  • In this study, transparent conducting oxide indium zinc oxide (IZO) thin films were deposited by pulsed laser deposition (PLD) Process as a function of the deposition time on the glass substrates at $400^{\circ}C$. The crystal structures, electrical and optical properties of IZO films analyzed by XRD, AFM, and UV spectrometer. High quality IZO thin film with the resistivity of $9.1{\times}10^{-4}$ ohm cm and optical transmittance over 85% was obtained for sample when deposition time was 15min. Thin films with the preferred orientations along the c axis were observed as the deposition time increased.

  • PDF

펄스레이저 공정으로 제조한 Sb가 도핑된 SnO2 박막의 전기적 및 광학적 특성 (Electrical and Optical Properties of Sb-doped SnO2 Thin Films Fabricated by Pulsed Laser Deposition)

  • 장기선;이정우;김중원;유상임
    • 한국세라믹학회지
    • /
    • 제51권1호
    • /
    • pp.43-50
    • /
    • 2014
  • We fabricated undoped and Sb-doped $SnO_2$ thin films on glass substrates by a pulsed laser deposition (PLD) process. Undoped and 2 - 8 wt% $Sb_2O_3$-doped $SnO_2$ targets with a high density level of ~90% were prepared by the spark plasma sintering (SPS) process. Initially, the effects of the deposition temperature on undoped $SnO_2$ thin films were investigated in the region of $100-600^{\circ}C$. While the undoped $SnO_2$ film exhibited the lowest resistivity of $1.20{\times}10^{-2}{\Omega}{\cdot}cm$ at $200^{\circ}C$ due to the highest carrier concentration generated by the oxygen vacancies, 2 wt% Sb-doped $SnO_2$ film exhibited the lowest resistivity value of $5.43{\times}10^{-3}{\Omega}{\cdot}cm$, the highest average transmittance of 85.8%, and the highest figure of merit of 1202 ${\Omega}^{-1}{\cdot}cm^{-1}$ at $400^{\circ}C$ among all of the doped films. These results imply that 2 wt% $Sb_2O_3$ is an optimum doping content close to the solubility limit of $Sb^{5+}$ substitution for the $Sb^{4+}$ sites of $SnO_2$.

펄스 레이저 증착법에 의한 BST 박막 가변 Capacitors 제작 (Fabrication of High Tunable BST Thin Film Capacitors using Pulsed Laser Deposition)

  • 김성수;송상우;노지형;김지홍;고중혁;문병무
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.79-79
    • /
    • 2008
  • We report the growth of $Ba_{0.5}Sr_{0.5}TiO_3$(BST) thin films and their substrate-dependent electrical characteristics. BST thin films were deposited on alumina(non-single crystal), $Al_2O_3$(100) substrates by Nd:YAG Pulsed Laser Deposition(PLD) with a 355nm wavelength at substrate temperature of $700^{\circ}C$ and post-deposition annealing at $750^{\circ}C$ in flowing $O_2$ atmosphere for 1hours. BST materials had been chosen due to high dielectric permittivity and tunability for high frequency applications, To analyze the oxygen partial pressure effects, deposited films at 1, 10, 50, 100, 150, 200, 300 mTorr. The effects of oxygen pressure on structural properties of the deposited films have been investigated by X-ray diffraction(XRD) and atomic force microscope(AFM), respectively. Then we manufactured a inter-digital capacitor(IDC) patterns twenty fingers and $10{\mu}m$ gap, $700{\mu}m$ length and electrical properties were characterized. The results provide a basis for understanding the growth mechanisms and basic structural and electrical properties of BST thin films as required for tunable microwave devices applications such as varactors and tunable filters.

  • PDF

A12O3을 하지층으로 하는 Ba-ferrite 박막의 제조 및 자기적 특성에 관한 연구 (The Preparation and Magnetic Properties in Ba-ferrite Film on the A12O3 Substrate)

  • 서정철;박철진;최정완
    • 한국자기학회지
    • /
    • 제15권2호
    • /
    • pp.125-129
    • /
    • 2005
  • $A1_2O_3$ 기판을 하지층으로 하는 Ba-ferrite 박막을 pulsed laser deposition system으로 제조하여 결정학적 및 자기적 성질을 SEM, $M\ddot{o}ssbauer$ 분광법 및 VSM을 사용하여 연구하였다. Ba-ferrite박막은 $A1_2O_3$ 기판위에 PLD를 이용하여 기판온도 $400^{\circ}C$, 산소압력 0.1 Torr로 증착 하였고 증착 시간을 달리하여 두께 조절하였다. Ba-ferrite 박막은 5분 증착한 시료에서만 판상으로 결정이 형성되었음을 볼 수 있고 그보다 두꺼운 시료의 경우에는 침상모양과 판상모양이 임의의 방향으로 혼재되었음을 확인하였다. $M\ddot{o}ssbauer$ssbauer 분광법으로부터 측정된 Ba-ferrite결정 내 Fe 원자의 스핀 방향은 두께가 얇을수록 판상의 결정이 많이 존재하여 기판에 수직으로 정렬하려는 경향을 보이고 있다. VSM으로 측정한 자기이력곡선은 판상과 침상의 상이한 2가지 형태가 공존하는 것으로 나타났다.

