• 제목/요약/키워드: Poor machinability

검색결과 37건 처리시간 0.022초

고경도 금형강의 CBN 볼 엔드밀 가공에서 가공성 평가 (Machinability Evaluation of CBN Ball End Milling in Die & Mold Steels with High Hardness)

  • 김홍규;심재형;이종찬
    • 한국공작기계학회논문집
    • /
    • 제16권4호
    • /
    • pp.119-126
    • /
    • 2007
  • Generally, the machinability of materials that have a good mechanical properties is poor. The material having a high strength, high toughness in high temperature and wear resistance, it is difficult to remove a chip from workpiece. STD11 and NAK80 are kinds of these materials and these materials can be used in many industrial fields. But it is limited in use because of high cost and poor machinability. In this experimental study, the cutting of STD11 and NAK80 were used to decide the machinability and the tool shape of CBN ball end mill. From the results, the CBN ball end mill is verified that the estimated cutting edge shape of rake angle 30 degree has consistent effect on the tool wear and cutting force.

STS304의 태핑과 탭 형상에 관한 연구 (A Study on Tapping for STS304 and Tap Geometry)

  • 이정길;최만성
    • 한국정밀공학회지
    • /
    • 제17권11호
    • /
    • pp.55-62
    • /
    • 2000
  • The poor machinability material such as austenite stainless steel(STS304) is emphasized on the wide use of HSSE for the tapping operation. The difficulty can be entirely to tapping torque due to chip formation through the hole of tap. The object of this study is to investigate tap geometry affecting the tapping torque from a practical point of view. The study shows that the optima tapping torque is affected by the tap geometry and cutting condition for STS304.

  • PDF

저순도 알루미나 예비소결체 선삭시의 공구 마멸 (Tool Wear in Turning of the Presintered Low Purity Alumina)

  • 이재우
    • 한국정밀공학회지
    • /
    • 제22권1호
    • /
    • pp.39-46
    • /
    • 2005
  • In this study, unsintered, presintered and full-sintered low purity alumina ceramics were machined with various tools to clarify the machinability and the optimum cutting conditions. The main conclusions obtained were as follows. (1) Machined with alloy steel tool, the machinability of the presintered ceramics becomes better with the decrease of presintering temperature, but that of unsintered ceramics(white body) was extremely poor. (2) In the case of carbide, K01, the tool life in machining the white body was the longest, and the machinability of presintered ceramics becomes poorer with the increase of the presintering temperature. (3) The K01 tools exhibit longer life than the P10 tools in machining both the white body and the ceramics presintered at $1450^\circC$ or higher temperatures, but the P10 tools shows longer tool life than the K10 tools in machining of the ceramics presintered at temperatures below $1450^\circC$.

PRODUCTION AND MACHINABILITY OF SiCp-REINFORCED AL-2014 ALLOY MATRIX COMPOSITES

  • Ciftci, I.;Sahin, Y.
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.313-314
    • /
    • 2002
  • SiCp-reinforced metal matrix composites (MMCs) containing 8 wt % and 16 wt % of $SiC_p-reinforced$ with 30 and $45\;{\mu}m$ in sizes were prepared by a melt stirring-squeeze casting technique. Microstructural observation showed that particle distributions were reasonably well. Turning experiments were carried out on the composites using uncoated and triple-layer coated carbide tools at various cutting speeds under a constant feed rate and depth of cut. Coated tools indicated better performance than uncoated tools for all the materials while the poor surface finish was obtained for coated tools.

  • PDF

저순도 알루미나 세라믹 가소결재의 피삭성

  • 이재우
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1995년도 춘계학술대회 논문집
    • /
    • pp.33-38
    • /
    • 1995
  • In this study, unsistered, pre-sintered and sintered low purity alumina ceramics were machined with various tools to clarify the machniability, the optimum tool materials and the optimum tool materials and the optimum cutting conditions. The maon conclusions obtained were as follows. (1) Machined withalloy steel tool, the machinabilty of te pre-sintered ceramics becomes better with the decrease of pre-sintering temperature, but that of unsintered ceramics(white body) was extremely poor. (2) In the case of carbide tool K01, the tool life in machining white body was the longest, and the machinabilty of pre-sintered ceramics becomes poorer with the increase of the pre-sintering temperature. (3) In the case of ceramic tool, the 10000-1100 .deg. C pre-sintered ceramics showed te best machinability within a certain cutting speed range. So far as dry machining, the above combination and conditions showed the highest productivity. (4) When the pre-sintered ceramics were wet machined withsintered diamond tool, the tool life becomes extremelylong, and higher cutting speed can be can be used than in the case offull-sintered ceramics. The productivity of wet cutting is much higher than that ofdry cutting.

  • PDF

Inconel 718의 평엔드밀링가공에서 가공성평가에 관한 연구 (A Study on Machinability Evaluation of Inconel 718 in Flat End Milling)

  • 정지훈;권해웅;구준영;김평호;김정석
    • 한국생산제조학회지
    • /
    • 제21권6호
    • /
    • pp.982-987
    • /
    • 2012
  • Inconel 718 alloy has been widely used in the aerospace, heavy industry and electronic industry. However, the machinability of this alloy is very poor, which is attributed to their inherent high strength that is maintained at elevated temperatures. The tool life is dominant problem in machining difficult-to-cut materials, so it is necessary to select the efficient cutting conditions for the improvement of tool life. In this study, the cutting force, tool wear and surface roughness are investigated in end milling machining under various cutting conditions. By this experiment, the efficient machining condition of this alloy is suggested to adopt in various industries.

