:Tb가 결합된 센서의 적용가능성 연구)

  • Yang, Seung-Woo;Park, Yoon-Hee;Park, Ji-Koon;Heo, Ye-Ji
    • Journal of the Korean Society of Radiology
    • /
    • v.16 no.4
    • /
    • pp.381-386
    • /
    • 2022
  • Non-Destruction Test (NDT) is a method to check internal defects without destroying the product. Among them, radiographic testing (RT) uses high-energy radiation, so it is very important to prevent radiation exposure of workers. Therefore, in this study, in this study, a radiation sensor structure that improves radiation detection performance compared to the existing PbI2 and can immediately detect accidents in RT was presented. For evaluation, the conversion efficiency was analyzed in the gamma ray source through FLUKA simulation. PbI2 with overlapping Gd2O2S:Tb presented in this study showed a higher radiation sensitivity from 1.22 to 3.22 times than that of non-overlapping PbI2. This indicates that the presented sensor is suitable for use as a radiation sensor for source detection in RT.

Development of Welding Quality Monitoring Method for TIG Cladding (TIG클래딩 공정에 대한 품질 모니터링기법의 개발)

  • Cho, Sang Myung;Son, Min Su;Park, Jung Hyun
    • Journal of Welding and Joining
    • /
    • v.31 no.6
    • /
    • pp.90-95
    • /
    • 2013
  • Pipe inside clad welding is mainly used to the flow pipe of sub-sea or chemical plant. For the inside clad welding to the medium pipe with the diameter of about 12", TIG welding is frequently applied with filler metal. In this case, the clad welding has the very broad weld area over $10m^2$. And, the non-destructive test (NDT) such as ultrasonic test (UT) or radiographic testing (RT) should be conducted on the broad weld area, and it costs very high due to the time-consuming work. Therefore, the present study investigated the variation of arc voltage to develop the in-line quality monitoring system for the pipe inside TIG cladding. The 4 experimental parameters (current, arc length, wire feed position, and shield gas flow rate) varied to observe the change of arc voltage and to establish the model for the monitoring. The arc voltage was decreased when the wire was fed to the backward eccentric position(over 2mm), and the shield gas flow rate was insufficient under 10L/min. In the case of the backward eccentric position over 2mm, the bead appearance was not good and the dilution ratio was increased due to deep penetration. When the shield gas flow rate was lower than 10L/min, the bead surface was oxidized.

Usefulness of Tuberculin Skin Test by Tuberculin PPD RT23 2 TU (Tuberculin PPD RT23 2 TU를 이용한 투베르쿨린 피부반응 검사의 의의)

  • Yang, Jong-Wuk;Jeon, Man-Jo;Kim, Sung-Jung;Lee, Hyang-Lim;Lee, Seung-Jun;Lee, Myoung-Goo;Kim, Dong-Gyu;Park, Myoung-Jae;Kang, Min-Jong;Hyoen, In-Gyu;Jung, Ki-Suck
    • Tuberculosis and Respiratory Diseases
    • /
    • v.53 no.4
    • /
    • pp.401-408
    • /
    • 2002
  • Background : Tuberculin skin test is a method to examine M. tuberculosis infection and has been used all over the world. But various factors make it difficult to understand testing results. In 2000, the American Thoracic Society recommended that skin test results should be decided by considering risk factors of the tested. In Korea, high tuberculosis infection rate and BCG vaccination rate make it difficult to differentiate current infection, past infection, and no infection by the skin test. This study was attempted to examine a negative predictive value of the skin test to understand how the skin test acts on deciding administration of anti-tuberculosis drug. Methods : From Mar. 1 to Jul. 31 in 2001, the test was performed for patients hospitalized in Department of Internal Medicine, Hallym University College of Medicine, Chunchon, Korea by administering Tuberculin PPD RT23 2 TU (0.1 ml)to them that has been currently used in Korea based on Mantoux method. They were decided to be infected with tuberculosis bacilli by following diagnostic standard: 1) tuberculosis bacilli was cultured in sputum by microbiological diagnostic standard or Acid-fast bacilli was proven on a microscopic examination or 2) tuberculosis bacilli was not proven in the aforesaid microbiological test by clinical diagnostic standard, while there was opinion or symptom suitable for tuberculosis by radiographic or histological standard so the doctor decided to apply the tuberculosis treatment. Results : In this study, total 210 patients except 20 patients (8.7%) among 230 hospitalized patients were evaluated. Their average age was 60±16.8 years, and male-female rate was 1.28 : 1 (male: 118, female: 92). Number of patient, who was diagnosed and decided as tuberculosis, was 53(25.2%). Pulmonary tuberculosis was found in 45 patients (84.9%); 22 patients were decided to be positive in the Acid-fast bacilli smear test by microbiological examination (culture positive: 13, culture negative: 9), and 23 patients were decided to be tuberculosis patients by clinical diagnosis standard. Tuberculosis pleuritis was found in 8 patients (15.1%); 4 patients were diagnosed and decided by histological standard, and 4 patients were decided and treated by clinical standard. In differentiating patients into 'Negative' and 'Positive' by the skin test standard of the American Thoracic Society, negative predictive value 92.3%, positive predictive value 47.3%, sensitivity and specificity were 83%, 68.8%, respectively. Conclusion : In hospitalized respiratory patients, there was high negative predictive vlaue 92.3% by tuberculin skin test, therefore skin test would be a important factor for deciding administration of anti-tuberculosis drug on negative skin test patient.