PLD법으로 제작된 xPb(Al0.5Nb0.5)O3-(1-x)Pb(Zr0.52Ti0.48)O3박막의 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of xPb(Al0.5Nb0.5)O3-(1-x)Pb(Zr0.52Ti0.48)O3 Thin films Prepared by PLD)

  • 김민철;박용욱;최지원;강종윤;안병국;김현재;윤석진
    • 한국전기전자재료학회논문지
    • /
    • 제16권9호
    • /
    • pp.795-800
    • /
    • 2003
  • The dielectric and piezoelectric properties of the xPb(A $l_{0.5}$N $b_{0.5}$) $O_3$-(1-x)Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$ [xPAN-(1-x)PZT] thin films by pulsed laser deposition (PLD) were investigated as a function of PAN contents. The effect of texture on dielectric and piezoelectric properties of the 0.05PAN-0.95PZT thin films having the highest piezoelectric constant( $d_{33}$) was studied more precisely. For 0$\leq$x$\leq$0.15 compositions in xPAN-(1-x)PZT thin films, the well-developed perovskite phase with (111) preferred orientation was obtained at the deposition temperature of 50$0^{\circ}C$. With increasing PAN content, remanent polarization and coercive field decreased. The dielectric constant increased with an increase of PAN content until it reached 1450 at $\chi$= 0.05, and then decreased for higher PAN content. The maximum points of dielectric constant coincides with the maximum points of the piezoelectric constant $d_{33}$.33/.33/././.

Laser Ablation of a ZnO:P2O5 Target under the Presence of a Transverse Magnetic Field

  • Alauddin, Md.;Park, Jin-Jae;Gwak, Doc-Yong;Song, Jae-Kyu;Park, Seung-Min
    • Bulletin of the Korean Chemical Society
    • /
    • 제31권4호
    • /
    • pp.798-802
    • /
    • 2010
  • From time-resolved optical emission spectra, we have investigated the effects of a transverse magnetic field on the expansion of a plasma plume produced by laser ablation of a ZnO:$P_2O_5$ ceramic target in oxygen active atmosphere. The emission spectra of $Zn^{+*}$, $P^{+*}$, and $Zn^*$ neutrals in the presence of magnetic field turn out to be considerably different from those without magnetic field. The characteristics of the deposited films grown on amorphous fused silica substrates by pulsed laser deposition (PLD) are examined by analyzing their photoluminescence (PL), X-ray diffraction (XRD), and UV-visible spectra.

ZnO 박막 성장과 광학적 특성 분석을 위한 펄스 레이저증착(PLD)방법 적용 (Application of Pulsed Laser Deposition Method for ZnO Thin Film Growth and Optical Properties)

  • 홍광준;김재열
    • 한국공작기계학회논문집
    • /
    • 제14권2호
    • /
    • pp.33-41
    • /
    • 2005
  • ZnO epilayer was synthesized by the pulsed laser deposition(PLD) process on Al$_2$O$_3$ subsorte after irradiating the surface of ZnO sintered pellet by ArF(193nm) excimer laser. The epilayers of ZnO were achieved on sapphire(A1203) substrate at the 境mperature of 400$^{circ}$C. The crystalline structure of epilayer was investigated by the Photoluminescence and double crystal X-ray diffraction(DCXD). The carrier density and mobility of ZnO epilayer measure with Hall effect by van der Pauw mothod are $8.27\times$1016cm$^{-3}$ and 299 cm$^{2}$/V$\cdot$s at 293 K respectively, The temperature dependence of the energy band gap of the ZnO obtained from the absorption spectra was well described by the Varshni's relation, E$_g$(T)= 3.3973 eV - ($2.69\times$ 10$^{-4}$ eV/K)T$^{2}$/(T + 463K). After the as-grown ZnO epilayer was annealed in Zn atmospheres, oxygen and vaccum the origin of point defects of ZnO atmospheres has been investigated by the photoluminescence(PL) at 10K. The native defects of V$_{Zn}$, V$_{O}$, Zn$_{int}$, and O$_{int}$ obtained by PL measurements were classified as a donor or acceptor type. In addition we concluded that the heat-treatment in the oxygen atmosphere converted ZnO thin films to an optical p-type. Also, we confirmed that vacuum in ZnO/Al$_2$O$_3$ did not firm the native defects because vacuum in ZnO thin films existed in the form of stable bonds.

