• Title/Summary/Keyword: Quality Restoration Agent

Search Result 5, Processing Time 0.021 seconds

A Study on the Performance Restoration of Deteriorated Concrete by Long Distance Delivery (장시간 운반에 따라 저하된 콘크리트의 품질회복에 관한 연구)

  • Pei Chang-Chun;Jin Hu-Lin;Hwang Yin-Seong;Lee Hyung Won;Yang Seong-Hwan;Han Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • v.y2004m10
    • /
    • pp.7-10
    • /
    • 2004
  • This paper investigated the possibility of quality restoration of deteriorated concrete caused by long distance delivery using chemical admixtures such as superplasticizer. AE agent and retarding agent. According to test results, long distance delivery lead to reducing fluidity and air content markedly, while setting time accelerated. Quality restoration agent(QRA) was made by combining super- plasticizer. AE agent and retarding agent with the proportion of 1:0.0025:0.1. It was confirmed that deteriorated concrete achieved quality restoration with the level of target slump, air content and setting time without strength loss when using QRA with proper amount.

  • PDF

The effect of the gold based bonding agents on the bond between Ni-Cr alloys and ceramic restorations (Ni-Cr합금과 도재간의 결합력에 gold-based bonding agent가 미치는 영향)

  • Lee, Jung-Hwan;Joo, Kyu-Ji
    • Journal of Technologic Dentistry
    • /
    • v.29 no.2
    • /
    • pp.213-223
    • /
    • 2007
  • The success of a porcelain fused to metal (PFM) restoration depends upon the quality of the porcelain-metal bond. The adhesion between metal substructure and dental porcelain is related to the diffusion of oxygen to the reaction layer formed on cast-metal surface during firing. The purposed of this investigation was to study the effects of gold based bonding agent on Ni-Cr alloy-ceramic adhesion between porcelain matrix, gold based bonding agent and metal substructure interface. gold based bonding agent have been applied as an intermediate layer between a metal substructure and a ceramic coating. gold based bonding agent(Aurofilm NP, Metalor, Swiss) was applied on Ni-Cr alloy surface by four method. Surfaces only air abraded with 110${\beta}\neq$ Al2O3 particles were used as control. metal ceramic adhesion was evaluated by a biaxial flexure test(N=5) and volume fraction of adherent porcelain was determined by SEM/EDS analysis. Result of this study suggest that the layering sequence of gold based bonding agent is very important and can improve porcelain adherence to PFM.

  • PDF

Schisantherin B Improves the Pathological Manifestations of Mice Caused by Behavior Desperation in Different Ages-Depression with Cognitive Impairment

  • Xu, Mengjie;Xiao, Feng;Wang, Mengshi;Yan, Tingxu;Yang, Huilin;Wu, Bo;Bi, Kaishun;Jia, Ying
    • Biomolecules & Therapeutics
    • /
    • v.27 no.2
    • /
    • pp.160-167
    • /
    • 2019
  • Depression is a major mood disorder. Abnormal expression of glial glutamate transporter-1 (GLT-1) is associated with depression. Schisantherin B (STB) is one bioactive of lignans isolated from Schisandra chinensis (Turcz.) Baill which has been commonly used as a traditional herbal medicine for thousands of years. This paper was designed to investigate the effects of STB on depressive mice induced by forced swimming test (FST). Additionally, we also assessed the impairment of FST on cognitive function in mice with different ages. FST and open field test (OFT) were used for assessing depressive symptoms, and Y-maze was used for evaluating cognition processes. Our study showed that STB acting as an antidepressant, which increased GLT-1 levels by promoting PI3K/AKT/mTOR pathway. Although the damage is reversible, short-term learning and memory impairment caused by FST test is more serious in the aged mice, and STB also exerts cognition improvement ability in the meanwhile. Our findings suggested that STB might be a promising therapeutic agent of depression by regulating the GLT-1 restoration as well as activating PI3K/AKT/mTOR pathway.