매트릭스(matrix)형 냉간금형강의 기계적 특성에 미치는 NbC 탄화물 첨가의 영향 (Effect of NbC Carbide Addition on Mechanical Properties of Matrix-Type Cold-Work Tool Steel)

  • 강전연;김호영;손동민;이재진;윤효윤;이태호;박성준;박순근
    • 열처리공학회지
    • /
    • 제28권5호
    • /
    • pp.239-249
    • /
    • 2015
  • Various amount of NbC carbide was intentionally formed in a matrix-type cold-work tool steel by controlled amount of Nb and C addition. And the effect of NbC addition on the mechanical properties was investigated. Four alloys with different Nb and C contents were cast by vacuum induction melting, then hot forging and spheroidizing annealing were conducted. The machinability of the annealed specimens was examined with 3 different cutting tools. And tensile tests at room temperature were conducted. After quenching and tempering, hardness and impact toughness were measured, while wear resistance was evaluated by disk-on-plate type wear test. The increasing amount of NbC addition resulted in degraded machinability with increased strength, whereas the absence of NbC also led to poor machinability due to high toughness. After quenching and tempering, the additional NbC improved wear resistance with increasing hardness, whereas it deteriorated impact toughness. Therefore, it could be found that a moderate addition of NbC was desirable for the balanced combination of mechanical properties.

Fe-23Cr-2.5C-1.2Si-1.08Mn-0.48Mo-0.3V-xNi 주철의 내식성 및 피삭성에 미치는 Ni의 영향 (Effect of Nickel Content on Corrosion Resistance and Machinability of Fe-23Cr-2.5C-1.2Si-1.08Mn-0.48Mo-0.3V-xNi Cast Iron)

  • 김기빈;정성식;백민숙;윤동주
    • 한국산학기술학회논문지
    • /
    • 제21권3호
    • /
    • pp.576-584
    • /
    • 2020
  • 압출기 스크류 소재는 주로 냉간 금형 공구강(SKD11)이 사용되고 있는데, 최근 합성 수지의 발달로 화학적 부식 및 마모 발생이 증가하고 있다. 이를 개선하기 위해 내마모성과 내식성이 우수한 고크롬 주철의 사용이 요구되지만, 난가공성으로 사용이 기피되고 있다. 본 연구에서는 고크롬 합금의 난가공성을 개선하기 위해 Fe-23Cr-2.5C-1.2Si-1.08Mn-0.48Mo-0.3V 조성의 고크롬 주철에 가공성이 우수한 니켈을 0, 0.5, 1.0, 1.5 % 첨가하여 주조하고 열처리를 진행한 후, 선삭 시험과 동전위 분극 시험을 통해 니켈이 피삭성 및 내식성에 미치는 영향을 분석하여 SKD11과 비교하였다. 고크롬 주철은 고주파 진공유도용해로를 사용하여 주조하고, 이후 750 ℃에서 5시간 동안 풀림 처리와 풀림 처리 후 1100 ℃에서 5시간동안 재열처리를 실시하였다. 750 ℃ 풀림 처리 후 선삭 시험을 실시한 결과 니켈의 함량이 1.0% 이상에서 피삭성은 현저히 향상되었다. 5% NaCl 용액에서 동전위 분극 시험 결과 주방상태와 750 ℃ 풀림 처리에서는 니켈의 함량이 증가할수록 내식성은 저하되었으나, 1100 ℃ 재열처리 후에는 1.5% 니켈에서 가장 우수한 내식성을 나타냈다.

단결정 실리콘의 초정밀가공 (Nano-turning of single crystal silicon)

  • 김건희;도철진;홍권희;유병주;원종호;박상진;안병민
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 추계학술대회 논문집
    • /
    • pp.939-942
    • /
    • 2000
  • Single point diamond turning technique for optical crystals is reported in this paper. The main factors influencing the machined surface quality are discovered and regularities of machining process are drawn. Optical crystals have found more and more important applications in the field of modern optics. Optical crystals are mostly brittle materials of poor machinability. The traditional machining method is polishing which has many shortcomings such as low production efficiency, poor ability to be automatically controlled and edge effect of the workpiece. The purpose of our research is to find the optimum machining conditions for ductile cutting of optical crystals and apply the SPDT technique to the manufacturing of ultra precision optical components of brittle material.

  • PDF

광학소자의 초정밀절삭 특성에 관한 연구 (The Characteristics of Ultra Precision Machining of Optical Crystal)

  • 김주환;박원규;김건희;원종호
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2003년도 춘계학술대회 논문집
    • /
    • pp.529-532
    • /
    • 2003
  • Machining technique for optical crystals with single point diamond turning tool is reported in this paper. The main factors influencing the machined surface quality are discovered and regularities of machining process are drawn. Optical crystals have found more and more important applications in the field of modern optics. Optical crystals are mostly brittle materials of poor machinability. The traditional machining method is polishing which has many shortcomings such as low production efficiency. poor ability to be automatically controlled and edge effect of the workpiece. The purpose of our research is to find the optimum machining conditions for ductile cutting of optical crystals and apply the SPDT technique to the manufacturing of ultra precision optical components of brittle materials. As a result. the surface roughness is good when spindle speed is 200m/min. and teed rate is small. The influence of depth of cut is very small.

  • PDF