Tunable Magnetism by Magnetic Phase in $Fe_3O_4$/ZnO Multilayer

  • 윤종구;박창엽;윤순길
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 추계학술발표대회
    • /
    • pp.21.2-21.2
    • /
    • 2011
  • $Fe_3O_4$ having half metallic property is one of the efficient spin filtering materials which are widely used in spintronic research field and ZnO is wide band gap semiconductor which can be used by tunnel barrier or semiconductor channel in spin MOSFET. We investigated the magnetic and the electric properties of $Fe_3O_4$/ZnO multilayer fabricated on c-$Al_2O_3$ substrate by pulsed laser deposition (PLD). For multilayer films, PLD was performed at variable temperatures such as $200{\sim}750^{\circ}C$ and at target distance from 40 to 80 mm, KrF eximer laser of 1.5 $J/cm^2$ and a reputation rate of 2Hz. $Fe_3O_4$/ZnO multilayers were deposited at $4{\times}10^{-6}$ Torr. After fabricating $Fe_3O_4$/ZnO multilayers, $Fe_3O_4$/ZnO multilayers were treated by RTA(Rapid Thermal Annealing) at various temperature to change magnetic phase. The magnetism of the multilayer is changed by thickness of the ZnO tunnel barrier. Magnetic phase of FexOy showed a very small magnetism due to $Fe_2O_3$ ${\alpha}$-phase, but large magnetism from $Fe_3O_4$ or $Fe_2O_3$ ${\gamma}$-phase was observed. In the present study, effect of the ZnO thickness on the MR (magnetoresistance) ratio was investigated in detail.

  • PDF

Effect of Substrate Temperature and Post-Annealing on Structural and Electrical Properties of ZnO Thin Films for Gas Sensor Applications

  • 도강민;김지홍;노지형;이경주;문성준;김재원;박재호;조슬기;신주홍;여인형;문병무;구상모
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.105-105
    • /
    • 2011
  • ZnO is a promising material since it could be applied to many fields such as solar cells, laser diodes, thin films transistors and gas sensors. ZnO has a wide and direct band gap for about 3.37 eV at room temperature and a high exciton binding energy of 60 meV. In particular, ZnO features high sensitivity to toxic and combustible gas such as CO, NOX, so on. The development of gas sensors to monitor the toxic and combustible gases is imperative due to the concerns for enviromental pollution and the safety requirements for the industry. In this study, we investigated the effect of substrate temperature and post-annealing on structural and electrical properties of ZnO thin films. ZnO thin films were deposited by pulsed laser deposition (PLD) at various temperatures at from room temperature to $600^{\circ}C$. After that, post-annealing were performed at $600^{\circ}C$. To inspect the structural properties of the deposited ZnO thin films, X-ray diffraction (XRD) was carried out. For gas sensors, the morphology of the films is dominant factor since it is deeply related with the film surface area. Therefore, the atomic force microscopy (AFM) and field emission scanning electron microscopy (FE-SEM) were used to observe the surface of the ZnO thin films. Furthermore, we analyzed the electrical properties by using a Hall measurement system.

  • PDF

펄스레이저 증착법을 이용한 대면적 BSTO 박막의 성장 (Growth of Large Area BSTO Thin Films using Pulsed Laser Deposition)

  • 강대원;곽민환;강승범;백문철;최상국;김성일;류한철;김지선;정세영;정동철;강광용;이병영
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.249-249
    • /
    • 2009
  • We have grown large area BSTO($(Ba_{1-x}Sr_x)TiO_3$) thin films (x=0.4) on 2 inch diameter MgO (001) single crystal substrates using a pulse laser deposition(PLD) system. Substrate temperature and oxygen pressure in the deposition chamber, and the laser optics for ablating a target have been controlled to obtain the uniform thickness and preferred orientation of the films. Results of x-ray diffraction and rocking curve analysis revealed that the BSTO films were grown on MgO substrates with a preferred orientation (002), and the full width half maximum of the rocking curve was measured to be 0.86 degree at optimum condition. Roughness of the films have been measured to be $3.42{\AA}$ rms by using atomic force microscopy. We have successfully deposited the large area BSTO thin films of $4000{\AA}$ thickness on 50 mm diameter MgO substrates.