The Effect of a Au Based Bonding Agent Coating on Non-Precious Metals-Ceramic Bond Strength (비귀금속 합금에 적용한 Au Based Bonding Agent가 금속-도재 결합에 미치는 영향)

  • Lee, Jung-Hwan;Ahn, Jae-Seok
    • Journal of dental hygiene science
    • /
    • v.9 no.4
    • /
    • pp.405-412
    • /
    • 2009
  • The purpose of this study investigated the effect of Au coating on adhesion between porcelain matrix and metal substructure interface. Titanium, Ni-Cr alloy and Co-Cr alloy are well known as proper metal for the dental restorations. The success of a porcelain fused to metal (PFM) restoration depends upon the quality of the porcelain-metal bond. However, adhesion between dental alloys and porcelain is related to diffusion of oxygen during ceramic firing. The excessive oxidized layers make hard adhesion between dental alloy and ceramic. Ni-Cr and Co-Cr specimens were divided into test and a control group and Titanium specimens were divided into three test groups and a control group. Each group had 20 specimens. The adhesion characteristics of porcelain and metal with Au coating layer and without Au coating layer were observed with scanning electron microscopy(SEM). The adhesion was evaluated by a biaxial flexure test and volume fraction of adherent porcelain was determined by SEM/EDS analysis. Result of this study suggest that Au coating layer is effective barrier to diffuse oxide layer completely protect non-precious alloys from oxidation during the porcelain firing. The SEM photomicrographs of cross-section specimens showed a smooth interface between Au coating layer and metals and porcelain which suggested proper chemical bonding, and no gap, porosity were observed. The mode of failure was mainly adhesive for Ti tested specimens, but mixed failures with adhesive and cohesive were observed in Ni-Cr and Co-Cr specimens. The adhesion between non-precious metals and porcelain would not be improved by Au coating agent. However, It is suggested that the continuous study is required further investigation and development.

  • PDF

Jangdo(Small Ornamental Knives) manufacturing process and restoration research using Odong Inlay application (오동상감(烏銅象嵌)기법을 활용한 장도(粧刀)의 제작기술 및 복원연구)

  • Yun, Yong Hyun;Cho, Nam Chul;Jeong, Yeong Sang;Jang, Chu Nam
    • Korean Journal of Heritage: History & Science
    • /
    • v.49 no.2
    • /
    • pp.172-189
    • /
    • 2016
  • In this research, literature research on the Odong material, mixture ratio, casting method and casting facility was conducted on contemporary documents, such as Cheongong Geamul. Also, a long sword was produced using the Odong inlay technique. The sword reproduction steps were as follows; Odong alloying, silver soldering alloying, Odong plate and Silver plate production, hilt and sheath production, metal frame and decorative elements, such as a Dugup (metal frame), production, Odong inlay assembly and final assembly. For the Odong alloy production, the mixture ratio of the true Odong, which has copper and gold ratio of 20:1, was used. This is traditional ratio for high quality product according to $17^{th}$ century metallurgy instruction manual. The silver soldering alloy was produced with silver and brass(Cu 7 : Zn 3) ratio of 5:1 for inlay purpose and 5:2 ratio for simple welding purpose. The true Odong alloy laminated with silver plate was used to produce hilt and sheath. The alloy went through annealing and forging steps to make it into 0.6 mm thick plate and its backing layer, which is a silver plate, had the matching thickness. After the two plates were adhered, the laminated plate went through annealing, forging, engraving, silver inlaying, shaping, silver welding, finishing and polishing steps. During the Odong colouring process, its red surface turns black by induced corrosion and different hues can be achieved depending on its quality. To accomplish the silver inlay Odong techniques, a Hanji saturated with thirty day old urine is wrapped around a hilt and sheath material, then it is left at warm room temperature for two to three hours. The Odong's surface will turn black when silver inlay remains unchanged. Various scientific analysis were conducted to study composition of recreated Odong panel, silver soldering, silver plate and the colouring agent on Odong's surface. The recreated Odong had average out at Cu 95.57 wt% Au 4.16wt% and Cu 98.04 wt% Au 1.95wt%, when documented ratio in the old record is Cu 95wt% and Au 5wt%. The recreated Odong was prone to surface breakage during manufacturing process unlike material made with composition ratio written in the old record. On the silver plate of the silver and Odong laminate, 100wt% Ag was detected and between the two layers Cu, Ag and Au were detected. This proves that the adhesion between the two layers was successfully achieved. The silver soldering had varied composition of Ag depending on the location. This shows uneven composition of the silver welding. A large quantities of S, that was not initially present, was detected on the surface of the black Odong. This indicates that presence of S has influence on Odong colour. Additional study on the chromaticity, additional chemical compounds and its restoration are needed for the further understanding of the origin of Odong colour. The result of Odong alloy testing and recreation, Odong silver inlay long sword production, scientific analysis of the Odong black colouring agent will form an important foundation of knowledge for conservation of Odong artifact.