Sulfonated poly(ether sulfone)을 함유한 고분자 전해질 연료전지용 기체 확산 전극에 관한 연구 (Gas diffusion electrode containing sulfonated poly(ether sulfone) as ionomer for polymer electrolyte fuel cells)

  • 류성관;최영우;양태현;임성대;김한성;김창수
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2010년도 추계학술대회 초록집
    • /
    • pp.75.2-75.2
    • /
    • 2010
  • Polymer electrolyte fuel cells (PEFCs) have received a lot of attention as a power source for both stationary and mobile applications due to their attractive feature. In general, the performance of PEFCs is highly affected by the property of the electrodes. A PEFC electrode essentially consists of a gas diffusion layer and a catalyst layer. The gas difusion layer is highly porous and hydrophobicized with PTFE polymer. The catalyst layer usually contains electrocatalyst, proton conducting polymer, even PTFE as additive. Particularly, the proton conducting ionomer helps to increase the catalytic activity at three-phase boundary and catalyst utilization. Futhermore, it helps to retain moisture, resulting in preventing the electrodes from membrane dehydration. The most widely used proton conducting ionomer is perfluorinated sulfonic acid polymer, namely, Nafion from DuPont due to its high proton conductivity and good mechanical property. However, there are great demands for alternative ionomers based on non-fluorinated materials in terms of high temperature availability, environmental adaptability and production cost. In this study, the electrodes with the various content of the sulfonated poly(ether sulfone) ionomer in the catalyst layer were prepared. In addition, we evaluated electrochemical properties of the prepared electrodes containing the various amount of the ionomers by using the cyclic voltammetry and impedance spectroscopy to find an optimal ionomer composition in the catalyst layer.

  • PDF

동결/해동 조건에서 기체확산층의 물성이 고분자전해질연료전지의 내구성에 미치는 영향 (Effect of the gas diffusion layer on freeze/thaw durability in polymer electrolyte fuel cells)

  • 박구곤;임수진;박진수;손영준;임성대;김창수;양태현
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2009년도 춘계학술대회 논문집
    • /
    • pp.640-643
    • /
    • 2009
  • The effect of the kind of gas diffusion layers (GDLs) on the freeze/thaw condition durability in polymer electrolyte fuel cells (PEFCs) were investigated. For this purpose, three kinds of GDLs, i.e., felt, paper and cloth types with different basic properties have been first prepared, then the changes in the properties and performance of cells was observed during the freeze/thaw cycles ranging from -30 to 70 $^{\circ}C$. The single cells consisting of different GDLs were evaluated for performance. The performance degradation and the cell resistance increase could be directly correlated. The physical destruction of electrode was shown by SEM analysis. It was presented that mechanical supporting force of interface between materials can help enhancing the durability of PEFCs in the freeze/thaw condition.

  • PDF

1 kW 급 가정용 연료전지 코제너레이션 시스템이 설치된 주택 내 플러그인 하이브리드 자동차의 스마트 충전전략 연구 (A Study on the Strategy of Smart Charging System to Charge the PHEV in the House Which has a 1 kW Fuel Cell Cogeneration System)

  • 노철우;김민수
    • 대한설비공학회:학술대회논문집
    • /
    • 대한설비공학회 2008년도 하계학술발표대회 논문집
    • /
    • pp.838-843
    • /
    • 2008
  • Cause of struggling to escape from dependency of fossil fuels, the fuel cell and the Plug-in Hybrid Electric Vehicle (PHEV) draw attention in the all of the world. Especially, the Polymer Electrolyte Membrane Fuel Cell (PEMFC) systems have been anticipated for next generation's energy supplying system, and we can predict the PHEV will enlarge the market share in the next few years to reduce not only the air pollution in the metropolis but the fuel-expenses of commuters. This paper presents simulation results about the strategy of smart charging system for PHEV in the residential house which has 1 kW PEMFC cogeneration system. The smart charging system has a function of recommending the best time to charge the battery of PHEV by the lowest energy cost. The simulated energy cost for charging the battery based on the electricity demand data pattern in the house. The house which floor area is $132\;m^2$ (40 pyeong.). In these conditions, the annual gasoline, electricity, and total energy cost to fuel the PHEV versus Conventional Vehicle (CV) have been simulated in terms of cars' average life span in Korea.

  • PDF

동결/해동 조건에서 기체확산층이 고분자전해질연료전지의 내구성에 미치는 영향에 관한 연구 (Investigation of Gas Diffusion Layer Effects on the Freeze/Thaw Condition Durability in PEFCs)

  • 임수진;박구곤;박진수;손영준;임성대;양태현;김창수
    • 한국수소및신에너지학회논문집
    • /
    • 제20권4호
    • /
    • pp.309-316
    • /
    • 2009
  • The effect of gas diffusion layers (GDLs) on the freeze/thaw condition durability in polymer electrolyte fuel cells (PEFCs) were investigated. For this purpose, three kinds of GDLs, such as, felt, paper and cloth types with different basic properties have been first prepared, then the changes in the properties and performance of cells was observed during the freeze/thaw cycles ranging from -30 to $70^{\circ}C$. The performance evaluations were conducted by using the single cells consisting of different GDLs. The performance degradation and the cell resistance increase could be directly correlated. The physical destruction of electrode was shown by SEM analysis. The mechanically supporting ability on the interface between the cell components can help enhancing the durability of PEFCs in the freeze/thaw condition.

고온 PEFC용 수소이온 전도 향상을 위한 가교된 이온성 액체를 갖는 세공충진막 (Pore-filling membrane with ionic liquids immobilized by cross-linking for high temperature PEFCs)

  • 백지숙;최영우;이미순;양태현;김창수
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2010년도 추계학술대회 초록집
    • /
    • pp.80.2-80.2
    • /
    • 2010
  • The development of high temperature-proton exchange fuel cell (HT-PEFC) is a key in solving the problem of carbon monoxide poisoning of the platinum at anode as well as water management in PEFCs operated below $90^{\circ}C$. In order to overcome these main issues, PEFCs must be operated at high temperature above $120^{\circ}C$. Ionic liquids are available for HT-PEFC due to exhibiting non-volatility and thermal stability. Ionic liquids are however leached out from polymeric matrix resulting in the increase of gas permeability. In this study, we have prepared and characterized the composite membranes with the ionic liquids consisting of 1-(4-vinylbenzyl)-3-butyl imidazolium chloride immobilized by the cross-linkers in pore-filling membrane to prevent to be leached out from the membrane. We confirmed that cross-linked ionic liquids were not leached out from the composite membranes through the various characteristic analyses. It was also verified that the prepared membranes are thermally stable from the result of TG analysis. The pore-filling membranes with the immobilized ionic liquids have a high proton conductivity over $10^{-2}$ S/cm at high temperature (> $120^{\circ}C$).

  • PDF

공기호흡형 고분자연료전지의 운전특성에 대한 연구 (The Operating Characteristics of Air-Breathing Type PEFCs)

  • 손영준;임성대;박구곤;김경연;김민진;이원용
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2008년도 추계학술대회 논문집
    • /
    • pp.44-46
    • /
    • 2008
  • Air-breathing polymer electrolyte membrane fuel cells (PEMFC) are highly promising particularly for small-power applications up to tens watts class. A distinctive feature of the air-breathing PEMFC is its simple system configuration in which axial fans operate for dual purposes, supplying both oxidant and coolant in a single manner. In the present study, a nominal 80W air-breathing PEMFC system is developed and investigated to determine the optimal operating strategy through parametric studies (i.e., reactant humidity, and fanblowing flow rate). The cell voltage distributions are examined as a function of time to evaluate the system performance under various operating conditions.

  • PDF

고분자 연료전지용 MEA 연속 코팅공정 개발 (Continuous Coating Process Development for PEFC Membrane Electrode Assembly)

  • 박석희;윤영기;김창수;이원용
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2006년도 춘계학술대회
    • /
    • pp.110-112
    • /
    • 2006
  • Membrane electrode assembly (MEA) for polymer electrolyte fuel cell (PEFC) are commonly prepared in the research laboratory by spraying, screen-printing and brushing catalyst slurry onto membrane or other support material like carbon paper or polyimide film in a batch style. These hand applications of the catalyst slurry are painstaking process with respect to precision of catalyst loading and reproducibility. It has been generally mentioned that the adoption of continuous process is very helpful to develop the reliable product. In the present work, we report the results of using continuous type coater with doctor-blade to coat catalyst slurry for preparing the MEA catalyst layers In a faster and highly reproducible fashion. We show that while expectedly faster than batch style, the machine coater requires the use of slurry of appropriate composition and a properly selected transfer decal material in order to achieve superior MEA plat lnw loading reproducibility. To make highly viscous catalyst slurry that is imperative for using coater, we use 40wt.% Nafion solution and minimize the content of organic solvent. And the choice of proper high surface area catalyst is important in the viewpoint of making well-dispersed slurry. After catalyst coating onto the support material, we transferred the catalyst layer to both sides of Nafion membrane by hot-pressing In this case, the degree of transfer was Influenced by hot-pressing condition including temperature, pressure, and time. To compare the transferring ability, we compared so many films and detaching papers. And among the support, polyethylene terephthalate(PET) film shows the prominent result.

  • PDF

체결압이 고분자연료전지 기체확산층의 표면성질에 미치는 영향 (Effect of Clamping Pressure on Surface Properties of Gas Diffusion Layer in PEFCs)

  • 안은진;박구곤;윤영기;박진수;이원용;김창수
    • 전기화학회지
    • /
    • 제10권4호
    • /
    • pp.306-310
    • /
    • 2007
  • 고분자연료전지에 사용되는 다공성 매체인 기체확산층은 그 특성에 따라 원활한 기체의 확산과 물 배출을 결정지으며 그 결과 연료전지 성능과 내구성에까지 영향을 미친다. 최적의 물관리와 기체확산층 내에서의 이상(two phase) 유동이해를 위해서는 실제 체결 조건에서의 기체확산층의 성질을 아는 것이 중요하다. 이에 대해 물리적, 전기화학적, 기계적 성질을 알기 위한 실험 등이 수행되어져 왔다. 하지만 실제 스택의 체결 조건에서 기체확산층의 표면 화학적 변화에 대한 실험은 그다지 알려져 있지 않다. 본 연구에서는 단순한 체결 과정만으로도 기체확산층에 대한 물리화학적인 변화를 야기할 수 있음을 확인하였으며, 기체확산층을 구성하는 탄소 섬유 및 PTFE의 손상과 변형을 전자주사현미경으로 직접 관찰할 수 있었다. 관찰된 물리적 손상이 표면의 소수성 변화에 미치는 영향을 알아보기 위해 표면 원소성분 분석과 농도가 다른 에탄올 수용액 흡수량 측정을 수행하였다. 그 결과 체결압에 의해서 분리판의 rib 전단 및 아래에서 심한 파손이 일어나며, 탄소 섬유의 끊어짐 및 섬유 사이에 존재하는 탄소 파우더 역시 심하게 눌린 현상을 관찰할 수 있었다. 체결과정을 경험한 기체확산층에 대한 liquid uptake양을 확인한 결과, 표면 PTFE 함량의 상대적 감소가 기체확산층의 표면을 소수성에서 친수성으로 변화시켰음을 직접적으로 확인하였다.